Filtern
Erscheinungsjahr
- 2013 (9) (entfernen)
Dokumenttyp
Schlagworte
- Rheology (4)
- Adsorption (2)
- Polycarboxylate ether (2)
- Superplasticizers (2)
- Admixtures (1)
- Baustoffe (1)
- Betontechnologie (1)
- Cement (1)
- Cement hydration (1)
- Chloride (1)
Waste sludge, a solid recovered from wastewater of photovoltaic-industries, composes of agglomerates of nano-particles like SiO2 and CaCO3. This sludge deflocculates in aqueous solutions into nano-particles smaller than 1 µm. Thus, this sludge constitutes a potentially hazardous waste when it is improperly disposed. Due to its high content of amorphous SiO2, this sludge has a potential use as supplementary cementitious material (SCM) in concrete. In this study the main properties of three different samples of photovoltaic's silica-rich waste sludge (nSS) were physically and chemically characterized. The characterization techniques included: scanning electron microscopy (SEM), X-ray energy dispersive spectroscopy (EDS), X-ray diffraction (XRD), nitrogen physical adsorption isotherm (BET method), density by Helium pycnometry, particle size distribution determined by laser light scattering (LLS) and zeta-potential measurements by dynamic light scattering (DLS). In addition, a dispersability study was performed to design stable slurries to be used as liquid additives for the concrete production on site. The effects on the hydration kinetics of cement pastes by the incorporation of nSS in the designed slurries were determined using an isothermal calorimeter. A compressive strength test of standard mortars with 7% of cement replacement was performed to determine the pozzolanic activity of the waste nano-silica sludge. Finally, the hardened system was fully characterized to determine the phase composition. The results demonstrate that the nSS can be utilized as SCM to replace portion of cement in mortars, thereby decreasing the CO2 footprint and the environmental impact of concrete.
Innovative admixture technology has significantly widened up the ränge of possibilities of concrete engineers. For many decades the water to cement ratio (w/c) was the major influencing factor for the performance of concrete. Due to the need to adjust a consistency, which still allowed reasonable workability, the w/c was typically significantly higher than technologically reasonable. Rheology modifying admixtures Support adjusting the concrete consistency largely independent of the w/c. It was only after the invention of the first superplasticizers that modern concrete technology significantly evolved in terms of flowability, strength, and durability, and only due to the steady evolution of the technology modern innovations, such as Self-Compacting Concrete, Ultra-High-Performance Concrete, or Engineered Cementitious Composites were made possible. Today’s superplasticizers are extremely versatile and can be adjusted to individual technologicalspecifications. However, the other side of the coin of versatility is that cementitious Systems incorporating superplasticizers have become more sensitive against environmental influences, such as the environmental temperature, which may cause unwanted effects or demand for supplementary admixture use such as stabilizing admixtures. Hence, concrete mixture composition with admixtures demands for a high level of expertise and offen there is lack of awareness about the mode of Operation of rheology modifying admixtures among concrete technologists. The paper gives a comprehensive overview about rheology modifying admixtures such as superplasticizers or stabilizing agents, and how they can be used depending upon the application in the most favourable way. Based on experiences with the sub-Saharan African concreting boundary conditions, which exhibit many challenges in terms of environmental boundary conditions and construction site logistics, conclusions are finally drawn, how admixtures can be used in the most beneficial way to improve the concrete casting Situation.
Innovative admixture technology has significantly widened up the ränge of possibilities of concrete engineers. For many decades the water to cement ratio (w/c) was the major influencing factor for the performance of concrete. Due to the need to adjust a consistency, which still allowed reasonable workability, the w/c was typically significantly higher than technologically reasonable. Rheology modifying admixtures Support adjusting the concrete consistency largely independent of the w/c. It was only after the invention of the first superplasticizers that modern concrete technology significantly evolved in terms of flowability, strength, and durability, and only due to the steady evolution of the technology modern innovations, such as Self-Compacting Concrete, Ultra-High-Performance Concrete, or Engineered Cementitious Composites were made possible. Today’s superplasticizers are extremely versatile and can be adjusted to individual technological specifications. However, the other side of the coin of versatility is that cementitious Systems incorporating superplasticizers have become more sensitive against environmental influences, such as the environmental temperature, which may cause unwanted effects or demand for supplementary admixture use such as stabilizing admixtures. Hence, concrete mixture composition with admixtures demands for a high level of expertise and offen there is lack of awareness about the mode of Operation of rheology modifying admixtures among concrete technologists. The paper gives a comprehensive overview about rheology modifying admixtures such as superplasticizers or stabilizing agents, and how they can be used depending upon the application in the most favourable way. Based on experiences with the sub-Saharan African concreting boundary conditions, which exhibit many challenges in terms of environmental boundary conditions and construction site logistics, conclusions are finally drawn, how admixtures can be used in the most beneficial way to improve the concrete casting Situation.
ln order to observe the influence of stabilising agents (STA) based on starch and diutan gum, rheometric experiments and setting tests were conducted on cement pastes with and without PCE superpiasticizers. The results show that with regard to yield stress both STAs show differing behaviours in Systems without PCE. In presence of PCE, yield stress infiuences of the STAs retreat into the background. The Vicat results exhibit that STAs can reduce the retard ing effect of PCE.
