Filtern
Erscheinungsjahr
Dokumenttyp
Schlagworte
- Elastomer (19) (entfernen)
Organisationseinheit der BAM
A new method for the evaluation of the low temperature properties of rubber materials is presented. The method emulates the standardized compression set measurement, which is frequently used for sealing materials, but can be performed within a considerably shorter time. The results are compared with the standard test and found to be qualitatively the same. Slight differences are discussed on the basis of the differences in the measurement procedures. Further data evaluation is done by fitting functions to describe the material behaviour.
The excellent mechanical properties of elastomer seals at a wide range of temperatures as well as their high versatility and recovery potential under several load conditions make these materials well suitable for the application in containers designed for transport and disposal of negligible heat generating radioactive waste. While a seal exchange at defined intervals is typical in many conventional applications, it is impossible or at least hard to perform when principles of minimization of radiation exposure have to be considered which prohibit an avoidable cask handling. An extensive knowledge of the change of the elastomer properties during aging and the availability of reliable end-of-lifetime criteria to guarantee the safe enclosure of the radioactive material for the required time are mandatory. As BAM is involved in most of the national cask licensing procedures and in the evaluation of cask-related long-term safety issues, great efforts have already been made and are still ongoing to scientifically support this task.
Among other representative types of elastomers, specimen made from ethylene propylene diene rubber (EPDM) were tested before, during and after aging to capture the with respect to application most important of their complex mechanical properties.
Exemplary results of these investigations were used to calibrate material models implemented in the commercial finite element software ABAQUS/Standard®. The finite element model already presented in previous works uses a sequential temperature displacement coupling. The calculated compression stress relaxation (CSR) and compression set (CS) values do satisfactorily match the experimental results.
In many investigations performed at BAM both values (CSR and CS) were identified as key indicators of elastomer’s long-term performance.
However, the possibility to correlate these equivalent indicators with performance values such as tightness and leakage rate, measurable in the mounted state, is an important goal of our future work. In the presented study the ABAQUS® feature of “pressure penetration” is introduced in the suggested finite element model for this purpose. It provides the possibility to simulate the penetration of a gas into a possible gap between flange and O-ring causing an opening of a leakage path. Three dimensional and axis-symmetric finite element models were generated to represent flat and grooved flanges of different dimensions.
The sensitivity of the feature to several input parameters is investigated and the observed behavior of the O-ring is correlated with the results of performed leakage tests.
At BAM Federal Institute for Materials Research and Testing in Germany, it is our responsibility to audit the safety of casks designed for transport and/or storage of radioactive material. With regard to the requirements on long-term safety of the containers, it is necessary to evaluate the service lifetime of the elastomeric seals used in the containers. With ageing, the elastomers will gradually lose their elasticity and their ability for recovery, which might result in a leakage above the allowed level or in a release of radioactivity during an incident. It is important to know the rate of degradation and which property can be used as an practical and easily measurable end-of-lifetime criterion. For this reason, we devised ageing experiments on different kinds of elastomers, namely FKM, EPDM and HNBR. The former two are actually used in containers for radioactive wastes – either as auxiliary seal in casks containing high activity waste, or as main seal in casks for medium or low activity waste. The latter is an often used seal material that is tested for comparative reasons. In our ageing program, these three materials are aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) in order to extrapolate the data to service temperature using a suitable model. They are examined at logarithmic time intervals of several days up to 5 years. The samples are aged in their undeformed O-ring state as well as compressed between flanges with a deformation corresponding to the actual compression during service. Thus we can compare the ageing between relaxed and stressed sample. Additionally, we are ageing samples in flanges that allow leakage rate measurements. Other measurements include monitoring of the recovery force of the seal and the compression set. Furthermore, the samples are examined by thermal and dynamic-mechanical analysis for detecting changes in the glass transition temperature due to crosslinking or chain scission in the material. Besides, hardness is measured as a practical macroscopic indicator. Until now, we have analyzed samples aged up to 100 days. At the highest ageing temperature of 150 °C, the compressed EPDM has already reached a compression set of 95 %, while HNBR and FKM have reached 80 % and 30 %, respectively. Furthermore, HNBR has reached a Shore D hardness of 85, which is an immense increase after the initial value of 80 Shore A. However, when looking at the cross-section of the sample, it was obvious that only a layer of about 1 mm thickness has become so hard, while the inner part remained rubbery. This shows that there has been intense crosslinking mostly near the surface of the HNBR which forms a kind of oxygen diffusion barrier, inhibiting the thermooxidation of the inner part of sample which can retain elastic properties. In EPDM, the oxygen permeability is much greater, which leads to a more homogeneous degradation across the whole sample and thus resulted in a higher compression set. The low compression set of FKM shows the outstanding high-temperature properties of this material.
