The development within the offshore wind energy sector towards more powerful turbines combined with increasing water depth for new wind parks is challenging both, the designer as well as the manufacturer of support structures. Besides XL-monopiles the jacket support structure is a reasonable alternative due to the high rigidity combined with low material consumption. However, the effort for manufacturing of the hollow section joints reduces the economic potential of jacket structures significantly. Therefore, a changeover from an individual towards a serial production based on automated manufactured tubular joints combined with standardized pipes must be achieved. Hence, this paper addresses the welding process chain of automated manufactured tubular joints including digitization of the relevant manufacturing parameters such as laser scanning of the weld seam geometry. Additionally, a methodology for the computation of the notch radius as well as the weld seam angle is presented based on the scanned profiles of three analysis points of an automated manufactured tubular X-joint. Subsequently, these parameters are considered within the notch stress approach based fatigue design and their impact is quantified by a comparison with the structural stress approach using equivalent stress concentration factors.
The development within the offshore wind sector towards more powerful turbines combined with increasing water depth for new wind parks is challenging both the designer as well as the manufacturer of bottom fixed support structures. Besides XL-monopiles, the market developed an innovative and economic jacket support structure which is based on automatically manufactured tubular joints combined with standardized pipes. Besides the improvements for a serial manufacturing process the automatically welded tubular joints show a great potential in terms of fatigue resistance e.g. due to a smooth weld geometry without sharp notches. However, these benefits are not considered yet within the fatigue design process of automatically manufactured jacket substructures according to current standards due to the lack of suitable S-N curves. Therefore, 32 axial fatigue tests on single and double-sided automatically welded tubular X-joints have been performed to determine a new hot spot stress related S-N curve. Based on these constant amplitude fatigue tests a new S-N curve equal to a FAT 126 curve was computed which implicitly includes the benefits of the automatically welding procedure.
To increase the competitiveness of jacket substructures compared to monopiles a changeover from an individual towards a serial jacket production based on automated manufactured tubular joints com-bined with standardized pipes has to be achieved. Therefore, this paper addresses fatigue tests of automatical-ly welded tubular X-joints focusing on the location of the technical fatigue crack. For this X-joint, the detect-ed location of the technical crack is then compared to numerical investigations predicting the most fatigue prone notch considering the structural stress approach as well as the notch stress approach. Additionally, the fatigue prone hot spot according to both approaches is compared for a typical offshore jacket double-K-joint to emphasize the significance of the presented outcomes for the existing offshore structures. Besides, the welding process of the automated manufactured tubular X-joints is presented.
Reaktive Brandschutzsysteme finden im baulichen Brandschutz Anwendung zur Erhöhung des Feuerwiderstands von Stahlkonstruktionen. Neben den Anforderungen an die Feuerwiderstandsdauer können damit auch Ansprüche an die Ästhetik erfüllt werden. Die profilfolgende Applikation und die geringen Trockenschichtdicken der Produkte ermöglichen es, das filigrane Erscheinungsbild von Stahlkonstruktionen aufrechtzuerhalten. Neben der thermischen Schutzwirkung muss auch die Dauerhaftigkeit der Brandschutzbeschichtung sichergestellt werden. Die Bewertungsmethoden, die auf europäischer Ebene durch das EAD 350402-00-1106 zur Verfügung stehen, zielen auf eine Nutzungsdauer von zehn Jahren ab. Prüfverfahren für einen darüber hinausgehenden Zeitraum sind nicht beschrieben. In diesem Beitrag werden experimentelle Untersuchungen zum Einfluss der Bewitterung auf das Expansionsverhalten, zur thermischen Schutzwirkung und zu den während des Aufschäumens im Brandfall stattfindenden Reaktionen vorgestellt. Die Versuche wurden an einem wasserbasierten und einem epoxidharzbasierten reaktiven Brandschutzsystem durchgeführt. Die Ergebnisse wurden im Rahmen des IGF-Forschungsvorhabens 20470 N erzielt.