Filtern
Erscheinungsjahr
Dokumenttyp
- Beitrag zu einem Tagungsband (63)
- Vortrag (50)
- Zeitschriftenartikel (47)
- Posterpräsentation (9)
- Beitrag zu einem Sammelband (8)
- Buchkapitel (2)
- Dissertation (1)
Schlagworte
- Ageing (26)
- Seal (25)
- Compression set (23)
- Elastomer (19)
- Rubber (16)
- Degradation (11)
- Low temperature (11)
- Metal seal (11)
- Aging (10)
- Dichtung (8)
Organisationseinheit der BAM
- 3 Gefahrgutumschließungen; Energiespeicher (48)
- 3.4 Sicherheit von Lagerbehältern (48)
- 9 Komponentensicherheit (2)
- 5 Werkstofftechnik (1)
- 5.2 Metallische Hochtemperaturwerkstoffe (1)
- 7 Bauwerkssicherheit (1)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (1)
- 9.5 Tribologie und Verschleißschutz (1)
- 9.6 Additive Fertigung metallischer Komponenten (1)
Paper des Monats
- ja (1)
Eingeladener Vortrag
- nein (50)
Eine Aufgabe des Fachbereichs 3.4 Sicherheit von Lagerbehältern der Bundesanstalt für Materialforschung und -prüfung (BAM) ist es, die Sicherheit von Behältern zur Lagerung von radioaktivem Abfall mit vernachlässigbarer Wärmeentwicklung zu bewerten. Da solche Behälter vor der Entsorgung transportiert und gelagert werden, ist während dieser Zeit ein sicherer Einschluss des radioaktiven Inhalts von größter Bedeutung. Zur Abdichtung dieser Behälter sind Elastomer-O-Ringe weit verbreitet. Um für solche, wie auch für viele andere Anwendungen, eine Voraussage über die Lebensdauer dieser Komponenten treffen zu können, ist es unerlässlich zu verstehen, welchen Einfluss der durch Alterung hervorgerufene Abbau auf Dauer auf die Elastomerdichtungen hat. In einem Langzeittest wurden drei Kautschukarten (EPDM und FKM, die für die Anwendung relevant sind, und HNBR als Vergleich) über mehrere Jahre untersucht. Dabei wurden die Veränderungen der mechanischen Eigenschaften (z. B. Härte und Bruchdehnung) bei vier verschiedenen Alterungstemperaturen (75 °C, 100 °C, 125 °C und 150 °C) sowie das Dichtungsverhalten betrachtet. Um den Einfluss von Vernetzung und Kettenspaltung auf die beobachteten Alterungseffekte zu bestimmen, wurden Messungen zur kontinuierlichen und intermittierenden Druckspannungsrelaxation durchgeführt. Dadurch konnten Erkenntnisse über Kinetik und Mechanismus der Abbaureaktionen
gewonnen werden. Zur Einschätzung des Dichtungsverhaltens wurden Durckverformungsrest und Leckagerate gemessen. Die Ergebnisse zeigen, dass die O-Ringe unter statischen Bedingungen auch dann dicht halten, wenn die Werte für Druckverformungsrest, Druckspannungsrelaxation und mechanische Eigenschaften schon auf einen fortgeschrittenen Alterungsabbau hindeuten. Aus diesem Grund wurde ein modifizierter Dichtigkeitsversuch mit einer geringen und schnellen teilweisen Entlastung der Dichtung entwickelt, mit dessen Hilfe sich ein Lebensdauerkriterium bestimmen lässt, das eine Sicherheitsspanne für thermische Schrumpfung und Vibrationen beinhaltet.
Elastomere werden vielfach als Dichtungsmaterial für verschiedene Anwendungen eingesetzt.
In vielen Bereichen ist die Funktion der Dichtung auch bei tiefen Temperaturen erforderlich. Daher ist das Verständnis des Versagensmechanismus von großer Bedeutung.
Normalerweise werden Elastomere oberhalb ihres Glass-Gummi Umwandlungsbereiches eingesetzt, wobei die minimale Einsatztemperatur nicht exakt definiert ist. Daher ist es sinnvoll, diese untere Temperatureinsatzgrenze in Abhängigkeit von den Materialeigenschaften zu bestimmen. Hierfür werden die Ergebnisse der thermischen Analyse mit den Resultaten des Druckverformungsrests aus einer abgewandelten Messung mit der Dynamisch Mechanischen Analyse (DMA) kombiniert.
Weiterhin werden Ergebnisse von Bauteilversuchen vorgestellt und diskutiert.
Die vorgestellten Untersuchungen wurden zum großen Teil auf Untersuchungen im Rahmen der Dissertation von M. Jaunich durchgeführt.
Rubber is widely used as sealing material in various applications. In many fields the function of seal materials at low temperatures is necessary. Therefore, the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance.
It is known that the material properties of rubbers are strongly temperature dependent. At low temperatures this is caused by the rubber-glass transition (abbr. glass transition). During continuous cooling, due to the glass transition the material changes from rubber-like entropy-elastic behaviour to stiff energy-elastic behaviour, that allows nearly no strain or retraction. Hence, rubbers are normally used above their glass transition. But as the minimum working temperature limit of elastomers cannot be defined globally and precisely, the lower operation temperature limit of rubber seals should be determined in dependence of the application conditions and the most relevant material properties.
