Filtern
Dokumenttyp
- Beitrag zu einem Tagungsband (11)
- Zeitschriftenartikel (3)
- Vortrag (3)
- Forschungsbericht (1)
Referierte Publikation
- nein (18) (entfernen)
Schlagworte
- Grout (3)
- Bingham fluid (2)
- Crack formation (2)
- Crack pattern (2)
- Cyclic load (2)
- Fly ash (2)
- Grouted connection (2)
- Long-term shrinkage (2)
- Metakaolin (2)
- Micro silica (2)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (18) (entfernen)
Eingeladener Vortrag
- nein (3)
Grouting is a universal repair and strengthening technique, which is constantly used for structural remediation of concrete components, trenches, mine subsidence, dam joints, restoration of masonry structures, and geological stabilizations. Having an extremely small particle size of only few microns, ultrafine cements are ideal for grouting applications due to their superior permeability and compressive strength properties of the hardened cement paste compared to that of the less-expensive, but coarser ordinary Portland cements. Supplementary cementitious materials (SCMs) are often used to replace ultrafine cement in order to modify certain properties and to reduce costs. The aim of this experimental study is to investigate the effect of three supplementary materials: microsilica (MS), fly ash (FA), and metakaolin (MK) on the workability, and mechanical properties of an ultrafine cement based grout with a constant water-binder ratio and constant superplasticizer content. Maximum percentages of replacement with ultrafine cement were 6% by volume of cement for MS and 16% for FA, and MK. In general, results suggest that the workability is improved by addition of FA, whereas is reduced, when modified with MS and MK. The compressive strength of grout after cement replacement remains comparable to that of pure cement grout. However, there is a tendency of the MS to positively affect the compressive strength opposite to FA, whereas flexural strength is positively affected by FA. Based on the results, it is evident that grouts with Hägerman cone flow more than 500 mm and compressive strength of more than 90 MPa after 28 days can be produced.
Alkali-activated slag materials are known for their high Chloride penetration resistance. This makes them potentially applicable as repair systems for damaged steel-reinforced concrete structures, which are exposed to chloride attack. For this purpose, the influence of the activator composition, i.e. the SiO2 and Na2O concentration of the alkaline solution on a) the compressive strength, b) shrinkage and mass change and c) the resistance against chloride penetration of four alkali-activated slag mortars (AASM) were studied. An ordinary Portland cement-based mortar was used as the reference sample. Increasing SiO2 and Na2O concentrations increased the strength, shrinkage and mass loss of the AASMs. The resistance of the mortars against chloride penetration was evaluated using the non-steady-state migration coefficient Dnssm obtained from NT BUILD 492. The results indicate that the Dnssm is related to differences in the pore solution of the AASMs rather than to differences in their microstructure. An upcoming study of the authors is going to evaluate this hypothesis by the accelerated chloride penetration (diffusion) test.
Für die rechnerische Dimensionierung der Betondecken im Oberbau von Verkehrsflächen für den Neubau sowie die Erneuerung nach RDO-Beton 09 ist die statische Spaltzugfestigkeit an der unteren und oberen Bohrkernscheibe entsprechend der Vorgaben der AL Sp-Beton zu bestimmen. Aufgrund der unzureichenden Kenntnis der Präzision dieses Prüfverfahrens wurden, basierend auf dem Entwurf des FGSV-Merkblatts zur statistischen Auswertung von Prüfergebnissen, mit einem breit aufgestellten Ringversuch die statistischen Kennwerte an Labor- und Bestandsbetonen unter Vergleich- und Wiederholbedingungen ermittelt. Zur möglichst guten statistischen Absicherung nahmen an dem Ringversuch dreizehn erfahrene Prüfstellen teil, die vorab einem Audit unterzogen wurden. Zur Abdeckung des vielschichtigen Einsatzes des Prüfverfahrens erfolgte der Ringversuch an acht Prüflosen, die sowohl die Erst-/ Eignungsprüfung und Übereinstimmungskontrolle bei Neubaumaßnahmen, als auch die Restsubstanzbewertung von Betonfahrbahnplatten berücksichtigen. Zur Bewertung des Materialeinflusses wurde zusätzlich ein Prüflos mit Labormörtel untersucht.
