AbstractWe report on gold clusters with around 62 gold atoms and a diameter of 1.15±0.10 nm. Dispersions of the clusters are long‐term stable for two years at ambient conditions. The synthesis was performed by mixing tetrachloroauric acid (HAuCl4 ⋅ 3 H2O) with the ionic liquid 1‐ethyl‐3‐methylimidazolium dicyanamide ([Emim][DCA]) at temperatures of 20 to 80 °C. Characterization was performed with small‐angle X‐ray scattering (SAXS), UV‐Vis spectroscopy, and MALDI‐TOF mass spectrometry. A three‐stage model is proposed for the formation of the clusters, in which cluster growth from gold nuclei takes place according to the Lifshitz‐Slyozov‐Wagner (LSW) model followed by oriented attachment to form colloidal stable clusters.
We report on the development of ultra-small core-shell silver nanoparticles synthesized by an up-scaled modification of the polyol process. It is foreseen to use these thoroughly characterized particles as reference material to compare the catalytic and biological properties of functionalized silver nanoparticles. Small-angle X-ray scattering (SAXS) analysis reveal a narrow size distribution of the silver cores with a mean radius of RC = 3.0 nm and a distribution width of 0.6 nm. Dynamic light scattering (DLS) provides a hydrodynamic radius of RH = 10.0 nm and a PDI of 0.09. The particles’ surface is covered with poly(acrylic acid) (PAA) forming a shell with a thickness of 7.0 nm, which provides colloidal stability lasting for more than six months at ambient conditions. The PAA can be easily exchanged by biomolecules to modify the surface functionality. Replacements of PAA with glutathione (GSH) and bovine serum albumin (BSA) have been performed as examples. We demonstrate that the particles effectively catalyze the reduction of 4-nitrophenol to 4-aminophenol with sodium borohydride. The tunable catalytic activity of (436 ± 24) L g-1 s-1 is the highest reported in literature for silver nanoparticles.
The breadth of applications of nanoparticles and the access to food-associated consumer products containing nanosized materials lead to oral human exposure to such particles. In biological fluids nanoparticles dynamically interact with biomolecules and form a protein corona. Knowledge about the protein corona is of great interest for understanding the molecular effects of particles as well as their fate inside the human body. We used a mass spectrometry-based toxicoproteomics approach to elucidate mechanisms of toxicity of silver nanoparticles and to comprehensively characterize the protein corona formed around silver nanoparticles in Caco-2 human intestinal epithelial cells. Results were compared with respect to the cellular function of proteins either affected by exposure to nanoparticles or present in the protein corona. A transcriptomic data set was included in the analyses in order to obtain a combined multiomics view of nanoparticle-affected cellular processes. A relationship between corona proteins and the proteomic or transcriptomic responses was revealed, showing that differentially regulated proteins or transcripts were engaged in the same cellular signaling pathways. Protein corona analyses of nanoparticles in cells might therefore help in obtaining information about the molecular consequences of nanoparticle treatment.
The elucidation of mechanisms underlying the cellular uptake of nanoparticles (NPs) is an important topic in nanotoxicological research. Most studies dealing with silver NP uptake provide only qualitative data about internalization efficiency and do not consider NP-specific dosimetry. Therefore, we performed a comprehensive comparison of the cellular uptake of differently coated silver NPs of comparable size in different human intestinal Caco-2 cell-derived models to cover also the influence of the intestinal mucus barrier and uptake-specialized M-cells. We used a combination of the Transwell system, transmission electron microscopy, atomic absorption spectroscopy, and ion beam microscopy techniques. The computational in vitro sedimentation, diffusion, and dosimetry (ISDD) model was used to determine the effective dose of the particles in vitro based on their individual physicochemical characteristics. Data indicate that silver NPs with a similar size and shape show coating-dependent differences in their uptake into Caco-2 cells. The internalization of silver NPs was enhanced in uptake-specialized M-cells while the mucus did not provide a substantial barrier for NP internalization. ISDD modeling revealed a fivefold underestimation of dose–response relationships of NPs in in vitro assays. In summary, the present study provides dosimetry-adjusted quantitative data about the influence of NP coating materials in cellular uptake into human intestinal cells. Underestimation of particle effects in vitro might be prevented by using dosimetry models and by considering cell models with greater proximity to the in vivo situation, such as the M-cell model.
