Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste and in some countries for spent fuel transportation casks. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period.
In Germany the low and intermediate level radioactive waste is planned to be disposed in the Konrad repository in standardized containers. Many of these containers use an elastomer seal between lid and container body. Depending on the radiactive inventory and a possible containment of the waste in inner barrels and/or concrete structures, such containers may require a specific leak tightness. In such cases, specified leakage rates are shall not be exceeded by the the seals to keep potential activity releases from the inventories well below defined limits.
Generally, all waste containers have to fulfill the waste acceptance criteria for the Konrad repository as defined by the reports BfS SE-IB-29/08 and SE-IB-30/08. From these criteria several requirements for seal performance are derived. The seals have to:
- ensure full functionality until final container disposal,
- maintain its function in case of a thermal or mechanical accident,
- ensure encapsulation also at -20 °C.
This combination of requirements is challenging especially as a seal exchange, which is typical for many other applications, is hardly possible and thus a sound understanding of how to perform safety evaluation of containers is required. Therefore BAM has initiated investigations on elastomer seal behaviour. This work focuses on low temperature behaviour and sealing performance concerning static conditions as well as partial loss of compression and ageing of elastomer seals. Concerning ageing, property changes caused by long-term thermooxidative conditions as well as gamma irradiation are investigated.
This contribution presents an overview and explanation of the aims of the ongoing research and gives an update of the most relevant results.
Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste and in some countries for spent fuel transportation casks. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period.
In Germany the low and intermediate level radioactive waste is planned to be disposed in the Konrad repository in standardized containers. Many of these containers use an elastomer seal between lid and container body. Depending on the radiactive inventory and a possible containment of the waste in inner barrels and/or concrete structures, such containers may require a specific leak tightness. In such cases, specified leakage rates are shall not be exceeded by the the seals to keep potential activity releases from the inventories well below defined limits.
Generally, all waste containers have to fulfill the waste acceptance criteria for the Konrad repository as defined by the reports BfS SE-IB-29/08 and SE-IB-30/08. From these criteria several requirements for seal performance are derived. The seals have to:
- ensure full functionality until final container disposal,
- maintain its function in case of a thermal or mechanical accident,
- ensure encapsulation also at -20 °C.
This combination of requirements is challenging especially as a seal exchange, which is typical for many other applications, is hardly possible and thus a sound understanding of how to perform safety evaluation of containers is required. Therefore BAM has initiated investigations on elastomer seal behaviour. This work focuses on low temperature behaviour and sealing performance concerning static conditions as well as partial loss of compression and ageing of elastomer seals. Concerning ageing, property changes caused by long-term thermooxidative conditions as well as gamma irradiation are investigated.
This contribution presents an overview and explanation of the aims of the ongoing research and gives an update of the most relevant results.
At the Bundesanstalt für Materialforschung und -prüfung (BAM) in Division 3.4 Safety of Storage Containers, one of our tasks is to evaluate the safety of containers designed for disposal of low and intermediate radioactive waste. As such containers might be transported before and stored until disposal, safe enclosure of the radioactive inventory is important for this time span. Elastomer O-rings are widely used as barrier seals in these containers. Thus, as for many other applications, an understanding of the practical effects of ageing degradation on elastomer seals during long-term exposure is mandatory for predicting the lifetime of such components. According to a long-term test programme on three kinds of rubbers (EPDM and FKM (relevant for application), HNBR (for comparison)), over several years we have studied the degradation and the change of mechanical properties (e.g. hardness, strain at break) at four different ageing temperatures (75 °C, 100 °C, 125 °C and 150 °C) as well as the change of sealing properties. Continuous and intermittent compression stress relaxation (CSR) measurements were performed in order to investigate the respective contribution of crosslinking and chain scission to the observed degradation effects. Thus, the degradation kinetics and mechanisms could be resolved more clearly. For assessing the seal performance, compression set (CS) and leakage rate measurements were conducted. The experimental results showed that the O-rings remained leak-tight under purely static conditions even when CSR, CS and mechanical properties already indicated far advanced degradation. For this reason, a modified leakage test involving a small and rapid partial decompression of the seal was developed that enabled determining an end-of-lifetime criterion for O-rings with a safety margin for thermal shrinkage and vibrations.
Low temperature performance of rubber seals - Influence of crystallite formation on seal performance
(2018)
Rubbers are widely used as sealing materials in various applications. In many fields the function of seal materials at low temperatures is necessary. Therefore, the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance.
It is known that rubbers possess strongly temperature dependent material properties. At low temperatures high changes in the material properties are observed which can be caused by the rubber-glass transition (abbr. glass transition) or for some rubbers also by partial crystallisation at lower temperatures. During continuous cooling the material changes during rubber-glass transition from rubber-like entropy-elastic behaviour to stiff energy-elastic behaviour. In case of (thermal-) crystallisation the formed crystallites act as additional (physical) crosslinks within the material but the molecules in the amorphous phase can still behave like a rubber. Hence, rubbers are normally used above rubber-glass transition and (thermal-) crystallization temperature but the minimum working temperature limit is heavily depending on the application conditions. Therefore, the lower operation temperature limit of rubber seals is under investigation.
In the past we have investigated material properties and sealing behaviour of rubber seals at low temperatures. As the initial work was dedicated to purely static sealing conditions we started to investigate the effect of a small partial release of rubber seals at low temperatures to study the influence of dynamic events on leak tightness. In addition, other groups report on the influence of counterpart surface and adhesion.
In this contribution we focus on the difference between purely amorphous elastomers and elastomers which become partially crystalline at low temperatures. The influence of partial crystallization on the low temperature performance of rubber seals is discussed.
