Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (27)
- Beitrag zu einem Tagungsband (5)
- Beitrag zu einem Sammelband (1)
- Sonstiges (1)
- Posterpräsentation (1)
- Forschungsbericht (1)
Schlagworte
- Impurities (4)
- CO2 quality (3)
- Corrosion (3)
- Pipeline network (3)
- Recommendations (3)
- Whole-chain CCS scenario (3)
- Epoxy resin (2)
- SAXS (2)
- Additive manufacturing (1)
- Agricultural mycology (1)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (4)
- 5 Werkstofftechnik (3)
- 5.1 Mikrostruktur Design und Degradation (3)
- 7.6 Korrosion und Korrosionsschutz (3)
- 1 Analytische Chemie; Referenzmaterialien (2)
- 6 Materialchemie (2)
- 6.2 Material- und Oberflächentechnologien (2)
- 6.7 Materialsynthese und Design (2)
- 8 Zerstörungsfreie Prüfung (2)
- 1.1 Anorganische Spurenanalytik (1)
Determining the influence of impurities on the fixed-point emperatures
of the ITS-90 requires the completion of several tasks. In this paper, the Progress made at Physikalisch-Technische Bundesanstalt (PTB) and BAMFederal Institute for Materials Research and Testing is presented and remaining questions are discussed.
The projected characterization procedure at PTB, which is based on the established SIE method (sum of the individual estimates), using a new indium fixed-point cell is described as an example. This procedure includes an SI-traceable chemical Analysis of the material in the fixed-point cell with sufficiently low uncertainties, the individual experimental determination of the influence of the quantified impurities on the fixed-point temperature, and the establishment of direct links to the phase-transition temperatures of the national standard and of an assumed material of ideal purity.
A characteristic difference to the common practice is the chemical analysis of the fixed-point metal being done after determining the cells freezing temperature. This allows for the detection and consideration of contamination and purification effects due to the filling process, or due to the contact with the carbon crucible and other parts of the fixed-point cell. A chemical analysis of an indium fixed-point was carried out by BAM with relative measurement uncertainties below 30 % which have not been previously achieved. The results provide evidence for the precipitation of some impurities,
which is apparently inconsistent with the corresponding binary phase diagrams, but was explained in a recent publication. Implications for the use of the SIE method shall be described briefly at the end.
Austenitic stainless steels provide a beneficial combination of chemical and mechanical properties and have been used in a wide field of applications for over 100 years. Further improvement of the chemical and mechanical properties was achieved by alloying nitrogen. But the solubility of N within the melt is limited and can be increased in substituting Ni by Mn and melting under increased pressure. In order to avoid melting under pressure and decrease production costs, a part of N can also be substituted by C. This leads to austenitic high interstitial steels (AHIS). Within the solution annealed state strength and ductility of AHIS is comparable or even higher of those of AHNS and can be further improved by cold working. Unfortunately the endurance limit does not follow this trend as it is known from cold-worked austenitic CrNi steels. This is due to the differences of the slip behavior which is governed by the stacking fault energy as well as other near field effects. Construction components operating under cyclic loads over long periods of time cannot be considered being free of voids or even cracks. Thus the crack propagation behavior is of strong interest as well. This contribution presents the tensile, fatigue, crack propagation and fracture toughness properties of AHNS and AHIS in comparison to those of CrNi-steels. The differences are discussed in relation to microstructural characteristic as well as their alterations under cyclic loading.
A software prototype is developed for assessing and updating the reliability of single-cell prestressed concrete box girders subjected to chloride-induced reinforcement corrosion. The underlying system model consists of two integrated sub-models: a condition model for predicting the deterioration state of the box girder and a structural model for evaluating the overall system reliability. The condition model is based on a dynamic Bayesian network (DBN) model which considers the spatial variation of the corrosion process. Inspection data are included in the calculation of the system reliability through Bayesian updating on the basis of the DBN model. To demonstrate the effect of partial inspections, the software prototype is applied to a case study of a typical highway bridge with six spans. The case study illustrates that it is possible to infer the condition of uninspected parts of the structure due to the spatial correlation of the corrosion process.
