Composition and microstructure stability of cement compound under cyclic hydrothermal condition
(2020)
There have been many researches focused on the performance improvement of ultra-high performance concrete (UHPC) by autoclaving treatment. The goal of autoclaving is to increase the pozzolanic reaction, and to densify the cement stone and the transition zone which originates from the incorporation of supplementary cementitious materials (SCMs), such as silica fume, fly ash and blast furnace slag. Due to the superior properties, UHPC can also be utilized under high mechanical load and aggressive condition, for example, the fabrication of water tanks for thermal storage which is of great significance for saving energy and reducing CO2 emission. It is known that mineral stability of the hydration products of an inorganic binder is highly related to the temperature and pressure of the environment. A certain stable composition at room temperature, however, may undergo a phase transformation at high temperature and the performance decrease under this severe condition will generally be more severe. In this way, the rationale behind this deterioration under long-term hydrothermal condition involving many cycles and long duration has to be clarified, and then appropriate optimizing methods will be performed in order to obtain a kind of construction with high durability under aggressive environment. For this purpose, different types and amounts of SCMs are introduced into the standard mixture of UHPC and the phase compositions after autoclaving at 200 °C and 15.5 bar are determined by combined X-ray diffraction and scanning electron microscope. Mercury intrusion porosimeter is used to characterise the microstructure of the samples. In order to establish the relationship between microstructure and macroscopic properties, compressive and flexural strength are also investigated.
Inflammatory bowel diseases (IBD) comprise mainly ulcerative colitis (UC) and Crohn´s disease (CD). Both forms present with a chronic inflammation of the (gastro) intestinal tract, which induces excessive changes in the composition of the associated extracellular matrix (ECM). In UC, the inflammation is limited to the colon, whereas it can occur throughout the entire gastrointestinal tract in CD. Tools for early diagnosis of IBD are still very limited and highly invasive and measures for standardized evaluation of structural changes are scarce. To investigate an efficient non-invasive way of diagnosing intestinal inflammation and early changes of the ECM, very small superparamagnetic iron oxide nanoparticles (VSOPs) in magnetic resonance imaging (MRI) were applied in two mouse models of experimental colitis: the dextran sulfate sodium (DSS)-induced colitis and the transfer model of colitis. For further validation of ECM changes and inflammation, tissue sections were analyzed by immunohistochemistry. For in depth ex-vivo investigation of VSOPs localization within the tissue, Europium-doped VSOPs served to visualize the contrast agent by imaging mass cytometry (IMC). VSOPs accumulation in the inflamed colon wall of DSS-induced colitis mice was visualized in T2* weighted MRI scans. Components of the ECM, especially the hyaluronic acid content, were found to influence VSOPs binding. Using IMC, colocalization of VSOPs with macrophages and endothelial cells in colon tissue was shown. In contrast to the DSS model, colonic inflammation could not be visualized with VSOP-enhanced MRI in transfer colitis. VSOPs present a potential contrast agent for contrast-enhanced MRI to detect intestinal inflammation in mice at an early stage and in a less invasive manner depending on hyaluronic acid content.
Gußeisen mit Kugelgraphit und ferritischer bzw. ferritisch-perlitischer Matrix gehören zu einer Werkstoffgruppe, die ausreichende Festigkeiten mit hohen Duktilitäten verbindet. Mit der vorliegenden Arbeit wurden die Kenntnisse über die Zusammenhänge zwischen der chemischen Zusammensetzung, der Gefügeausbildung und den mechanischen Eigenschaften erweitert. Dabei wurden sowohl unterschiedliche Gießverfahren (Sand- und Kokillenguß) in der Herstellung, als auch die Auswirkungen von Umwandlungsprozessen im Gefüge infolge von Wärmebehandlungen diskutiert. Die statistische Auswertung von Einzelergebnissen aus der qualitätssichernden Begutachtung von Lager- und Transportbehältern für radioaktive Stoffe wurden durch mechanische und bruchmechanische Untersuchungen an 24 Werkstoffsorten aus Gußeisen mit Kugelgraphit ergänzt.