Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (219) (entfernen)
Schlagworte
- Flame retardancy (52)
- Flame retardant (26)
- Flammability (25)
- Flame retardance (22)
- Cone calorimeter (20)
- Epoxy resin (20)
- Nanocomposites (19)
- Fire retardancy (17)
- Pyrolysis (16)
- Nanocomposite (15)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (74)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (74)
- 7.3 Brandingenieurwesen (4)
- 6 Materialchemie (3)
- 7.1 Baustoffe (2)
- 5 Werkstofftechnik (1)
- 5.3 Polymere Verbundwerkstoffe (1)
- 6.0 Abteilungsleitung und andere (1)
- 6.3 Strukturanalytik (1)
- 6.6 Physik und chemische Analytik der Polymere (1)
- 8 Zerstörungsfreie Prüfung (1)
- 8.5 Röntgenbildgebung (1)
Paper des Monats
- ja (2)
The recently approved EU Construction Products Regulation (CPR) applies to cables as construction products.
The difficulty of predicting the fire performance of cables with respect to propagation of flame and contribution to fire hazards is well known. The new standard EN 50399 describes a full-scale test method for the classification of vertically mounted bunched cables according to CPR. Consideration of the material, time, and thus cost requires an alternative bench-scale fire test, which finds strong demand for Screening and development purposes. The development of such a bench-scale fire test to assess the fire Performance of multiple vertically mounted cables is described. A practical module for the cone calorimeter is proposed, simulating the fire scenario of the EN 50399 on the bench scale. The efficacy of this module in predicting full-scale CPR test results is shown for a set of 20 different optical cables. Key properties such as peak heat release rate (PHRR), fire growth rate (FIGRA), and flame spread are linked to each other by factors of around 5. In a case study, the bench-scale test designed was used to investigate the influence of the main components on the fire behaviour of a complex optical cable.
The effects of reducing specimen size on the fire behavior of polymeric materials were investigated by means of the rapid mass calorimeter, a high-throughput Screening instrument. Results from the rapid mass calorimeter were compared with those from the cone calorimeter. Correlation coefficients between the different measures of each method and between the two methods are discussed to elucidate the differences and similarities in the two methods. Materials with characteristic heat release rate (HRR) curves in the cone calorimeter were evaluated in detail. The rapid mass calorimeter produces valuable and interpretable results with HRR curve characteristics similar to cone calorimeter results. Compared to cone calorimeter measurements, material savings of 96% are achieved, while maintaining the Advantages of a macroscopic fire test.
Flexible polyurethane foams with densities of 40 ± 2 kg m−3 were prepared by combining different ecofriendly fillers such as layered double hydroxides (LDH) and kraft lignin (a byproduct of the pulp and paper industry) with a phosphorous polyol (E560) in order to study their effect on the mechanical performance and fire behavior of the foams. Two series of foams were prepared, some containing lignin or LDH separately, and some with a combination of both: one of the series was prepared without E560 (0E foam series) and the other with 5 parts per hundred of E560 polyol (5E series). The use of fillers resulted in increased viscosity of the reactive mixture, requiring higher blowing agent content in order to hold the density of the foams constant. It was observed that urea phase segregation was favored in the series of 0E foams due to their lower viscosity than the 5E series. This had consequent effects on the resilience, compression force deflection and compression set of these foams. In terms of fire behavior it was observed that while the limiting oxygen index decreased, cone calorimeter results showed that the combination of lignin, LDH and E560 decreased the heat release of the foams. In addition, the combination of fillers and E560 contributed to increase the viscosity of the pyrolysis products, preventing the dripping of the molten polymer, which is a key factor in flame propagation towards adjacent objects in fire scenarios.
Polyurethanes (PU) represent one of the most versatile classes of plastics. They are processed and used as thermoplastic, elastomer, and thermoset. The requirements regarding flammability are correspondingly versatile. Depending on the material and the field of application, specific fire tests have to be fulfilled. This paper describes the different concepts used to fulfil these requirements by choosing the right raw materials and flame retardants.
As most of polymeric materials are inherently flammable, flame retardants (FR) are commonly used to reduce their fire risks. Nevertheless, these flame retardant materials are often detrimental to smoke parameters like specific optical density or smoke toxicity. The influence of several smoke suppressants (SP)-zinc stannate, zinc phosphate, titanium oxide and hydrotalcite-were investigated with respect to flame retardancy, smoke emission, particle emission and smoke toxicity in a diethyl aluminum phosphinate (AlPi) flame retardant polyamide 6.6 (PA6.6). It was shown that the interaction between SP, FR and polymer is crucial for smoke and fire properties and can change the mode of action of the FR as well the decomposition mechanism of the polymer. Small amounts of SP show less effect on forced flaming behavior and the optical density, but they can influence flammability and the particle size distribution of the soot particles. The flame retardancy was significantly enhanced by 5 wt.-% zinc stannate in PA6.6 under forced flaming conditions. The charring mechanism was improved, and the mode of action of AlPi switched from the gas to the condensed phase. This resulted of in a reduced PHRR and TSP and an increase in residue yield. The smoke toxicity and optical density were reduced in the smoke density chamber as well. The smoke particles shifted to smaller sizes as the time in the pyrolytic zone increased. The formation of a dense char is assumed to be the key factor to enhance smoke suppression and flame retardancy properties.
