Filtern
Erscheinungsjahr
- 2017 (12) (entfernen)
Dokumenttyp
- Zeitschriftenartikel (8)
- Vortrag (4)
Schlagworte
- Upconversion (6)
- Quantum yield (5)
- NIR (4)
- Nanoparticle (4)
- Fluorescence (3)
- Integrating sphere spectroscopy (3)
- IR (2)
- Lanthanide (2)
- Quantum dot (2)
- Upconverion (2)
Eingeladener Vortrag
- nein (4)
Lanthanide-doped upconversion nanoparticles (UCNPs) are of great interest for biomedical applications. Currently, the applicability of UCNP bionanotechnology is hampered by the generally low luminescence intensity of UCNPs and inefficient energy Transfer from UCNPs to surface-bound chromophores used e.g. for photodynamic therapy or analyte sensing. In this work, we address the low-Efficiency issue by developing versatile core-Shell nanostructures, where high-concentration sensitizers and activators are confined in the core and Shell Region of representative hexagonal NaYF2:Yb,Er UCNPs. After Doping concentration optimization, the sensitizer-rich core is able to harvest/accumulate more excitation energy and generate almost one order of Magnitude higher luminescence intesity than conventional homogeneously doped nanostructures. At the same time, the activator Ions located in the Shell enable a ~6 times more efficient resonant energy Transfer from UCNPs to surface-bound acceptor dye molecules due to the short distance between donor-acceptor pairs. Our work provides new insights into the rational design of UCNPs and will greatly encrease the General applicability of upconversion nanotechnologies.
The rational design of brighter upconversion nanoparticles (UCNPs) requires a better understanding of the radiationless deactivation pathways in these materials. Here, we demonstrate the potential of excitation power density (P)-dependent studies of upconversion (UC) luminescence intensities, slope factors, and absolute quantum yields (ΦUC) of popular β-NaYF4:20% Yb3+,2% Er3+ UCNPs of different surface chemistries in organic solvents, D2O, and water as a tool to gain deeper insight into the UC mechanism including population and deactivation pathways particularly of the red emission. Our measurements, covering a P regime of three orders of magnitude, reveal a strong difference of the P-dependence of the ratio of the green and red luminescence bands (Ig/r) in water and organic solvents and P-dependent population pathways of the different emissive energy levels of Er3+. In summary, we provide experimental evidence for three photon processes in UCNPs, particularly for the red emission. Moreover, we demonstrate changes in the excited population dynamics via bi- and triphotonic processes dependent on the environment, surface chemistry, and P, and validate our findings theoretically
At the core of luminescence color and lifetime Tuning of rare earth doped upconverting nanoparticles (UCNPs), is the understanding of the Impact of the particle architecture for commonly used sensitizer (S) and activator (A) Ions. In this respect, a series of core@Shell NaYF4 UCNPs doped with Yb3+ and Ho3+ ions are presented here, where the same dopant concentrations are distributed in different particle architectures following the scheme: YbHo core and YbHo@..., ...@YbHo, Yb@Ho, Ho@Yb, YbHo@Yb, and Yb@YbHo core-Shell NPs. As refealed by quantitative steady-state and time-resolved luminescence studies, the relative spatial Distribution of the A and S ions in the UCNPs and their protection from surface quenching has a critical Impact on ther luminescence characteristics. Although the increased amount of Yb3+ Ions boosts UCNP Performance by amplifying the Absorption, the Yb3+ ions can also efficiently dissipate the energy stored in the material through energy Migration to the surface, thereby reducing the Overall energy Transfer Efficiency to the activator ions. The results provide yet another proof that UC Phosphor chemistry combined with materials Engineering through intentional core@shell structures may help to fine-tune the luminescence Features of UCNPs for their specific future applications in biosensing, bioimaging, photovoltaics, and Display technologies.
Trends in fluorometry and fluorescence imaging are increasing applications of molecular and nanoscale reporters with emission > 800 nm and recently also > 1000 nm for bioanalysis, medical diagnostics, bioimaging, and safety barcodes. Mandatory for the comparison of different emitter classes and the rational design of the next generation of reporters for the short wavelength infrared (SWIR) region are reliable and quantitative photoluminescence measurements in this challenging wavelength region. This is of special relevance for nanocrystalline emitters like semiconductor quantum dots and rods as well as lanthanide-based upconversion and downconversion nanocrystals, where surface states and the accessibility of emissive states by quenchers largely control accomplishable photoluminescence quantum yields and hence, signal sizes and detection sensitivities from the reporter side. Such measurements are currently hampered by the lack of suitable methods and standards for instrument calibration and validation and quantum yield standards with emission > 800 nm and especially > 1000 nm.
In this respect, we present the design of integrating sphere setups for absolute and excitation power density-dependent measurements of emission spectra and photoluminescence quantum yields in the wavelength region of 650 to 1650 nm including calibration strategies and first candidates for potential fluorescence standards. Subsequently, selected examples for spectroscopic studies of different types of nanocrystals are presented including the upconversion and downconversion emission of differently sized and surface functionalized lanthanide-doped nanoparticles
Upconversion nanoparticles (UCNPs) are attractive candidates for energy transfer-based analytical applications. In contrast to classical donor−acceptor pairs, these particles contain many emitting lanthanide ions together with numerous acceptor dye molecules at different distances to each other, strongly depending on the particle diameter.