In this paper, wesummarize results of our temperature dependent investigation of seal material properties by classical thermal analysis as Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA), combined with measurements of standardized tests as compression set and the seal performance determined in component tests. To reduce the test time of compression set tests a faster technique was developed and applied.
To study the influence of dynamic events on the seal performance and to enhance the understanding of occurring seal failure, a setup for a fast partial seal release was designed.
Ein wesentliches sicherheitstechnisches Kriterium für Transport und Lagerbehälter ist das Langzeitverhalten von verschraubten Deckel-Dichtsystemen unter Verwendung von Metall- und Elastomerdichtungen sowie von im Behälterkörper integrierten Polyethylenen zur Neutronen¬abschirmung.
Die ordnungsgemäße Funktion der Metalldichtungen ist Voraussetzung für die Einhaltung der geforderten Dichtheit des Deckelsystems, während die Elastomerdichtungen für die Messung der Leckagerate an den Metalldichtungen benötigt werden. Darüber hinaus kommen Elastomer-dichtungen als Primärdichtungen in Behältern für radioaktive Abfälle mit vernachlässigbarer Wärmeentwicklung zum Einsatz.
Zur Bewertung des Dichtungsverhaltens sind die alterungsabhängige verbleibende Rückstellkraft für die Metall- und Elastomerdichtungen sowie die sog. nutzbare Rückfederung bei Metalldichtungen von entscheidender Bedeutung. Für Elastomerdichtungen ist zusätzlich eine radiologisch bedingte Materialdegradation zu bewerten.
In Bezug auf das Alterungsverhalten von Polyethylen zur Neutronenabschirmung sind neben zeit- und temperaturabhängigen Materialveränderungen insbesondere auch durch Gammastrahlung induzierte Degradationseffekte wie Wasserstoffabspaltung, Vernetzung und Abbau der Polymer¬moleküle zu berücksichtigen. Über die eigentliche Bewertung der Abschirmeigenschaften hinaus sind somit zusätzlich Auswirkungen von Degradationsprodukten auf andere Behälterkomponenten zu diskutieren.
Die an der BAM im Fachbereich 3.4 Sicherheit von Lagerbahältern durchgeführten und aktuell laufenden Untersuchungen werden vorgestellt und diskutiert.
Ziel unserer Arbeit ist es, den sicheren Einschluss von gefährlichen Gütern in entsprechenden Verpackungen (z.B. Behälter für radioaktive Stoffe) unter verschiedenen Umgebungsbedingungen und über lange Zeiten sicher zu stellen bzw. die Materialauswahl entsprechend zu steuern. Aufgrund ihrer einfachen und zuverlässigen Anwendung werden Elastomere für viele Dichtungsaufgaben eingesetzt. In vielen Anwendungsbereichen wie z.B. Verkehr, Luftfahrt und Verfahrenstechnik können während des Einsatzes tiefe Temperaturen auftreten, bei denen die Funktionsfähigkeit der Dichtung erhalten bleiben muss. Daher ist die Untersuchung des Verhaltens von Elastomerdichtungen bei tiefen Temperaturen wichtig, um ihren Temperatureinsatzbereich nach unten abzugrenzen und dadurch einen verlässlichen Betrieb zu sichern. Dazu wurden umfangreiche Untersuchungen durchgeführt, auf deren Ergebnisse hier kurz eingegangen werden soll.
Bei allen Anwendungen ist die Frage nach der Lebenszeit einer Dichtung entscheidend für z.B. Austauschintervalle oder Wartung. Besondere Bedeutung hat die Lebensdauer allerdings bei Anwendungen, in denen ein Austausch der Dichtung nicht möglich ist. Hier kann die Dichtung über die Lebensdauer des Gesamtsystems entscheiden. Daher ist eine verlässliche Abschätzung der Lebensdauer für diese Anwendungen relevant. Dazu ist eine umfangreiche Datenbasis erforderlich. Entsprechende Arbeiten, die gerade begonnenen worden sind, sollen ergänzend vorgestellt werden. Erste konkrete Ergebnisse werden im Vortrag vorgestellt.
Recovery is an important measure for seal applications representing to which extent the elastomer regains its initial shape after deformation and release of an applied force. Compression set (CS) indicates the degree of recovery. Ethylene propylene diene rubber (EPDM) was aged at 75 ◦C, 100 ◦C, 125 ◦C and 150 ◦C for different ageing times up to five years and compression set measurements were performed at different times after disassembly and after additional tempering. Short- and long-term recovery up to one year after release for samples aged at 125 ◦C and 150 ◦C was also studied. To assess the curvature in the Arrhenius diagram that may occur due to non-sufficiently aged specimens, a degradation-rate based model was fitted to the CS data after tempering. For each ageing temperature, two decay fit functions were proposed, each with an activation energy and a corresponding degradative process. The influence of ageing on the leak-tightness after fast small partial release is investigated and estimated through the analysis of the shift factors from time temperature superposition (TTS) of CS measurements at different times after disassembly. Shift factors of CS measurement after 1 s and after additional tempering are in good agreement.
Rubbers are widely used as main sealing materials for containers for low and intermediate level radioactive waste and as additional component to metal seals in spent fuel and high active waste containers. The save encapsulation of the radioactive container inventory has to be guaranteed according to legislation and appropriate guidelines for long term storage periods as well as down to temperatures of -40 °C during transport.
Therefore the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance.
