Filtern
Erscheinungsjahr
Dokumenttyp
- Beitrag zu einem Tagungsband (34)
- Zeitschriftenartikel (20)
- Vortrag (8)
- Posterpräsentation (4)
- Beitrag zu einem Sammelband (1)
- Amtliche Bekanntmachung (1)
Sprache
- Englisch (68) (entfernen)
Schlagworte
- Radioactive material (15)
- Impact limiter (13)
- Transport (13)
- Wood (11)
- FEM (6)
- Package (6)
- Consequences (4)
- Drop test (4)
- Friction (4)
- Transport cask (4)
Organisationseinheit der BAM
- 3 Gefahrgutumschließungen; Energiespeicher (26)
- 3.3 Sicherheit von Transportbehältern (24)
- 2 Prozess- und Anlagensicherheit (4)
- 2.1 Sicherheit von Energieträgern (4)
- 8 Zerstörungsfreie Prüfung (4)
- 8.1 Sensorik, mess- und prüftechnische Verfahren (4)
- 9 Komponentensicherheit (4)
- 9.5 Tribologie und Verschleißschutz (4)
- 2.2 Prozesssimulation (2)
- 3.0 Abteilungsleitung und andere (2)
Eingeladener Vortrag
- nein (8)
Dynamic and quasi-static FE calculation of impact from 9 metre drop of spent fuel transport cask
(2009)
The drop from 9 m height onto a rigid target is one of the required proofs of safety for packages of radioactive materials. Direct dynamic finite element method (FEM) calculations and combined two step analytical quasi-static finite element (FE) calculations are both applied for the simulation of a 9 m drop test. This paper gives a comparative example of both approaches for the 9 m side drop simulation of the spent fuel transport cask with wood filled impact limiter. The model for dynamic FEM consists of cask body and impact limiter. Detailed material properties and geometry descriptions from each component of the impact limiter are required. The results (stress fields in the cask body) are obtained directly from the calculation. The combined method provides as intermediate results the force-deformation characteristic of impact limiter. The maximum impact limiter force determined by the law of energy conservation during the drop is then - in a second step - applied on the cask body in a quasi-static FE model in order to calculate the stresses. In this paper, the rigid body deceleration and the maximum stress in the middle of the cask body are used for the comparison between the dynamic FEM and the combined method. Similar maximum rigid body deceleration-time curves were obtained by both methods for the horizontal 9 m free fall. Concerning the stress in the cask body the dynamic FEM results oscillate about values calculated by the combined quasi-static approach. If the combined quasi-static approach is used in the safety assessment of a cask, a suitable factor has to be applied on its results to take into account the additional dynamic effects.
Diffusion of Cr, Fe, and Ti ions from Ni-base alloy inconel-718 into a transition alumina coating
(2012)
Heat treating metals at high temperatures trigger diffusion processes which may lead to the formation of oxide layers. In this work the diffusion of Cr, Fe and Ti into an alumina coating applied to Inconel-718 is being investigated. Mass gain measurements, UV–vis spectroscopy and transmission electron microscopy were applied in order to study the evolution of the diffusion process. It was found that mainly Cr as well as minor amounts of Fe and Ti are being incorporated into the alumina coating upon prolonged heat treatment at 700 °C. It could be shown that alumina coatings being void of Cr have the same oxidation related mass gain as uncoated samples. However, incorporation of Cr into the alumina coating decreased their mass gain below that of uncoated substrates forming a Cr oxide scale only.