Inspection and maintenance of concrete bridges is a major cost factor in transportation infrastructure, and there is significant potential for using information gained during inspection to update predictive models of the performance and reliability of such structures. In this context, this paper presents an approach for assessing and updating the reliability of prestressed concrete bridges subjected to chloride-induced reinforcement corrosion. The system deterioration state is determined based on a Dynamic Bayesian Network (DBN) model that considers the spatial variability of the corrosion process. The overall system reliability is computed by means of a probabilistic structural model coupled with the deterioration model. Inspection data are included in the system reliability calculation through Bayesian updating on the basis of the DBN model. As proof of concept, a software prototype is developed to implement the method presented here. The software prototype is applied to a typical highway bridge and the influence of inspection information on the system deterioration state and the structural reliability is quantified taking into account the spatial correlation of the corrosion process. This work is a step towards developing a software tool that can be used by engineering practitioners to perform reliability assessments of ageing concrete bridges and update their reliability with inspection and monitoring data.
We synthesized and characterized a set of ultrasmall hexagonal-phase NaGdF4: 20% Yb3+, 2% Er3+ upconversion nanoparticles with core diameters of 3.7 ± 0.5 nm. In order to assess passivation effects and the influence of possible core−shell intermixing and to identify optimum particle structures for combined imaging in the visible and near-infrared (vis−NIR: 410−850 nm) and short-wave infrared (SWIR: 1520 nm), NaYF4 shells of varying thicknesses (monolayer to 10 nm) were introduced and the influence of this parameter on the upconversion and downshifting photoluminescence of these particles was studied at different excitation power densities. This included excitation power-dependent emission spectra, slope factors, quantum yields, and excited state decay kinetics. These measurements revealed enhancement factors of the upconversion quantum yield of >10 000 in the low power region and an excitation power density-independent quantum yield of the downshifted emission at 1520 nm between 0.1 and 14%. The optimized shell thickness for combined vis and SWIR imaging was identified as 5 nm. Moreover, lifetimes and quantum yields can be continuously tuned by shell thickness which can be exploited for lifetime multiplexing and encoding. The fact that we did not observe a saturation of the upconversion quantum yield or the excited state decay kinetics with increasing shell thickness is ascribed to a strong intermixing of the active core with the inert shell during the shelling procedure. This indicates the potential of spectroscopic tools to detect cation intermixing.
Dieser Bericht beschreibt ein Systemmodell für eine integrale Ermittlung und Prognose der Schadens- und Zustandsentwicklung der Elemente eines Brückensystems unter Berücksichtigung von Ergebnissen aus Inspektionen und Überwachung. Das Systemmodell wurde anhand eines ausgesuchten Spannbetonüberbaus in einzelliger Kastenbauweise entwickelt. Es besteht aus zwei integralen Teilmodellen: ein Modell zur Beschreibung des Systemschädigungszustandes und ein Modell zur Beschreibung der Standsicherheit. Für die Modellierung des stochastischen Systemschädigungszustandes eines Brückensystems werden dynamische Bayes'sche Netze (DBN) vorgeschlagen. Dieser Ansatz ermöglicht es, alle relevanten Schädigungsprozesse und deren stochastische Abhängigkeiten zu berücksichtigen. Ein wesentlicher Vorteil dieses Ansatzes ist es, dass DBN ideal dafür geeignet sind, Bayes'sche Aktualisierungen auf Grundlage von Informationen aus Inspektionen und Überwachungsmaßnahme auf eine effiziente und robuste Art und Weise durchzuführen. Der DBN-Ansatz ist deshalb für die Entwicklung