Elastomers show a high versatility which makes them ideal materials for sealing applications in various fields. Especially under changing application conditions the high recovery potential of this class of material is beneficial to compensate temperature or pressure fluctuation, and geometrical changes resulting from mechanical loads in e.g. accident conditions. Out of these reasons elastomers are also used in containers for low and intermediate level radioactive waste and for spent fuel transportation casks. In cask designed for low and intermediate level waste elastomer seals can act as primary seal responsible for the containment function whereas in spent fuel storage and transportation casks (dual purpose casks (DPC)) elastomer seals are used as auxiliary seals to allow leakage rate measurements of metal barrier seals. An inherent prerequisite for this kind of application is the long time-scale of operation without or with limited possibility of seal replacement. In Germany an interim storage license for DPC`s is typically issued for 40 years, a timeframe which might increase in future due to challenges of the final repository siting procedure. For low and intermediate level waste, also long time periods are required before final disposal can be achieved. Therefore, the performance of elastomer seals over extended time periods is, as for other applications, of high importance.
A typical approach to ensure long-term functionality is to perform accelerated aging tests to calculate an estimated lifetime by assuming e.g. Arrhenius like equations for the time-temperature relationship. This approach requires a suitable end of life criterion considering the application of interest. This often can represent a challenge on its own.
As BAM is involved in most of the cask licensing procedures and especially responsible for the evaluation of cask-related long-term safety issues we initiated several test programs for investigating the behavior of elastomer seals. Experiments concerning the low temperature performance down to -40°C and the influence of gamma irradiation have been started first. Currently the thermal aging behavior of elastomer seals, which is the topic of this contribution, is examined.
For our aging investigations we use a broad approach to first determine the property changes in different elastomer materials due to thermo-oxidative aging at elevated temperatures and secondly we test how the typical methods of lifetime extrapolation can be applied to these results. This approach enables us to detect and exclude undesired side effects which very often influence lifetime estimations. In this contribution, our recent results are discussed.
For many sealing applications rubbers are applied due to their special material properties and easy use. In many applications as e.g. in aviation, traffic or process technology the material can be exposed to low temperatures during operation. Therefore, it is important to know the material behaviour at those low temperatures to determine the temperature range that allows a safe operation of the seal.
In this work, we focus on the behaviour of elastomer seals at low temperatures with regard to potential decrease of leak-tightness or catastrophic seal failure of O-ring rubber seals. This is required as material properties of rubbers are strongly temperature dependent but their temperature application range is not always clearly defined.
Based on previous investigations which considered the physical material properties and the seal behaviour under purely static conditions we widen the focus on the sealing performance after a fast partial relief of compressed seals and additional materials.
For the investigations, different typical rubber seal materials were used as e.g. fluorocarbon (FKM), ethylene propylene diene (EPDM) and hydrogenated acrylonitrile-butadiene (HNBR) rubber.
The correlation of the physical material properties with seal performance is studied. This includes as well purely static sealing applications as the Performance during/after fast partial relief of seals at low temperatures.
For many sealing applications rubbers are applied due to their special material properties and easy use. In many applications as e.g. in aviation, traffic or process technology the material can be exposed to low temperatures during operation. Therefore, it is important to know the material behaviour at those low temperatures to determine the temperature range that allows a safe operation of the seal.
In this work, we focus on the behaviour of elastomer seals at low temperatures with regard to potential decrease of leak-tightness or catastrophic seal failure of O-ring rubber seals. This is required as material properties of rubbers are strongly temperature dependent but their temperature application range is not always clearly defined.
Based on previous investigations which considered the physical material properties and the seal behaviour under purely static conditions we widen the focus on the sealing performance after a fast partial relief of compressed seals and additional materials.
For the investigations, different typical rubber seal materials were used as e.g. fluorocarbon (FKM), ethylene propylene diene (EPDM) and hydrogenated acrylonitrile-butadiene (HNBR) rubber.
The correlation of the physical material properties with seal performance is studied. This includes as well purely static sealing applications as the performance during/after fast partial relief of seals at low temperatures.
At BAM, which is the federal institute for materials research and testing in Germany, it is one of our tasks to evaluate the safety of casks designed for transport and/or storage of radioactive material. This includes assessment of elastomeric seals applied in the containers. Besides examining the low-temperature behaviour and irradiation effects of elastomeric seals, it is our goal to evaluate the service lifetime of the seals with regard to the requirements for long-term safety (40 years and more) of the containers. Therefore, we started an accelerated ageing programme with selected rubbers often used for seals (HNBR, EPDM and FKM) which are aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) up to 1 year. In order to assess sealability, O-rings are aged in compression by 25 % (corresponding to the compression during service) between plates as well as in flanges that allow leakage rate measurements. For comparison, uncompressed O-rings are aged as well. Further methods characterising seal performance are compression stress relaxation (CSR) reflecting the loss of sealing force of a compressed seal over time, and compression set (CS) which represents the recovery behaviour of a seal after release from compression. Additionally, hardness is measured for information about the change of mechanical properties. The experimental results indicate that while hardness, CSR and CS show considerable degradation effects, the leakage rate stays constant or even decreases until shrinkage and the loss of resilience of the aged seal leads to the formation of a leakage path. This indicates that static leakage rate, which is the only available direct seal performance criterion, has only limited sensitivity for the degradation of the seal material.
For many sealing applications low temperature performance is required. The overall understanding of the relevant influences on low temperature performance of rubber seals are summarized and the currently running investigations described.
The correlation of the physical material properties with seal performance is studied. This includes as well purely static sealing applications as the performance during/after fast partial relief of seals at low temperatures.