Filtern
Dokumenttyp
- Beitrag zu einem Tagungsband (16) (entfernen)
Schlagworte
- Carbonation (2)
- Crack formation (2)
- Cracks (2)
- Grout (2)
- Grouted connection (2)
- Repair (2)
- Shrinkage (2)
- Acoustic emission (1)
- Acoustic emission analysis (1)
- Alkali-activated materials (1)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (10)
- 7.4 Baustofftechnologie (10)
- 7.2 Ingenieurbau (6)
- 7.1 Baustoffe (2)
Grouting is a universal repair and strengthening technique, which is constantly used for structural remediation of concrete components, trenches, mine subsidence, dam joints, restoration of masonry structures, and geological stabilizations. Having an extremely small particle size of only few microns, ultrafine cements are ideal for grouting applications due to their superior permeability and compressive strength properties of the hardened cement paste compared to that of the less-expensive, but coarser ordinary Portland cements. Supplementary cementitious materials (SCMs) are often used to replace ultrafine cement in order to modify certain properties and to reduce costs. The aim of this experimental study is to investigate the effect of three supplementary materials: microsilica (MS), fly ash (FA), and metakaolin (MK) on the workability, and mechanical properties of an ultrafine cement based grout with a constant water-binder ratio and constant superplasticizer content. Maximum percentages of replacement with ultrafine cement were 6% by volume of cement for MS and 16% for FA, and MK. In general, results suggest that the workability is improved by addition of FA, whereas is reduced, when modified with MS and MK. The compressive strength of grout after cement replacement remains comparable to that of pure cement grout. However, there is a tendency of the MS to positively affect the compressive strength opposite to FA, whereas flexural strength is positively affected by FA. Based on the results, it is evident that grouts with Hägerman cone flow more than 500 mm and compressive strength of more than 90 MPa after 28 days can be produced.
Alkali-activated slag materials are known for their high Chloride penetration resistance. This makes them potentially applicable as repair systems for damaged steel-reinforced concrete structures, which are exposed to chloride attack. For this purpose, the influence of the activator composition, i.e. the SiO2 and Na2O concentration of the alkaline solution on a) the compressive strength, b) shrinkage and mass change and c) the resistance against chloride penetration of four alkali-activated slag mortars (AASM) were studied. An ordinary Portland cement-based mortar was used as the reference sample. Increasing SiO2 and Na2O concentrations increased the strength, shrinkage and mass loss of the AASMs. The resistance of the mortars against chloride penetration was evaluated using the non-steady-state migration coefficient Dnssm obtained from NT BUILD 492. The results indicate that the Dnssm is related to differences in the pore solution of the AASMs rather than to differences in their microstructure. An upcoming study of the authors is going to evaluate this hypothesis by the accelerated chloride penetration (diffusion) test.
Superplasticizer and Shrinkage Reducing Admixture Dosages for Microfine Cement in Grout Systems
(2019)
Grouts have numerous applications including crack repair as maintenance in construction industries. Microfine cements are intensively used for high strength mortar and grout products. They are ideal for injection grouting in structural repair. Such grouts should have suitable rheological properties to be injectable, especially those used in repair and rehabilitation. The use of superplasticizers (SP) in these products is thus becoming increasingly crucial to achieve favorable workability and viscosity properties. A difficulty in such grouts is the plastic shrinkage due to finer particles used. It is thus necessary to determine optimum SP and shrinkage reducing admixture (SRA) dosages for a microfine cement based grout. In this study, a saturation dosage was decided from two Polycarboxylate ether (PCE) based SPs in relation to neat cement using slump flow and rheological parameters. A range of grout mixtures was formulated containing micro silica (MS) and fly ash (FA), and tested for suitable rheological and mechanical parameters. Based on the results, a grout mixture with MS and FA was selected to determine optimum SRA content. According to the results, a SP dosage of 3% by weight of neat cement is sufficient to achieve saturation. The grout material including MS and FA can produce comparable properties to neat cement grout. MS is found to improve compressive strength within the range considered, whereas a higher FA content provides favourable rheological properties. Finally, a SRA dosage of 4%, which could reduce the shrinkage by about 43% after 28d days, is determined for the grout system.
