The friction at the interfaces between pieces of wood and steel is of crucial importance for the impact and energy absorption in impact limiters of transport casks for radioactive material. Here, the friction coefficient for the combinations wood-wood and wood-steel was measured in the temperature range between -40°C and 90°C. Results show decreasing friction with increasing temperature, ranging from 0.43 at -40°C to 0.22 for 90°C for wood-steel combinations and from 0.3 at -40°C to 0.24 at 90°C for a wood-wood combination.
Friction coefficients for wood-wood and wood-steel interfaces in impact limiters for transport casks
(2023)
Wood is widely used in impact limiters of transport casks for radioactive material. Encapsulated by an outer and inner steel structure, spruce wood is often applied in layers of alternating direction. The friction at the interfaces between these layers is of crucial importance for the impact and energy absorption e.g., at an accidental impact of a cask against a hard target. In order to get detailed information for corresponding numerical calculations, in this study the friction coefficient for the combinations wood-wood and wood-steel was measured in the temperature range between -40°C and 90°C according to the relevant stress conditions for such casks. Results show decreasing friction with increasing temperature, ranging from 0.43 at -40°C to 0.22 for 90°C for wood-steel combinations and from 0.3 at -40°C to 0.24 at 90°C to for a wood-wood combination.
Friction coefficients for wood-wood and wood-steel interfaces in impact limiters for transport casks
(2023)
Wood is widely used in impact limiters of transport casks for radioactive material. Encapsulated by an outer and inner steel structure, spruce wood is often applied in layers of alternating direction. The friction at the interfaces between these layers is of crucial importance for the impact and energy absorption e.g., at an accidental impact of a cask against a hard target. In order to get detailed information for corresponding numerical calculations, in this study the friction coefficient for the combinations wood-wood and wood-steel was measured in the temperature range between -40°C and 90°C according to the relevant stress conditions for such casks. Results show decreasing friction with increasing temperature, ranging from 0.43 at -40°C to 0.22 for 90°C for wood-steel combinations and from 0.3 at -40°C to 0.24 at 90°C to for a wood-wood combination.
Wood is widely used in impact limiters of Transport casks for radioactive material. Encapsulated by an outer and inner Steel structure, spruce wood is offen applied in layers of altemating direction. The friction at the interfaces between these layers is of crucial importance for the impact and energy absorption e.g., at an accidental impact of a cask against a hard component.
In order to get detailed Information for corresponding numerical calculations, in this study the friction coefficient for the combinations wood-wood and wood-steel was measured in the temperature ränge between -40 °C and 90 °C according to the relevant stress conditions for such casks. Results show decreasing friction with increasing temperature, ranging from 0.43 at -40 °C to 0.22 for 90 °C for wood-steel combinations and from 0.3 at -40 °C to 0.24 at 90 °C to for a wood-wood combination.