Aluminum has gathered toxicological Attention based on relevant human exposure and its suspected hazardous potential. Nanoparticles from food supplements or Food contact materials may reach the human gastrointestinal tract.
Here, we monitored the physicochemical fate of aluminum containing nanoparticles and aluminum ions when passaging an in vitro model of the human gastrointestinal tract. Smallangle X-ray scattering (SAXS), transmission electron microscopy (TEM), ion beam microscopy (IBM), secondary ion beam mass spectrometry (TOF-SIMS), and inductively coupled plasma mass spectrometry (ICP-MS) in the singleparticle mode were employed to characterize two aluminumcontaining nanomaterials with different particle core materials (Al0, γAl2O3) and soluble AlCl3. Particle size and shape remained unchanged in saliva, whereas strong Agglomeration of both aluminum nanoparticle species was observed at low pH in gastric fluid together with an increased ion release. The levels of free aluminum ions decreased in intestinal fluid and the particles deagglomerated, thus liberating primary particles again. Dissolution of nanoparticles was limited and substantial changes of their shape and size were not detected. The amounts of particle-associated phosphorus, chlorine, potassium, and calcium increased in intestinal fluid, as compared to nanoparticles in standard dispersion.
Interestingly, nanoparticles were found in the intestinal fluid after addition of ionic aluminum. We provide a comprehensive characterization of the fate of aluminum nanoparticles in simulated gastrointestinal fluids, demonstrating that orally ingested nanoparticles probably reach the intestinal epithelium. The balance between dissolution and de novo complex formation should be considered when evaluating nanotoxicological experiments.
Present data indicate that the quantification of silver nanoparticle internalization revealed a clear particle-specific and coatingrelated uptake. Furthermore, a high amount of silver nanoparticles is taken up in cell models of higher complexity. Thus, an underestimation of particle effects in vitro might be prevented by considering cell models with greater proximity to the in vivo situation.
SAXS for the determination of the size distribution of nanoparticles: Application in catalysis
(2017)
The open source software packages SASfit1 and McSAS2 are widely used to determine the size distribution of nanoparticles. SASfit is based on classical curve fitting. The type of size distribution needs to be provided as constraint for analysis. Very often the lognormal size distribution is useful as shown for the characterization of single- and multimodal magnetic iron oxide particles. The use of SASfit is part of efforts to standardize analyzing methods for magnetic nanoparticles within the EU project NanoMag (www.nanomag-project.eu). In contrast to SASfit, it is not necessary to provide the type of size distribution when using the program McSAS. Both programs provide tools that allow the user to estimate uncertainties of the derived size distributions. Such is helpful in the development of nanoscale reference materials for environmental, health and safety measurements. As an example, a detailed study on using SAXS in the characterization of ultra-small-silver nanoparticles is presented. These particles are useful in the catalytic reduction of 4-nitrophenol and display an adjustable activity (see Figure).
Figure. Core-shell silver nanoparticles catalyze the reduction of 4-nitrophenol and display an increasing catalytic activity when stabilized with different ligands in the line bovine serum albumin (BSA), glutathione (GSH) and polyacrylic acid (PAA).5
Aluminum (Al) can be taken up from food, packaging, or the environment and thus reaches the human gastrointestinal tract. Its toxic potential after oral uptake is still discussed. The fate of different solid and ionic Al species during the passage through the digestive tract is the focus of this research, as well as the cellular effects caused by these different Al species. The present study combines the physicochemical processing of three recently studied Al species (metallic Al0, mineral Al2O3, and soluble AlCl3) in artificial digestion fluids with in vitro cell systems for the human intestinal barrier. Inductively coupled plasma mass spectrometry (ICP-MS) and small-angle X-ray scattering (SAXS) methods were used to characterize the Al species in the artificial digestion fluids and in cell culture medium for proliferating and differentiated intestinal Caco-2 cells. Cytotoxicity testing and cellular impedance measurements were applied to address the effects of digested Al species on cell viability and cell proliferation. Microarray-based transcriptome analyses and quantitative real-time PCR were conducted to obtain a deeper insight into cellular mechanisms of action and generated indications for cellular oxidative stress and an influence on xenobiotic metabolism, connected with alterations in associated signaling pathways. These cellular responses, which were predominantly caused by formerly ionic Al species and only at very high concentrations, were not impacted by artificial digestion. A two-directional conversion of Al between ionic species and solid particles occurred throughout all segments of the gastrointestinal tract, as evidenced by the presence of nanoscaled particles. Nevertheless, this presence did not increase the toxicity of the respective Al species.