At BAM Federal Institute for Materials Research and Testing in Germany, it is our responsibility to evaluate the safety of casks designed for transport and/or storage of radioactive material. This includes the investigation of elastomeric seals applied in the containers. Besides examining the low-temperature behavior of elastomeric seals, it is our goal to evaluate the service lifetime of the seals with regard to the requirements for long-term safety (40 years and more) of the containers. Furthermore, we deem it necessary to exceed the requirements given in the ageing standard DIN 53508 and take into account diffusion-limited oxidation (DLO) effects and non-Arrhenius behavior when making lifetime predictions. Therefore, we started an ageing programme with selected rubbers (HNBR, FKM and EPDM) which are oven-aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) in order to extrapolate the data to service temperature using different models and check which one is appropriate. Samples are examined at different times up to 5 years. In order to be able to compare between compressed and relaxed rubber, they are aged in two conditions: the undeformed O-ring state as well as compressed between plates with a compression of 25 % corresponding to the actual compression during service. Additionally, we are ageing samples in flanges that allow leakage rate measurements which is the central performance criterion. Analysis methods include hardness as a quick indicator, compression set and compression stress relaxation as measures reflecting the actual properties of a compressed seal. Additionally, we are applying classical polymer analysis methods like dynamic mechanic analysis and thermogravimetric analysis which show changes in the polymeric structure due to chain scission and crosslinking. Furthermore, we are testing the leakage rate of the O-rings in order to correlate the changes in physical properties to the actual performance of the seal.
First results of samples aged up to 100 days show a strong increase in hardness for HNBR, a moderate increase for EPDM and hardly a change for FKM. A similar result is seen in the compression set of samples aged 100 d at 100 °C in compression as HNBR has reached 60 %, EPDM 25 % and FKM 15 % compression set. However, after ageing at 150 °C, EPDM shows a worse performance with 95 % compression set compared to HNBR with only 80 %. This is probably due to DLO effects in HNBR that appear because of the fast ageing and low oxygen permeability in HNBR. This leads to a deficit of oxygen in the center of the sample which is thus protected from ageing and can retain elastic properties. The full paper shall discuss the changes in material properties observed to date and the impact on the performance of elastomeric seals.
Elastomeric seals are used in many containers, including casks for radioactive waste. However, like all polymers, elastomers are prone to aging, which leads to a loss of sealing force and the ability for recovery which can ultimately result in leakage. Therefore it is important to be able to define an end-of-lifetime criterion and to judge the lifetime of elastomeric seals. For this reason, we started an aging program on three kinds of rubbers (HNBR, EPDM, FKM), monitoring the change of properties at four different aging temperatures over extended periods up to five years. The measured data is used for lifetime prediction by applying a suitable model.
Unsere Aufgabe im Fachbereich 3.4 der Bundesanstalt für Materialforschung und prüfung (BAM) ist die sicherheitstechnische Begutachtung von Transport- und Lagerbehältern für radioaktiven Abfall, die für langfristige Zwischenlagerung ausgelegt sind. Ein Arbeitsschwerpunkt ist die Bewertung der Lebensdauer von Metall- und Elastomerdichtungen in den Behältern im Hinblick auf die Anforderungen für langfristige Behältersicherheit (min. 40 Jahre in Deutschland). Um die Eigenschaftsänderungen der Elastomerdichtungen während einer beschleunigten Alterung über lange Zeiträume (bis zu fünf Jahre) untersuchen zu können, wurde ein Alterungsprogramm an ausgewählten Elastomeren (HNBR, EPDM, FKM) begonnen.
Im Gegensatz zu Normalterungsverfahren altern wir keine Normteile, sondern O-Ringe im unverpressten sowie verpressten Zustand. Diese Vorgehensweise ermöglicht die Bewertung des Einflusses der Verpressung auf die Alterung sowie die Untersuchung des Bauteilversagens mittels Leckageratenmessungen unter anwendungsnahen Bedingungen. Weitere Charakterisierungsmethoden sind Härtemessung, dynamisch-mechanische Analyse (DMA), Thermogravimetrie (TGA), Druckspannungsrelaxation, Druckverformungsrest (DVR), Dichtebestimmung und Zugversuch. Das Ziel ist, die Leckagerate mit anderen Eigenschaften bzw. Methoden zu korrelieren, um so ein aussagekräftiges und leichter zu bestimmendes Lebensdauerkriterium für elastomere O-Ringe abzuleiten.
