Filtern
Dokumenttyp
- Beitrag zu einem Tagungsband (12) (entfernen)
Sprache
- Englisch (12)
Referierte Publikation
- ja (12) (entfernen)
Schlagworte
- Elastomeric seals (3)
- Simulation (3)
- Ageing (2)
- Aging (2)
- Compression set (2)
- Low temperature behavior (2)
- Testing (2)
- Time dependent effects (2)
- Absorption (1)
- B1uTHz-region (1)
Organisationseinheit der BAM
Dry cask storage of spent fuel and high active waste front reprocessing is licensed and established in Germany for up to 40years so far. About 10years ago, the strategy has been shifted from centralized storage using facilities in Ahaus and Gorleben to cit-site storage facilities in Order to avoid immediate cask shipping from nuclear power plants. At present, several hundred casks are stored safeiy and without any major problem. BAM is highly involved in cask specific safety evaluations within the scope of licensing procedures as well as of quality assurance procedures during cask fabrication, loading and storage.
A major prerequisite for any cask storage license is a valid transport Type B license. Subsequently, cask transportability has to be ensured at any point during the entire storage period. So far, this requirement is met by continuous maintenance of the Type B license. Anyhow, IAEA Type B regulations do not consider permanently loaded storage casks that have the sole purpose of being finally shipped öfter decades of storage inducing ageing effects. No transport safety demonstration has to be performed on aged cask components.
Rubbers are widely used as main sealing materials for Containers for low and intermediate level radioactive waste and as additional component to metal seals in spent fuel and high active waste containers. The save enclosure of the radioactive container inventory has to be guaranteed according to legislation and appropriate guidelines for long term storage periods as well as down to temperatures of -40 °C for transportation. Therefore the understanding of failure mechanisms that lead to leakage at low temperatures is necessary to ensure a proper material choice which is certainly also influenced by additional factors as e.g. the aging behavior.
Elastomers are widely used as main sealing materials in Containers for low and intermediate level radioactive waste and as additional component to metal seals in spent fuel and high active waste Containers. They are applied due to their special material properties and easy use [1]. For this application several challenging prerequisites must be met for the essential reliable Operation of the seal.
In Germany, the concept of dry interim storage in dual purpose metal casks before disposal is being pursued for spent nuclear fuel (SF) and high active waste (HAW) management. However, since there is no repository available today, the initially planned and established dry interim storage license duration of up to 40 years will be too short and its extension will become necessary. For such a storage license extension it is required to assess the long-term performance of SF and all safety related storage system components in order to confirm the viability of extended storage.
The main safety relevant components are the thick-walled dual purpose metal casks. These casks consist of a monolithic cask body with integrated neutron shielding components (polymers, e.g. polyethylene) and a monitored double lid barrier system with metal and elastomeric seals. The metal seals of this bolted closure system guarantee the required leak-tightness whereas the elastomeric seals allow for leakage rate measurement of the metal seals.
This paper presents an update on running long-term tests on metal seals at different temperatures under static conditions over longer periods of time. In addition, first results of our approach to understand the aging behavior of different elastomeric seals and neutron radiation shielding material polyethylene are discussed.
THz and Mid IR Fourier transform spectroscopy on polyethylene irradiated with Gamma- Co60 radiation
(2014)
THz and mid IR spectroscopy of high molecular PE (HMW) and ultra high molecular PE (UHMW) reveals modifications of the molecular structure induced by γ-Co60 radiation. UHMW-PE and HMW-PE can be distinguished. The integral absorption in the B1u THz-region can quantitatively describe the amorphization of crystallinity. The formation of trans vinylene unsaturations and the decay of vinyl can be followed by mid IR spectroscopy
The Bundesanstalt für Materialforschung und –prüfung (BAM) is a federal institute for materials research and testing in Germany and has been involved in the qualification and safety evaluation procedures of metal seals from the early beginning of the interim storage licensing procedures for radioactive materials, stored in dual purpose casks. Regarding this subject, BAM investigates the long-term behavior of metal seals under the influence of temperature using experimental data and analytical approaches. The development of numerical models is in progress as well. Systematic experimental investigations performed by BAM indicate a continuous decrease of the remaining seal force and the usable resilience considering the leak tightness. Hence, there is a fundamental interest of describing time and temperature dependency to gain predictable values for the long-term behavior and to achieve reliable results with help of short-term tests.
The paper gives an overview about the sealing principle, test program and test results of metal seals of the type HELICOFLEX® HN200. The aging effect, respectively the long-term behavior in dependency of time and temperature, are introduced for two different outer liner materials, aluminum and silver.
Testing and numerical simulation of elastomeric seals under consideration of time dependent effects
(2016)
Due to delays in the siting procedure to establish a deep geological repository for spent nuclear fuel and high level waste and in construction of the already licensed Konrad repository for low and intermediate level waste, extended periods of interim storage will become more relevant in Germany. BAM is involved in most of the cask licensing procedures and is responsible for the evaluation of cask-related long-term safety issues. Elastomeric seals are widely used as barrier seals for containers for low and intermediate level radioactive waste. In addition they are also used as auxiliary seals in spent fuel storage and transportation casks (dual purpose casks (DPC)).
To address the complex requirements resulting from the described applications, BAM has initiated several test programs for investigating the behavior of elastomeric seals. These include experiments concerning the hyperelastic and viscoelastic behavior at different temperatures and strain rates, the low temperature performance down to -40°C, the influence of gamma irradiation and the aging behavior.
The first part of the paper gives an overview of these tests, their relevant results and their possible impact on BAM’s work as a consultant in the framework of approval and licensing procedures.