Hydrogels with a hierarchical structure were prepared from a new highly water-soluble crosslinker N,N,N′,N′-tetramethyl-N,N′-bis(2-ethylmethacrylate)-propyl-1,3-diammonium dibromide and from the sulfobetaine monomer 2-(N-3-sulfopropyl-N,N-dimethyl ammonium)ethyl methacrylate. The free radical polymerization of the two compounds is rapid and yields near-transparent hydrogels with sizes up to 5 cm in diameter. Rheology shows a clear correlation between the monomer-to-crosslinker ratio and the storage and loss moduli of the hydrogels. Cryo-scanning electron microscopy, low-field nuclear magnetic resonance (NMR) spectroscopy, and small-angle X-ray scattering show that the gels have a hierarchical structure with features spanning the nanometer to the sub-millimeter scale. The NMR study is challenged by the marked inhomogeneity of the gels and the complex chemical structure of the sulfobetaine monomer. NMR spectroscopy shows how these complications can be addressed via a novel fitting approach that considers the mobility gradient along the side chain of methacrylate-based monomers.
A look inside nanoparticles
(2019)
Small-angle scattering is the method of choice when it comes to obtaining information about the interior of nanoparticles. The aim is to make nanotechnology safer. While the use of small-angle neutron scattering (SANS) is limited to a few instruments in the world, small-angle X-ray scattering (SAXS) is widely accessible, with an upward trend. The example of core-shell particles shows how simple their analysis is with data from an Anton Paar laboratory system. Here, SAXS is a central tool for the development of new reference materials based on poly(methyl) acrylate-PVDF core-shell particles. The dimensions of the cores and shells can be precisely determined. A detailed analysis makes it possible to show that the cores contain fluorinated and nonfluorinated polymers, whereas the shell consist only of PVDF. This core-shell particles with a diameter around 40 nm show a significantly higher PVDF beta phase content than the PVDF homopolymer when using an emulsion polymerization technique. This finding is of importance with respect to applications in electroactive devices.
The development of novel dendrimers containing oligospiroketal (OSK) rods as building blocks is described. The linkage between the core unit (CU), branching units (BU), and OSK rods relies on the CuAAC reaction between terminal alkynes and azides. Two different strategies of dendrimer synthesis were investigated and it was found that the convergent approach is clearly superior to the divergent one. SAXS measurements and MD simulations indicate that the obtained dendrimer features a globular structure with very low density. Obviously, the OSK rods stabilize a rather loose mass-fractal structure.
tNegatively charged ultrathin gold nanotriangles (AuNTs) were synthesized in a vesicular dioctyl sodiumsulfosuccinate (AOT)/phospholipid-based template phase. These “naked” AuNTs with localized surfaceplasmon resonances in the NIR region at about 1300 nm and special photothermal properties are ofparticular interest for imaging and hyperthermia of cancerous tissues. For these kinds of applicationsthe toxicity and the cellular uptake of the AuNTs is of outstanding importance. Therefore, this studyfocuses on the toxicity of “naked” AOT-stabilized AuNTs compared to polymer-coated AuNTs. Poly-meric coating consisted of non-modified hyperbranched poly(ethyleneimine) (PEI), maltose-modifiedpoly(ethyleneimine) (PEI-Mal) and heparin. The toxicological experiments were carried out with twodifferent cell lines (embryonic kidney carcinoma cell line HEK293T and NK-cell leukemia cell line YTS).This study revealed that the heparin-coating of AuNTs improved biocompatibility by a factor of 50 whencompared to naked AuNTs. Of note, the highest nontoxic concentration of the AuNTs coated with PEI andPEI-Mal is drastically decreased. Overall, this is mainly triggered by the different surface charges of poly-meric coatings. Therefore, AuNTs coated with heparin were selected to carry out uptake studies. Theirpromising high biocompatibility and cellular uptake may open future studies in the field of biomedicalapplications.
