Filtern
Erscheinungsjahr
Dokumenttyp
- Beitrag zu einem Tagungsband (20)
- Vortrag (6)
- Forschungsbericht (5)
- Zeitschriftenartikel (3)
Sprache
- Englisch (34) (entfernen)
Referierte Publikation
- nein (34) (entfernen)
Schlagworte
- Acoustic emission analysis (4)
- Cracks (4)
- Durability (4)
- Crack formation (3)
- Grout (3)
- Nano-silica (3)
- Shrinkage (3)
- Tensile strength (3)
- accident prevention (3)
- building industry (3)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (14)
- 7.4 Baustofftechnologie (14)
- 7.2 Ingenieurbau (8)
- 8 Zerstörungsfreie Prüfung (3)
- 8.2 Zerstörungsfreie Prüfmethoden für das Bauwesen (3)
- 7.1 Baustoffe (2)
- 2 Prozess- und Anlagensicherheit (1)
- 2.4 Prüfung und Bewertung von Explosivstoffen/Pyrotechnik (1)
- 2.5 Konformitätsbewertung Explosivstoffe/Pyrotechnik (1)
- 8.6 Faseroptische Sensorik (1)
Eingeladener Vortrag
- nein (6)
It is important to protect critical buildings (shopping centres, government buildings and embassies), infrastructure and utilities, train and underground stations against being damaged, destroyed or disrupted by deliberate acts of terrorism, criminal activity and malicious behaviour. Normal regulations and building guidelines do not generally take into account these threats. The introduction of appropriate regulations or guidelines, where deemed necessary, should enhance the resilience of buildings and infrastructure against explosion incidents. In order to protect the built infrastructure, methods are required to quantify the resistance of structural components against explosive loading and to assess the hazards resulting from the failure of an element. The applicable state-of-the-art techniques may include either experimental or numerical methods, or a combination of both. Therefore, the thematic group (TG) on the resistance of structures to explosion effects was formed in order to bring the required expertise together, make it commonly available and to find and define harmonised methods and solutions which can be provided to the decision-makers responsible for critical infrastructure protection. This report discusses the differences between the existing standards for testing blast-resistant glazing and windows and it presents basic recommendations for the future development of the suite of European standards in this area.
The determination of the blast protection level of laminated glass windows and facades is of crucial importance, and it is normally done by using experimental investigations. In recent years numerical methods have become much more powerful also with respect to this kind of application. This report attempts to give a first idea of a possible standardisation concerning such numerical simulations. Attention is drawn to the representation of the blast loading and of the behaviour of the material of the mentioned products, to the geometrical meshing, as well as to the modelling of the connections of the glass components to the main structure. The need to validate the numerical models against reliable experimental data, some of which are indicated, is underlined.
Alkali-activated materials are ideal for the repair of concrete structures in harsh environmental conditions due to their high durability in chemically aggressive environments. However, slag-based mortars, in particular, are prone to shrinkage and associated cracks. In this respect, the application of steel fibres is one solution to reduce the formation of shrinkage induced cracks and to improve post cracking behaviour of these mortars. This study investigated the influence of two different types of steel fibres on the tensile properties of two alkali-activated mortars. Direct tensile tests and single fibre pull-outs were performed to analyse the determining failure modes both on macro and micro scale. Mechanical testing was accompanied by non-destructive testing methods such as digital image correlation and acoustic emission for a detailed analysis of the fracture process.
