This study compares the mercury distribution in the vapor phase, the phosphor powder and the glass matrix of new and spent fluorescent lamps. The spent fluorescent lamps were obtained at the collection yards of a public waste management company in Hamburg, Germany. An innovative systematic sampling method is utilized to collect six spent and eight corresponding new, off-the-shelf fluorescent lamp samples. The efficiency of several acid digestion methods for the determination of the elemental composition was studied and elemental mass fractions of K, Na, Y, Ca, Ba, Eu, Al, Pb, Mg, Hg, and P were measured. The study also finds aqua regia to be the best reagent for acid digestion. However, no significant difference in mercury distribution was found in the different phases of the new and spent fluorescent lamps.
Recovery of rare earth elements - optimized elemental analysis of fluorescent lamp shredder waste
(2016)
Rare earth elements (REE) are a crucial component of fluorescence lamps. Several procedures have been developed to recovery these technological important elements. Nevertheless, actual REE recycling from fluorescence lamps is scarce so far (recovery rate of less than 1 %), with current recycling approaches concentrating on glass recovery. Since most recycling processes include several, also wet-chemical steps, a complete knowledge of the actual elemental composition of the respective mass flows is necessary for an efficient REE recovery. We tested seven different reagent mixtures for microwave-assisted digestion of fluorescent lamp shredder, including HF, HClO4, and H2O2. We determined the concentrations of 25 of the most relevant rare earth and other trace elements in the respective dilutions. Two independent digestions, one a mixture of perchlorid/nitric/hydrofluoric acid and the other aqua regia, showed the highest concentrations of 23 of these elements, excluding only Sn and Tb. The REE concentrations in the tested lamp shredder sample (stated in g/kg) were 10.2 (Y), 12.1 (La), 7.77 (Ce), 6.91 (Eu), 1.90 (Gd), and 4.11 (Tb).
Fluorescence lamps contain considerable amounts of rare earth elements (REE). Several recycling procedures for REE recovery from spent lamps have been established. However, despite their economic importance, the respective recycling is scarce so far, with an REE recovery rate of less than 1%. A reliable analysis of REE and other relevant metals like Yttrium is crucial for a thorough and complete recovery process. This applies both to the solid matter and aqueous phase, since most of the recycling processes include wet-chemical steps. We tested seven different reagent mixtures for microwave-assisted digestion of fluorescent lamp shredder, including hydrofluoric acid, perchloric acid, and hydrogen peroxide. We determined the concentrations of 25 of the most relevant rare earth and other trace elements (Al, P, Ti, V, Cr, Fe, Ni, Cu, Ga, Ge, As, Y, Ag, Cd, Sn, Sb, La, Ce, Eu, Gd, Tb, W, Au, Hg, and Pb) in the respective dilutions. Two independent digestions, one a mixture of perchlorid/nitric/hydrofluoric acid and the other aqua regia, showed the highest concentrations of 23 of these elements, excluding only Sn and Tb. The REE concentrations in the tested lamp shredder sample (stated in g/kg) were 10.2 (Y), 12.1 (La), 7.77 (Ce), 6.91 (Eu), 1.90 (Gd), and 4.11 (Tb).
This work is aimed at exploring the recovery of heavy metals from the fine fraction of solid waste incineration bottom ash.
For this study, wet-discharged bottom ash fine-fraction samples from full-scale treatment plants in Germany and Sweden were analyzed. The potential for the recovery of heavy metal compounds was investigated through wet density-separation with a shaking table. The feed materials were processed without any pre-treatment and the optimum processing conditions were determined by means of design of experiments. Tilt angle and stroke frequency were identified as the most relevant parameters, and the optimum settings were − 7.5° and 266 rpm, respectively. The obtained balanced copper enrichments (and yields) were 4.4 (41%), 6.2 (28%) and 2.4 (23%). A maximum copper enrichment of 14.5 with 2% yield was achieved, providing a concentrate containing 35.9 wt.% relevant heavy metal elements. This included 26.3 wt.% iron, 4.3 wt.% zinc and 3.8 wt.% copper. In conclusion, density separation with shaking tables can recover heavy metals from bottom ash fine fractions. Medium levels of heavy metal enrichment (e.g., for Cu 2.7–4.4) and yield (Cu: 26–41%) can be reached simultaneously.
However, the separation performance also depends on the individual bottom ash sample.
In 2018, the production of Municipal SolidWaste (MSW) in EU-28 reached 250.6 Mt, with the adoption of different management strategies, involving recycling (48 wt %), incineration and thermal valorization (29 wt %) and landfilling (23 wt %). This work was based on the analysis of the baseline situation of MSW management in EU-28 in 2018, considering its progress in 2008–2018, and discussed the possible improvement perspectives based on a framework involving incineration and recycling as the only possible alternatives, specifically evaluating the capability of already-existing incineration plants to fulfill the EU needs in the proposed framework. The results of the assessment showed two main crucial issues that could play a pivotal role in the achievement of Circular Economy action plan targets: the need to increase the recycling quotas for specific MSW fractions through the separate collection, and therefore the improvement of definite treatment process chains; the optimization of the recovery of secondary raw materials from incineration bottom ash, involving the Recycling of ferrous and nonferrous metals and the mineral fraction. Both issues need to find an extensive application across all member states to decrease the actual differences in the adoption of sustainable MSW management options.
The main obstacle to bottom ash (BA) being used as a recycling aggregate is the content of salts and potential toxic elements (PTEs), concentrated in a layer that coats BA particles. This work presents a dry treatment for the removal of salts and PTEs from BA particles. Two pilotscale abrasion units (with/without the removal of the fine particles) were fed with different BA samples. The performance of the abrasion tests was assessed through the analyses of particle size and moisture, and that of the column leaching tests at solid-to-liquid ratios between 0.3 and 4.
The results were: the particle-size distribution of the treated materials was homogeneous (25 wt % had dimensions <6.3 mm) and their moisture halved, as well as the electrical conductivity of the leachates. A significant decrease was observed in the leachates of the treated BA for sulphates (44%), chlorides (26%), and PTEs (53% Cr, 60% Cu and 8% Mo). The statistical analysis revealed good correlations between chloride and sulphate concentrations in the leachates with Ba, Cu, Mo, and Sr, illustrating the consistent behavior of the major and minor components of the layer surrounding BA particles. In conclusion, the tested process could be considered as promising for the improvement of BA valorization.
The main obstacle to bottom ash (BA) being used as a recycling aggregate is the content of salts and potential toxic elements (PTEs), concentrated in a layer that coats BA particles. This work presents a dry treatment for the removal of salts and PTEs from BA particles. Two pilotscale abrasion units (with/without the removal of the fine particles) were fed with different BA samples. The performance of the abrasion tests was assessed through the analyses of particle size and moisture, and that of the column leaching tests at solid-to-liquid ratios between 0.3 and 4. The results were: the particle-size distribution of the treated materials was homogeneous (25 wt % had dimensions <6.3 mm) and their moisture halved, as well as the electrical conductivity of the leachates. A significant decrease was observed in the leachates of the treated BA for sulphates (44%),
chlorides (26%), and PTEs (53% Cr, 60% Cu and 8% Mo). The statistical analysis revealed good correlations between chloride and sulphate concentrations in the leachates with Ba, Cu, Mo, and Sr, illustrating the consistent behavior of the major and minor components of the layer surrounding BA particles. In conclusion, the tested process could be considered as promising for the improvement of BA valorization.