Negatively charged flat gold nanotriangles, formed in a vesicular template phase and separated by an AOT-micelle-based depletion flocculation, were reloaded by adding a cationic polyelectrolyte, that is, a hyperbranched polyethylenimine (PEI). Heating the system to 100 °C in the presence of a gold chloride solution, the reduction process leads to the formation of gold nanoparticles inside the polymer shell surrounding the nanoplatelets. The gold nanoparticle formation is investigated by UV−vis spectroscopy, small-angle X-ray scattering, and dynamic light scattering measurements in combination with transmission electron microscopy. Spontaneously formed gold clusters in the hyperbranched PEI shell with an absorption maximum at 350 nm grow on the surface of the nanotriangles as hemispherical particles with diameters of ∼6 nm. High-resolution micrographs show that the hemispherical gold particles are crystallized onto the {111} facets on the bottom and top of the platelet as well as on the edges without a grain boundary. Undulated gold nanoplatelet superstructures with special properties become available, which show a significantly modified performance in SERS-detected photocatalysis regarding both reactivity and enhancement factor.
Core-shell nanoparticles are widespread in nature, industrial applications and nanotechnology research. Facile ways of modern synthesis will be discussed and possibilities to reveal their structures with small-angle X-ray scattering (SAXS). A recent review on using block copolymer templates as one of the most reliable routes for tuning size and shape of nanoparticles is provided by Li et al.1 Ferritin and apoferritin are archetypical examples for protein-based core-shell nanoparticles. Their structures are easily accessed by synchrotron SAXS2 but also with commercial instruments and allow fast performance tests.3 SASfit4 is a suitable program tool based on classical curve fitting and McSAS5 is a complementary program based on a Monte Carlo technique. Detailed refinements of SAXS data evaluation are on the way for better data analysis.6 A sub nanometer resolution is state-of-the-art for quantification of the size distribution of polyacrylic acid stabilized silver nanoparticles.3 Such particles are useful in catalysis.7 It was observed that the catalytic activity can be tuned easily by varying the shell material of the particles.
Surface self-assembly of spherical nanoparticles of sizes below 10 nm into hierarchical heterostructures is under arising development despite the inherent difficulties of obtaining complex ordering patterns on a larger scale. Due to template-mediated interactions between oil-dispersible superparamagnetic nanoparticles (MNPs) and polyethylenimine-stabilized gold nanoparticles (Au(PEI)NPs) at the water–oil interface of microemulsions, complex nanostructured films can be formed. Characterization of the reverse microemulsion phase by UV–vis absorption revealed the formation of heteroclusters from Winsor type II phases (WPII) using Aerosol-OT (AOT) as the surfactant. SAXS measurements verify the mechanism of initial nanoparticle clustering in defined dimensions. XPS suggested an influence of AOT at the MNP surface. Further, cryo-SEM and TEM visualization demonstrated the elongation of the reverse microemulsions into cylindrical, wormlike structures, which subsequently build up larger nanoparticle superstructure arrangements. Such WPII phases are thus proven to be a new form of soft template, mediating the self-assembly of different nanoparticles in hierarchical network-like filaments over a substrate during solvent evaporation.
The structure of nanoparticles typically differs
from its bulk counterpart. Predominantly, the structures of
gold nanoparticles have been under exceedingly intense
discussion since the discovery of their high catalytic
activity. We found an increasing bond length contraction
with decreasing particle size for citrate-stabilized gold
nanoparticles in aqueous solution as determined by in situ
extended X-ray absorption fine structure (EXAFS) spectroscopy.
Particle sizes and size distributions were determined
by small-angle X-ray scattering. The analysis of the
obtained EXAFS spectra employing ab initio calculations
reveals that the Au–Au bond length undergoes a contraction
of 2 pm for nanoparticles with a radius of 2.9 nm. NIST
reference material RM 8011 gold nanoparticles with a
radius of 4.4 nm exhibit a smaller contraction of approximately
1 pm. Finally, gold atoms in RM 8013 particles
with a radius of 25.7 nm show distances of 288 pm—
identical to the distance in gold foil—and exhibits bulk-like
properties. The observed bond length contraction of gold
nanoparticles in solution is significantly smaller than
previously reported for gold nanoparticle deposited on
surfaces, which is up to 15 pm. This indicates that the
bond length contraction effect of 'free' and 'surfaceimmobilized'
nanoparticles differ fundamentally. Such
difference could be essential for the understanding of
nanoparticle-supported catalysis.