Während der Alterung können in Abhängigkeit von Material sowie Alterungsdauer und –temperatur Inhomogenitäten aufgrund von diffusionsbegrenzter Oxidation auftreten, durch die sich unterschiedliche Eigenschaften an der Oberfläche und im Volumen der Dichtung ergeben, was zu falschen Lebensdauerabschätzungen führen kann. Mittels Mikrohärtemessung über den Querschnitt werden diese Effekte charakterisiert und bei der Extrapolation mittels Zeit-Temperatur-Verschiebung und Arrheniusgraph berücksichtigt. Bisher liegen Daten von bis zu einem Jahr bei vier verschiedenen Temperaturen (75 °C, 100 °C, 125 °C und 150 °C) gealterten Proben vor. Nach 100 Tagen bei 150 °C weisen HNBR und EPDM schon einen DVR von über 80 % auf, aber noch keinen signifikanten Anstieg der Leckagerate. Diese sinkt zunächst während der Alterung, da die Permeabilität aufgrund von Vernetzungsreaktionen sinkt. Bei HNBR ist dies aufgrund der dominanteren Vernetzungsreaktionen während der Alterung noch stärker ausgeprägt als bei EPDM.
Elastomers are widely used as main sealing materials for Containers for low and intermediate Ievel radioactive waste and as additional component to metal seals in spent fuel and high active waste Containers. According to appropriate guidelines and regulations safe enclosure of the radioactive Container contents has to be guaranteed for long storage periods as well as down to temperatures of -40 °C for transportation. Therefore the understanding of seal behaviour in general is of high importance and ageing of elastomeric seals has to be considered with regard to possible dynamic events taking possibly place during transport after storage.
The method for the determination of compression set values with a Dynamic Mechanical Analysis (DMA) setup at low temperatures, which was presented previously, allows a much faster and readily automated procedure than the standardized compression set test according to ISO 815-2. This method is applied to a series of different elastomeric materials that are commonly used for sealing applications. The results of the compression set test are compared with results from thermal analysis to allow an in depth comparison of the material behaviour at low temperatures.
Furthermore, a comparison between two EPDM materials is presented. These materials show very similar properties determined by thermo analytical methods such as Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) but differ clearly in their compression set behaviour. This comparison shows the importance and value of information of the compression set test in addition to thermal analysis to judge the behaviour of sealing materials and confirms the relevance of the new compression set test method for the investigation of low temperature properties of elastomers.
Einfluss der Alterung auf dichtungsrelevante Eigenschaften von FKM-, VMQ- und EPDM-Elastomeren
(2017)
Da Elastomere in vielfältigen Dichtungsanwendungen eingesetzt werden und dabei teilweise großen Einfluss auf die Funktionsfähigkeit und Sicherheit haben, ist der Einfluss der Alterung auf dichtungsrelevante Eigenschaften relevant. Eine strukturierte Untersuchung des Einflusses von verschiedenen Mischungsrezepturen auf die Bauteileigenschaften, das Alterungsverhalten und die Funktion wird vorgestellt.
Aufgrund ihrer einfachen und zuverlässigen Anwendung werden Elastomere für viele Dichtungsaufgaben eingesetzt. In vielen Anwendungsbereichen, wie z.B. Verkehr, Luftfahrt und Verfahrenstechnik, können während des Einsatzes tiefe Temperaturen auftreten, bei denen die Funktionsfähigkeit der Dichtung erhalten bleiben muss. Daher ist die Untersuchung des Verhaltens von Elastomerdichtungen bei tiefen Temperaturen wichtig, um ihren Temperatureinsatzbereich nach unten abzugrenzen und dadurch einen verlässlichen Betrieb zu sichern. Ziel dieser Arbeit ist es, den sicheren Einschluss von gefährlichen Gütern unter verschiedenen Umgebungsbedingungen und über lange Zeiten zu ermöglichen bzw. die Materialauswahl entsprechend zu steuern.
O-rings made of HNBR, EPDM and FKM were aged in the compressed and uncompressed state at 150 °C, 125 °C, 100 °C, 75 °C, 60 °C and 23 °C for aging times of up to five years. Hardness was measured and increased with aging time and temperature for HNBR and EPDM, but it remained practically constant for FKM. Indenter modulus measurements were performed on the lateral O-ring surface (that was free of DLO effects) to assess an influence of the compression during aging, but none was detected. The equilibrium compression set (CS) exhibited faster and stronger degradation than hardness and was used for lifetime predictions using the time-temperature superposition (TTS) principle. With an end-of-lifetime criterion of 70 % CS, lifetimes of 4.5 years, 50 years and 526 years at 75 °C were estimated for HNBR, EPDM and FKM, respectively. The activation energies derived from an Arrhenius plot of the shift factors from the TTS were 85 kJ/mol, 99 kJ/mol and 78 kJ/mol for HNBR, EPDM and FKM, respectively, revealing that a higher activation energy does not necessarily mean that the material has a higher lifetime at lower temperatures. Furthermore, the measured lifetime of EPDM O-rings at 100 °C (5 years) was compared to that predicted on the basis of the lifetime at 150 °C as well as 125 °C using the corresponding shift factors. The error of the prediction was only ± 4 %. However, this precise prediction could only be achieved using the five-year long-term aging data. When using only data from aging times up to 0.5 years and 2 years, the lifetime of EPDM O-rings at 100 °C was underestimated by 31 % and 22 %, respectively.