It is known that the material properties of rubbers are strongly temperature dependent. At low temperatures this is caused by the rubber-glass transition (abbr. glass transition). During continuous cooling the material changes from rubber-like entropy-elastic to stiff energy-elastic behaviour, that allows nearly no strain or retraction, due to the glass transition. Hence rubbers are normally used above their glass transition but the minimum working temperature limit is not defined precisely, what can cause problems during application. Therefore the lower operation temperature limit of rubber seals should be determined in dependence of the material properties.
The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with the results of standardized measurements as the compression set according to ISO 815. To reduce the test time of the standard tests a faster technique was developed.
Additionally, the breakdown temperature of the sealing function of complete O-ring seals is measured in a component test setup to compare it with the results of the other tests. The experimental setup is capable of measuring the leakage rate at low temperatures by the pressure rise method.
A fluorocarbon rubber (FKM) was selected for this investigation as it is often used for radioactive waste containers. Some materials (seals and test sheets) were purchased from a commercial seal producer and some materials were compounded and cured at BAM in form of rubber sheets.
In Germany, the concept of dry interim storage in dual purpose metal casks before disposal is being pursued for spent nuclear fuel (SF) and high active waste (HAW) management. However, since there is no repository available today, the initially planned and established dry interim storage license duration of up to 40 years will be too short and its extension will become necessary. For such a storage license extension it is required to assess the long-term performance of SF and all safety related storage system components in order to confirm the viability of extended storage.
The main safety relevant components are the thick-walled dual purpose metal casks. These casks consist of a monolithic cask body with integrated neutron shielding components (polymers, e.g. polyethylene) and a monitored double lid barrier system with metal and elastomeric seals. The metal seals of this bolted closure system guarantee the required leak-tightness whereas the elastomeric seals allow for leakage rate measurement of the metal seals.
This paper presents an update on running long-term tests on metal seals at different temperatures under static conditions over longer periods of time. In addition, first results of our approach to understand the aging behavior of different elastomeric seals and neutron radiation shielding material polyethylene are discussed.
Elastomers are widely used as the main sealing materials for containers for low and intermediate level radioactive waste and as an additional component to metal seals in spent fuel and high active waste containers. The safe encapsulation of the radioactive container inventory has to be guaranteed according to regulation and appropriate guidelines for long term storage periods as well as for temperatures as low as -40°C during transport. Therefore, the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance. It is known that the material properties of elastomers are strongly temperature dependent. At low temperatures, this is caused by the rubber-glass transition (abbreviated: glass transition). During continuous cooling, the material changes from a rubber-like entropy elastic to a stiff energy elastic behaviour, which allows nearly no strain or retraction. Hence, rubbers are normally used above their glass transition, but the minimum working temperature limit is not defined precisely; this can cause problems during the above noted applications. Therefore, the lower operation temperature limit of elastomer seals must be determined in dependence of the material properties. Differential scanning calorimetry (DSC) and dynamic mechanical analysis (DMA) are combined with standardised measurements to determine the compression set according to ISO 815. To reduce the test time of the standard tests, a faster technique than normally used was developed. Additionally, the breakdown temperature of the sealing function of complete O ring seals was measured in a component test set-up to compare it with the results of the other tests. The experimental set-up is capable of measuring the leakage rate at low temperatures by the pressure rise method. A fluorocarbon rubber (FKM) was selected for this investigation as it is often used for radioactive waste containers. The materials (seals and test sheets) were purchased from a commercial seal producer.
Ultra high molecular weight polyethylene (UHMW-PE) - due to its high hydrogen content - is used as neutron shielding material in casks for storage and transport of radioactive materials. Besides this, UHMW-PE - as a high-performance polymer - has been used for several years in medical technology due to its excellent slip and wear properties. Due to the special properties of UHMW-PE which result basically from its extreme chain lengths and its high degree of crystallinity, it is predestinated for the aforementioned applications.
In both cases, irradiation and its impact on the molecular structure of polyethylene play an important role. In the first case, irradiation exists as a by-product of inserting the radioactive material in the cask. Hence PE has to withstand any type of degradation affecting safety relevant aspects to be applicable for long term radiation shielding purposes for instance over a period of 40 years. In the second case irradiation is applied deliberately for purposes such as sterilization and crosslinking, leading to partial improvement of the mechanical properties (e.g. fracture toughness, crack propagation resistance, wear resistance) and better Chemical stability.
Specifically concerning their use in the field of medical technology, different types of UHMW-PE have been objects of numerous publications. It is generally accepted that two parallel and competitive processes, based on chain scission and reactions of Ccentered radicals and molecular fragments, occur in PE as a consequence of radiation: radical recombination accounts for crosslinking, together with some disproportionation, formation of low molecular weight fragments, and recrystallization. Furthermore, formation of oxygenated structures in the presence of traces of oxygen is an antagonist of the C-centered radicals. Radiation induced scission preferentially takes place in the amorphous phase and noncrystalline surface of the crystals. It is followed by folding of molecular fragments, crystallinity growth and increased perfection in the crystal lamellae [4, 5]. Chain scission results in shorter polymer molecules, fewer entanglements, and consequently, increased molecular mobility.
The scope of our investigation comprises an estimation of the radiation and thermal impact on the molecular and supra molecular structure of the two types of PE used for neutron shielding cask components. A further point which is worth to explore is to what extent these changes are detectable by thermo-analytical (TA) methods, such as Differential Scanning Calorimetry (DSC), Thermo Mechanical Analysis (TMA), Dynamic Mechanical Analysis (DMA) and Thermogravimetry (TG). Additionally FT-IR and solubility measurements have been performed.
