Filtern
Dokumenttyp
- Zeitschriftenartikel (11)
Referierte Publikation
- ja (11) (entfernen)
Schlagworte
- Leaching (5)
- Batch tests (2)
- Column tests (2)
- Contaminated soil (2)
- Leaching procedures (2)
- Waste materials (2)
- Antimony (1)
- Artificial weathering (1)
- Aufbereitung (1)
- Circular economy (1)
Organisationseinheit der BAM
- 4 Material und Umwelt (7)
- 4.3 Schadstofftransfer und Umwelttechnologien (7)
- 1 Analytische Chemie; Referenzmaterialien (3)
- 1.7 Organische Spuren- und Lebensmittelanalytik (2)
- 1.8 Umweltanalytik (2)
- 3 Gefahrgutumschließungen; Energiespeicher (1)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (1)
- 4.1 Biologische Materialschädigung und Referenzorganismen (1)
Paper des Monats
- ja (1)
Laboratory leaching tests may be used for source term determination as a basis for risk assessment for soilgroundwater pathways on contaminated sites. In order to evaluate different leaching procedures, batch extraction tests and percolation tests were performed using three reference materials produced from contaminated soil, demolition waste and municipal solid waste incinerator bottom ash. Emphasis was placed on the investigation of the leachability of the heavy metals copper and chromium, polycyclic aromatic hydrocarbons (PAHs) and the anions chloride and sulfate. Significant discrepancies between column experiments and batch/extraction tests were found for the release of PAHs and to a lesser extent for the heavy metals Cu and Cr. Additionally interlaboratory comparisons were conducted based on different leaching tests with the reference materials and evaluated using the criteria of comparability and reproducibility. The best reproducibility was achieved for all investigated substances in column tests. The reproducibility of batch tests was acceptable except for PAHs. The results from the experimental work will help establish standardized and feasible laboratory procedures as fundamental for substance specific risk assessment of contaminated sites.
Laboratory leaching tests may be used for source term determination as a basis for risk assessment for soilgroundwater pathway (leachate forecast) on contaminated sites in Germany. Interlaboratory comparisons on the evaluation of the reproducibility of column percolation tests were conducted within the framework of an integrated R + D program using three waste reference materials.
The interlaboratory comparisons of column percolation tests showed good reproducibility of the results for inorganic and organic parameters as well as for the accompanying parameters. This is due to the stipulations concerning the time of contact between leachant and sample material as well as the sample placement in the columns. Different column dimensions used by the participants of the interlaboratory comparisons did not have any substantial influence on the column test results.
When reusing or disposing of contaminated granular waste materials there is a need to evaluate how the contaminants will interact on the pathway soil-groundwater and the effect this interaction will have on the surrounding environment. While column testing can provide a closer approximation to field percolation conditions than batch testing, there is still a need to develop column testing procedures that consider the requirements of practical testing time frames. This study evaluates the effect of different column contact times (2.5, 5, and 16 h) on the release of inorganic constituents from bottom ash and demolition waste, two commonly reused granular materials. Leaching data for representative constituents of concern, such as copper, chromium, sulfate and chloride, as well as pH and electrical conductivity was compared for all different contact times studied.
Results for the materials investigated in this study showed that variations in contact time have no significant effect on the release of the selected constituents and leaching parameters at low liquid to solid ratios. However, after a liquid to solid ratio of 1 L/kg, the effect is more noticeable, and higher contact times show lower pH values as well as a reduction in the release of constituents of concern from bottom ash. In the case of demolition waste, the variation of contact time did not have a strong effect on the leaching behavior.
This Special Issue, ‘Measurement of the Environmental Impact of Materials’, is focused on the impact that materials have on the environmental compartments of soil, water and air. Leaching and emission processes, including underlying mechanisms, are a recurring topic in most published articles in the present Special Issue. Contributions have come from three continents and numerous countries (USA, Germany, France, Latvia, Poland, Russia, Japan, Korea and Thailand) indicating the global dimension of the subject.
Leaching tests are fundamental tools for the assessment of long-term impact of contaminated waste materials on the soil-groundwater pathway. Experiments were carried out in the framework of standardization and validation of column percolation and batch test procedures, in particular concerning the stipulation of the experimental setup. The colloid release of column and batch experiments was compared and the influence of different column filling heights (12.5–50 cm) on the release of polycyclic aromatic hydrocarbons (PAH) from soil was studied, as well as the effect of varying contact times (2.5–16 h) on the release of chromium from construction and demolition (C&D) waste and municipal solid waste incineration (MSWI) bottom ash. The results indicate that filtration of the eluate, which is required for batch tests, does not always allow the simulation of the actual colloid amount in soil pore water. Medium column heights four times the inner diameter of the column seemed to provide reasonable equilibrium adjustment conditions and avoid major biodegradation. The release of chromium was only marginally affected by the contact time, varied between 0.115 and 0.150 mg/kg for demolition waste eluate at a liquid-to-solid ratio of approximately 5 L/kg.