Additive manufacturing of concrete structures is a novel and emerging technology. Freecontouring in civil engineering, which allows for entirely new designs, is a significant advantage. Inthe future, lower construction costs are expected with increased construction speeds and decreasingrequired materials and workers. However, architects and civil engineers rely on a certain quality ofexecution to fulfil construction standards. Although several techniques and approaches demonstratethe advantages, quality control during printing is highly challenging and rarely applied. Due to thecontinuous mixing process commonly used in 3D concrete printing, it is impossible to exclude varia-tions in the dry mixture or water content, and a test sample cannot be taken as a representative samplefor the whole structure. Although mortar properties vary only locally, a defect in one layer duringprinting could affect the entire integrity of the whole structure . Therefore, real-time process monitor-ing is required to record and document the printing process.At the Bundesanstalt für Materialforschung und -prüfung (BAM) a new test rig for the additive man-ufacturing of concrete is built. The primary purpose is measuring and monitoring the properties of amortar during the printing process.The following study investigates an approach for calculating yield stress and plastic viscosity based onexperimentally recorded pressure data. The calculations assume that fresh mortar behaves as a Bing-ham fluid and that the Buckingham-Reiner-equation is applicable. A test setup consisting of rigid pipeswith integrated pressure sensors at different positions is utilized.Monitoring the printing process with different sensors is crucial for the quality control of an ongoingprocess.
During the past 20 years, innovative developments in concrete technology have enabled the production of ultra-high performance fibre reinforced concretes (UHPFC) for the protection and preservation of concrete structures. The main characteristics of UHPFC comprise high compressive and flexural strength as well as high ductility compared to normal strength, normal weight concrete (NSC). This paper focuses on the analysis of crack formation and crack propagation in UHPFC under tensile loading under quasistatic conditions by using acoustic emission (AE) and optical deformation analysis (ODA).
AE is a non-destructive technique to monitor the development of micro structural damage processes caused by external forces. In this context, AE allows for a continuous monitoring of changes in the microstructure (cracks) over time and the corresponding localisation by appropriate algorithms. The AE measurements were performed along with ODA at the surface of the samples in order to analyse the deformation behaviour of the samples and the crack propagation.
For the tests, a UHPFC reference mixture was developed and tested with three different volume percentages of steel fibres (1.0 V.-%, 2.0 V.-%, and 3.0 V.-%). This paper shows that the application of AE is a suitable method to analyse the crack propagation in UHPFC specimens under tensile loading and to localise the crack initiation. Furthermore, insights into the failure mechanism of the fibres are offered by the analysis of the signals of the AE measurements, which allows for a better understanding of UHPFC and its general performance.
The aim of an ongoing research project is to develop a design approach for typical offshore driven piles (e.g. Jacket piles) based on the application of injections by compaction grouting directly at the pile shaft. The paper aims to present the results of laboratory and in-situ tests, which reveal the efficiency and the promising potential of the optimised foundation concept for a more economic dimensioning of pile foundations and to increase their bearing capacity in non-cohesive soil at any moment after installation.
Global energy consumption will increase in the future necessitating both fossil fuels and renewable energy choices - especially wind energy. Such high energy demand requires installation of offshore energy structures, rigs, platforms and towers, which are susceptible to adverse environmental conditions along with maintenances. Due to their large size and remote locations, cylindrical grouted joints are often adopted between substructure and foundation in these offshore platforms and wind structures such as monopiles. However, these connections are composite structures with exterior sleeve, interior pile and infill mortar. Degradation and settlements were reported inside similar connections, which were installed in last three decades. Besides, grouting in the offshore sites were proven difficult to obtain ideal load bearing capacity. In-situ loading conditions were also found to be affecting the failure mechanism inside such connections. This study aims at characterizing the nature of cracks generated in these grouted connections under both static and cyclic loading. Scaled grouted joints were manufactured using a novel reusable mold, and connections were loaded to failure to visualize the main failure patterns. An assessment between failure under these two types of load is drawn along with comparison to previously available literature.
Global energy consumption will increase in the future necessitating both fossil fuels and renewable energy choices - especially wind energy. Such high energy demand requires installation of offshore energy structures, rigs, platforms and towers, which are susceptible to adverse environmental conditions along with maintenances. Due to their large size and remote locations, cylindrical grouted joints are often adopted between substructure and foundation in these offshore platforms and wind structures such as monopiles. However, these connections are composite structures with exterior sleeve, interior pile and infill mortar. Degradation and settlements were reported inside similar connections, which were installed in last three decades. Besides, grouting in the offshore sites were proven difficult to obtain ideal load bearing capacity. In-situ loading conditions were also found to be affecting the failure mechanism inside such connections. This study aims at characterizing the nature of cracks generated in these grouted connections under both static and cyclic loading. Scaled grouted joints were manufactured using a novel reusable mold, and connections were loaded to failure to visualize the main failure patterns. An assessment between failure under these two types of load is drawn along with comparison to previously available literature.