The high demand for sustainable and durable building materials requires profound knowledge on the material properties. In this respect, the phenomena occurring at nano-level are of crucial importance for the design of new building materials. Therefore, all around the world, increasing amounts of funding are being directed to research projects dealing with material properties on nano-level, which is claimed to have tremendous potential for the future. One of the most referred to and used cementitious nano-material is amorphous silica with a particle size in the nano-range, even though its application and effects on concrete have not been fully understood yet. Olivine (Mg,Fe)2Si04 is the fastest weathering siiicate mineral dissolving easily in acid. Düring dissolution in acid the metallic ions (Mg2+,Fe2+) are replaced by H+, yielding Si(OH)4 monomers and metallic ions in solution. After cleaning treatments an amorphous nano-silica is obtained. The produced olivine nano-silica (OnS) has a specific surface area between 100 and 400 m2/g, the size of the primary particles, which are agglomerated in Clusters, ranges from 10 to 25 nm and the impurity content is below 5 % IV. Literature related with the application of OnS in cement based materials is scarce; only one research work performed by Justnes and Ostnor 121 is available. Thus, the effect of adding OnS in cement based Systems has been not studied. Based on this, the present research aims on elucidating the effects of OnS in the fresh and hardened state of cement pastes and mortars.
Polysaccharides provide high potential to be used as rheology modifying admixtures in mineral binder systems for the construction industry such as concrete or mortar. Since superplasticizers have become state of technology, today, concrete is more and more adjusted to flowable consistencies. This often goes along with the risk of segregation, which can be effectively avoided by adding stabilising agents supplementary to superplasticizers. Stabilising agents are typically based on polysaccharides such as cellulose, sphingan gum, or starch. Starch clearly distinguishes in its effect on rheology from other polysaccharides, mainly due to the strong influence of amylopectin on the dispersion and stabilisation of particles. Based on rheometric investigations on cementitious and limestone based dispersions with different volumetric water to solid ratios, the mode of operation of modified potato starch is explained in comparison to a sphingan gum. It is shown that the stabilising effect of starch in a coarsely dispersed system is mainly depending upon the water to solid ratio and that above a certain particle volume threshold starch mainly affects the dynamic yield stress of dispersions, while plastic viscosity is affected only to a minor degree. Sphingans operate more independent of the particle volume in a coarsely dispersed system and show significantly higher effect on the plastic viscosity than on the yield stress. In systems incorporating superplasticizers, influences of both stabilising agents on yield stress retreat into the background, while both observed polysaccharides maintain their effect on the plastic viscosity.
Todays superplasticizers for self-compacting concrete and high Performance cementitious materials are very versatile. Typically superplasticizers are composed of a polycarboxylic backbone equipped with polyethylene oxide graft chains of variable length and grafting degree. The mode of operation of these admixtures is based on the steric repulsion of the particles upon adsorption. The adsorption is strongly depending upon the charge density of a superplasticizer and the time dependent Adsorption processes control the retention of the flow performance – an important issue particularly for ready-mix and construction site concrete. However, the properties of polycarboxylic superplasticizers typically remain a black box for users. The paper suggests a simple and rapid test method, which can be conducted without sophisticated equipment, to qualitatively distinguish between two types of superplasticizers based on the adsorption mechanism. Interpreting the results in the right way provides a powerful tool to choose the right admixture for individual time dependent flow specifications.
Selbstverdichtender Beton verhält sich unter Temperatureinfluss anders als Normalbeton, da die Rheologie neben der fortschreitenden Hydratation zusätzlich durch die von der Zeit und dem Hydratationsfortschritt abhängige Adsorption von Fließmitteln beeinflusst wird. Anhand rheometrischer Betonversuche an SVB unterschiedlicher Entwurfskonzepte mit variierter anionischer Ladungsdichte im Fließmittel wird verdeutlicht, dass mehlkornreiche SVB bei niedrigen Temperaturen sehr robust sind, während bei hohen Temperaturen mehlkornärmere Entwürfe zu bevorzugen sind. Darüber hinaus wird gezeigt, wie sich unterschiedliche Fließmittelmodifikationen in bestimmten Temperaturbereichen verhalten. Anhand des Wasser-Feststoff-Verhältnisses und des Adsorptionsverhaltens von Fließmitteln werden die maßgeblichen Prozesse erläutert und Möglichkeiten für die Entwicklung robuster Mischungen für individuelle Temperaturbereiche aufgeführt.--------------------------------------------------------------------------------------------------------------------------------------------------------------
Regarding the temperature dependent performance, self-compacting concrete (SCC) distinguishes from normal concrete, since its rheology does not only depend upon the hydration itself but supplementary upon the adsorption of superplasticizers, which is affected by the time and the hydration progress. Based on rheometric concrete investigations with different SCC mixture compositions and varied anionic charge densities of the superplasticizers, it is shown that SCC, which is rich in powder components, shows robust performance at low temperatures, while compositions with lower powder contents are favourable at high temperatures. Furthermore, the performance of different superplasticizer modifications at different temperature ranges is demonstrated. The relevant processes are explained by means of the water to powder ratio as well as the adsorption behaviour of superplasticizers, and options for the development of robust mixture compositions for individual temperature ranges are itemised.
Since its invention in the early 1990’s, self-consolidating concrete has never become well established in the ready-mix sectors worldwide. The reason for this can be mainly found in the fact that the sophisticated compositions are sensitive against changing environments. This lack of robustness can be attributed to the interaction between cement hydration reaction and high range water reducing agent (HRWRA). Understanding the relevant mechanisms that control the initial flow performance as well as the flow retention helps optimizing SCC mixtures that perform either steadily in one specific environment or that perform largely similarly at steadily changing environments.
This paper depicts how HRWRAs interact with clinker and hydration phases and discusses the important role of the charge density of a polycarboxylic HRWRA in the way the rheology is affected. Based on rheometric results and observations of the Vicat setting times, it is shown that increasing charge densities of the HRWRA and decreasing water to powder ratios (w/p) reduce the flow retention and have lesser retarding effect on the setting. Based on the discussion, optimization procedures for the mixture composition and the HRWRA modification are suggested to achieve optimized performance for varying environmental situations or highest robustness for specific conditions.