The second part presents an approach of the development of a finite element model using the finite element code ABAQUS®. The long-term goal is to simulate the complex elastomeric behavior in a complete lid closure system under specific operation and accident conditions.
Due to delays in the siting procedure to establish a deep geological repository for spent nuclear fuel and high level radioactive waste as well as in construction of the already licensed Konrad repository for low and intermediate level radioactive waste, extended periods of interim storage become more relevant in Germany. BAM is involved in most of the cask licensing procedures and especially responsible for the evaluation of cask-related long-term safety issues.
The long-term performance of elastomer seals for lid systems of transport and storage casks, whether used as auxiliary seals in spent fuel casks or as primary seals for low and intermediate level waste packages, is an important issue in this context. The polymeric structure of these seals causes a complex mechanical behavior with time-dependent sealing force reduction.
The results of a comprehensive purpose-designed test program consisting of basic compression and tension tests as well as relaxation tests on unaged specimens of representative types of elastomers (fluorocarbon rubber (FKM) and ethylene propylene diene rubber (EPDM)) at different temperatures and strain rates are presented. They were used to identify the constitutive behavior and to obtain parameters for finite element material models provided by the computer code ABAQUS®. After estimating the influence of uncertainties such as Poisson’s ratio and friction coefficient by sensitivity analyses, the chosen parameters had to prove their suitability for the finite element simulation of the specimen tests themselves.
Based on this preliminary work the simulation of a specific laboratory test configuration containing a typical elastomer seal with circular cross section is presented. The chosen finite element material model and the implemented parameters had to show that they are able to represent not only the specimen behavior under predominantly uniaxial load but also the more complex stress states in real components. Deviations between the measured and calculated results are pointed out and discussed.
For the consideration of long-term effects in the simulation of elastomer behavior, test results of aged specimens are needed. First information about a new test program, started recently and planned to provide these data, are given.
The Bundesanstalt für Materialforschung und –Prüfung (BAM) runs an investigation program on the long-term behavior of multi-component metal seals. Such seals are used in a wide area of applications including transport and storage casks for spent nuclear fuel and high level radioactive waste.
The seal function is mainly based on the compression of the inner helical spring, which generates the necessary seal force to keep the sealing surfaces in close contact. This in turn leads to a plastic deformation of the outer jacket of the seal, comprised of highly ductile aluminum or silver that adapts to the sealing surfaces of cask body and bolted lid, thus providing high Level leak tightness. In Germany, those casks are licensed for Interim storage periods of up to 40 years or more if extended Interim storage would become necessary before a final repository is available. Thus, the sealing performance has to be evaluated, including factors like elevated temperature due to decay heat or mechanical loads due to transport under normal as well as accident conditions. Long-term investigations at BAM have been running over the last nine years to identify and evaluate the seal performance by measuring the remaining seal force, the useable resilience and the leakage rate after various time intervals at temperatures ranging from room temperature up
to 150 °C. It was found that the seal force and useable resilience decrease with time and temperature, caused by creep deformation of the outer jacket. In order to obtain an analytical description for the seal behavior and to achieve more information on the material behavior under application conditions a comprehensive investigation program with Focus on aluminum as outer jacket material was launched. The program includes material investigations such as compression and tension creep tests with representative basic materials. An additional test setup allows for the continuous measurement of the remaining seal force at temperatures of up to 150 °C. Furthermore, seal segments are compressed and stored in heating chambers, thus producing segments at different stages of the aging process. The segments are investigated regarding the development of the contact area width, jacket thickness and microstructural changes. This data will be used to develop material models and an analytical description of the time and temperature dependent long-term sealing behavior. This paper explains the current status of gained test results and modelling approaches and closes with an outlook to the future Project plans.
Elastomers show a high versatility which makes them ideal materials for sealing applications in various fields. Especially under changing application conditions the high recovery potential of this class of material is beneficial to compensate temperature or pressure fluctuation, and geometrical changes resulting from mechanical loads in e.g. accident conditions. Out of these reasons elastomers are also used in containers for low and intermediate level radioactive waste and for spent fuel transportation casks. In casks designed for low and intermediate level waste elastomer seals can act as primary seal responsible for the containment function whereas in spent fuel storage and transportation casks (dual purpose casks (DPC)) elastomer seals are used as auxiliary seals to allow leakage rate measurements of metal barrier seals. An inherent prerequisite for this kind of application is the Long time-scale of operation without or with limited possibility of seal replacement. In Germany an interim storage license for DPC`s is typically issued for 40 years, a timeframe which might increase in the future due to challenges of the final repository siting procedure. For low and intermediate level waste, also long time periods are required before final disposal can be achieved. Therefore, the performance of elastomer seals over extended time periods is, as for other applications, of high importance.
A typical approach to ensure long-term functionality is to perform accelerated aging tests to calculate an estimated lifetime by assuming e.g. Arrhenius like equations for the timetemperature relationship. This approach requires a suitable end of life criterion considering the application of interest. This often can represent a challenge on its own.
As BAM is involved in most of the cask licensing procedures and especially responsible for the evaluation of cask-related long-term safety issues we initiated several test programs for investigating the behavior of elastomer seals. Experiments concerning the low temperature performance down to -40 °C and the influence of gamma irradiation have been started first.
Currently the thermal aging behavior of elastomer seals, which is the topic of this contribution, is examined. For our aging investigations we use a broad approach to first determine the property changes in different elastomer materials due to thermo-oxidative aging at elevated temperatures and secondly, we test how the typical methods of lifetime extrapolation can be applied to these results. This Approach enables us to detect and exclude undesired side effects which very often influence lifetime estimations. In this contribution, our recent results are extended. The results show that lifetime estimation based on single material properties can be misleading and therefore a combination of several methods is recommended.