Design of a cementitious coating system for corrosion protection: Phase 1 binder materials selection
(2014)
This paper presents the first results of an ongoing research project on the development of a cementitious thin layer coating system with high resistance against chloride penetration and carbonation. It is intended to display the decision process used for selecting raw materials as well as the conclusions based on test results and theoretical deliberations. In this phase, only the influence of the binder materials was analyzed concerning mechanical properties. The system should enhance the durability of new and old concrete structures exposed to aggressive environments, be based on market available materials and fulfill the requirements of the German guideline for concrete repair (Rili-SIB).
The determination of the blast protection level of laminated glass windows and facades is of crucial importance, and it is normally done by using experimental investigations. In recent years numericalmethods have becomemuch more powerful also with respect to this kind of application. This paper attempts to give a first idea of a possible standardization concerning such numerical simulations. Attention is drawn to the representation of the blast loading and to the proper description of the behaviour of the material of the mentioned products, to the geometrical meshing, and to the modelling of the connections of the glass components to the main structure.The need to validate the numerical models against reliable experimental data, some of which are indicated, is underlined.
Reinforced concrete buildings are frequently damaged by cracks, spalling and corroded
reinforcement bars. The present article focuses on the damage analysis of one of the first
buildings in Berlin that was constructed using reinforced lightweight concrete, which makes it
historically important. The compressive strength, carbonation depth, location and diameter of
reinforcement bars as well as moisture and salt profiles were determined. The carbonationinduced corrosion of the reinforcement bars represented the main damage of the building.
Certified repair mortars with lightweight aggregates (LWA) do not exist on the German
market. Therefore, an appropriate repair mortar was developed in accordance with DIN EN
1504 and the German guideline for the repair and protection of concrete structures (RL-SIB).
On the one hand, historic preservation requirements, such as: colour of the mortar,
possibilities of surface patterning, maximum preservation of the original substance and
reversibility of any Intervention must be met. On the other hand, technical requirements of the
relevant Standards must be achieved. The developed mix was designed to resist the identified
causes of deterioration. Thermal strains within the repair mortar and between the repair
mortar and the Substrate influence the crack formation and thus the durability. Therefore,
special attention was paid to the bonding and shrinking behaviour of the concrete repair
System. By using polymers, both hardened mortar properties and durability were influenced
positively.
The high demand for sustainable and durable building materials requires profound knowledge on the material properties. In this respect, the phenomena occurring at nano-level are of crucial importance for the design of new building materials. Therefore, all around the world, increasing amounts of funding are being directed to research projects dealing with material properties on nano-level, which is claimed to have tremendous potential for the future. One of the most referred to and used cementitious nano-material is amorphous silica with a particle size in the nano-range, even though its application and effects on concrete have not been fully understood yet. Olivine (Mg,Fe)2Si04 is the fastest weathering siiicate mineral dissolving easily in acid. Düring dissolution in acid the metallic ions (Mg2+,Fe2+) are replaced by H+, yielding Si(OH)4 monomers and metallic ions in solution. After cleaning treatments an amorphous nano-silica is obtained. The produced olivine nano-silica (OnS) has a specific surface area between 100 and 400 m2/g, the size of the primary particles, which are agglomerated in Clusters, ranges from 10 to 25 nm and the impurity content is below 5 % IV. Literature related with the application of OnS in cement based materials is scarce; only one research work performed by Justnes and Ostnor 121 is available. Thus, the effect of adding OnS in cement based Systems has been not studied. Based on this, the present research aims on elucidating the effects of OnS in the fresh and hardened state of cement pastes and mortars.
