Filtern
Dokumenttyp
- Beitrag zu einem Tagungsband (9) (entfernen)
Schlagworte
Organisationseinheit der BAM
- 4 Material und Umwelt (2)
- 4.2 Material-Mikrobiom Wechselwirkungen (2)
- 1 Analytische Chemie; Referenzmaterialien (1)
- 1.1 Anorganische Spurenanalytik (1)
- 1.4 Prozessanalytik (1)
- 1.7 Organische Spuren- und Lebensmittelanalytik (1)
- 1.8 Umweltanalytik (1)
- 4.0 Abteilungsleitung und andere (1)
- 4.1 Biologische Materialschädigung und Referenzorganismen (1)
- 4.5 Kunst- und Kulturgutanalyse (1)
With the implementation of glass casting in France in the second half of the 17th century, larger mirrors could be produced. So-called tin-mercury mirrors were made by coating glass with tin amalgam. Today, many historical mirrors are partly damaged, the image quality is compromised, and the material integrity of the mirror is threatened. The transformation from tin into an oxide starts at the surface of the amalgam and proceeds down to the glass surface. The mercury dissolves as a liquid or gaseous phase. The amalgam layer is destroyed, so that conservation is necessary. Conservators must follow strict safety precautions while handling amalgam mirrors because of possible mercury emissions and corrosion of the amalgam, during which elemental mercury accumulates near the mirror frame in droplets and is emitted into the air.
In a research project, the quantity of the mercury emissions from historical mirrors was examined and a technique to decrease these emissions was developed.
Scientific investigation for a medieval stained glass conservation project at Lincoln Cathedral
(2015)
Between 2013 and 2017 four medieval lancet windows located in the south-west transept of Lincoln Cathedral are being restored and conserved at the Cathedral Glazing Department. The great majority of the glass dates from the 13th century with some pieces dating from the 13th century (Morgan 1983, pp. 21-24). in order for the conservation and cleaning of the medieval glass to take place, scientific investigations were carried out at the Federal Institute for Materials Research and Testing (BAM), Berlin. The pre-conservation analysis examined the glass before any cleaning method had taken place to establish the state of the glass and its surface. A later post-cleaning analysis would provide information regarding the effectiveness of the different cleaning methods.
Corrosion of historic timber
(2014)
Nach 1850 wurde zur weiteren Herabsetzung der Einbrenntemperatur von Glasmalfarben Borax (Na2B4O7 · 10 H2O) zugesetzt. Das Verhältnis war nun 1 Teil SiO2, 3 Teile PbO und 0,5 Teile Borax. Der analytische Nachweis von Bor in eingebrannten Malschichten war bisher jedoch nicht möglich.Daher wurden in Laborversuchen Glasmalfarben mit unterschiedlichem Gehalt an Borax auf Modellgläser aufgetragen, eingebrannt und anschließend unter simulierten Umweltbedingungen zeitraffend im Klimaschrank bewittert.
Mit Hilfe von elektronenmikroskopischen Untersuchungen können Malschichten charakterisiert werden und somit Hinweise auf mögliche Schadensursachen liefern. Erste Versuche zum Nachweis von Bor erfolgten mit Hilfe von LIBS-Messungen (Laser Induced Breakdown Spectroscopy) an im Labor hergestellten Glasmalfarben mit unterschiedlichem Boraxgehalt.
A number of environmental monitoring projects were performed on historic stained-glass Windows in Germany from 1994 to 2012. The quality of the protective glazing was assessed by recording environmental Parameters in the interspace between the original and the protective glazing and on the inside of the original window. Tor this purpose, temperature, humidity and air velocity were measured. Particles were sampled with different methods and analysed by scanning electron microscopy combined with energy dispersive X-ray spectroscopy to determine their chemical composition. The effect of particles on model glass samples was investigated in climate chambers under accelerated weathering conditions. The results from in situ measurements and laboratory tests were combined to evaluate the potential effect of particulate matter on historic stained-glass Windows.
Mediaeval stained glass has been treated with Polymethylmetacrylate coatings by Kwiatkowski in Poland during the 1950th. Such treated panels were found in the Johannis Church of Toruń (without protective glazing), in the Cathedral of Włocławek (behind a protective glazing), and on glass kept in exhibition cases in the museum of Toruń. Surface coatings have been detected and analyzed. There was no extensive contamination by fungi or bacteria if the glass was either coated or not.
In this study, bulked adhesives were examined regarding changes in properties for their use in the restoration of stained-glass windows. Two epoxy adhesives commonly used in the restoration of flat glass, Araldite® 2020 and Hxtal NYL-1™, were investigated. The adhesives were mixed with various silica-based micro- and nano-particles as fillers. Different tests were carried out on the adhesives with and without fillers in order to characterise their chemical and mechanical properties. The tests included colorimetry, dynamic-mechanical methods of analysis and tests on bending strength. No property changes could be ascertained in the bulked adhesives that would be negative for the restoration of delicate flat glass.
Gegenstand der vorzustellenden Arbeiten ist die Prüfung der Umwelt-beständigkeit und -verträglichkeit von Materialien und Produkten hinsichtlich der Emission von potenziellen Schadstoffen in die Umwelt. Hierzu werden chemisch-physikalische Einflüsse (Bewitterung) und mikrobielle Beanspruchungen an Modellmaterialien evaluiert. So werden die Freisetzungsraten von Schadstoffen in Abhängigkeit der Beanspruchung beschrieben. Als Modellmaterialien kommen die Polymere Polystyrol (PS) und Polypropylen (PP) zum Einsatz. Synergistische Effekte der Bewitterungsparameter und der mikrobiologischen Beanspruchung sollen dabei ebenso betrachtet werden, wie die gezielte Alterung. Auch findet eine Beschreibung des Verhaltens der ausgetragenen Schadstoffe in den Umweltkompartimenten Boden oder Wasser statt. Hier sind mit Hilfe der zu entwickelnden Screening- und non-Target-Analyseverfahren die Transformation und der Metabolismus durch Mikroorganismen zu beschreiben. Aus den Ergebnissen sollen Korrelationen zwischen den künstlichen Alterungsverfahren und realen Szenarien abgeleitet werden.