This paper demonstrates exemplarily how numerical and experimental approaches can be combined reasonably in mechanical assessment of package integrity according to the IAEA regulations. The paper also concentrates on the question about how static mechanical approaches can be applied, and what their problems are in relation to dynamic calculation approaches. Under defined impact tests, which represent accident transport conditions, the package has to withstand impact loading, e.g. resulting from a 9 m free drop onto an unyielding target in sequence with a 1 m puncture drop test. Owing to the local character of the interaction between the puncture bar and the cask body, it is possible to develop a dynamic numerical model for the 1 m puncture drop which allows an appropriate simulation of the interaction area. Results from existing experimental drop tests with prototype or small scale cask models can be used for verification and validation of applied analysis codes and models. The link between analysis and experimental drop testing is described exemplarily by considering a regulatory 1 m puncture bar drop test onto the cask body of a recently approved German high level waste transport package. For the 9 m drop test of the package, it is difficult to develop a dynamic numerical model of the package due to the complexity of the interaction between cask body, impact limiters and unyielding target. Dynamic calculations require an extensive verification with experimental results. The simulation of a 9 m drop of a package with impact limiters is thereby often more complex than the simulation of a 1 m puncture drop onto the cask body. A different approximation method can be applied for the consideration of dynamic effects on the impact loading of the package. In a first step, maximum impact force and rigid body deceleration of the cask body during the impact process can be calculated with simplified numerical tools. This rigid body deceleration can subsequently be applied on a verified static numerical model. Dynamic effects, which cannot be covered by the static numerical analysis, have therefore to be considered by using an additional dynamic factor. The paper describes this approach exemplarily for a 9 m horizontal drop of a typical spent fuel cask design.
The friction at the interfaces between pieces of wood and steel is of crucial importance for the impact and energy absorption in impact limiters of transport casks for radioactive material. Here, the friction coefficient for the combinations wood-wood and wood-steel was measured in the temperature range between -40°C and 90°C. Results show decreasing friction with increasing temperature, ranging from 0.43 at -40°C to 0.22 for 90°C for wood-steel combinations and from 0.3 at -40°C to 0.24 at 90°C for a wood-wood combination.
With integration of the new para 613A into SSR-6 [1] the consideration of ageing mechanisms is now obligatory for the design of packages and their approval. In addition, para 809(f) of SSR-6 [1] requires consideration of the effects of storage on ageing mechanisms, safety analyses and operation and maintenance instructions.
German competent authorities Bundesanstalt für Materialforschung und -prüfung (BAM) and Bundesamt für die Sicherheit der nuklearen Entsorgung (BASE) are considering the aspect of ageing in approval procedures. Ageing assessment is mainly focused on dual purpose casks (DPC) package designs which are long-term stored in interim storage facilities. For these package designs, the evaluation of ageing management is now mandatory for the maintenance of the package design approvals with a validity period of 5 years and beyond. The ageing management includes amongst others a gap analysis, the assessment of ageing effects and operational experiences during operation and interim storage.
BAM works on the compilation of a guideline for implementation of paras 613A, 809(f) and 809(k) for packages requiring competent authority approval at the application procedure in Germany. The paper describes essential items of ageing mechanisms and will give a foresight to the ageing management evaluation by BAM.
Transport packages shall satisfy various safety criteria regarding mechanical, thermal and radiation phenomena. Typical requirements focusing mechanical aspects are usually drop tests in accordance with IAEA regulations. The drop tests are usually carried out experimentally and, as an additional measure, finite element analyses (FEA) are performed. A specific part of the investigations presented is the evaluation of the welding seam connecting cask shell and cask bottom. Experimental results and FEA are presented and compared. The evaluation of the welding seam performed includes a variety of aspects. In addition to the experimental and analytical stresses determined, different standards are used to investigate a possible crack initiation. Several destructive and non-destructive tests are performed for quality assurance in the manufacturing process as well as for different input parameters. The necessary monitoring and non-destructive measurement methods to define the boundary conditions of the standards are introduced. Taking into account all required parameters, the welding seam is examined and evaluated using the failure assessment diagrams (FAD) of the respective standards. It can be shown under the given boundary conditions that considering the experimental data, the welding seam is in the context of crack initiation below the enveloping curve in the acceptable region. More critical drop tests to be conducted are proposed and need to be investigated in future work.