In our studies we focused on the UHMW-PE material GUR 4120 which was y irradiated at RT and compared to the untreated material.
Elastomerdichtungen finden als Bauteil oder Maschinenelement vielseitige Verwendung. Jedoch war trotz ihrer zentralen Bedeutung die untere Temperaturgrenze, bis zu der solche Dichtungen eingesetzt werden können, bisher nicht tiefgehend verstanden. Dieser Umstand erschwert die entsprechende notwendige sicherheitsrelevante Beurteilung. Mit der vorliegenden Arbeit ist deshalb das Ziel verfolgt worden, dass Materialverhalten repräsentativer Elastomerwerkstoffe in Abhängigkeit von der Temperatur zu verstehen und daraus dann abzuleiten, bis zu welcher Temperatur eine daraus hergestellte Dichtung unter Berücksichtigung der jeweiligen Einsatzbedingungen ihre Funktion noch sicher erfüllen kann. Ausgehend von der in der Literatur beschriebenen Aussage, dass eine Dichtung auch unterhalb der „Glasübergangstemperatur“ funktionsfähig ist, wurde der Einfluss des Glas-Gummi-Übergangs auf das Dichtungsversagen untersucht. Zunächst wurden dazu die Glasübergangstemperaturen an einer Vielzahl von Elastomeren mit gebräuchlichen Verfahren bestimmt, um diese mit dem Verhalten der Dichtung vergleichen zu können. Weiterhin wurde im Rahmen der Arbeit eine neue Charakterisierungsmethode des Tieftemperaturverhaltens von Elastomeren entwickelt, die die bisher für Dichtungen eingesetzte Normprüfung des Druckverformungsrests nachstellt. Mit dieser Methode ist im Vergleich zur Normprüfung jedoch eine deutlich schnellere und automatisierbare Untersuchung des Materialverhaltens gegeben. Darüber hinaus ist durch eine modellgestützte Auswertung eine Extrapolation der Messdaten auf zusätzliche Temperaturen möglich, wodurch der experimentelle Aufwand weiter reduziert wird. Zur temperaturabhängigen Charakterisierung des Versagensvorgangs an realen Bauteilen wurde deren Dichtverhalten mittels eines dafür entwickelten Versuchsstandes untersucht. Die festgestellte Abhängigkeit der Versagenstemperatur vom Verpressgrad konnte unter Verwendung der Ergebnisse aller angewandten Charakterisierungsmethoden für die hier untersuchten statisch beanspruchten Dichtungen erklärt werden. Zudem lassen sich aus dem mit Hilfe des Zeit-Temperatur- Superpositionsprinzips gewonnenen Informationen zur Zeitabhängigkeit der Materialeigenschaften auch Aussagen zum Verhalten von dynamisch beanspruchten Dichtungen ableiten. Mit dem Ergebnis der Arbeit zum Verständnis des Verhaltens von Elastomerdichtungen bei tiefen Temperaturen wird die gezielte Beurteilung und Auswahl von sicherheitsrelevanten Dichtsystemen in Zukunft vereinfacht.
Die Messung des dynamischen Speichermoduls mit der Dynamisch-Mechanischen-Analyse ermöglicht einen schnellen Überblick über das temperaturabhängige Verhalten von elastomeren Dichtungsmaterialien. Ein direkter Rückschluss von der so ermittelten Glasübergangstemperatur Tg auf die Versagenstemperatur einer Dichtung ist aber ohne zusätzliche Messungen bisher nicht möglich.
Mit den Ergebnissen des Druckverformungsrestes DVR und des DVRDMA ist eine ge-nauere Beschreibung der Tieftemperatureigenschaften und dadurch der Funktion von elastomeren Dichtungsmaterialien möglich. Messungen ergeben beispielsweise, dass sich das EPDM bei einer Temperatur von -40 °C laut der Dynamisch Mechanischen Analyse noch im gummielastischen Bereich befindet. Die DVRDMA-Werte zeigen eine Rückstellung um mehr als 40 % der Ausgangsdeformation in wenigen Minuten.
Mit derart detailliert bestimmten Eigenschaften lassen sich Rückschlüsse auf einsatzspezifische Anforderungen wie z. B. die Dichtwirkung in Abhängigkeit von Betriebstemperatur und mechanischer Belastungsgeschwindigkeit ziehen, so dass je nach Einsatzbedingungen für die Dichtungen eine geeignete Materialauswahl getrof-fen werden kann.
Tieftemperaturverhalten und Alterung von Elastomerdichtungen - Aktuelle Tätigkeiten und Ziele
(2012)
THz and Mid IR Fourier transform spectroscopy on polyethylene irradiated with Gamma- Co60 radiation
(2014)
THz and mid IR spectroscopy of high molecular PE (HMW) and ultra high molecular PE (UHMW) reveals modifications of the molecular structure induced by γ-Co60 radiation. UHMW-PE and HMW-PE can be distinguished. The integral absorption in the B1u THz-region can quantitatively describe the amorphization of crystallinity. The formation of trans vinylene unsaturations and the decay of vinyl can be followed by mid IR spectroscopy
The thermal expansion of polymeric parts can be an issue in many applications where the available space is limited, or exact dimensions of the part are required. For this study, a device was designed and built that allowed measuring the thermal expansion simultaneously in all three spatial directions on cubic samples with real-scale dimensions (78 mm edge length). The results are shown between 25 °C and 125 °C for two PE materials, one HMWPE and one tempered UHMWPE, for non-irradiated samples as well as cubes that have been irradiated with 100 and 400 kGy. The results measured with the new device were very similar to those measured with conventional thermo-mechanical analysis equipment and to literature data of UHMWPE. The HMWPE material shows a much larger thermal expansion coefficient in one direction compared to the other two directions during the first heating due to frozen stresses from the pressing step during material manufacturing. These stresses are mostly released by the expansion during the first heating, so that the expansion during the second heating is more uniform. The overall volumetric expansion is the same for both heating runs. By contrast, the tempered UHMWPE material shows no significant difference between first and second heating run, as the stresses from processing could already relax in the tempering step. The irradiation treatment does not affect the values significantly for the given test set-up.