von Software für das Erhaltungsmanagement von alternden Brückenbauwerken, die vom Benutzer keine vertieften Kenntnisse der Zuverlässigkeitstheorie verlangt, ideal geeignet. Für die Modellierung der Standsicherheit eines alternden Kastenträgers wird vereinfachend Biegeversagen des globalen Längssystems betrachtet. Zur Berechnung der maximalen Traglast eines Kastenträgers infolge des Systemschädigungszustandes wird ein plastisch-plastisches Verfahren eingesetzt, wobei die Beanspruchungen mittels der Fließgelenktheorie unter Ausnutzung der plastischen Beanspruchbarkeit der Querschnitte des Kastenträgers ermittelt werden. Ein Kastenträger versagt, wenn sich durch die Ausbildung einer ausreichend großen Anzahl von Fließgelenken eine kinematische Kette ausbildet. Dieser Modellierungsansatz berücksichtigt Redundanzen, die sich aus der plastischen Beanspruchbarkeit der Querschnitte und der statischen Unbestimmtheit eines Kastenträgers ergeben. Zum Nachweis der praktischen Einsetzbarkeit des entwickelten Systemmodells wurde ein Software-Prototyp entwickelt, der eine intuitiv benutzbare graphische Benutzeroberfläche (Front-End) mit einem Berechnungskern (Back-End) koppelt. Die aktuelle Version des Software-Prototyps implementiert ein Modell der chloridinduzierten Bewehrungskorrosion und ein Tragwerksmodell, welches das Verfahrens der stetigen Laststeigerung zur Bestimmung der maximalen Traglast des Kastenträgers auf der Grundlage eines Finite-Elemente-Modells umsetzt. Zur Durchführung von Bayes'schen Aktualisierungen des Systemschädigungszustandes auf der Grundlage des DBN-Modells implementiert der Prototyp den Likelihood-Weighting-Algorithmus. Die entwickelte Architektur des Prototyps ermöglicht eine Erweiterung der Software um weitere Schädigungsprozesse. Der entwickelte Software-Prototyp ermöglicht Benutzern ohne vertiefte Kenntnisse der Zuverlässigkeitstheorie eine Berechnung des Einflusses von Bauwerksinformationen auf den Systemschädigungszustand und die Tragsicherheit eines Kastenträgers. Auf dieser Grundlage können effiziente Inspektions- und Überwachungsmaßnahmen identifiziert und das Erhaltungsmanagement optimiert werden.
The aim of this study is to develop nanometer-thin epoxy-based films on aluminium alloy AA2024-T3 as a model coating system for high resolution corrosion studies. Spin coating was used for the layer-by-layer (LbL) deposition of poly-(ethylenimine) (PEI) and poly([o-cresyl glycidyl ether]-co-formaldehyde) (CNER) bilayers. The film chemistry and the cross-linking process were characterized by means of Fourier-transform infrared spectroscopy (FTIR).
Ellipsometric data confirmed the linear increase of film thickness. The potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) results indicate the improvement of the film barrier properties with increasing film thickness. Mapping of the topography and the volta potential was performed by means of scanning Kelvin probe force microscopy (SKPFM).
The results indicate the presence of a homogeneous film structure, while the intermetallic phases can still be identified below the coating. The SKPFM Analysis confirmed that the model films are suitable for investigation of corrosion processes at the coating/metal interface.
The influence of size effects on the thermoelectric properties of thin platinum films is investigated and compared to the bulk. Structural properties, like the film thickness and the grain size, are varied. We correlate the electron mean free path with the temperature dependence of the electrical conductivity and the absolute Seebeck coefficient SPt of platinum. A measurement platform was developed as a standardized method to determine SPt and show that SPt,film is reduced compared to SPt,bulk. Boundary and surface scattering reduce the thermodiffusion and the phonon drag contribution to SPt,film by nearly the same factor. We discuss in detail on behalf of a model, which describes the temperature dependence of the absolute Seebeck coefficient, the influence of size effects of electron-phonon and phonon-phonon interaction on SPt.