TN®24 E, a new package design, was developed and applied for by Areva TN for German transport approval certificate. The certificate was issued by BfS, Federal Office for Radiation Protection, on 24th of July 2013. The package is designed as a dual purpose cask for transport and storage of up to 21 PWR spent fuel assemblies from German NPPs. BAM is the German competent authority responsible for the design assessment of RAM packages regarding mechanical and thermal safety cases, activity release analysis and all issues of quality assurance during manufacturing and operation of packages. Certain assessment experiences as well as new developments resulting from the BAM TN®24E approval procedure are presented. The mechanical safety case of the TN®24E is based mainly on finite element calculations, which were verified by the TN®81 1/3 scale drop test program performed at BAM. Thermal analyses rely upon calculations, while the activity release criterion is based upon leakage rate results of TN®81 drop tests. The BAM-GGR 012 guideline for the analysis of bolted lid and trunnion systems has been fully implemented. Due to requirements by BAM, AREVA TN developed a new assessment strategy for fracture mechanical evaluation of welding seams. The material qualification and documentation is also an important aspect of BAM assessment; the qualification of borated aluminum basket material, the determination of strength values for thermal aged hardened aluminum alloys for the basket or consideration of high burn-up fuel assemblies are remarkable issues in this context. In addition, the consideration of the material compatibility, especially taking into account a transport after 40 years of dry interim storage in German facilities, has gained significant importance in the licensing process of the TN®24E. Next to obvious mechanical issues such as the assessment of shell ovalization under 9 m drop test scenario and its impact on basket load, thermo-mechanical interactions had to be addressed in the safety case. Due to BAM requirements, AREVA TN performed a full thermo-mechanical analysis of the cask behavior under fire test conditions.
Packages for the transport of SNF and HLW are usually equipped with impact limiters to reduce the loads that result from the regulatory 9 m drop test. A common impact limiter design in Germany is a welded steel sheet structure filled with wood. The material wood is the main energy absorber, while the steel sheet provides the integrity of the impact limiter. The IAEA allows mechanical safety cases of transport packages to be carried out computationally, as long as the models used are reliable. In this context, a Finite Element (FE) modeling approach for wood and its application to impact limiters in the calculation of a 9 m drop test is presented.
A user material model for wood was developed for the dynamic FE-Code LS-DYNA. Its features are based on a series of crush tests with spruce wood specimens. The model considers wood as a material with transversely isotropic properties, i.e. in the directions parallel and perpendicular to the fiber. The plastic material behavior depends on the state of stress. This has shown to be important to account for the lateral constraint of wood in impact limiters resulting from steel sheet encapsulation. Lateral constraint or respectively, a multiaxial stress state, increases the compression strength level of wood, limits the softening effect and increases the hardening effect. Lateral constraint also increases volumetric and reduces deviatoric deformation. The wood material model considers various hardening and softening characteristics via input flow curves. It considers effects of temperature and strain rate on strength as well. The development of a multi-surface yield criterion and a plastic potential that enables the user input of plastic Poisson's ratios were the challenges during the development of material model.
A dynamic FE calculation of a horizontal drop test with an 18,000 kg test package was performed. The wood material model was used to model the wooden impact limiter inlays. The impact limiter deformation and the package deceleration were compared to the experimental drop test results to rate the performance of the wood material model.
Impact limiting components of packages for the transport of radioactivematerials are often designed as wood filled steel constructions. Wood absorbs major part of the impact energy in order to minimise the impact load acting upon the containment. Dynamic impact experiments with wood filled impact limiters showed different crushing mechanisms for axially loaded wood depending on their lateral constraint. Tests on spruce wood samples (Picea abies) were performed in order to clarify the influence of strain rate from static to 30 s-1 on a) compression strength, b) stress at a global strain level of 50%, and c) energy absorption capacity at 50% deformation, including statistical evaluation of the results. Results were as follows: strain rate increase led to significantly higher compression strength, stress and strain energy at a strain level of 50%. Lateral strain restriction had no effect on compression strength; it had a significant effect on stress and strain energy at strain level of 50%. Therefore, the definition of a general yield curve for wood under large deformations is not possible, the yield curve has to be chosen taking into account lateral constraints.
BAM as competent authority regarding assessment of mechanical and thermal design, activity release and quality assurance aspects of SNF and HLW transport packages developed a thesaurus of experience feedback topics from recent approval procedures. The list is structured according to the European PDSR guide. It involves issues, which from BAM point of view, needed clarification during last package design assessment procedures. The list contains issues from operation (e.g. deactivation of handling lugs not intended for package handling), maintenance (e.g. leak tightness of impact limiting devices) to technical assessment (e.g. formation of hydrogen by radiolysis and its impact on pressure and ignitability, consideration of ageing mechanisms, thermo-mechanical assessment, impact of gaps between content and flask, spent fuel behaviour) as well as to general and specific safety analysis report requirements (e.g. report structure and required data).