Die Probenvorbereitung erfolgte zentral an der BAM. Zur Sicherstellung einheitlicher Prüfbedingungen bei den Prüfstellen wurde zusätzlich eine detaillierte Standardarbeitsanweisung erarbeitet, die partiell bereits Eingang in das Normenwerk gefunden hat. Bei der Plausibilitätsprüfung aller prüflosspezifischen Einzelwerte der Spaltzug- und Druckfestigkeit wurden vereinzelt sowohl Ausführungsfehler als auch Übertragungs- und Tippfehler festgestellt. Der sich anschließende Lilliefors-Test zeigt, dass die ermittelten Einzelwerte bis auf wenige Aus-nahmen normalverteilt sind und damit die Voraussetzungen für die statistische Auswertung gegeben sind.
Mittels grafischer Darstellung der Mandel’s h- und k-Werte wurden die Auffälligkeiten hinsichtlich der Mittelwerte und Varianzen prüflosspezifisch für die einzelnen Prüfstellen visualisiert und anschließend einige von ihnen mittels Grubbs- und Cochran-Test als Ausreißer identifiziert. Nach Ausreißerelimination wurde mit dem klassischen Verfahren bei der Spaltzugfestigkeit der geringste Variationskoeffizient unter Vergleich- und Wiederholbedingungen bei der Erst-/Eignungsprüfung mit 6,2 und 6,4 Prozent ermittelt. Bei einer Verminderung des Materialeinflusses durch die Verwendung eines Labormörtels verbessern sich die statistischen Kennwerte auf 4,5 und 5,3 Prozent. Mit 8,2 und 9,5 Prozent beziehungsweise 8,6 und 9,5 Prozent werden bei der Restsubstanzbewertung von Wasch- und Unterbetonen die höchsten Werte bestimmt.
Das robuste Auswerteverfahren (ohne Eliminierung der Ausreißer) nach dem Entwurf des FGSV-Merkblatts zur statistischen Auswertung von Prüfergebnissen erwies sich in der Form als ungeeignet und bedurfte einer Überarbeitung. Bezüglich der vergleichend mit klassischen und robusten Verfahren gewonnenen Kennwerte ist festzustellen, dass bei sehr homogenen Messergebnissen eines Prüfloses beide Verfahren nahezu die gleichen statistischen Kennwerte liefern. Bei der Eliminierung von Ausreißern sind die Ergebnisse des robusten Verfahrens in der Regel etwas größer als die des klassischen Verfahrens.
Die begleitenden vertiefenden Untersuchungen bei der Spaltzugprüfung mit innovativen Prüftechniken lieferten wertvolle Erkenntnisse zur Bewertung der Prüfeinflüsse.
Remediation of Cracks Formed in Grouted Connections of Offshore Energy Structures under Static Loads
(2018)
The future energy demand necessitates the exploration of all potential energy sources both onshore and offshore. Global trend has shifted towards offshore energy, which can be obtained from either carbon intensive or renewable options, hence requiring structures such as rigs, platforms, and monopiles. Most of these structures adopt easily installable construction techniques, where lower foundation need to be connected with the super structure by mean of grouted composite joints. Generally, these composite connections have exterior sleeve, interior pile and infill grout. Being located in remote offshore conditions, connections can experience considerable adverse loading during their lifetimes. Degradations were reported inside similar connections, which were installed in last three decades. Besides, grouting in the offshore sites may often be proven difficult, which eventually leads to reduced capacity of connections in the long run. Thus, repair and rehabilitation of such connections should be planned ahead to minimize operational delays and costs in the future. This study aims at characterizing the nature of crack generation in grouted connections and thereby identifying the potential of repair using suitable repair material. Scaled grouted joints were manufactured using a novel mold, and connections were loaded under static load to visualize the main failure pattern. The failure mechanism and loading capacity are found compatible to previous results from earlier literature. Grouted connection was then repaired using cementitious injectable grout. The effectiveness of the repair system is also discussed.
Grouts have numerous applications in construction industry such as joint sealing, structural repair, and connections in precast elements. They are particularly favoured in rehabilitation of structures due to penetrability and convenience of application. Grouts for repair applications typically require high-performance properties such as rapid strength development and superior shrinkage characteristics. Sometimes industrial by-products referred as supplementary cementitious materials (SCM) are used with neat cement due to their capabilities to provide binding properties at delayed stage. Micro silica, fly ash and metakaolin are such SCMs, those can modify and improve properties of cement products. This study aims at investigating long-term mass loss and linear shrinkage along with long-term compressive and flexural strength for grouts produced from ultrafine cement and SCMs. A series of mixtures were formulated to observe the effect of SCMs on these grout properties. Properties were determined after 365 days of curing at 23oC and 55% relative humidity. The effect of SCMs on the properties are characterised by statistical models. Response surfaces were constructed to quantify these properties in relation to SCMs replacement. The results suggested that shrinkage was reduced by metakaolin, while micro silica and fly ash had positive effects on compressive and flexural strength, respectively.