UCNPs with precisely controlled sizes between 10 and 43 nm were prepared and functionalized with rose bengal and sulforhodamine B by a ligand-exchange procedure. Timeresolved studies of the upconversion luminescence of the UCNP donor revealed a considerable shortening of the donor lifetime as a clear hint for Förster resonance energy transfer (FRET). FRET was most pronounced for 21 nm-sized UCNPs, yielding a FRET efficiency of 60%. At larger surface-to-volume ratios, the FRET efficiency decreased by an increasing competition of nonradiative surface deactivation. Such dye-UCNP architectures can also provide an elegant way to shift the UCNP emission color, since the fluorescence intensity of the organic dyes excited by FRET was comparable to that of the upconversion emission of smaller particles.
The direct measure for the conversion efficiency of absorbed photons into emitted light by an emissive species or chromophore is the photoluminescence quantum yield (pl).1 pl is the fluorometric key quantity that controls the suitability of a molecule or material e.g. for application as a label, probe or sensor molecule or as a converter material. A straightforward approach to pl values presents their absolute determination using an integrating sphere set up. This procedure circumvents the use of standards thereby avoiding additional measurements and uncertainties related to their often debated pl values. In this respect, we discuss the experimental requirements on absolute measurements of down and upconversion quantum yields (UC), the later presents currently one of the most challenging spectroscopic measurements due to its multiphotonic character. We explore the challenges for determination of excitation power density (P) dependent pl(P), present the design and characterization of a unique integrating sphere setup for such measurements in the vis to IR spectral region including its calibration, and the influence of the excitation beam profile to perform pl measurements of liquid and solid materials.
As an example for downshifting materials we present doped core-shell CdSe/ZnS semiconductor quantum dots (d-dots) which show a nearly host material and crystal size independent emission with large Stokes shifts and minimum reabsorption.2 Systematic variation of the reaction components, parameters and thickness of the ZnS shell yielded doped nanocrystals with a very high pl, high reproducibility and large quantities. Application of these NCs in the light conversion layers of commercial monocrystalline silicon (mono-Si) solar cells led to a significant enhancement of the external quantum efficiency (EQE) of this devices in the ultraviolet spectral region between 300 and 400 nm. On the other hand, lanthanide-doped up-converting nanoparticles (UCNPs), are promising light converters from the near infrared to the visible region. These NPs show multiple narrow emission bands in the visible (vis) and NIR, excellent photostability, and long luminescence lifetimes. The rational design of brighter UCNP requires an improved understanding of the radiationless deactivation pathways, that are affected by size, surface chemistry, and microenvironment.3 We give an insight into the influences of these parameters on the photophysical key characteristics of the upconversion process such as UC(P), the luminescence decay behavior, the power dependent red-to-green intensity ratio, and intensities of the individual emission bands.
Scattering of Particles
(2017)
In a proof-of-concept study, we assessed different analytical and spectroscopic parameters for stability screening of differently sized β-NaYF4:20 mol % Yb3+, 2 mol % Tm3+ upconversion nanoparticles (UCNPs) exemplarily in the bioanalytically relevant buffer phosphate buffered saline (PBS; pH 7.4) at 37 and 50 °C. This included the potentiometric determination of the amount of released fluoride ions, surface analysis with X-ray photoelectron spectroscopy (XPS), and steady-state and time-resolved fluorescence measurements.
Based on these results, the luminescence lifetime of the 800 nm upconversion emission was identified as an Optimum parameter for stability screening of UCNPs and changes in particle surface chemistry.
The excitation wavelength (lexc) dependence of the photoluminescence (PL) quantum yield (FPL) and decay behavior (tPL) of a series of CdSe/CdS quantum dot/Quantum rods (QDQRs), consisting of the same spherical CdSe core and rod-shaped CdS shells, with aspect ratios ranging from 2 to 20 was characterized. lexc between 400–565 nm were chosen to cover the first excitonic absorption band of the CdSe core material, the onset of absorption of the CDs shell, and the region of predominant shell absorption. A strong lexc dependence of relative and absolutely measured FPL and tPL was found particularly for the longer QDQRs with higher aspect ratios. This is attributed to combined contributions from a length-dependent shell-to-core exciton localization efficiency, an increasing number of defect states within the shell for the longest QDQRs, and probably also the presence of absorbing, yet non-emitting shell material. Although the FPL values of the QDQRs decrease at shorter wavelength, the extremely high extinction coefficients introduced by the shell outweigh this effect, leading to significantly higher brightness values at wavelengths below the absorption onset of the CdS Shell compared with direct excitation of the CdSe cores. Moreover, our results present also an interesting example for the comparability of absolutely measured FPL using an integrating sphere setup and FPL values measured relative to common FPL standards, and underline the Need for a correction for particle scattering for QDQRs with high aspect ratios.