BAM as competent authority regarding assessment of mechanical and thermal design, activity release and quality assurance aspects of SNF and HLW transport packages developed a thesaurus of experience feedback topics from recent approval procedures. The list is structured according to the European PDSR guide. It involves issues, which from BAM point of view, needed clarification during last package design assessment procedures. The list contains issues from operation (e.g. deactivation of handling lugs not intended for package handling), maintenance (e.g. leak tightness of impact limiting devices) to technical assessment (e.g. formation of hydrogen by radiolysis and its impact on pressure and ignitability, consideration of ageing mechanisms, thermo-mechanical assessment, impact of gaps between content and flask, spent fuel behaviour) as well as to general and specific safety analysis report requirements (e.g. report structure and required data).
BAM as competent authority regarding assessment of mechanical and thermal design, activity release and quality assurance measures of Type-B(U) transport packages developed a thesaurus of experience feedback topics from recent assessment procedures. The list is structured according to the European PDSR guide. It involves issues, which from BAM's point of view, needed clarification during the last package design assessment procedures. The list contains issues from Operation (e.g. deactivation of handling lugs not intended for package handling), maintenance (e.g. leak tightness of impact limiting devices) to technical assessment (e.g. formation of hydrogen by radiolysis and its impact on pressure and ignitability, consideration of ageing mechanisms, thermo-mechanical assessment, impact of gaps between content and flask) as well as to general and specific safety analysis report requirements (e.g. report structure and required data).
Typical transport packages used in Germany are equipped with encapsulated wooden impact limiting devices. We would like to present the current status regarding the development of a Finite Element (FE) material model for the crush of wood for the FE-code LS-DYNA. The crush of is a phenomenon governed by macroscopic fracture. Here, we would like to reproduce fracture and failure mechanisms over the continuous volume. In a first step we altered an existing LS-DYNA material model for foams, which considers an ellipse shaped yield surface. For the use for longitudinal compression of wood, we modified the existing material model to consider the deviatoric strain for the evolution of the yield surface as well. This is in accordance with the results of crush tests with spruce wood specimens, where the crushing deformation was rather deviatoric for uniaxial stress states and rather volumetric for multiaxial stress states We rate the basic idea of this approach to be reasonable, though other problems exist regarding the shape of the yield surface and the assumption of isotropic material properties. Therefore we developed a new transversal isotropic material model with two main directions, which considers different yield curves according to the multiaxiality of the stress state via a multi-surface yield criterion and a non-associated flow rule. The results show the ability to reproduce the basic strength characteristics of spruce wood. Nevertheless, problems with regularization etc. show that additional investigations are necessary.
Typical transport packages used in Germany are equipped with encapsulated wooden impact limiting devices. We would like to present the current status regarding the development of a Finite Element (FE) material model for the crush of wood for the FE-code LS-DYNA. The crush of is a phenomenon governed by macroscopic fracture. Here, we would like to reproduce fracture and failure mechanisms over the continuous volume. In a first step we altered an existing LS-DYNA material model for foams, which considers an ellipse shaped yield surface. For the use for longitudinal compression of wood, we modified the existing material model to consider the deviatoric strain for the evolution of the yield surface as well. This is in accordance with the results of crush tests with spruce wood specimens, where the crushing deformation was rather deviatoric for uniaxial stress states and rather volumetric for multiaxial stress states We rate the basic idea of this approach to be reasonable, though other problems exist regarding the shape of the yield surface and the assumption of isotropic material properties. Therefore we developed a new transversal isotropic material model with two main directions, which considers different yield curves according to the multiaxiality of the stress state via a multi-surface yield criterion and a non-associated flow rule. The results show the ability to reproduce the basic strength characteristics of spruce wood. Nevertheless, problems with regularization etc. show that additional investigations are necessary.
Assessment of Quality Management for Transport Packages not requiring Authority Design Approval
(2018)
The poster presents the german approach for the assessment of quality management systems for transport packages for radioactive material not requiring authority design approval. As legal basis the IAEA regulations, the ADR as well as the GGVSEB are highlighted and examples for these transport packages are given. The GGR 016 is mentioned, main duties and responsibilities as well as the manufacturing and quality surveillance system are described.