Filtern
Dokumenttyp
Schlagworte
Organisationseinheit der BAM
Osteoclastic bioresorption of biomaterials: Two- and three-dimensional imaging and quantification
(2010)
Purpose: Bioresorbable materials have been developed in the hope that the body will replace them with newly formed tissue. The first step of this remodeling process in bone is the bioresorption of the material by osteoclasts. The aim of this study was to analyze osteoclastic resorption of biomaterials in vitro using the commonly used two-dimensional methods of light-microscopy (LM) and scanning electron microscopy (SEM) in comparison with infinite focus microscopy (IFM), a recently developed imaging method allowing for three-dimensional surface analysis. Methods: Human hematopoietic stem cells were cultivated in the presence of the cytokines M-CSF and RANK-L for 4 weeks directly on dentin and a calcium phosphate cement. Osteoclast development was surveyed with standard techniques. After removal of the cells, resorption was characterized and quantified by LM, SEM and IFM. Results: Osteoclast cultures on the biomaterials presented the typical osteoclast-specific markers. On dentin samples LM, SEM as well as IFM allowed for discrimination of resorption. Quantification of the resorbed area showed a linear correlation between the results (LM vs. SEM: r=0.996, p=0.004; SEM vs. IFM: r=0.989, p=0.011; IFM vs. LM: r=0.995). It was not possible to demarcate resorption pits on GB14 using LM or SEM. With IFM, resorption on GB14 could be visualized and quantified two- and three-dimensionally.
Commonly, to determine osteoclastic resorption of biomaterials only the resorbed area is measured. The depth of the resorption pit, however, may also be important for the performance of a material. To generate such data we used two calcium phosphate ceramics (Ca10 and Ca2). The solubility of the materials was determined according to DIN EN ISO 10993-14. They were scanned three-dimensionally using infinite focus microscopy and subsequently cultivated for 4 weeks in simulated body fluid without (control) or with human osteoclasts. After this cultivation period osteoclasts number was determined and surface changes were evaluated two- and three-dimensionally. Ca10 and Ca2 showed solubilities of 11.0 ± 0.5 and 23.0 ± 2.2 mg g-1, respectively. Both materials induced a significant increase in osteoclast number. While Ca10 did not show osteoclastic resorption, Ca2 showed an increased pit area and pit volume due to osteoclastic action. This was caused by an increased average pit depth and an increased number of pits, while the average area of single pits did not change significantly. The deduced volumetric osteoclastic resorption rate (vORR) of Ca2 (0.010.02 µm3 µm-2 day-1) was lower than the remodelling speed observed in vivo (0.08 µm3 µm-2 day-1), which is in line with the observation that implanted resorbable materials remain in the body longer than originally expected. Determination of volumetric indices of osteoclastic resorption might be valuable in obtaining additional information about cellular resorption of bone substitute materials. This may help facilitate the development of novel materials for bone substitution.
Over the last decade there have been increasing efforts to develop three-dimensional (3D) scaffolds for bone tissue Engineering from bioactive ceramics with 3D printing emerging as a promising technology. The overall objective of the present study was to generate a tissue engineered synthetic bone graft with homogenously distributed osteoblasts and mineralizing bone Matrix in vitro, thereby mimicking the advantageous properties of autogenous bone grafts and facilitating usage for reconstructing segmental discontinuity defects in vivo . To this end, 3D scaffolds were developed from a silica-containing calcium alkali orthophosphate, using, fi rst, a replica technique – the Schwartzwalder – Somers method – and, second, 3D printing, (i.e. rapid prototyping). The mechanical and physical scaffold properties and their potential to facilitate homogenous colonization by osteogenic cells and extracellular bone matrix formation throughout the porous scaffold architecture were examined.
Osteoblastic cells were dynamically cultured for 7 days on both scaffold types with two different concentrations of 1.5 and 3 × 10⁹ cells/l. The amount of cells and bone matrix formed and osteogenic marker expression were evaluated using hard tissue histology, immunohistochemical and histomorphometric analysis. 3D-printed scaffolds (RPS) exhibited more micropores, greater compressive strength and silica release. RPS seeded with 3 × 10⁹ cells/l displayed greatest cell and extracellular Matrix formation, mineralization and osteocalcin expression. In conclusion, RPS displayed superior mechanical and biological properties and facilitated generating a tissue engineered synthetic bone graft in vitro, which mimics the advantageous properties of autogenous bone grafts, by containing homogenously distributed terminally differentiated osteoblasts and mineralizing bone matrix and therefore is suitable for subsequent in vivo implantation for regenerating segmental discontinuity bone defects.
Recently, efforts towards the development of patient-specific 3D printed scaffolds for bone tissue engineering from bioactive ceramics have continuously intensified. For reconstruction of segmental defects after subtotal mandibulectomy a suitable tissue engineered bioceramic bone graft needs to be endowed with homogenously distributed osteoblasts in order to mimic the advantageous features of vascularized autologous fibula grafts, which represent the standard of care, contain osteogenic cells and are transplanted with the respective blood vessel. Consequently, inducing vascularization early on is pivotal for bone tissue engineering. The current study explored an advanced bone tissue engineering approach combining an advanced 3D printing technique for bioactive resorbable ceramic scaffolds with a perfusion cell culture technique for pre-colonization with mesenchymal stem cells, and with an intrinsic angiogenesis technique for regenerating critical size, segmental discontinuity defects in vivo applying a rat model. To this end, the effect of differing Si-CAOP (silica containing calcium alkali orthophosphate) scaffold microarchitecture arising from 3D powder bed printing (RP) or the Schwarzwalder Somers (SSM) replica fabrication technique on vascularization and bone regeneration was analyzed in vivo. In 80 rats 6-mm segmental discontinuity defects were created in the left femur.
The use of biodegradable bone substitutes is advantageous for alveolar ridge augmentation, since it avoids second-site surgery for autograft harvesting. This study examines the effect of novel, rapidly resorbable calcium phosphates on the expression of bone-related genes and proteins by human bone-derived cells (HBDC) and compares this behavior to that of tricalciumphosphate (TCP). Test materials were a-TCP, and four materials which were created from ß-Rhenanite and its derivatives: R1-ß-Rhenanite (CaNaPO4); R1/M2 composed of CaNaPO4 and MgNaPO4; R1+SiO2 composed of CaNaPO4 and 9% SiO2 (wt%); and R17-Ca2KNa(PO4)2. HBDC were grown on the substrata for 3, 5, 7, 14 and 21 days, counted and probed for various mRNAs and proteins (Type I collagen, osteocalcin, osteopontin, osteonectin, alkaline phosphatase and bone sialoprotein). All substrata supported continuous cellular growth for 21 days. At day 21, surfaces of R1+SiO2 and R17 had the highest number of HBDC. At 14 and 21 days, cells on R1 and on R1+SiO2 displayed significantly enhanced expression of all osteogenic proteins. Since all novel calcium phosphates supported cellular proliferation together with expression of bone-related proteins at least as much as TCP, these ceramics can be regarded as potential bone substitutes. R1 and R1+SiO2 had the most effect on osteoblastic differentiation, thus suggesting that these materials may possess a higher potency to enhance osteogenesis than TCP.