Grouts are particularly favoured in rehabilitation of structures due to penetrability and convenience of application. Grouts for repair applications typically require high-performance properties such as rapid strength development and superior shrinkage characteristics. Sometimes industrial by-products referred as supplementary cementitious materials (SCM) are used with neat cement due to their capabilities to provide binding properties at delayed stage. Micro silica, fly ash and metakaolin are such SCMs, those can modify and improve properties of cement products. This study aims at investigating long-term mass loss and linear shrinkage along with long-term compressive and flexural strength for grouts produced from ultrafine cement and SCMs. A series of mixtures were formulated to observe the effect of SCMs on these grout properties. Properties were determined after 365 days of curing at 23 °C and 55% relative humidity. The effect of SCMs on the properties are characterised by statistical models. Response surfaces were constructed to quantify these properties in relation to SCMs replacement. The results suggested that shrinkage was reduced by metakaolin, while micro silica and fly ash had positive effects on compressive and flexural strength, respectively.
The structural integrity of outer reinforced concrete (RC) containments of nuclear power plants provides an essential shield against external hazards. If this containment is damaged by an impact event, such as an aircraft crash, the question arises to which degree the reinforced concrete containment still has its protective capability. This concerns both purely structural protection and protection against liquids penetrating the interior of the containment. Due to the dimensions of the containment structures, it is difficult to perform real scale impact experiments, so in the past decades plate geometries at medium scale have been used for investigations. Detailed investigations on the structural behaviour of RC members or RC plates subjected to impact loading have already been presented in Just et al., Hering, Hering et al., Bracklow et al., Hille et al. and Nerger et al.
The following investigations deal with the single and multiple impact event (first hard impact and/or subsequent soft impact) on a RC specimen, which provides the basis for further investigations. A description of the test setup and the test procedure as well as a presentation of the test results from the impact tests are provided.
Furthermore, the experimental program is presented, which the damaged RC specimens are to undergo to deal with the question of how much the impact-damaged RC structure has become permeable to liquid media, such as water and kerosene, depending on the intensity of the impact. The aim of these following investigations is to develop a test setup that can be applied to investigate the liquid penetration behaviour (LPB) of small, medium, and large-scale RC members.
In addition to the liquid penetration experiments, the damaged specimens are to be examined by planar tomography to obtain the damage inside the specimen. The combination of damaging event, fluid penetration behaviour and tomography should enable a comprehensive understanding of the damage to the RC specimen.
Introduction of a monitoring system for Bingham fluids in additive manufacturing with concrete
(2022)
Freeform additive manufacturing of concrete structures is a rising technology in civil engineering with several fascinating advantages. Nonetheless, to ensure reliability and structural integrity, standards and quality control are required in the future to bring this technology into the market. As the concrete is manufactured continuously, continuous quality control of the printing process is also required, i.e. comprehensive process monitoring. At BAM, a test rig will be installed, enabling the printing of concrete structures with a maximum size of 2 m x 1 m x 1 m (l x w x h). Here, process monitoring is the focus of the test rig. In this study, we show the results of the first pump tests, including the measurement of several parameters such as temperature and pressure along the supply system, i.e. from the concrete pump to the printer head.
Concrete-glass windows or commonly referred to as “Dalle de Verre” windows are prevalent in historical monuments across Europe. “Dalle de Verre” windows were made by placing cut stained glasses, of various shapes and sizes, into a steel reinforced concrete frame. In addition to the steel reinforcement, a few steel wires run across the concrete elements to hold the glass windows into place. Much of these structures have been damaged due to carbonation of the thin concrete covers and consequent corrosion of the steel reinforcement; and exhibit several cracks due to the expansive nature of corrosion products formed at the steel–concrete interface. This study focussed on understanding the efficacy of electrochemical realkalisation in reinstating the passive state of the steel reinforcement embedded in such concrete glass windows. Simulant “Dalle de Verre” windows (representative of windows at Kaiser-Wilhelm Gedächtniskirche) were produced using different cements with a water/cement ratio of 0.6 and carbonated under accelerated conditions. Post carbonation, the concrete glass windows were electrochemically realkalised using a sacrificial anode. The influence of highly alkaline conditions due to electrochemical realkalisation on the glass-concrete interface has also been investigated. This study shows that the passive state of the steel reinforcement in “Dalle de Verre” windows, particularly at the Kaiser-Wilhelm Gedächtniskirche (memorial church) in Berlin, can be reinstated using the electrochemical realkalisation method.