We report dielectric and calorimetric studies on metathesis and addition-type polytricyclononenes, both based on the same monomer bearing three pendant OSiMe3 groups. For the addition-type polymer, dielectric spectroscopy reveals a β*-process related to the microporosity, whereas for its metathesis counterpart, the segmental dynamics manifests as an α-process related to a glass transition. Besides active dielectric processes, a significant conductivity contribution is detected for both samples which for the microporous additiontype polymer is three orders of magnitude greater than for the metathesis polymer. The broadband dielectric spectroscopy is complemented by detailed calorimetric investigations, comprising DSC, FSC, and TMDSC. The calorimetric methods detected the glass transition for the metathesis polymer in agreement with the observed dielectric α-process. Furthermore, the already reported gas transport properties for both polymers are compared, setting them in correlation with the observed molecular mobility and conductivity behavior. The discussed results reflect significant differences in molecular mobility of the two polymers affecting the appearance of microporosity which strongly determines the gas transport properties.
During the service life of structural sealant glazing (SSG) facades, the loadbearing capacity of the silicone bonds needs to be guaranteed. Laboratory Tests can assess the durability of SSG-systems based on mechanical characteristics of the bond after simultaneous exposure to both climatic and mechanical loads.
This article studies how the material characteristics of two common structural sealants are affected by laboratory and field exposure. Dynamic mechanical Analysis (DMA) confirms a reduction in the dynamic modulus of exposed Silicone samples. Results from thermogravimetric analysis, Fourier-transform infrared spectroscopy, differential scanning calorimetry, and small-angle X-ray scattering/wide-angle X-ray scattering show differences between the two sealants and indicate no/minor changes in the composition and morphology of the laboratory and field exposed sealants. Mechanical characterization methods, such as DMA, and tensile and shear testing of the structural bond, are shown to be sensitive toward the combined climatic and mechanical loadings, and are hence suitable for studying degradation mechanisms of structural sealants.
Polymers of intrinsic microporosity (PIMs) are promising candidates for the active layer in gas separation membranes due to their high permeability and reasonable permselectivity. These appealing properties originate from a microporous structure as a result of inefficient segment packing in the condensed state due to a combination of a ladder-like rigid backbone and sites of contortion. However, this class of polymers suffers from a significant decrease in the permeability with time due to physical aging, whereby typically, the permselectivity increases. The initial microporous structures approach a denser state via local rearrangements, leading to the reduction of the permeability. Hence, a detailed characterization of the molecular mobility in such materials can provide valuable information on physical aging. In this work, the dielectric behavior of PIM-1 films and their behavior upon heating (aging) were revisited by isothermal frequency scans during different heating/cooling cycles over a broad temperature range between 133 and 523 K (−140 to 250 °C). In addition, the obtained results were compared with data of samples that were annealed at ambient temperatures over different time scales. Multiple dielectric processes were observed: several relaxation processes due to local fluctuations and a Maxwell−Wagner−Sillars polarization effect related to the microporosity. The temperature dependence of the rates of all processes follows the Arrhenius law where the estimated activation energy depends on the nature of the process. The influence of the thermal history (aging) on the processes is discussed in detail.
For the first time, dielectric and calorimetric investigations of an homologous series of Janus polynorbornenes with rigid main backbones and flexible -Si(OR)3 side groups, of differing length alkyl chains (R = Propyl, Butyl, Hexyl, Octyl, Decyl) is reported. Generally, this class of polymers has some potential for applications in the field of gas separation membranes. Two dielectrically active processes are observed at low temperatures, denoted as β- and α- relaxation. The former can be assigned to localized fluctuations, whilst the latter is related to the glassy dynamics of the flexible -Si(OR)3 side groups, creating a nanophase separation in both the alkyl chain rich and backbone rich domains. This is confirmed through temperature modulated DSC measurements and X-ray scattering experiments. The glass transition temperatures of the backbone rich domains, which are beyond or near to their degradation temperatures in terms of conventional DSC, are determined for the first time using Fast Scanning Calorimetry employing both fast heating and cooling rates. This is complimented with scattering experiments that show how the size of the alkyl chain rich domains increases with chain length. Alongside these results, a significant conductivity contribution was observed for all poly(tricyclononenes) with -Si(OR)3 side groups, which is interpreted in terms of a percolation model.