Filtern
Dokumenttyp
- Beitrag zu einem Tagungsband (15)
- Zeitschriftenartikel (6)
- Vortrag (3)
- Forschungsbericht (1)
Schlagworte
- Grout (4)
- Fly ash (3)
- Grouted connection (3)
- Metakaolin (3)
- Repair (3)
- Alkali-activated materials (2)
- Bending (2)
- Box-Behnken (2)
- Crack formation (2)
- Crack pattern (2)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (25) (entfernen)
Eingeladener Vortrag
- nein (3)
Grouting is a universal repair and strengthening technique, which is constantly used for structural remediation of concrete components, trenches, mine subsidence, dam joints, restoration of masonry structures, and geological stabilizations. Having an extremely small particle size of only few microns, ultrafine cements are ideal for grouting applications due to their superior permeability and compressive strength properties of the hardened cement paste compared to that of the less-expensive, but coarser ordinary Portland cements. Supplementary cementitious materials (SCMs) are often used to replace ultrafine cement in order to modify certain properties and to reduce costs. The aim of this experimental study is to investigate the effect of three supplementary materials: microsilica (MS), fly ash (FA), and metakaolin (MK) on the workability, and mechanical properties of an ultrafine cement based grout with a constant water-binder ratio and constant superplasticizer content. Maximum percentages of replacement with ultrafine cement were 6% by volume of cement for MS and 16% for FA, and MK. In general, results suggest that the workability is improved by addition of FA, whereas is reduced, when modified with MS and MK. The compressive strength of grout after cement replacement remains comparable to that of pure cement grout. However, there is a tendency of the MS to positively affect the compressive strength opposite to FA, whereas flexural strength is positively affected by FA. Based on the results, it is evident that grouts with Hägerman cone flow more than 500 mm and compressive strength of more than 90 MPa after 28 days can be produced.
Bending beams and slabs are typical examples for structural elements used for reinforced concrete structures such as bridge girders, T-beams and bridge decks. Their strength related failure modes at maximum loading can be divided into bending and shear failure. The failure of beams loaded in bending can occur with or without indication. Therefore, conventional design concepts aim on failure modes with sufficient indication (e.g. large deflections or cracks), as it occurs in the case of secondary flexural compression failure. These indicating factors can also be used for Structural Health Monitoring (SHM) of civil infrastructure systems (e.g. bridges) to identify structural changes. In this context, non-destructive testing (NDT) methods offer different techniques for measuring deflections or crack formation and opening. However, profound knowledge on the determining failure modes of bending beams and their detection by NDT methods is required for the reliable application of SHM. Different NDT methods have been used in this study for analysing the load-bearing behaviour of a reinforced concrete beam in bending. The different measuring techniques are briefly described and their applicability is discussed by means of experimental results. For this purpose, the load-bearing behaviour of a reinforced concrete beam having a span of 2.75 m was investigated in a four-point bending flexural test at laboratory scale. The focus is on the characterization of determining failure modes by optical NDT and the comparison with classical measuring techniques (e.g. deformation measurements by displacement transducers). The bending beam was equipped with two single-mode (SM) sensor fibres. One fibre served as Distributed Optical Fibre Sensor (DOFS), whereas the other fibre contained Fibre Bragg Grating (FBG) sensors. In addition, optical deformation measurements using Digital Image Correlation (DIC) and Stereophotogrammetry (SP) were conducted.
Alkali-activated slag materials are known for their high Chloride penetration resistance. This makes them potentially applicable as repair systems for damaged steel-reinforced concrete structures, which are exposed to chloride attack. For this purpose, the influence of the activator composition, i.e. the SiO2 and Na2O concentration of the alkaline solution on a) the compressive strength, b) shrinkage and mass change and c) the resistance against chloride penetration of four alkali-activated slag mortars (AASM) were studied. An ordinary Portland cement-based mortar was used as the reference sample. Increasing SiO2 and Na2O concentrations increased the strength, shrinkage and mass loss of the AASMs. The resistance of the mortars against chloride penetration was evaluated using the non-steady-state migration coefficient Dnssm obtained from NT BUILD 492. The results indicate that the Dnssm is related to differences in the pore solution of the AASMs rather than to differences in their microstructure. An upcoming study of the authors is going to evaluate this hypothesis by the accelerated chloride penetration (diffusion) test.