The potential release of hazardous substances from polymer-based products is currently in the focus of environmental policy. Environmental simulations are applied to expose such products to selected aging conditions and to investigate release processes. Commonly applied aging exposure types such as solar and UV radiation in combination with water contact, corrosive gases, and soil contact as well as expected general effects on polymers and additional ingredients of polymer-based products are described. The release of substances is based on mass-transfer processes to the material surfaces. Experimental approaches to investigate transport processes that are caused by water contact are presented. For tailoring the tests, relevant aging exposure types and release quantification methods must be combined appropriately. Several studies on the release of hazardous substances such as metals, polyaromatic hydrocarbons, flame retardants, antioxidants, and carbon nanotubes from polymers are summarized exemplarily. Differences between natural and artificial exposure tests are discussed and demonstrated for the release of flame retardants from several polymers and for biocides from paints. Requirements and limitations to apply results from short-term artificial environmental exposure tests to predict long-term environmental behavior of polymers are presented.
Potential use of incineration bottom ash in construction – Evaluation of the environmental impact
(2020)
Knowledge of the long-term leaching behavior of potentially harmful substances is crucial for the assessment of the environmental compatibility of reusing municipal solid-waste incineration bottom ash (MSWI BA) in construction, i.e., as a road base layer.
BA fractions obtained from wet-processing aiming at the improvement of environmental quality were used to investigate the mobility of relevant substances. Eluates from laboratory-scaled leaching procedures (column percolation and lysimeters) were analyzed to learn about the long-term release of substances. Unsaturated conditions and artificial rainwater (AR) were used in the lysimeter tests to simulate field conditions. In addition, batch test eluates were generated at usual liquid-to-solid ratios (L/S) for compliance testing purposes. A variety of cations and anions was measured in the eluates.
The wet treatment reduces the leaching of chloride and particularly sulfate by more than 60%. The release of typical contaminants for the treated MSWI BA such as the heavy metals Cu and Cr was well below 1% in the conducted leaching tests.
An increase in the Sb concentration observed in the lysimeter experiments starting at L/S 0.75 L/kg and in the column experiment at L/S 4 L/kg is assumed to be related to decreasing concentrations of Ca and thus to the dissolution of sparingly soluble calcium antimonate. The same leaching mechanism applies with V, but the concentration levels observed are less critical regarding relevant limit values. However, on the long term the behavior of Sb could be problematic for the application of MSWI BA in construction.
Das Recycling von gemischten Baustoffen führt neben der Herstellung von Gesteinskörnungen parallel zu einem stärker schadstoffbelasteten Stoffstrom, der circa ein Drittel der ursprünglichen Masse ausmacht. Dieser sogenannte Brechsand endet derzeit in der Deponierung und wird somit der Kreislaufwirtschaft entzogen. Der vorliegende Beitrag untersucht nun die Aufbereitung dieses Materials unter Verwendung einer Setzmaschine im Pilotmaßstab. Hierbei wird die Eignung dieser Technik evaluiert und das Aufbereitungsprodukt als möglicher Ersatzbaustoff untersucht.
For the first time, µ-X-ray fluorescence (µ-XRF) mapping combined with fluorine K-edge µ-X-ray absorption near-edge structure (µ-XANES) spectroscopy was applied to depict per- and polyfluoroalkyl substances (PFAS) contamination and inorganic fluoride in samples concentrations down to 100 µg/kg fluoride. To demonstrate the matrix tolerance of the method, several PFAS contaminated soil and sludge samples as well as selected consumer product samples (textiles, food contact paper and permanent baking sheet) were investigated. µ-XRF mapping allows for a unique element-specific visualisation at the sample surface and enables localisation of fluorine containing compounds to a depth of 1 µm. Manually selected fluorine rich spots were subsequently analysed via fluorine K-edge µ-XANES spectroscopy. To support spectral interpretation with respect to inorganic and organic chemical distribution and compound class determination, linear combination (LC) fitting was applied to all recorded µ-XANES spectra. Complementarily, solvent extracts of all samples were target-analysed via LC-MS/MS spectrometry. The detected PFAS sum values range from 20 to 1136 µg/kg dry weight (dw). All environmentally exposed samples revealed higher concentration of PFAS with a chain length >C8 (e.g. 580 µg/kg dw PFOS for Soil1), whereas the consumer product samples showed a more uniform distribution with regard to chain lengths from C4 to C8. Independent from quantified PFAS amounts via target analysis, µ-XRF mapping combined with µ-XANES spectroscopy was successfully applied to detect both point-specific concentration maxima and evenly distributed surface coatings of fluorinated organic contaminants in the corresponding samples.
Half of global material consumption involves mineral material. The circularity is still low so that the enhanced use of secondary building material is required to close loops. Three different secondary building materials are discussed based on exemplary research results: construction and demolition waste (C&D waste), soil-like material, and incineration bottom ash (IBA). Focus was placed on the environmental compatibility of the materials examined mainly by standardized leaching tests. C&D waste was investigated after a wet treatment using a jigging machine, and soil-like material and IBA were characterized with respect to their material composition. Their environmental compatibilities in particular were studied using standard leaching tests (batch tests and column tests).
It was concluded that soil-like material can mostly be utilized even when the precautionary limit values set are exceeded by a factor of less than two. For C&D waste, the fine fraction below 2 mm and the content of brick material is problematic. IBA fulfills quality level “HMVA-2” following German regulations. Improved levels of utilization might be achievable with better treatment technologies.