The demonstration of competency and equivalence for the assessment of levels of contaminants and nutrients in primary foodstuffs is a priority within the 10-year strategy for the OAWG Track A core comparisons. The measurements are core challenges for reference material producers and providers of calibration Services. This key comparison related to low polarity analytes in a high fat, low protein, low carbohydrate food matrix and Benzo[a]pyrene in edible oil was the model System selected to align with this class within the OAWG strategy. Evidence of successful participation in formal, relevant international comparisons is needed to document measurement capability claims (CMCs) made by national metrology institutes (NMIs) and designated institutes (Dis). 16 National Metrology Institutions participated in the Track A Key Comparison CCQM-K146 Low-Polarity Analyte in high fat food: Benzo[a]pyrene in Olive Oil. Participants were requested to evaluate the mass fractions, expressed in µg/kg, of Benzo[a]pyrene in the olive oil material. The KCRV was determined from the results of all NMIs/DIs participating in the key comparison that used appropriately validated methods with demonstrated metrological traceability. Different methods such as liquid-liquid extraction, GPC and SPE were applied in the sample pretreatment and HPLC-FLD, HPLC-MS/MS, and GC-MS or GC-MS/MS were applied for detection by the participants. The mass fractions for BaP were in the range of (1.78 to 3.09) µg/kg with Standard uncertainties of (0.026 to 0.54) µg/kg, with corresponding relative Standard uncertainties from 0.9% to 21%. Five labs withdrew their result from the Statistical evaluation of the KCRV for technical reasons. One lab was excluded from the KCRV evaluation, as they did not meet the CIPM metrological traceability requirements. A Hierarchical Bayes option was selected for the KCRV value, which was determined as 2.74 µg/kg with a Standard uncertainty of 0.03 µg/kg. The 10 institutes those were included in the calculation of the consensus KCRV all agreed within their Standard uncertainties. Successful participation in CCQM-K146 demonstrates the measurement capabilities in determining mass fraction of organic compounds, with molecular mass of 100 g/mol to 500 g/mol, having low polarity pKow < -2, in mass fraction range from 0.1 µg/kg to 1000 µg/kg in a high fat, low protein, low carbohydrate food matrix.
Recent results from a three-year multi-disciplinary project on Ancient Egyptian gold jewellery revealed that items of jewellery from the Middle Kingdom to the New Kingdom were manufactured using a variety of alluvial gold alloys. These alloys cover a wide range of colours and the majority contain Platinum Group Elements inclusions. However, in all the gold foils analysed, these inclusions were found to be absent. In this work a selection of gilded wood and leather items and gold foil fragments, all from the excavations by John Garstang at Abydos (primarily from Middle Kingdom graves), were examined using Scanning Electron Microscopy-Energy Disperse Spectroscopy (SEM-EDS), X-Ray Fluorescence (µXRF), Particle Induced X-Ray Emission (µPIXE) and Double Dispersive X-Ray Fluorescence (D²XRF). The work allowed us to characterise the composition of the base-alloys and also to reveal the presence of Pt at trace levels, confirming the use of alluvial gold deposits. Corrosion products were also investigated in the foils where surface tarnish was visually observed. Results showed that the differences in the colour of corrosion observed for the foils are related not only to the thickness of the corrosion layer but also to a multi-layer structure containing the various corrosion products.
Synchrotron radiation X-ray fluorescence spectroscopy, in conjunction with atomic absorption and Raman spectroscopy, was used to analyze a set of top brand tattoo inks to investigate the presence of toxic elements and hazardous substances. The Cr, Cu, and Pb contents were found to be above the maximum allowed levels established by the Council of Europe through the resolution ResAP(2008)1 on requirements and criteria for the safety of tattoos and permanent makeup. Raman analysis has revealed the presence of a set of prohibited substances mentioned in ResAP(2008)1, among which are the pigments Blue 15, Green 7, and Violet 23. Other pigments that were identified in white, black, red, and yellow inks are the Pigment White 6, Carbon Black, Pigment Red 8, and a diazo yellow, respectively. The present results show the importance of regulating tattoo ink composition.
Several glazed ceramic fragments (XVIth to XVIIIth centuries) from two production centers in Portugal (Coimbra and Lisbon) were the object of this study. The ones from Coimbra comprise two sets of samples: faiences and tiles. The ones from Lisbon are only tiles (azulejos, in Portuguese). The three main divisions of such pieces are the ceramic support (body), glaze and surface decoration. The system decoration/glaze is not easy to investigate, due to the high heterogeneity resulting from the mixing procedures and firing temperatures used. Moreover, the ability of the pigment to diffuse into the base glaze varies depending on the composition of both the pigment and the glaze in terms of fusibility. In order to raster these effects, high resolution techniques are required. In this work, synchrotron micro-X-ray fluorescence (µ-XRF) analysis was performed to monitor the profiles of the characteristic elements from the colors used and the glaze in well prepared cross-sections of the samples. Key elements are: Co for blue, Mn for purple, Cu for green, Sb for yellow, Pb for the glaze and Fe for the body. The major difference observed is that faiences have glaze thicknesses between 150 and 200 µm and tiles have glaze thicknesses between 350 and 400 µm. Furthermore, in faiences all the pigments except the yellow ones are well dispersed into the glassy matrix, while in tiles, all of them are just partially diffused throughout the glaze. However, differences between the tiles from Coimbra and Lisbon were observed. In the samples from Lisbon, a higher intake from the pigment throughout the glaze is observed.
This manuscript reviews the most used optical systems for X-ray microprobes and summarizes the experiences in research with synchrotron radiation as well as with X-ray tube generators.
The need for smaller beam spot sizes for various applications and the unique properties of X-rays have induced a remarkable and fast development in X-ray optical systems. These systems are divided into three main categories: diffractive, reflective and refractive. Examples of the three will be covered in this paper, highlighting the properties that allow having spot sizes down to sub-micrometer regime.
However, the extraordinary capabilities of such systems are always relative. Therefore, an overview of the techniques that use such optical systems will be given, emphasizing their applicability on several case studies.
Morphological and compositional features regarding blue and yellow pigments used in glazed ceramics from Portugal are investigated by means of a SEM/EDX system. Fragments of samples produced in the main pottery-making centres between the XVIXVIII centuries (Lisbon and Coimbra) were the objects of study. The main question to be answered is whether there are differences in the manufacturing procedures employed. For this purpose, two types of samples were analysed: faiences and wall-tiles (the famous 'Azulejos', in Portuguese). Differences between the manufacturing techniques of the two production centres were veritably found. The expected linkage between Fe–Co–Ni–As–Bi was challenging to investigate. Thus, Co was found in Fe- or Ni-rich structures, but with no structural connection to As or Bi. However, the As-needle-like structures were always identified in blue regions. One interesting finding related particularly to the blue pigment was the presence of SnO2 agglomerates throughout the whole glaze, which suggests its intentional addition for 'lightening' the well known dark Co blue. Concerning the yellow pigment differences established in the crystal shape and size are indicative of different firing temperatures used.