Filtern
Erscheinungsjahr
Dokumenttyp
Sprache
- Englisch (38)
- Deutsch (3)
- Mehrsprachig (1)
Referierte Publikation
- ja (42) (entfernen)
Schlagworte
- Rheology (13)
- Cement (9)
- Concrete (5)
- Self-compacting concrete (4)
- Adsorption (3)
- Africa (3)
- DFG SPP 2005 (3)
- Mixture composition (3)
- Rice husk ash (3)
- Superplasticizer (3)
Organisationseinheit der BAM
Effect of Polycarboxylate Superplasticizer in Ordinary Portland Cement and Sulfate Resistant Cement
(2023)
Polycarboxylate superplasticizers (PCE) are the most widely used admixtures in today’s cementitious construction materials. The molecular structure has a decisive influence on the effectiveness of PCE, which also can be tailored to serve in a different cementitious system.
The current study investigates the influence of the backbone charge density of PCE on the rheology, hydration kinetics, and adsorption behavior of ordinary Portland cement (OPC) and sulfate-resistant cement (SRC). The results indicate that regardless of the PCE type, OPC requires a higher amount of PCE to be adsorbed to induce changing of rheological parameters and hydration kinetics. Regardless of the cement type, the PCE with a higher charge density exhibits higher adsorption behavior, corresponding to lower viscosity measurement.
Compared to OPC, SRC is more sensitive to the introduction of both PCEs and has a lower saturation dosage, indicating that SRC generally provides better workability properties regardless of the PCE.
The structural build-up of fresh cement paste is often considered as a purely thixotropic phenomenon in literature even though cementitious materials undergo a non-reversible hydration process that can have an influence on the structuration process. In the current paper a method is proposed to validate the impact of the non-reversible structural build-up. It is shown that fresh cement paste samples lose their structural gain almost completely due to thixotropy while the structural build-up due to hydration can be observed but occurs in a significantly lower order of magnitude over the course of the first hours of hydration. In addition, it is shown, that the chemical component of the structural build-up accelerates with the onset of the acceleration period of hydration, while its contribution in the entire structural build-up remains constant.
Self-compacting concrete typically contains a higher content of powder materials than normal concrete. Furthermore it is assumed that the use of superplasticizers yields a more homogenous microstructure in the hardened paste. Both aspects generate a very dense microstructure, which can be assumed to cause material behaviour that differs from than normal concrete when it is exposed to elevated temperatures. However, the paste volumes in SCC can vary significantly based on the mixture composition. At a low paste volumes SCC can be very similar to normal concrete at hardened state while it can vary greatly at higher paste volumes. Since the high temperature behaviour of concrete is strongly affected by the different physical behaviour of the paste and the aggregates, it is likely that the high temperature behaviour is consequently strongly affected by the ratio of these mixture components. In the present study different SCC mixtures were observed with similar mechanical properties, but with significantly differing paste to aggregate ratios. Based on observations of the heat evolution at the fire exposed surface and at different depths inside the specimens as well as based on photogrammetric observations of the spalled dimensions, the results indicate that with increasing paste volumes the heat conductivity is reduced and as a result concrete with higher paste to aggregate ratios shows less spalling.
Numerical simulations of concrete castings are complex and time consuming. In order to decrease simulation time and to simplify simulation procedure, an innovative modelling approach, which treats reinforced sections in a formwork as porous media, was proposed. In the previous studies, this numerical model was proved suitable to simulate casting of model yield-stress fluids through reinforced elements. This article focuses on the experimental validation of the proposed model at the concrete scale. For this purpose, a large-scale laboratory casting of a highly reinforced beam is performed. The casting process is numerically simulated and the numerical results are compared to the experimental measurements.
Supplementary cementitious materials (SCM) can reduce the total amount of Portland cement clinker in concrete production. Rice husk ashes (RHA) can be converted from an agricultural by-product to a high-performance concrete constituent due to a high amount of reactive silica with pozzolanic properties if they are burnt under controlled conditions. The way and duration of combustion, the cooling process as well as the temperature have an effect on the silica form and thus, the chemical and physical performance of the RHA. Various studies on the best combustion technique have been published to investigate the ideal combustion techniques. Yet, the process mostly took place under laboratory conditions. Investigating the difference between the performance of RHA produced in a rural environment and laboratory conditions is useful for the assessment and future enhancement of RHA production, and its application both as building material, for example in rural areas where it is sourced in large quantities, and as additive for high performance concrete. Thus, the paper presents a comparison between RHA produced under rudimentary conditions in a self-made furnace in the rural Bagamoyo, Tanzania and under controlled laboratory conditions at the Technical University of Munich, Germany, with different combustion methods and temperatures. In a second step, RHA was ground to reach particle size distributions comparable to cement. In a third step, cement pastes were prepared with 10%, 20% and 40% of cement replacement, and compared to the performance of plain and fly ash blended cement pastes. The results show that controlled burning conditions around 650 °C lead to high reactivity of silica and, therefore, to good performance as SCM. However, also the RHA burnt under less controlled conditions in the field provided reasonably good properties, if the process took place with proper burning parameters and adequate grinding. The knowledge can be implemented in the field to improve the final RHA performance as SCM in concrete.