Remediation of Cracks Formed in Grouted Connections of Offshore Energy Structures under Static Loads
(2018)
The future energy demand necessitates the exploration of all potential energy sources both onshore and offshore. Global trend has shifted towards offshore energy, which can be obtained from either carbon intensive or renewable options, hence requiring structures such as rigs, platforms, and monopiles. Most of these structures adopt easily installable construction techniques, where lower foundation need to be connected with the super structure by mean of grouted composite joints. Generally, these composite connections have exterior sleeve, interior pile and infill grout. Being located in remote offshore conditions, connections can experience considerable adverse loading during their lifetimes. Degradations were reported inside similar connections, which were installed in last three decades. Besides, grouting in the offshore sites may often be proven difficult, which eventually leads to reduced capacity of connections in the long run. Thus, repair and rehabilitation of such connections should be planned ahead to minimize operational delays and costs in the future. This study aims at characterizing the nature of crack generation in grouted connections and thereby identifying the potential of repair using suitable repair material. Scaled grouted joints were manufactured using a novel mold, and connections were loaded under static load to visualize the main failure pattern. The failure mechanism and loading capacity are found compatible to previous results from earlier literature. Grouted connection was then repaired using cementitious injectable grout. The effectiveness of the repair system is also discussed.
The authors are currently investigating the possibility to apply compaction grouting for offshore pile foundations (Jacket piles as well as monopiles) as a possible retrofitting technique for an optimised foundation concept. In this research project, we are developing a design approach aiming to predict the ideal amount and properties of a grout for a specific soil situation and desired improvement of pile bearing capacity after Installation and during service time. Both numerical and experimental tests have been carried out to investigate the injection process during which a highly viscous grout is injected into the soil under high pressure to displace and compact the surrounding soil without fracturing it. The implicit Material Point Method (MPM) based on a mixed formulation is the numerical technique chosen to deal with the expected large deformations and the arbitrary shape of the developing grout bulb. The usage of MPM prevents both the need of remeshing and the numerical instability induced by extensive mesh distortion. For validation with experimental results, we have constructed a testing chamber with one transparent sidewall. This chamber enables us to observe the injection process directly at the transparent vertical window and to measure the in-plane soil displacements and strains by means of the Digital Image Correlation (DIC) technique.
The results already reveal the interrelation of soil and grout properties for a successful usage of this common ground improvement technique.
At present, Wind Turbine Generators (WTGs) operating in onshore and offshore wind farms are primary sources of renewable energy around the world. Cylindrical grouted sleeve connections are usually adopted in these WTG structures to connect the upper structure and foundation for ease of installation. These structures including grouted connections experience considerable adverse loading during their lifetimes. Settlements were reported inside similar connections used in energy structures especially oil and gas platforms, which were installed in last three decades. Thus, repair and rehabilitation of such connections in existing wind structures should also be planned ahead to keep them operating in the future. The nature of failure and crack generation in grouted connections are crucial prior to adopt a strengthening strategy. This pilot study is carried out to actualize the failure mechanism in the grouted connection, when subjected to axial loading. A novel reusable scaled cylindrical grouted connection with shear keys was designed and tested for its load bearing behaviour. The mechanical test was accompanied by classical measuring techniques (e.g. displacement transducer) as well as non-destructive measuring techniques (e.g. digital image correlation (DIC), acoustic emission analysis (AE)). The failure mechanism incorporating slippage of the shear keys and cracking of the grout was investigated. The capacity and applicability of such test mould were also discussed. The knowledge is expected to pave way towards repair of deteriorated grouted connections with similar geometry and failure pattern.
Entwicklung eines PCC-Leichtmörtels zur Instandsetzung einer denkmalgeschützten Sichtbetonfassade
(2015)
Der Schutz und Erhalt der Originalsubstanz stehen im Mittelpunkt jeglicher denkmalpflegerischer Instandhaltungsmaßnahmen. Das äußere Erscheinungsbild spielt hierbei - im Gegensatz zur klassischen Betoninstandsetzung - eine größere Rolle. Nichtsdestotrotz dürfen die technischen Belange auch hier nicht außer Acht gelassen werden. Die Ermittlung des Ist- und Sollzustands stellt die Grundlage einer dauerhaften Instandsetzung dar. Der vorliegende Beitrag zeigt Schäden und Schadensursachen an einem denkmalgeschützten Gebäude in Leichtbetonbauweise auf. Das Bauwerk wurde hinsichtlich seines Schädigungsgrads, -umfangs und der maßgeblichen Schadensursachen untersucht. Im Rahmen dieser Untersuchungen wurden gehäuft Risse, Abplatzungen und Bewehrungskorrosion festgestellt. Die durch eine Brettschalung strukturierte Sichtbetonfassade soll im Zuge der Instandsetzungsmaßnahme möglichst originalgetreu wiederhergestellt werden.
