Filtern
Erscheinungsjahr
Dokumenttyp
- Beitrag zu einem Tagungsband (34) (entfernen)
Schlagworte
- Weathering (9)
- Bewitterung (6)
- Spectral sensitivity (4)
- UV (4)
- Irradiation (3)
- Umweltsimulation (3)
- Artificial weathering (2)
- Bestrahlung (2)
- Polymer 3R (2)
- UV radiation (2)
Organisationseinheit der BAM
- 3 Gefahrgutumschließungen; Energiespeicher (9)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (9)
- 7 Bauwerkssicherheit (7)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (7)
- 4 Material und Umwelt (1)
- 4.0 Abteilungsleitung und andere (1)
- 4.1 Biologische Materialschädigung und Referenzorganismen (1)
To determine a polymer’s spectral response of photo degradation, two main methods have been established. The so-called “filter technique” uses polychromatic radiation, which is filtered by a set of various sharp cut-on filters. This procedure provides separated reading points of an activation spectrum of the investigated material. With the "spectrographic technique” a specimen is irradiated with pectrally dispersed radiation, locally quasi monochromatically, and the local property changes.are related to the radiant exposure at the respective wavelengths. A third method, the irradiation of specimens with quasi monochromatic radiation behind interference filters, is rarely used.
These methods have advantages and disadvantages and therefore, there are limits for conclusions from these spectral data. Concerning the quasi monochromatic Irradiation of specimens the development of new UV radiation sources looks promising.
With the rapid development of inexpensive UV Light-emitting diodes (LEDs), new : sources of nearly monochromatic radiation in the UV ränge are available, even down to about 250 nm. To determine the spectral response, the use of such UV-LEDs in TO-18 ) and TO-39 metal cases combines the advantages of low cost and energy efficiency, stable spectral irradiance, temperature.and humidity control, larger specimen areas, and an easy and stable analysis.
Combinations of different UV LEDs are also discussed as replacement for xenon arc ' radiation sources, see patent application EP01528388A1.
Drei grundlegend verschiedene Ansätze für Umweltsimulation werden an Beispielen illustriert:
(i) Ganzheitlicher Ansatz - Nachstellen von Umweltmilieus im Labor
Ziel ist hier das Nachstellen von (kombinierten) Umweltbedingungen im Labor; die Umweltparameter werden mit all ihren Wechselwirkungen aufgebracht.
Hauptnutzen ist eine gegenüber der natürlichen Beanspruchung erhöhte Reproduzierbarkeit der Umweltbedingungen. Hat man sein Laborsetup entwickelt, ist es auf verschiedene Materialien anwendbar.
Unter solchen Laborbedingungen ermittelte Lebensdauern sind dabei nicht auf die typischerweise sehr variablen Real-Umweltbedingungen übertragbar.
(ii) Parametrisierter Ansatz - Ermittlung einzelner Materialempfindlichkeiten
Hierbei werden im Labor die Wirkungen separater Umweltparameter auf Materialien nachgestellt. Für eine solche Separation der Einflussfaktoren ist insbesondere die Aufschlüsselung möglicher Wechselwirkungen der Umwelt-parameter (z.B. Mikroklima an bestrahlten Oberflächen) erforderlich. Einzelne (meist Alterungs-) Empfindlichkeiten können qualitativ nachgewiesen werden oder sogar – als Beanspruchungs-Wirkungs-Funktionen – quantifiziert werden, was einen wesentlichen Schritt in Richtung der Digitalisierung der Material¬prüfung darstellt. Insbesondere ist dann auch eine Lebensdauer-vorhersage für vorgegebene Zeitreihen der Beanspruchungs¬parameter umsetzbar.
(iii) Rückwirkungen auf die Umwelt
Umweltbeanspruchungen können zur Freisetzung von Schadstoffen in die Umwelt führen. Durch die Nachstellung kritischer, aber realitätsnaher Einsatzszenarien kann die Menge an freigesetzten Substanzen abgeschätzt werden.
Egal, welcher Ansatz verfolgt wird – ein Vergleich mit der oder einer Real-beanspruchung ist unerlässlich, ebenso wie die Messdatenaufzeichnung (data logging) aller potenziell relevanten Beanspruchungsparameter während dieser Realbeanspruchung.
Obwohl die naturnahe Umwelt – sowohl in der BAM als auch bei der GUS – gegenüber der technischen Umwelt eher untergeordnet auftritt, werden zur Illustration Beispiele aus der naturnahen Umwelt verwendet.
