The container of high-level radioactive waste (HLRW) being in deep geological disposal, the backfill material is needed to serve as the second defense for HLRW and the highly compacted bentonite is generally selected. As the time goes, the underground water will infiltrate the backfill, causing the corrosion of materials for the building of containers in the formed electrolyte. Carbon steel, titanium and its alloy are the potential candidate materials for the fabrication of HLRW containers.
The current investigation aims at assessing the safety of HLRW container in deep geological disposal for hundreds of thousands of years and facilitating the material selection for future Container fabrication by estimating their corrosion behavior in compacted bentonite with a series of moisture content at different temperatures through electrochemical methods including open circuit potential (OCP), electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization curve (PC) measurements. The corrosion rates were estimated for a carbon steel, a pure titanium and a titanium alloy in compacted Gaomiaozi Bentonite infiltrated with simulated underground water in Beishan area of China over an expected disposal period up to 106 years respectively, showing that titanium and its alloy are more reliable materials for building HLRW containers than carbon steel.
The influence of interfacial pH between AISI 4135 steel and seawater under different polarization potentials on the formation of calcareous deposits has been studied. An interfacial pH of 9.61 at −0.9 V vs. SCE using state of the art iridium oxide microelectrode was found to be the critical pH for the precipitation of magnesium hydroxide. Calcareous deposits with a double-layer structure comprising an inner-brucite layer and an outer-aragonite layer were found to form at potentials between −1.0 V and −1.2 V vs. SCE. Furthermore, the facilitation of hydrogen permeation into steel induced by the formation of calcareous deposits was verified using the Devanathan-Stachurski electrochemical test. The mechanism of calcareous deposits facilitates hydrogen permeation into steel is related to its inhibition on hydrogen recombination and escape processes.