Thermoanalytische Charakterisierung von Ethylen-Vinylacetat-Copolymer (EVA) für Photovoltaikmodule
(2011)
Das Ziel der Untersuchungen war mit Hilfe von DSC und DMA EVA-Folien im Anlieferungszustand hinsichtlich der Lage der Glasübergangstemperatur, des Schmelzverhaltens und der Temperaturabhängigkeit der Vernetzungsreaktion zu charakterisieren. Auf dieser Basis sollte die Lieferstabilität im Sinne einer Wareneingangskontrolle auf eine messtechnische Basis gestellt werden. In einem 2. Schritt sollte die vernetzte Folie dahingehend charakterisiert werden, ob infolge der Vernetzung eine Änderung der
Due to delays in the siting procedure to establish a deep geological repository for spent nuclear fuel and high level radioactive waste as well as in construction of the already licensed Konrad repository for low and intermediate level radioactive waste, extended periods of interim storage become more relevant in Germany. BAM is involved in most of the cask licensing procedures and especially responsible for the evaluation of cask-related long-term safety issues.
The long-term performance of elastomer seals for lid systems of transport and storage casks, whether used as auxiliary seals in spent fuel casks or as primary seals for low and intermediate level waste packages, is an important issue in this context. The polymeric structure of these seals causes a complex mechanical behavior with time-dependent sealing force reduction.
The results of a comprehensive purpose-designed test program consisting of basic compression and tension tests as well as relaxation tests on unaged specimens of representative types of elastomers (fluorocarbon rubber (FKM) and ethylene propylene diene rubber (EPDM)) at different temperatures and strain rates are presented. They were used to identify the constitutive behavior and to obtain parameters for finite element material models provided by the computer code ABAQUS®. After estimating the influence of uncertainties such as Poisson’s ratio and friction coefficient by sensitivity analyses, the chosen parameters had to prove their suitability for the finite element simulation of the specimen tests themselves.
Based on this preliminary work the simulation of a specific laboratory test configuration containing a typical elastomer seal with circular cross section is presented. The chosen finite element material model and the implemented parameters had to show that they are able to represent not only the specimen behavior under predominantly uniaxial load but also the more complex stress states in real components. Deviations between the measured and calculated results are pointed out and discussed.
For the consideration of long-term effects in the simulation of elastomer behavior, test results of aged specimens are needed. First information about a new test program, started recently and planned to provide these data, are given.
Testing and numerical simulation of elastomeric seals under consideration of time dependent effects
(2016)
Due to delays in the siting procedure to establish a deep geological repository for spent nuclear fuel and high level waste and in construction of the already licensed Konrad repository for low and intermediate level waste, extended periods of interim storage will become more relevant in Germany. BAM is involved in most of the cask licensing procedures and is responsible for the evaluation of cask-related long-term safety issues. Elastomeric seals are widely used as barrier seals for containers for low and intermediate level radioactive waste. In addition they are also used as auxiliary seals in spent fuel storage and transportation casks (dual purpose casks (DPC)).
To address the complex requirements resulting from the described applications, BAM has initiated several test programs for investigating the behavior of elastomeric seals. These include experiments concerning the hyperelastic and viscoelastic behavior at different temperatures and strain rates, the low temperature performance down to -40°C, the influence of gamma irradiation and the aging behavior.
The first part of the paper gives an overview of these tests, their relevant results and their possible impact on BAM’s work as a consultant in the framework of approval and licensing procedures.
The second part presents an approach of the development of a finite element model using the finite element code ABAQUS®. The long-term goal is to simulate the complex elastomeric behavior in a complete lid closure system under specific operation and accident conditions.
A device has been designed, built and tested that allows the investigation of effects of dynamic loads on the leak tightness of elastomer seals at low temperatures. With the test setup, the compression of the tested seal can be reduced by a defined degree in a time period of less than 1 s. For the evaluation of the leak tightness, leakage rates can be determined.
It was shown that the rapid partial release of an elastomer seal leads to its failure already at the beginning of the rubber–glass transition and, therefore, at significantly higher temperatures than the loss of leak tightness observed under static conditions.
It is common practice in the application of finite element analysis to model compression set (CS) of elastomers during aging with two different material models according to the two-network theory of Tobolsky. The theory relies on the existence of two networks. The first one represents the original network after vulcanization and is sensitive to chain scission. The second network accounts for the formation of additional crosslinking during aging. Besides the use of user subroutines to describe the two-network model, an element overlay technique is also needed as the full set of both material behaviors did not exist for assignment to a single element. This element overlay technique is valuable for research and developmental purposes but makes extension to industrial usage quite challenging. Our goal is to simulate the CS of elastomers after long-term aging in a commercial finite element software with no need for extra subroutine codes or mesh superposition.