Time-resolved in situ investigation of Portland cement hydration influenced by chemical admixtures
(2016)
Numerous admixtures are used in the building practice to customize the properties of the cement paste during application. The influences of admixtures on the course of cement hydration and formation of hydrate phases have to be considered. Polycarboxylate ether (PCE) based polymeric superplasticizers (SPs) are known to retard the setting of the cement paste. The extent of the retardation differs depending on the molecular structure of the SP. Additionally, the presence of a stabilizing agent (SA) in the cement paste has a retarding side effect on the setting. The initial cement hydration processes and the detailed mechanisms of the retardation influenced by PCEs, as well as their interactions with particular SAs, are insufficiently understood. Up to now, only the results of phenomenological studies were taken into account to describe this retardation process. A detailed structure analysis monitoring the change of the phase composition during the hydration was never applied. Both SP and SA affect the adsorption of the sulphate ions on the clinker particles, causing changes in the formation of ettringite during the initial hydration, and are therefore a crucial part of the setting process itself. Here, the initial hydration of cement influenced by the interaction of SP and SA was monitored in situ by synchrotron X-ray diffraction. The high time resolution of the measurements allowed a continuous detection of the hydrates formed. The hydration was followed from the starting point of water addition and for couple of hours afterwards. The hydration of the levitated cement pellets containing starch as SA was initialized by adding aqueous solutions of different commercial SPs. Changes in the ettringite formation were detected in comparison to the reference hydration of pure cement.
Fünf verschiedene Messverfahren wurden zur Partikelgrößenanalyse von nanodispersen ZrO₂-Pulver verglichen. Mit der Laserstreulichtanalyse, der dynamischen Lichtstreuung (heterodyne DLS und homodyne DLS-PCS), der Sedimentationsanalyse im Zentrifugalfeld und der Ultraschallspektrometrie wurden wässrige ZrO₂-Suspensionen mit verschiedenen Feststoffkonzentrationen hinsichtlich ihrer Partikelgrößenverteilung analysiert. Als Referenz diente die REM-Analyse zur Ermittlung der Primärpartikelgröße (ca. 40 nm). Mit den hier vorgestellten Messverfahren konnten in den entsprechenden Suspensionen nur Sekundärpartikel im Bereich von 105 nm bis 224 nm detektiert werden, die somit auf das Vorhandensein von Aggregaten bzw. harten Agglomeraten hinweisen.
Repair is an indispensable part of the maintenance of structures over their lifetimes. Structural grouting is a widely used remediation technique for concrete components, trenches, mine subsidence, dam joints, restoration of masonry structures, and geological stabilizations. A structural grout system should be injectable in narrow spaces and hence include ingredients with finer particles. Ultrafine cements are ideal for these type of demanding grouts due to their superior properties compared to that of the less expensive, but coarser ordinary Portland cement (OPC). Supplementary cementitious materials (SCMs) are often used to replace OPC clinker based binder in order to modify certain properties and to reduce costs. The most commonly used SCMs are fly ash (FA), and ground granulated blast furnace slag (GGBS). For various special applications microsilica (MS), and metakaolin (MK) are also used. Identifying the optimum replacement contents of OPC by SCMs are a challenge during the design of such grouts. The aim of this experimental study is to investigate the effect of the selected SCMs (FA, MS and MK) on the slump flow, time of efflux, viscosity, shrinkage, and compressive and flexural strength of ultrafine cement based grouts with constant water-binder ratio and superplasticizer content. The test program was formulated using Box-Behnken design principles. Maximum percentages of replacement with ultrafine cement was 6% by volume of cement for MS and 16% for FA, and MK. The results suggest that most investigated grouts have the potential to be used for structural applications. The appropriate quadratic models are then formulated through statistical tools and presented as response surfaces. The trends indicate that fly ash improves the rheological properties, whereas microsilica and metakaolin positively affect shrinkage and mechanical properties to some extent. Based on the influence of SCMs and priorities among the properties, Decision Matrix Analysis (DMA) is carried out to select the most suitable ones among the SCMs. The analysis suggests that microsilica and fly ash are more suitable as SCMs than metakaolin without affecting the properties.
Superplasticizer and Shrinkage Reducing Admixture Dosages for Microfine Cement in Grout Systems
(2019)
Grouts have numerous applications including crack repair as maintenance in construction industries. Microfine cements are intensively used for high strength mortar and grout products. They are ideal for injection grouting in structural repair. Such grouts should have suitable rheological properties to be injectable, especially those used in repair and rehabilitation. The use of superplasticizers (SP) in these products is thus becoming increasingly crucial to achieve favorable workability and viscosity properties. A difficulty in such grouts is the plastic shrinkage due to finer particles used. It is thus necessary to determine optimum SP and shrinkage reducing admixture (SRA) dosages for a microfine cement based grout. In this study, a saturation dosage was decided from two Polycarboxylate ether (PCE) based SPs in relation to neat cement using slump flow and rheological parameters. A range of grout mixtures was formulated containing micro silica (MS) and fly ash (FA), and tested for suitable rheological and mechanical parameters. Based on the results, a grout mixture with MS and FA was selected to determine optimum SRA content. According to the results, a SP dosage of 3% by weight of neat cement is sufficient to achieve saturation. The grout material including MS and FA can produce comparable properties to neat cement grout. MS is found to improve compressive strength within the range considered, whereas a higher FA content provides favourable rheological properties. Finally, a SRA dosage of 4%, which could reduce the shrinkage by about 43% after 28d days, is determined for the grout system.