Repair is an indispensable part of the maintenance of structures over their lifetimes. Structural grouting is a widely used remediation technique for concrete components, trenches, mine subsidence, dam joints, restoration of masonry structures, and geological stabilizations. A structural grout system should be injectable in narrow spaces and hence include ingredients with finer particles. Ultrafine cements are ideal for these type of demanding grouts due to their superior properties compared to that of the less expensive, but coarser ordinary Portland cement (OPC). Supplementary cementitious materials (SCMs) are often used to replace OPC clinker based binder in order to modify certain properties and to reduce costs. The most commonly used SCMs are fly ash (FA), and ground granulated blast furnace slag (GGBS). For various special applications microsilica (MS), and metakaolin (MK) are also used. Identifying the optimum replacement contents of OPC by SCMs are a challenge during the design of such grouts. The aim of this experimental study is to investigate the effect of the selected SCMs (FA, MS and MK) on the slump flow, time of efflux, viscosity, shrinkage, and compressive and flexural strength of ultrafine cement based grouts with constant water-binder ratio and superplasticizer content. The test program was formulated using Box-Behnken design principles. Maximum percentages of replacement with ultrafine cement was 6% by volume of cement for MS and 16% for FA, and MK. The results suggest that most investigated grouts have the potential to be used for structural applications. The appropriate quadratic models are then formulated through statistical tools and presented as response surfaces. The trends indicate that fly ash improves the rheological properties, whereas microsilica and metakaolin positively affect shrinkage and mechanical properties to some extent. Based on the influence of SCMs and priorities among the properties, Decision Matrix Analysis (DMA) is carried out to select the most suitable ones among the SCMs. The analysis suggests that microsilica and fly ash are more suitable as SCMs than metakaolin without affecting the properties.
Superplasticizer and Shrinkage Reducing Admixture Dosages for Microfine Cement in Grout Systems
(2019)
Grouts have numerous applications including crack repair as maintenance in construction industries. Microfine cements are intensively used for high strength mortar and grout products. They are ideal for injection grouting in structural repair. Such grouts should have suitable rheological properties to be injectable, especially those used in repair and rehabilitation. The use of superplasticizers (SP) in these products is thus becoming increasingly crucial to achieve favorable workability and viscosity properties. A difficulty in such grouts is the plastic shrinkage due to finer particles used. It is thus necessary to determine optimum SP and shrinkage reducing admixture (SRA) dosages for a microfine cement based grout. In this study, a saturation dosage was decided from two Polycarboxylate ether (PCE) based SPs in relation to neat cement using slump flow and rheological parameters. A range of grout mixtures was formulated containing micro silica (MS) and fly ash (FA), and tested for suitable rheological and mechanical parameters. Based on the results, a grout mixture with MS and FA was selected to determine optimum SRA content. According to the results, a SP dosage of 3% by weight of neat cement is sufficient to achieve saturation. The grout material including MS and FA can produce comparable properties to neat cement grout. MS is found to improve compressive strength within the range considered, whereas a higher FA content provides favourable rheological properties. Finally, a SRA dosage of 4%, which could reduce the shrinkage by about 43% after 28d days, is determined for the grout system.
Für die rechnerische Dimensionierung der Betondecken im Oberbau von Verkehrsflächen für den Neubau sowie die Erneuerung nach RDO-Beton 09 ist die statische Spaltzugfestigkeit an der unteren und oberen Bohrkernscheibe entsprechend der Vorgaben der AL Sp-Beton zu bestimmen. Aufgrund der unzureichenden Kenntnis der Präzision dieses Prüfverfahrens wurden, basierend auf dem Entwurf des FGSV-Merkblatts zur statistischen Auswertung von Prüfergebnissen, mit einem breit aufgestellten Ringversuch die statistischen Kennwerte an Labor- und Bestandsbetonen unter Vergleich- und Wiederholbedingungen ermittelt. Zur möglichst guten statistischen Absicherung nahmen an dem Ringversuch dreizehn erfahrene Prüfstellen teil, die vorab einem Audit unterzogen wurden. Zur Abdeckung des vielschichtigen Einsatzes des Prüfverfahrens erfolgte der Ringversuch an acht Prüflosen, die sowohl die Erst-/ Eignungsprüfung und Übereinstimmungskontrolle bei Neubaumaßnahmen, als auch die Restsubstanzbewertung von Betonfahrbahnplatten berücksichtigen. Zur Bewertung des Materialeinflusses wurde zusätzlich ein Prüflos mit Labormörtel untersucht.
Die Probenvorbereitung erfolgte zentral an der BAM. Zur Sicherstellung einheitlicher Prüfbedingungen bei den Prüfstellen wurde zusätzlich eine detaillierte Standardarbeitsanweisung erarbeitet, die partiell bereits Eingang in das Normenwerk gefunden hat. Bei der Plausibilitätsprüfung aller prüflosspezifischen Einzelwerte der Spaltzug- und Druckfestigkeit wurden vereinzelt sowohl Ausführungsfehler als auch Übertragungs- und Tippfehler festgestellt. Der sich anschließende Lilliefors-Test zeigt, dass die ermittelten Einzelwerte bis auf wenige Aus-nahmen normalverteilt sind und damit die Voraussetzungen für die statistische Auswertung gegeben sind.