Ethylene propylene diene (EPDM) O-rings were aged in a compressed state at 75 °C, 100 °C, 125 °C and 150 °C for up to 183 days. Investigations of the experimental test results were used to identify material models and their parameters to develop a finite element model to simulate CS. The model was implemented in the finite element software ABAQUS/Standard® with a sequential temperature-displacement coupling.
Regarding the influence of temperature, the Arrhenius equation is adopted for the time-temperature relationship. The activation energy value that is required for the simulation is firstly determined from shifting the experimental CS results with the time-temperature superposition technique and plotting the shift factors in an Arrhenius diagram. The experiments were compared with the simulation results. Afterwards different activation energies were used in the simulation and discussed. A suitable choice of the activation energy value with regard to the reference temperature and the test temperature is presented. With the chosen activation energies, the match between numerical CS values after long-term aging and the experimental results was improved.
Elastomers are susceptible to chemical ageing, i.e., scission and cross-linking, at high temperatures. This thermally driven ageing process affects their mechanical properties and leads to limited operating time. Continuous and intermittent stress Relaxation measurements were conducted on ethylene propylene diene rubber (EPDM) and hydrogenated nitrile butadiene rubber (HNBR) samples for different ageing times and an ageing temperature of 125 °C. The contributions of chain scission and cross-linking were analysed for both materials at different ageing states, elucidating the respective ageing mechanisms. Furthermore, compression set experiments were performed under various test conditions. Adopting the two-network model, compression set values were calculated and compared to the measured data. The additional effect of physical processes to scission and cross-linking during a long-term thermal exposure is quantified through the compression set analysis. The characteristic times relative to the degradation processes are also determined.
Both chain scission and crosslinking reactions occur during ageing of EPDM rubber. However, with many conventional polymer analysis methods such as hardness and DMA, it is hardly possible to obtain information about the contribution of each reaction type to the measured data. For example, hardness and Tg both increase during ageing of EPDM, indicating crosslinking during ageing, but it is not clear whether this is partly counterbalanced by chain scission reactions which would lower hardness and Tg. An indication that chain scission reactions probably counteract the hardness or Tg increase by crosslinking is given by Compression Set (CS) measurements. CS exhibits a higher change than hardness or Tg, as CS increases additively through both chain scission and crosslinking reactions. In order to elucidate the share of chain scission reactions in the total degradation, a method testing relaxation and recovery behaviour using DMA equipment was applied. The method revealed the strong influence of chain scissions, leading to more pronounced relaxation and higher residual strain after compression.
Safety of long term containment and storage of radioactive waste is an essential issue, which is increasingly gaining international attention. Extending interim storage beyond initial license periods is one of the major challenges worldwide.
BAM has been involved in all kinds of radioactive waste container safety evaluation for storage and transportation including their long term performance from the very beginning. Today, all work related to the safe management of radioactive waste is linked by the activity field “Nuclear Waste Management” within the Focus Area “Energy” at BAM and in conjunction with a research strategy and agenda. Most recently, the working group “Long Term Safety of Container Systems and Components” was established to launch and perform research projects related to safety issues concerning the extended interim storage of radioactive waste.
For example, within our project LaMEP, we investigate ageing effects of metal and elastomer seals as well as polymeric neutron shielding materials, which are container components that fulfil major safety functions. The results of the experiments help to understand the long term behaviour of these components. Likewise, our project BRUZL started at BAM in 2018 with the aim of developing a fracture mechanics approach to understand and describe a potential brittle failure mechanism of fuel cladding during long-term interim storage. BAM also contributes to the GRS project “Development of methods and models and international exchange for safety evaluation in the frame of interim storage of radioactive waste”. Additionally, BAM is involved in several international research programmes dealing with extended interim storage, such as the European Joint Programme on Radioactive Waste Management (EURAD), the Extended Storage Collaboration Program (ESCP) and IAEA Coordinated Research Projects.
The present contribution provides a comprehensive overview of BAM research activities contributing to national and international gap analyses and to filling knowledge gaps regarding the safe long term management of radioactive waste.
Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste and in some countries for spent fuel transportation casks. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period.
In Germany the low and intermediate level radioactive waste is planned to be disposed in the Konrad repository in standardized containers. Many of these containers use an elastomer seal between lid and container body. Depending on the radiactive inventory and a possible containment of the waste in inner barrels and/or concrete structures, such containers may require a specific leak tightness. In such cases, specified leakage rates are shall not be exceeded by the the seals to keep potential activity releases from the inventories well below defined limits.
Generally, all waste containers have to fulfill the waste acceptance criteria for the Konrad repository as defined by the reports BfS SE-IB-29/08 and SE-IB-30/08. From these criteria several requirements for seal performance are derived. The seals have to:
- ensure full functionality until final container disposal,
- maintain its function in case of a thermal or mechanical accident,
- ensure encapsulation also at -20 °C.
This combination of requirements is challenging especially as a seal exchange, which is typical for many other applications, is hardly possible and thus a sound understanding of how to perform safety evaluation of containers is required. Therefore BAM has initiated investigations on elastomer seal behaviour. This work focuses on low temperature behaviour and sealing performance concerning static conditions as well as partial loss of compression and ageing of elastomer seals. Concerning ageing, property changes caused by long-term thermooxidative conditions as well as gamma irradiation are investigated.
This contribution presents an overview and explanation of the aims of the ongoing research and gives an update of the most relevant results.
Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste and in some countries for spent fuel transportation casks. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period.
In Germany the low and intermediate level radioactive waste is planned to be disposed in the Konrad repository in standardized containers. Many of these containers use an elastomer seal between lid and container body. Depending on the radiactive inventory and a possible containment of the waste in inner barrels and/or concrete structures, such containers may require a specific leak tightness. In such cases, specified leakage rates are shall not be exceeded by the the seals to keep potential activity releases from the inventories well below defined limits.
Generally, all waste containers have to fulfill the waste acceptance criteria for the Konrad repository as defined by the reports BfS SE-IB-29/08 and SE-IB-30/08. From these criteria several requirements for seal performance are derived. The seals have to:
- ensure full functionality until final container disposal,
- maintain its function in case of a thermal or mechanical accident,
- ensure encapsulation also at -20 °C.
This combination of requirements is challenging especially as a seal exchange, which is typical for many other applications, is hardly possible and thus a sound understanding of how to perform safety evaluation of containers is required. Therefore BAM has initiated investigations on elastomer seal behaviour. This work focuses on low temperature behaviour and sealing performance concerning static conditions as well as partial loss of compression and ageing of elastomer seals. Concerning ageing, property changes caused by long-term thermooxidative conditions as well as gamma irradiation are investigated.
This contribution presents an overview and explanation of the aims of the ongoing research and gives an update of the most relevant results.
The temperature dependences of dielectric permittivity and elastic modulus of poly(vinylidene fluoride - hexafluoropropylene) (P(VDF-HFP)) are compared and explained by use of structural data obtained by differential scanning calorimetry and X-ray analysis. Special emphasis is put on the effect of uniaxial stretching which renders the polymer ferroelectric. It is shown that dielectric and mechanical relaxations at the glass transition (aa relaxation) are closely related and not significantly affected by stretching. It is further confirmed that stretching destroys the non-polar spherulitic crystalline structure and produces relatively small-sized polar crystallites. This manifests in the disappearence of the so-called ac relaxation which is associated to molecular motions within the spherulitic crystalline lamellae. However, there are discrepancies between dielectric and mechanical losses above the glass transition which point towards a still not described structural transition.
The special properties of high molecular weight polyethylene (HMW-PE) and ultra high molecular
weight polyethylene (UHMW-PE) result basically from their extreme chain lengths and their high
degree of crystallinity. As high-performance polymers, they are used for a variety of applications.
UHMW-PE in particular is often utilized for endoprothesis (due to its excellent slip and wear
properties) and due to its high hydrogen content as a neutron moderator in casks for storage and
transport of radioactive materials.
To prepare the material for instance for its use as a total joint replacement, it is exposed to radiation
for several reasons, such as sterilization and crosslinking, leading to partial improvement of the
mechanical properties (e.g. fracture toughness, crack propagation resistance, wear resistance) and
better chemical stability.
To be applicable for long term radiation shielding purposes for instance over a period of 40 years,
PE has to withstand any type of degradation affecting safety relevant aspects.
The scope of our investigation comprises an estimation of the radiation impact on the molecular and
supra molecular structure of two types of PE and to what extent these changes are detectable by
thermo-analytical (TA) methods, such as Differential Scanning Calorimetry (DSC), Thermo
Mechanical Analysis (TMA), Dynamic Mechanical Analysis (DMA) and Thermo Gravimetric
Analysis (TGA). Additionally FT-IR spectroscopy as well as density and gas sorption
measurements were carried out.
Due to the poor solubility of HMW-PE and UHMW-PE, some classical analytical techniques are
not applicable. But TA-methods represent a feasible approach to detect structural and
morphological features of these materials as well as changes caused by external influences, such as
thermal treatment and/or irradiation. With the combination of the applied TA-techniques it is
possible to distinguish between crosslinking and degradation.
Polymer Testing - Editorial
(2016)
Polymer Testing - Editorial
(2016)
Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste and for spent fuel transportation casks. In addition, they are also used for spent fuel storage and transportation casks (dual purpose casks (DPC)) as auxiliary seals to allow leakage rate measurements of metal barrier seals for demonstration of their proper assembling conditions. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal, and environmental conditions as well as irradiation during the entire operation period. Concerning DPC, degradation effects should be limited in a way that, for example, effects from potentially released decomposition elements may not harm e.g. metal barrier seals. Leakage rate measurements should be possible also after long interim storage periods prior to subsequent transportation.
Because of the complex requirements resulting from the various applications of containers for radioactive waste and spent nuclear fuel, BAM has initiated several test programmes for investigating the behaviour of elastomer seals. In this contribution the current status is described and first results are discussed.
During an extensive test programme at the Bundesanstalt für Materialforschung und prüfung, material property changes of EPDM O-rings were investigated at different ageing times and two ageing temperatures of 125∘C and 150∘C. To exclude possible diffusion-limited oxidation (DLO) effects that can distort the data, IRHD microhardness measurements were taken over the cross section of compressed O-rings. Continuous stress relaxation measurements were taken on samples free of DLO effects. The additional effect of physical processes to irreversible chemical ones during a long-term thermal exposure is quantified by the analysis of compression set measurements under various test conditions. By combining the different experimental methods, characteristic times relative to the degradation processes were determined. On the basis of experimental data, a microphysically motivated model that takes into account reversible and irreversible processes was developed. The parameter identification strategy of the material model is based on our experimental investigations on homogeneously aged elastomer O-rings. The simulated results are in good agreement with the experiments.
