Pure and Al-doped ZnO powders have been sintered by Spark Plasma Sintering. Al doping allows the ceramics to reach a relative density greater than 90% at a sintering temperature of 500°C. The morphology of powder nanoparticles impacts the final grain size of the sintered bulk compounds. A ceramic sintered from isotropic nanoparticles of 30 nm in diameter can reach an average grain size of 110 nm, whereas a ceramic sintered from platelets and isotropic nanoparticles exhibits an average grain size in the submicrometric range. The influence of ceramic grain size on the thermal conductivity has been investigated. It shows that substantial decrease of the grain size from several microns down to 100 nm reduces the thermal conductivity from 29.5 to 7.8 W/m K at 100°C. The stability of nanostructured ceramic has also been checked. After SPS, an annealing at 500°C in air also leads to grain growth.
The synthesis route and thermoelectric characterization of n-type Fe2-xTi1+xO5 (0 ≤ x ≤ 0.5) and Fe1.75(Ti1-yNby)1.25O5 (0 ≤ y ≤ 0.05) are presented. Their electrical conductivity obeys the small polaron model and their Seebeck coefficient is weakly dependent on temperature. The carrier concentration is increased with increasing Ti content in Fe2-xTi1+xO5, thus improving the electrical conductivity and decreasing the absolute values of the Seebeck coefficient. The composition with x = 0.5 shows reduced electrical conductivity contradicting the change in the carrier concentration, as it contains more microcracks than the other compositions. Fe2-xTi1+xO5 exhibits extremely low thermal conductivity. Fe2-xTi1+xO5 with x = 0.25 exhibits the highest ZT, ~ 0.014 at 1000 K. Therefore, a limited extent microcracks are beneficial to thermoelectric properties; however, when they are too extended they can be detrimental. On the contrary to Fe2TiO5, Nb substitution into Fe1.75Ti1.25O5 does not obviously improve its thermoelectric properties.
A wide range of solid-state synthesis routes for calcium manganate is reported in the literature, but there is no systematic study about the influence of the solid-state synthesis conditions on thermoelectric properties. Therefore, this study examined the influence of calcination temperature and calcination cycles on the Seebeck coefficient, electrical conductivity, and thermal conductivity. Higher calcination temperatures and repeated calcination cycles minimized the driving force for sintering of the synthesized powder, leading to smaller shrinkage and lower densities of the sintered specimens. As the electrical conductivity increased monotonously with increasing density, a higher energy input during calcination caused deterioration of electrical conductivity. Phase composition and Seebeck coefficient of sintered calcium manganate were not influenced by the calcination procedure. The highest thermoelectric properties with the highest power factors and figures of merit were obtained by means of reaction-sintering of uncalcined powder.