Hydration is the exothermic reaction between anhydrous cement and water, which forms the solid cement matrix of concrete. Being able to evaluate the hydration is of high interest for the use of both conventional and more climate-friendly building materials. The experimental monitoring is based on temperature or moisture measurements. The first needs adiabatic conditions, which can only be achieved in laboratory. The latter is often measured comparing the weight of the material sample before and after oven drying, which is time-consuming. This study investigates the moisture content of two cement-based and two calcium sulphate based mixtures for the first 90 days by using the calcium carbide method and oven drying at 40 °C and 105 °C (Darr method). Thereby, the amount of chemically bound water is determined to derive the degree of hydration. The calcium carbide measurements highly coincide with oven drying at 40 °C. The calcium carbide method is therefore evaluated as a suitable alternative to the time-consuming Darr drying. The prompt results are seen as a remarkable advantage and can be obtained easily in laboratory as well as in the field.
Subfloors are layered structures, consisting largely of porous building materials, such as screed. They are often suffering damage from tap water leakage, which is a typical problem in buildings, and which has largely contributed to repair costs of almost 3 billion Euro in 2018 alone in Germany. In this context, especially mould plays a role, which is both destroying the structure and posing severe health risks.
To determine the damaging effects of moisture, it is necessary to know the respective processes occurring in building materials, especially to quantify the amount of moisture and its progress in the material. In this study, humidity sensors are used to derive the material moisture experimentally.
Capacitive sensors recording the relative humidity are embedded into the screed and in the insulation materials such as expanded polystyrene, extruded polystyrene, perlite and glass wool. For the application in screed, the sensors need to be shielded against the aggressive alkaline materials. To ensure an appropriate exchange with the environment, a permeable membrane is requested. Different membrane materials have been investigated regarding their robustness and their permeability.
In the first experimental setup, two humidity sensor arrays with seven individual sensors are embedded in homogeneous screed samples. The measured corresponding relative humidity of the screed is converted to the material moisture based on the approach of Hillerborg. In a second experimental setup, a layered structure of a complete subfloor is built in a box of 0.8 m times 0.8 m. The humidity sensors are positioned in the different insulation materials of various thicknesses. By adding water, leakage damage is simulated and its progress and effect is investigated experimentally.
The investigations point at the question if the observed moisture is able to generate damage such as mould. The moisture and corresponding humidity values are discussed. It will be shown that this low-cost hygrometric approach can be used easily for moisture monitoring of screed and insulation materials as well