Mittels grafischer Darstellung der Mandel’s h- und k-Werte wurden die Auffälligkeiten hinsichtlich der Mittelwerte und Varianzen prüflosspezifisch für die einzelnen Prüfstellen visualisiert und anschließend einige von ihnen mittels Grubbs- und Cochran-Test als Ausreißer identifiziert. Nach Ausreißerelimination wurde mit dem klassischen Verfahren bei der Spaltzugfestigkeit der geringste Variationskoeffizient unter Vergleich- und Wiederholbedingungen bei der Erst-/Eignungsprüfung mit 6,2 und 6,4 Prozent ermittelt. Bei einer Verminderung des Materialeinflusses durch die Verwendung eines Labormörtels verbessern sich die statistischen Kennwerte auf 4,5 und 5,3 Prozent. Mit 8,2 und 9,5 Prozent beziehungsweise 8,6 und 9,5 Prozent werden bei der Restsubstanzbewertung von Wasch- und Unterbetonen die höchsten Werte bestimmt.
Das robuste Auswerteverfahren (ohne Eliminierung der Ausreißer) nach dem Entwurf des FGSV-Merkblatts zur statistischen Auswertung von Prüfergebnissen erwies sich in der Form als ungeeignet und bedurfte einer Überarbeitung. Bezüglich der vergleichend mit klassischen und robusten Verfahren gewonnenen Kennwerte ist festzustellen, dass bei sehr homogenen Messergebnissen eines Prüfloses beide Verfahren nahezu die gleichen statistischen Kennwerte liefern. Bei der Eliminierung von Ausreißern sind die Ergebnisse des robusten Verfahrens in der Regel etwas größer als die des klassischen Verfahrens.
Die begleitenden vertiefenden Untersuchungen bei der Spaltzugprüfung mit innovativen Prüftechniken lieferten wertvolle Erkenntnisse zur Bewertung der Prüfeinflüsse.
Remediation of Cracks Formed in Grouted Connections of Offshore Energy Structures under Static Loads
(2018)
The future energy demand necessitates the exploration of all potential energy sources both onshore and offshore. Global trend has shifted towards offshore energy, which can be obtained from either carbon intensive or renewable options, hence requiring structures such as rigs, platforms, and monopiles. Most of these structures adopt easily installable construction techniques, where lower foundation need to be connected with the super structure by mean of grouted composite joints. Generally, these composite connections have exterior sleeve, interior pile and infill grout. Being located in remote offshore conditions, connections can experience considerable adverse loading during their lifetimes. Degradations were reported inside similar connections, which were installed in last three decades. Besides, grouting in the offshore sites may often be proven difficult, which eventually leads to reduced capacity of connections in the long run. Thus, repair and rehabilitation of such connections should be planned ahead to minimize operational delays and costs in the future. This study aims at characterizing the nature of crack generation in grouted connections and thereby identifying the potential of repair using suitable repair material. Scaled grouted joints were manufactured using a novel mold, and connections were loaded under static load to visualize the main failure pattern. The failure mechanism and loading capacity are found compatible to previous results from earlier literature. Grouted connection was then repaired using cementitious injectable grout. The effectiveness of the repair system is also discussed.
The bond between polymer fibers and the surrounding cementitious matrix is essential for the development of concrete reinforcement. The single fiber pull-out test (SFPT) is the standard characterization technique for testing the bond strength. However, the different phases of debonding cannot be distinguished by the SFPT. This study investigates the debonding of different polymer fibers from the surrounding cementitious matrix with a modified SFPT and proposes methods to change the SFPT setup to generate more valuable information on the debonding mechanism. The SFPT was equipped with linear variable differential transformers (LVDT), digital image correlation (DIC) and acoustic emission (AE) analysis. The results demonstrate that the modified SFPT allows a better understanding of the different phases of debonding during fiber pull-out. Furthermore, bond strength values calculated by different methods reveal that the chemical bond of the investigated polymers is not different as reported by previous studies. Deformation measurements performed using LVDTs and DIC are suitable measuring techniques to characterize the debonding mechanism in SFPT. A correlation between recorded AE and debonding phases was not found.
Grouted connections are intensively used in offshore rigs, platforms as well as jacket and monopile offshore wind turbine structures. Being located in remote offshore conditions, these connections can experience considerable adverse loading during their lifetimes. Degradation was reported inside similar connections, which were installed in the last three decades. Grouting in the offshore sites may often be proven difficult, which eventually leads to reduced load-bearing capacity of connections in the long run. Thus, repair and rehabilitation of such connections should be planned ahead to minimize operational delays and costs. In this study, scaled grouted connections were manufactured using a novel mould, whose integrity were monitored using digital image correlation (DIC). The connections were loaded under static load to visualize the main failure pattern using distributed fibre optic sensors and acoustic emission (AE) analysis. Grouted connections were then repaired using a cementitious injectable grout. The effectiveness of the grout injection was monitored using dye penetration technique. Finally, specimens are reloaded to identify the potential of such repair for grouted connections.