Bei der Auswahl von geeigneten Instandsetzungsmethoden und -produkten konnte aufgrund fehlender Normen und Richtlinien für die Instandsetzung von denkmalgeschützten Leichtbetonbauten nicht auf bereits existierende Produkte und Methoden zurückgegriffen werden. Daher wurde in Anlehnung an die Richtlinie "Schutz und Instandsetzung von Betonbauteilen" (RL SIB) des DAfStB eine polymermodifizierte Betonergänzungsmasse mit leichter Gesteinskörnung entwickelt. Ausgehend von der Hauptschadensursache, der karbonatisierungsinduzierten Bewehrungskorrosion, wurden erforderliche Eigenschaften der Betonergänzungsmasse in enger Absprache mit der zuständigen Denkmalschutzbehörde und dem involvierten Fachplaner abgestimmt. Neben den grundlegenden mechanischen Eigenschaften spielen in diesem Anwendungsfall spezielle Eigenschaften wie z.B. farbliehe Anpassung der Betonergänzungsmasse, Möglichkeit der Oberflächenstrukturierung, Zeitfenster der Verarbeitbarkeit sowie die Modellierbarkeit eine wichtige Rolle. Der entwickelte PCC-Leichtmörtel berücksichtigt dabei auch den Einfluss einer geringen Schwind- und Quellneigung der Betonergänzungsmasse um Delaminierung infolge unterschiedlicher Längenänderungen zu vermeiden und somit eine dauerhafte Instandsetzung zu gewährleisten. Weiterhin wurde das Verbundverhalten des entwickelten PCCL Leichtmörtels für unterschiedliche Schichtaufbauten untersucht.
Concrete-glass windows or commonly referred to as “Dalle de Verre” windows are prevalent in historical monuments across Europe. “Dalle de Verre” windows were made by placing cut stained glasses, of various shapes and sizes, into a steel reinforced concrete frame. In addition to the steel reinforcement, a few steel wires run across the concrete elements to hold the glass windows into place. Much of these structures have been damaged due to carbonation of the thin concrete covers and consequent corrosion of the steel reinforcement; and exhibit several cracks due to the expansive nature of corrosion products formed at the steel–concrete interface. This study focussed on understanding the efficacy of electrochemical realkalisation in reinstating the passive state of the steel reinforcement embedded in such concrete glass windows. Simulant “Dalle de Verre” windows (representative of windows at Kaiser-Wilhelm Gedächtniskirche) were produced using different cements with a water/cement ratio of 0.6 and carbonated under accelerated conditions. Post carbonation, the concrete glass windows were electrochemically realkalised using a sacrificial anode. The influence of highly alkaline conditions due to electrochemical realkalisation on the glass-concrete interface has also been investigated. This study shows that the passive state of the steel reinforcement in “Dalle de Verre” windows, particularly at the Kaiser-Wilhelm Gedächtniskirche (memorial church) in Berlin, can be reinstated using the electrochemical realkalisation method.
Die Kaiser-Wilhelm-Gedächtniskirche (KWG) gilt als eine der wichtigsten Sehenswürdigkeiten Berlins in der City West und als ein herausragendes Beispiel für die „Dalle de Verre“ Verglasungen in sakralen Gebäuden. Der vorliegende Beitrag widmet sich der Fassade und den Glasfenstern des neuen Glockenturms, wobei die beschriebenen Szenarien aufgrund der annähernd gleichen Bauweise der restlichen neuen Baukörper in weiten Teilen starke Analogien aufweisen und insofern übertragbar sind.
Reinforced concrete buildings are frequently damaged by cracks, spalling and corroded
reinforcement bars. The present article focuses on the damage analysis of one of the first
buildings in Berlin that was constructed using reinforced lightweight concrete, which makes it
historically important. The compressive strength, carbonation depth, location and diameter of
reinforcement bars as well as moisture and salt profiles were determined. The carbonationinduced corrosion of the reinforcement bars represented the main damage of the building.
Certified repair mortars with lightweight aggregates (LWA) do not exist on the German
market. Therefore, an appropriate repair mortar was developed in accordance with DIN EN
1504 and the German guideline for the repair and protection of concrete structures (RL-SIB).
On the one hand, historic preservation requirements, such as: colour of the mortar,
possibilities of surface patterning, maximum preservation of the original substance and
reversibility of any Intervention must be met. On the other hand, technical requirements of the
relevant Standards must be achieved. The developed mix was designed to resist the identified
causes of deterioration. Thermal strains within the repair mortar and between the repair
mortar and the Substrate influence the crack formation and thus the durability. Therefore,
special attention was paid to the bonding and shrinking behaviour of the concrete repair
System. By using polymers, both hardened mortar properties and durability were influenced
positively.