Rubber is widely used as sealing material in various applications. In many fields the sealing function at low temperatures is necessary. Therefore the understanding of failure mechanisms is of high importance. Rubbers are normally used above their glass-rubber transition region but the minimum working temperature limit is not defined precisely. Therefore the lower operation temperature limit of rubber seals should be determined in dependence of the material properties. The results of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are combined with the results of the standardized compression set according to ISO 815 respectively a modified test using the DMA equipment.
Monitoring the vulcanization of elastomers: Comparison of curemeter and ultrasonic online control
(2009)
The vulcanization of elastomeric materials has a high impact on the properties of the final product. Therefore, it is important to monitor and control this crosslinking process. A common technique to attain the necessary curing time is the use of a curemeter in accordance with ISO 6502 in order to determine the time for full cure of a sample with a standardized geometry. Based on this result and a lot of practical experience, the required curing time for a given product geometry is estimated. Within the scope of this work, a new analysis technique will be compared with the standard procedure. The ultrasonic online control employs ultrasound waves to measure the changes in material properties caused by vulcanization. For this study, a natural rubber compound with a conventional curing system was investigated by both techniques. It was found that the results of the ultrasonic technique show good agreement with the results of the curemeter.
In consideration of the influence of the curing reaction on the material properties of elastomers, it is very important to control the vulcanization process properly.
As shown previously [1], the effects of the vulcanization reaction of an elastomer can be monitored by use of ultrasonic sound waves. This technique has to a certain degree a high similarity to the standard curemeter test according to ISO 6502 but can be applied also inside a production tool.
So far, the method was only applied to the vulcanization of one compound at a given temperature and sample thickness. This is now complemented with measurements on another compound system at different temperatures and sample thicknesses.
The expected effects of temperature and thickness on the curing behaviour were found by use of the ultrasound online control.
Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste and for spent fuel transportation casks. In addition, they are also used for spent fuel storage and transportation casks (dual purpose casks (DPC)) as auxiliary seals to allow leakage rate measurements of metal barrier seals for demonstration of their proper assembling conditions. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal, and environmental conditions as well as irradiation during the entire operation period. Concerning DPC, degradation effects should be limited in a way that, for example, effects from potentially released decomposition elements may not harm e.g. metal barrier seals. Leakage rate measurements should be possible also after long interim storage periods prior to subsequent transportation.
Because of the complex requirements resulting from the various applications of containers for radioactive waste and spent nuclear fuel, BAM has initiated several test programmes for investigating the behaviour of elastomer seals. In this contribution the current status is described and first results are discussed.
A device has been designed, built and tested that allows the investigation of effects of dynamic loads on the leak tightness of elastomer seals at low temperatures. With the test setup, the compression of the tested seal can be reduced by a defined degree in a time period of less than 1 s. For the evaluation of the leak tightness, leakage rates can be determined.
It was shown that the rapid partial release of an elastomer seal leads to its failure already at the beginning of the rubber–glass transition and, therefore, at significantly higher temperatures than the loss of leak tightness observed under static conditions.