Effects of amorphous nano-silica additions on mechanical and durability performance of SCC mixtures
(2012)
In the recent years the application of nanotechnology in building materials has increased
exponentially. One of the most referred and used nano-materials is amorphous silica with
particles size in the nano-range, even though its application and effect in concrete has not been
fully understood yet. It has been reported that nano-silica (nS) addition increases the
compressive strength and reduces the overall permeability of hardened concrete due to the
pozzolanic properties which are resulting in finer hydrated phases (C-S-H gel) and densified
microstructure (nano-filler and anti leaching effects). These effects enhance the durability of
concrete structures such as bridges, quays or off-shore oil facilities in marine environments.
In this study two different types of nano-silica were applied in self-compacting concrete (SCC),
both having similar particle size distributions (PSD) but produced in two different processes
(fumed powder silica and precipitated silica in colloidal suspension). The influence of nanosilica
on SCC was investigated with respect to the properties of concrete in the fresh state
(workability) and hardened state (mechanical properties and durability). Additionally, the
densification of microstructure of the hardened concrete was verified by SEM and EDS analyses.
The obtained results demonstrate that an efficient use of nano-silica in SCC can improve its
mechanical properties and durability. Considering the reactivity of the two nano-silica studied,
colloidal type shown more reactivity at early age, which influenced all the final SCC properties.
Concrete-glass windows or commonly referred to as “Dalle de Verre” windows are prevalent in historical monuments across Europe. “Dalle de Verre” windows were made by placing cut stained glasses, of various shapes and sizes, into a steel reinforced concrete frame. In addition to the steel reinforcement, a few steel wires run across the concrete elements to hold the glass windows into place. Much of these structures have been damaged due to carbonation of the thin concrete covers and consequent corrosion of the steel reinforcement; and exhibit several cracks due to the expansive nature of corrosion products formed at the steel–concrete interface. This study focussed on understanding the efficacy of electrochemical realkalisation in reinstating the passive state of the steel reinforcement embedded in such concrete glass windows. Simulant “Dalle de Verre” windows (representative of windows at Kaiser-Wilhelm Gedächtniskirche) were produced using different cements with a water/cement ratio of 0.6 and carbonated under accelerated conditions. Post carbonation, the concrete glass windows were electrochemically realkalised using a sacrificial anode. The influence of highly alkaline conditions due to electrochemical realkalisation on the glass-concrete interface has also been investigated. This study shows that the passive state of the steel reinforcement in “Dalle de Verre” windows, particularly at the Kaiser-Wilhelm Gedächtniskirche (memorial church) in Berlin, can be reinstated using the electrochemical realkalisation method.
Ultra-high performance fiber-reinforced concretes (UHPFRCs) are most suitable for applications with extreme mechanical loads. These extreme conditions require ductile behavior under tensile loading, which is obtained solely by the working mechanism of steel fibers. Profound knowledge on the working mechanism of the steel fibers is necessary to optimize this material. Usually, this knowledge is obtained by means of classical destructive measuring techniques. Adopting measuring techniques from non-destructive material testing helps to analyze and to identify the different stages of the fracture mechanism of UHPFRC in detail. The application of different non-destructive measuring techniques is shown exemplary on tensile tests conducted on an UHPFRC mix and its applicability for analyzing the fracture behavior of such concretes is discussed. The main focus is on the characterization of the relevant failure modes under tensile loading by the different measuring techniques and the comparison with classical measuring techniques (e.g. extensometer). The tensile tests have been analyzed by optical deformation measurements using digital image correlation (DIC), acoustic emission analysis (AE), and 3D computed tomography (CT).
