Filtern
Dokumenttyp
Sprache
- Englisch (4) (entfernen)
Referierte Publikation
- ja (4)
Schlagworte
- Dielectric spectroscopy (1)
- Layered double hydroxide (1)
- Nanocomposites (1)
- Polymer based Nanocomposites (1)
- Polymer based nanocomposites (1)
- Polymer-based nanocomposites (1)
- Polypropylene (1)
- Rigid amorphous fraction (1)
- Temperature modulated differential scanning calorimetery (1)
- Temperature modulated differential scanning calorimetry (1)
Organisationseinheit der BAM
Based on the three-phase model of semi-crystalline polymers, we determined all phase fractions of the NiAl-LDH/PLLA nanocomposites in dependence on the concentration of the nanofiller. Moreover, the rigid amorphous fraction (RAF) was separated into the RAFcrystal and the RAFfiller unbiasedly. A detailed comparison to the related nanocomposite system MgAl-LDH/PLLA was made considering that Mg and Ni have different atomic weights. As a first result is was found that NiAl-LDH/PLLA displays a higher crystallization rate compared to MgAl-LDH/PLLA, which is related to the different morphologies of the two nanocomposite systems. For both systems RAFcrystal increases with increasing concentration of the nanofiller. This means in the case of the nanocomposite not each crystal produces the same amount of RAF, as often assumed. Also, RAFfiller increases with the concentration for both systems but in a different way. This is discussed considering again the different morphologies of both nanocomposites.
Polymer based nanocomposites by melt blending of synthesized ZnAl-Layered Double Hydroxide (ZnAl-LDH) and polypropylene (PP) were investigated by temperature modulated differential scanning calorimetry (TMDSC). The LDH was organically modified by using a surfactant, sodium dodecylbenzene sulfonate (SDBS) to increase the interlayer spacing of the LDH, so that polymer segments can intercalate the inter layer galleries. The glass transition temperature (Tg) and the thermal relaxation strength (Δcp) were determined. The Tg remains constant for concentration till 12 wt% of LDH and a slight reduction of 3 K might be observed for 16 wt% LDH but within the experimental error. The thermal relaxation strength decreases indicating reduction in the amount of mobile polymer segments from amorphous fraction. This finding is supported by the increase in the rigid amorphous fraction (RAF) which is attributed to the polymer molecules which are in close proximity to the crystals and the LDH sheets, as they hinder their mobility. This is analyzed in detail and related to the dielectric relaxation spectroscopy (BDS) results.
Semicrystalline polymers have to be described by a three phase model consisting of a mobile amorphous (MAF), a crystalline (CF), and a rigid amorphous fraction (RAF). For nanocomposites based on a semicrystalline polymer the RAF is due to both the crystallites (RAFcrystal) and the filler (RAFfiller). Polymer nanocomposite based on poly(L-lactide) and MgAl layered double hydroxide nanofiller were prepared.
Due to the low crystallization rate of PLA ist crystallization can be suppressed by a high enough cooling rate, and the RAF is due only to the nanofiller. The MAF, CF, and RAF were estimated by Temperature Modulated DSC. For the first time CF, MAF, RAFcrystal, and RAFfiller could be estimated. It was found, that RAFfiller increases linearly with the concentration of the nanofiller for this system. Furthermore, RAFcrystal is only slightly influenced by the presence of the nanofiller.
A detailed calorimetric study on an epoxy-based nanocomposite system was performed employing bisphenol A diglycidyl ether (DGEBA) cured with diethylenetriamine (DETA) as the polymer matrix and taurine-modified MgAL layered double hydroxide (T-LDH) as nanofiller. The -NH2 group of taurine can react with DGEBA improving the interaction of the polymer with the filler. The combined X-ray scattering, and electron microscopy data showed that the nanocomposite has a partially exfoliated morphology. Calorimetric studies were performed with conventional DSC, temperature modulated DSC (TMDSC) and fast scanning calorimetry (FSC) in the temperature modulated approach (TMFSC) to investigate the vitrification and molecular mobility in dependence of the filler concentration. First, TMDSC and NMR were used to estimate the amount of the rigid amorphous fraction which consists of immobilized polymer segments at the nanoparticle surface. It was found to be 40 wt% for the highest filler concentration, indicating that the interface dominates the overall macroscopic properties and behavior of the material to a great extent. Second, the relaxation rates of the α-relaxation obtained by TMDSC and TMFSC were compared with the thermal and dielectric relaxation rates measured by static FSC. The investigation revealed that the system shows two distinct α-relaxation processes. Furthermore, also two separate vitrification mechanisms were found for a bulk network-former without geometrical confinement as also confirmed by NMR. This was discussed in terms of the intrinsic spatial heterogeneity on a molecular scale, which becomes more pronounced with increasing nanofiller content.