Radiation in the spectral ranges of UV and VIS are environmental impact factors that can cause ageing of many materials or products. The reason for this is that especially organic materials, such as food or many pharmaceutical, are subject to photochemical degradation. Of course, suited transparent packaging material may give protection against such impact for radiation sensitive fillings. But for this, it is necessary to know about the spectral range of the fillings sensitivity as well as about the radiation impact of the radiation sources that are relevant during the life time of the product.
The spectral irradiance for characterizing the emission of various radiation sources is easily measured by means of a spectroradiometer. The spectral sensitivity of a filling's property can be determined by spectrally dispersed irradiation, where the positions on a sample are related to the different wavelengths. Thus, the damaging effect of the different wavelengths can be directly evaluated. A lateral measurement of the relevant property change shows the activation spectrum, which is the product of the spectral radiant exposure and the spectral sensitivity. By measuring the spectral irradiance for each sample position, the spectral sensitivity of the ageing property can be calculated.
Comparing the fillings spectral sensitivity and the spectral irradiance of a potential radiation source during later transport and storage, conclusions can be drawn about necessary spectral absorption of a (partly) transparent packaging to give sufficient protection.
The setup for such investigation will be shown and several illustrating samples from daily food experience will be given.
Die Grenzen der Oberflächentemperaturen von Proben, die der natürlichen oder einer künstlichen Globalstrahlung ausgesetzt sind, können grob mit sog. Schwarzstandard Thermometern BST oder Weißstandard Thermometern WST ermittelt werden [ 1a) ].
Um einige Mängel der aktuellen Konstruktion zu beseitigen, wird ein neues Konzept dieser Thermometer vorgeschlagen, das sie weniger träge und ihre physikalischen Eigenschaften ähnlicher denen einer 5 mm dicken Polymerplatte macht. Es wird auch gezeigt, dass eine Anforderung an die Reaktionszeit von weniger als 1 min in EN 513 unrealistisch ist.
Es ist bekannt, dass Wellpappe als meistgenutztes Material für Gefahrgutverpackungen wesentliche Schwächen unter feuchten bzw. nassen Bedingungen zeigt. Verlässliche quantifizierbare Daten hierzu sind leider Mangelware. Obwohl das Material für den weltweiten Versand verwendet wird, werden die Zulassungsprüfungen, v.a. aus Gründen der Reproduzierbarkeit, bei Normklima durchgeführt.
Der Berstdruck als wesentliche Größe zur Materialspezifikation wird in Abhängigkeit seiner Vorgeschichte untersucht. Es werden Zeitverlauf und Reversibilität des Berstdruckes nach feuchter Konditionierung für verschiedene Wellpappen-Typen gezeigt.
Vorgestellt wird ein Aufbau zur Kopplung des Box-Compression-Tests als Bauteiltest an verschieden feuchte Klimata.
Jerrycans made from three different types of high-density polyethylene (HDPE) were exposed outdoors, for one Berlin summer season. They were filled with a 55 percent nitric acid solution (HN03), pure water, or air, and half of them were protected from sunlight by an UV absorbing canvas. Thus, the separate effects of UV radiation and nitric acid could be compared to the combined impact. Combined impact was mainly affected by decomposition of nitric acid, resulting in presence of reactive nitrogen oxides, increased oxygen partial pressure, and UV radiation energy, simultaneously in vapour phase.
To investigate the degradation effects after the outdoor exposure, jerrycans were exposed to a so called hydraulic internal pressure test, similar to an approval test for dangerous goods packaging. After combined impact of UV radiation and nitric acid, internal pressure tests showed very fast failures, whereas after separate impacts no remarkable deteriorations were observed, compared to unaged jerrycans.
Temperature is an important parameter in weathering tests. In many (photo-)chemical degradation processes a Variation of the specimen temperature by A t = + 1 °C can cause a Variation of AP(property change) by ± 8%.
Since the early eighties it is well known that some types of black panel thermometers can show temperatures that are far below the maximum surface temperature of a black specimen. Although, there were precise requirements for the black coating of the BPT, a replacement by a white coating - depending on the design of the BPT - did not really change the temperature shown by the thermometer. There was no correlation between the BPT and the specimen surface temperature.
In Europe and later at ISO the so-called black- and white-standard thermometers BST/WST were introduced. Now, there are BST and WST (ISO) and there are thermally uninsulated and insulated BPT and WPT (ASTM), partly for artificial or for outdoor exposure. And there are other adventurous procedures to determine surface temperatures.
The different types of thermometers and different procedures will be discussed and it will be shown that there is no procedure which establishes a correlation between outdoor surface temperatures and surface temperatures in artificial exposure tests.