We report on the characterization of the solution structure of poly(N-vinyl-2-pyrrolidone)s (PVP) by small-angle X-ray scattering (SAXS) and by online coupling of asymmetrical flow field-flow fractionation (A4F), SAXS and dynamic light scattering (DLS). The commercial products PVP K30 and PVP K90 with nominal molar masses of 40 × 103 and 360 × 103 g mol-1, respectively, were investigated separately and as binary mixture. Detailed information for all polymer fractions is available on the polymer contour lengths and the diffusion coefficients. Key areas of applications for the A4F-SAXS-DLS coupling are seen in comparison to static light scattering for polymers with radii of gyration smaller than 10 nm, for which only SAXS produces precise analytical results on the size of the polymers in solution.
The application of appropriate analytical techniques is essential for nanomaterial (NM) characterization. In this study, we compared different analytical techniques for NM analysis. Regarding possible adverse health effects, ionic and particulate NM effects have to be taken into account. As NMs behave quite differently in physiological media, special attention was paid to techniques which are able to determine the biosolubility and complexation behavior of NMs. Representative NMs of similar size were selected: aluminum (Al0) and aluminum oxide (Al2O3), to compare the behavior of metal and metal oxides. In addition, titanium dioxide (TiO2) was investigated. Characterization techniques such as dynamic light scattering (DLS) and nanoparticle tracking analysis (NTA) were evaluated with respect to their suitability for fast characterization of nanoparticle dispersions regarding a particle's hydrodynamic diameter and size distribution. By application of inductively coupled plasma mass spectrometry in the single particle mode (SP-ICP-MS), individual nanoparticles were quantified and characterized regarding their size. SP-ICP-MS measurements were correlated with the information gained using other characterization techniques, i.e. transmission electron microscopy (TEM) and small angle X-ray scattering (SAXS). The particle surface as an important descriptor of NMs was analyzed by X-ray diffraction (XRD). NM impurities and their co-localization with biomolecules were determined by ion beam microscopy (IBM) and confocal Raman microscopy (CRM). We conclude advantages and disadvantages of the different techniques applied and suggest options for their complementation. Thus, this paper may serve as a practical guide to particle characterization techniques.
Data correction is probably the least favourite activity amongst users experimenting with small-angle X-ray scattering: if it is not done sufficiently well, this may become evident only during the data analysis stage, necessitating the repetition of the data corrections from scratch. A recommended comprehensive sequence of elementary data correction steps is presented here to alleviate the difficulties associated with data correction, both in the laboratory and at the synchrotron. When applied in the proposed order to the raw signals, the resulting absolute scattering cross section will provide a high degree of accuracy for a very wide range of samples, with its values accompanied by uncertainty estimates. The method can be applied without modification to any pinhole-collimated instruments with photon-counting direct-detection area detectors.
Fate of fluorescence labels - Their adsorption and desorption kinetics to silver nanoparticles
(2018)
Silver nanoparticles are among the most widely used and produced nanoparticles. Because of their frequent application in consumer products, the assessment of their toxicological potential has seen a renewed importance. A Major difficulty is the traceability of nanoparticles in in vitro and in vivo experiments. Even if the particles are labeled, for example, by a fluorescent marker, the dynamic exchange of ligands often prohibits their spatial localization. Our study provides an insight into the adsorption and desorption kinetics of two different fluorescent labels on silver nanoparticles with a core radius of 3 nm by dynamic light scattering, small-angle X-ray scattering, and fluorescence spectroscopy. We used BSA-FITC and tyrosine as examples for common fluorescent ligands. It is shown that the adsorption of BSA-FITC takes at least 3 days, whereas tyrosine adsorbs immediately. The quantitative amount of stabilizer on the particle surface was determined by fluorescence spectroscopy and revealed that the particles are stabilized by a monolayer of BSA-FITC (corresponding to 20 ± 9 molecules), whereas tyrosine forms a multilayered structure consisting of 15900 ± 200 molecules. Desorption experiments show that the BSA-FITC-stabilized particles are ideally suited for application in in vitro and in vivo experiments because the ligand desorption takes several days. Depending on the BSA concentration in the particles surroundings, the rate constant is k = 0.2 per day or lower when applying first order kinetics, that is, 50% of the BSAFITC molecules are released from the particle’s surface within 3.4 days. For illustration, we provide a first application of the fluorescence-labeled particles in an uptake study with two different commonly used cell lines, the human liver cell model HepG2 and the human intestinal cell model of differentiated Caco-2 cells.