Filtern
Dokumenttyp
Schlagworte
- Automobilindustrie (2)
- Feinblech (2)
- Kennwerte (2)
- Automobilbau (1)
- Automotive engineering (1)
- Chalcopyrite-type (1)
- Chemical mapping (1)
- Comparison (1)
- Cu(In,Ga)Se2 (1)
- Cyclic properties (1)
- Dehnungswöhlerlinie (1)
- Depth profiling (1)
- Druckmessgerät (1)
- Elasto-plastic material behaviour (1)
- Elasto-plastisches Werkstoffverhalten (1)
- Elemental distributions (1)
- FE-Simulation (1)
- FEM-Simulation (1)
- Karosseriestähle (1)
- Lebensdauerberechnung (1)
- Monotonic and cyclic stress-strain curve (1)
- Sicherheit (1)
- Solar cells (1)
- Strain-life curve (1)
- Strukturen (1)
- Technical crack (1)
- Technischer Anriss (1)
- Thin films (1)
- Thin steel sheets (1)
- Zyklische Kennwerte (1)
- Zyklische Werkstoffkennwerte (1)
- Zügige und zyklische Spannung-Dehnung-Kurve (1)
The present work shows results on elemental distribution analyses in Cu(In,Ga)Se2 thin films for solar cells performed by use of wavelength-dispersive and energy-dispersive X-ray spectrometry (EDX) in a scanning electron microscope, EDX in a transmission electron microscope, X-ray photoelectron, angle-dependent soft X-ray emission, secondary ion-mass (SIMS), time-of-flight SIMS, sputtered neutral mass, glow-discharge optical emission and glow-discharge mass, Auger electron, and Rutherford backscattering spectrometry, by use of scanning Auger electron microscopy, Raman depth profiling, and Raman mapping, as well as by use of elastic recoil detection analysis, grazing-incidence X-ray and electron backscatter diffraction, and grazing-incidence X-ray fluorescence analysis. The Cu(In,Ga)Se2 thin films used for the present comparison were produced during the same identical deposition run and exhibit thicknesses of about 2 µm. The analysis techniques were compared with respect to their spatial and depth resolutions, measuring speeds, availabilities, and detection limits.
Im Rahmen eines gemeinschaftlichen Projektes der Stahl- und Automobilindustrie wurden für 17 Stahlfeinbleche des Automobilbaus in verschiedenen Anlieferungs- und Verformungszuständen unter -40°C, Raumtemperatur und +100°C mit 37 Versuchsreihen Anrisswöhlerlinien und zügige bzw. zyklische Spannung-Dehnung-Kurven bestimmt. Sämtliche Versuchspunkte, Hysteresen und ermittelte zyklische Kennwerte liegen in einer Datenbank vor. Eine Korrelationen zwischen den Kennwerten aus dem Zugversuch und den Kennwerten aus den zyklischen, dehnungsgeregelten Versuchen ist grundsätzlich möglich.