CO2-corrosion of injection pipe steels is a relevant safety issue when emission gasses are compressed in deep geological layers (CCS). The reliability of the steels used at the geological onshore CCS-site at Ketzin, Germany, is demonstrated in laboratory experiments under an equivalent corrosive environment (T=60 °C,p=1-60 bar, aquifer water, CO2-flow rate of 3 l/h, 700 h8000 h heat treatment). Corrosion kinetics and microstructures were characterized using samples of the heat treated steel 1.7225 (AISI 4140, 42CrMo4) used for casing, and samples of the martensitic stainless injection-pipe steel 1.4034 (AISI 420, X46Cr13).
In engineering storage sites for Carbon Sequestration the CO2-induced corrosion of injection pipe steels is a relevant safety issue when emission gasses are compressed in deep geological layers. The reliability of the steels suitable for the geological onshore CCS-site (Carbon Capture and Storage) at Ketzin, Germany, is demonstrated in laboratory experiments in equivalent corrosive environment (T = 60 °C, p = 160 bar, aquifer water, CO2-flow rate of 3 L/h, 7008000 h exposure time). Corrosion kinetics and microstructures were characterized using specimens of the heat treated steel 42CrMo4 (1.7225) used for casing, and specimens of the martensitic stainless injection-pipe steel X46Cr13 (1.4034).