Metal seals of O-ring form are often used in lid-systems of transport and storage casks for radioactive waste in Germany. To investigate their mechanical behaviour, three dimensional (3D) finite element (FE) models were created using solid elements for all of the seal components. The material behaviour of each component is described with a unified static elastic-plastic material model. The total strain is defined as the sum of linear elastic strain and plastic strain with power-law hardening. The model was carefully validated by comparison of Simulation results with experimental results. The influence of material fluctuation of each seal component due to varying properties and the sensitivity of different seal diameters on the seal force are analysed and discussed.
The results show that the material properties of helical spring have major influence on seal force and that the influence of seal diameters is negligible small in the studied range. This is very important to use the test results from seals with small diameter for the assessment of seal behaviour with larger diameter as used in transport and storage cask.
The safety evaluation of cask components made of ductile cast iron includes investigations to prevent brittle fracture. Generally, ductile cast iron is endangered by brittle fracture especially at low temperatures (down to -40°C) and in combination with existing crack-like material defects. An applicable method is the assessment of fracture resistance using fracture mechanics according to the IAEA guidelines. The approach is based on the prevention of fracture initiation. For application of these principles for drop loads, account must be taken both of dynamic stresses within the component and dynamic material behavior. Basically, the dynamic stress intensity factor of postulated pre-existing crack-like defects is compared with the dynamic fracture toughness of the material. Applicable numerical and experimental methods for the safety assessment of cask components are demonstrated for the case of an artificially pre-cracked cylindrical cast iron cask which undergoes dynamic loading conditions as result of the hard impact between the cask and a concrete target. The proposed evaluation procedure is a combination of numerical and experimental steps. Exemplarily, the calculated stress intensity factor is compared with measured fracture toughness values from single edge notched bending specimens.