Ultra-high performance fiber-reinforced concretes (UHPFRCs) are most suitable for applications with extreme mechanical loads. These extreme conditions require ductile behavior under tensile loading, which is obtained solely by the working mechanism of steel fibers. Profound knowledge on the working mechanism of the steel fibers is necessary to optimize this material. Usually, this knowledge is obtained by means of classical destructive measuring techniques. Adopting measuring techniques from non-destructive material testing helps to analyze and to identify the different stages of the fracture mechanism of UHPFRC in detail. The application of different non-destructive measuring techniques is shown exemplary on tensile tests conducted on an UHPFRC mix and its applicability for analyzing the fracture behavior of such concretes is discussed. The main focus is on the characterization of the relevant failure modes under tensile loading by the different measuring techniques and the comparison with classical measuring techniques (e.g. extensometer). The tensile tests have been analyzed by optical deformation measurements using digital image correlation (DIC), acoustic emission analysis (AE), and 3D computed tomography (CT).
At present, Wind Turbine Generators (WTGs) operating in onshore and offshore wind farms are primary sources of renewable energy around the world. Cylindrical grouted sleeve connections are usually adopted in these WTG structures to connect the upper structure and foundation for ease of installation. These structures including grouted connections experience considerable adverse loading during their lifetimes. Settlements were reported inside similar connections used in energy structures especially oil and gas platforms, which were installed in last three decades. Thus, repair and rehabilitation of such connections in existing wind structures should also be planned ahead to keep them operating in the future. The nature of failure and crack generation in grouted connections are crucial prior to adopt a strengthening strategy. This pilot study is carried out to actualize the failure mechanism in the grouted connection, when subjected to axial loading. A novel reusable scaled cylindrical grouted connection with shear keys was designed and tested for its load bearing behaviour. The mechanical test was accompanied by classical measuring techniques (e.g. displacement transducer) as well as non-destructive measuring techniques (e.g. digital image correlation (DIC), acoustic emission analysis (AE)). The failure mechanism incorporating slippage of the shear keys and cracking of the grout was investigated. The capacity and applicability of such test mould were also discussed. The knowledge is expected to pave way towards repair of deteriorated grouted connections with similar geometry and failure pattern.
At present, Wind Turbine Generators (WTGs) operating in onshore and offshore wind farms are primary sources of renewable energy around the world. Cylindrical grouted sleeve connections are usually adopted in these WTG structures to connect the upper structure and foundation for ease of installation. These structures including grouted connections experience considerable adverse loading during their lifetimes. Settlements were reported inside similar connections used in energy structures especially oil and gas platforms, which were installed in last three decades. Thus, repair and rehabilitation of such connections in existing wind structures should also be planned ahead to keep them operating in the future. The nature of failure and crack generation in grouted connections are crucial prior to adopt a strengthening strategy. This pilot study is carried out to actualize the failure mechanism in the grouted connection, when subjected to axial loading. A novel reusable scaled cylindrical grouted connection with shear keys was designed and tested for its load bearing behaviour. The mechanical test was accompanied by classical measuring techniques (e.g. displacement transducer) as well as non-destructive measuring techniques (e.g. digital image correlation (DIC), acoustic emission analysis (AE)). The failure mechanism incorporating slippage of the shear keys and cracking of the grout was investigated. The capacity and applicability of such test mould were also discussed. The knowledge is expected to pave way towards repair of deteriorated grouted connections with similar geometry and failure pattern.
Alkali-activated slag materials are known for their high Chloride penetration resistance. This makes them potentially applicable as repair systems for damaged steel-reinforced concrete structures, which are exposed to chloride attack. For this purpose, the influence of the activator composition, i.e. the SiO2 and Na2O concentration of the alkaline solution on a) the compressive strength, b) shrinkage and mass change and c) the resistance against chloride penetration of four alkali-activated slag mortars (AASM) were studied. An ordinary Portland cement-based mortar was used as the reference sample. Increasing SiO2 and Na2O concentrations increased the strength, shrinkage and mass loss of the AASMs. The resistance of the mortars against chloride penetration was evaluated using the non-steady-state migration coefficient Dnssm obtained from NT BUILD 492. The results indicate that the Dnssm is related to differences in the pore solution of the AASMs rather than to differences in their microstructure. An upcoming study of the authors is going to evaluate this hypothesis by the accelerated chloride penetration (diffusion) test.