Overview of ongoing research and future prospects on polyethylene neutron shielding materials at bam
(2023)
The extension of the interim storage period of radioactive waste before disposal will cause additional challenges for the nuclear waste management in Germany, so that an extensive knowledge of the long-term performance of casks, including their components and inventories, will be required for future extended storage licenses.
Ultra-high and high molecular weight polyethylenes ((U)HMW-PE) are used for neutron shielding purposes in casks for storage and transport of spent fuel and high-level waste due to their extremely high hydrogen content. During their service life of several decades as cask components, the PE materials are exposed to neutron and gamma radiation from the radioactive inventory of the casks, mechanical assembling stresses and temperature. All these combined effects affect the material properties of such components which in turn may be crucial for some possible accident scenarios.
At the Bundesanstalt für Materialforschung und -prüfung (BAM), the effects of high temperature exposure in combination with subsequent or previous irradiation were investigated with a comprehensive aging program including thermal aging at 125 °C for different aging periods up to 5 years and irradiation with doses ranging from 50 to 600 kGy.
This contribution provides an overview of the ongoing research related to the structural changes of (U)HMW-PE induced by gamma irradiation and high temperature exposure and focuses on current research perspectives at BAM with regard to the prediction of the dynamic behavior of the material during extended interim storage in case of an accident scenario. First results of the coupled effect of temperature, radiation and mechanical loading will be presented. The effect of microstructural changes induced by gamma irradiation and high temperature on the mechanical behavior of (U)HMW-PE will be assessed.
At the Bundesanstalt für Materialforschung und -prüfung (BAM) in Division 3.4 Safety of Storage Containers, one of our tasks is to evaluate the safety of containers designed for disposal of low and intermediate radioactive waste. As such containers might be transported before and stored until disposal, safe enclosure of the radioactive inventory is important for this time span. Elastomer O-rings are widely used as barrier seals in these containers. Thus, as for many other applications, an understanding of the practical effects of ageing degradation on elastomer seals during long-term exposure is mandatory for predicting the lifetime of such components. According to a long-term test programme on three kinds of rubbers (EPDM and FKM (relevant for application), HNBR (for comparison)), over several years we have studied the degradation and the change of mechanical properties (e.g. hardness, strain at break) at four different ageing temperatures (75 °C, 100 °C, 125 °C and 150 °C) as well as the change of sealing properties. Continuous and intermittent compression stress relaxation (CSR) measurements were performed in order to investigate the respective contribution of crosslinking and chain scission to the observed degradation effects. Thus, the degradation kinetics and mechanisms could be resolved more clearly. For assessing the seal performance, compression set (CS) and leakage rate measurements were conducted. The experimental results showed that the O-rings remained leak-tight under purely static conditions even when CSR, CS and mechanical properties already indicated far advanced degradation. For this reason, a modified leakage test involving a small and rapid partial decompression of the seal was developed that enabled determining an end-of-lifetime criterion for O-rings with a safety margin for thermal shrinkage and vibrations.
The investigation of the long-term performance of sealing systems employed in containers for radioactive waste and spent nuclear fuel is one research focus area for division 3.4 “Safety of Storage Containers” at the Bundesanstalt für Materialforschung und -prüfung. The behaviour of metallic seals, which are employed in interim storage casks for used fuel and high active waste, over time is of high importance for ensuring safe enclosure. Therefore, investigations on these systems were started at BAM to get a general understanding of the relevant processes. Our investigations comprise investigations on different parameters which influence the seal performance and the main part is focussed on the time and temperature dependent behaviour.
In this contribution an overview of the performed tests and their respective results will be given. A focus will lie on a comparison between seals with large torus diameter in comparison to small diameters.
Our aim is to understand the long-term behaviour of the sealing systems for evaluation of their performance during possible extended interim storage and subsequent transportation.
The investigation of the long-term performance of sealing systems employed in containers of radioactive waste and spent nuclear fuel is one research focus area for division 3.4 \Safety of Storage Containers" at the Bundesanstalt für Materialforschung und -prüfung. The behaviour of metallic seals, which are employed in interim storage casks for spent nuclear fuel and high active waste, over time is of high importance for ensuring safe enclosure. Therefore, investigations on these systems were started at BAM to get a general understanding of the relevant processes. Our investigations comprise investigations on different parameters which influence the seal Performance and the main part is focussed on the time and temperature dependent behaviour. Our aim is to understand the longterm behaviour of the sealing systems for evaluation of their performance during possible extended interim storage and subsequent transportation. In this contribution an overview of the performed tests and their respective results is given. A focus lies on a comparison between seals with large torus diameter in comparison to small diameters.
Optical and thermal analysis of PVB encapsulant polymer functionalized with luminescent organic dyes
(2018)
This work focused on the technology of luminescent down shift (LDS), with a primary aim to identify and investigate a methodology to introduce the luminescent organic dye into PVB polymer encapsulant as emergent material for photovoltaic application. For this goal, we propose to study the feasibility to implement the LDS functionality and to identify suitability of available luminescent to be incorporated into the host polymer encapsulant material. The first step to this direction was through a comprehensive optical study of Violet 570 (V) organic dye in ethanol solvent. The methodology and experimental conditions such as laboratory polymer preparation and luminescence dye concentration were presented. Also, the emergent polymer encapsulant sheets were characterized by using optical and thermal analysis techniques. The absorption spectrum of the prepared PVB material shifts towards longer wavelengths, with increasing organic dye concentration.