Elastomerdichtungen finden als Bauteil oder Maschinenelement vielseitige Verwendung. Jedoch war trotz ihrer zentralen Bedeutung die untere Temperaturgrenze, bis zu der solche Dichtungen eingesetzt werden können, bisher nicht tiefgehend verstanden. Dieser Umstand erschwert die entsprechende notwendige sicherheitsrelevante Beurteilung. Mit der vorliegenden Arbeit ist deshalb das Ziel verfolgt worden, dass Materialverhalten repräsentativer Elastomerwerkstoffe in Abhängigkeit von der Temperatur zu verstehen und daraus dann abzuleiten, bis zu welcher Temperatur eine daraus hergestellte Dichtung unter Berücksichtigung der jeweiligen Einsatzbedingungen ihre Funktion noch sicher erfüllen kann. Ausgehend von der in der Literatur beschriebenen Aussage, dass eine Dichtung auch unterhalb der „Glasübergangstemperatur“ funktionsfähig ist, wurde der Einfluss des Glas-Gummi-Übergangs auf das Dichtungsversagen untersucht. Zunächst wurden dazu die Glasübergangstemperaturen an einer Vielzahl von Elastomeren mit gebräuchlichen Verfahren bestimmt, um diese mit dem Verhalten der Dichtung vergleichen zu können. Weiterhin wurde im Rahmen der Arbeit eine neue Charakterisierungsmethode des Tieftemperaturverhaltens von Elastomeren entwickelt, die die bisher für Dichtungen eingesetzte Normprüfung des Druckverformungsrests nachstellt. Mit dieser Methode ist im Vergleich zur Normprüfung jedoch eine deutlich schnellere und automatisierbare Untersuchung des Materialverhaltens gegeben. Darüber hinaus ist durch eine modellgestützte Auswertung eine Extrapolation der Messdaten auf zusätzliche Temperaturen möglich, wodurch der experimentelle Aufwand weiter reduziert wird. Zur temperaturabhängigen Charakterisierung des Versagensvorgangs an realen Bauteilen wurde deren Dichtverhalten mittels eines dafür entwickelten Versuchsstandes untersucht. Die festgestellte Abhängigkeit der Versagenstemperatur vom Verpressgrad konnte unter Verwendung der Ergebnisse aller angewandten Charakterisierungsmethoden für die hier untersuchten statisch beanspruchten Dichtungen erklärt werden. Zudem lassen sich aus dem mit Hilfe des Zeit-Temperatur- Superpositionsprinzips gewonnenen Informationen zur Zeitabhängigkeit der Materialeigenschaften auch Aussagen zum Verhalten von dynamisch beanspruchten Dichtungen ableiten. Mit dem Ergebnis der Arbeit zum Verständnis des Verhaltens von Elastomerdichtungen bei tiefen Temperaturen wird die gezielte Beurteilung und Auswahl von sicherheitsrelevanten Dichtsystemen in Zukunft vereinfacht.
Elastomers are widely used as the main sealing materials for containers for low and intermediate level radioactive waste and as an additional component to metal seals in spent fuel and high active waste containers. The safe encapsulation of the radioactive container inventory has to be guaranteed according to regulation and appropriate guidelines for long term storage periods as well as for temperatures as low as -40°C during transport. Therefore, the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance. It is known that the material properties of elastomers are strongly temperature dependent. At low temperatures, this is caused by the rubber-glass transition (abbreviated: glass transition). During continuous cooling, the material changes from a rubber-like entropy elastic to a stiff energy elastic behaviour, which allows nearly no strain or retraction. Hence, rubbers are normally used above their glass transition, but the minimum working temperature limit is not defined precisely; this can cause problems during the above noted applications. Therefore, the lower operation temperature limit of elastomer seals must be determined in dependence of the material properties. Differential scanning calorimetry (DSC) and dynamic mechanical analysis (DMA) are combined with standardised measurements to determine the compression set according to ISO 815. To reduce the test time of the standard tests, a faster technique than normally used was developed. Additionally, the breakdown temperature of the sealing function of complete O ring seals was measured in a component test set-up to compare it with the results of the other tests. The experimental set-up is capable of measuring the leakage rate at low temperatures by the pressure rise method. A fluorocarbon rubber (FKM) was selected for this investigation as it is often used for radioactive waste containers. The materials (seals and test sheets) were purchased from a commercial seal producer.
Elastomere werden vielfach als Dichtungsmaterial für verschiedene Anwendungen eingesetzt.
In vielen Bereichen ist die Funktion der Dichtung auch bei tiefen Temperaturen erforderlich. Daher ist das Verständnis des Versagensmechanismus von großer Bedeutung.
Normalerweise werden Elastomere oberhalb ihres Glass-Gummi Umwandlungsbereiches eingesetzt, wobei die minimale Einsatztemperatur nicht exakt definiert ist. Daher ist es sinnvoll, diese untere Temperatureinsatzgrenze in Abhängigkeit von den Materialeigenschaften zu bestimmen. Hierfür werden die Ergebnisse der thermischen Analyse mit den Resultaten des Druckverformungsrests aus einer abgewandelten Messung mit der Dynamisch Mechanischen Analyse (DMA) kombiniert.
Weiterhin werden Ergebnisse von Bauteilversuchen vorgestellt und diskutiert.
Die vorgestellten Untersuchungen wurden zum großen Teil auf Untersuchungen im Rahmen der Dissertation von M. Jaunich durchgeführt.