Most of the polymeric materials used are easy to ignite and show extensive flame spread along their surfaces. Apart from extensive heat release rates, their short time to ignition (tig), in particular, is a key fire hazard. Preventing ignition eliminates fire hazards completely. Protection layers that shift tig by more than an order of magnitude are powerful flame retardancy approaches presenting an alternative to the usual flame retardancy concepts.
Coatings are proposed that consist of a three-layer system to ensure adhesion to the substrate, acting as an infrared (IR) mirror and protecting against oxidation. The IR-mirror layer stack is realised by physical vapour deposition in the sub-micrometre (<1 µm) range, reducing heat absorption by up to an order of magnitude. Not only is the ease of ignition diminished (tig is increased by several minutes), the flame spread and fire growth indices are also remarkably reduced to as little as 1/10 of the values of the uncoated polymers open for further optimization. Sub-micrometre thin IR-mirror coatings yielding surface absorptivity <0.1 are proposed as a novel and innovative flame retardancy approach.
An experimental and numerical investigation of the effect of bisphenol A bis(diphenyl phosphate) (BDP) and polytetrafluoroethylene (PTFE) on the fire behaviour of bisphenol A polycarbonate/acrylonitrile butadiene styrene (PC/ABS) in the vertical UL 94 scenario is presented. Four PC/ABS blends were discussed, which satisfy different UL 94 classifications due to the competing effects of gasification, charring, flame inhibition and melt flow/dripping. For numerical investigation, the particle finite element method (PFEM) is used. Its capability to model the complex fire behaviour of polymers in the UL 94 is analysed. The materials' properties are characterised, in particular the additives impact on the dripping behaviour during thermal exposure. BDP is an efficient plasticiser; adding PTFE prevents dripping by causing a flow limit. PFEM simulations reproduce the dripping and burning behaviour, in particular the competition between gasification and dripping. The thermal impact of both the burner and the flame is approximated taking into account flame inhibition, charring and effective heat of combustion. PFEM is a promising numerical tool for the investigation of the fire behaviour of polymers, particularly when large deformations are involved. Not only the principal phenomena but also the different UL 94 classifications and the extinction times are well predicted.
Two different numerical simulation tools, Fire Dynamic Simulator (FDS) and ThermaKin, are investigated with respect to their capability to predict the mass loss rate of polymer materials exposed to different fires. For validation, gasification apparatus and cone calorimeter tests are conducted. The main focus is on the influence of residue formation. Therefore, poly (butylene terephthalate) (PBT) and PBT reinforced with glass fibres (PBT-GF) are investigated and compared. PBT decomposes almost completely, while PBT-GF forms residue. The materials are characterised in order to provide suitable input parameters. Additionally the total incident heat flux to the sample is measured. With accurate input parameters, FDS and ThermaKin predicted the pyrolysis behaviour of PBT very well. Only some limitations are identified regarding the residue-forming PBT-GF. Both numerical simulation tools demonstrate a high value regarding the assessment of parameters' relative impacts and thus the evaluation of optimisation routes in polymer and composite development.
The pyrolysis and fire behavior of glass-fiber reinforced poly(butylene terephthalate) (PBT/GF) with two different metal phosphinates as flame retardants in combination with and without melamine cyanurate (MC) were analyzed by means of thermogravimetry, thermogravimetry coupled with infrared spectroscopy, flammability, and cone calorimeter tests as well as scanning electron microscopy/energy dispersive X-ray spectroscopy and X-ray fluorescence spectroscopy. In PBT/GF, dosages of 13-20% of the halogen-free flame retardant aluminum phosphinate or aluminum phosphinate in combination with MC fulfill the requirements for electrical engineering and electronics applications (UL 94 = V-0; LOI > 42%), whereas the use of the same amount of zinc phosphinate or zinc phosphinate in combination with MC does not improve the fire behavior satisfactorily (UL 94 = HB; LOI = 27-28%). The performance under forced flaming conditions (cone calorimeter) is quite similar for both of the metal phosphinates. The use of aluminum and zinc salts results in similar flame inhibition predominantly due to the release of the phosphinate compounds in the gas phase. Both metal phosphinates and MC interact with the polymer changing the decomposition characteristics. However, part of the zinc phosphinate vaporizes as a complete molecule. Because of the different decomposition behavior of the metal salts, only the aluminum phosphinate results in a small amount of thermally stable carbonaceous char. In particular, the aluminum phosphinate-terephthalate formed is more stable than the zinc phosphinate-terephthalate. The small amount of char has a crucial effect on the thermal properties and mechanical stability of the residue and thus the flammability.
Fire stability of glass-fibre sandwich panels: The influence of core materials and flame retardants
(2017)
Fire resistance has become a key property for structural lightweight sandwich components in aviation, shipping, railway vehicles, and construction. The development of future composite materials and components demands adequate test procedures for simultaneous application of compression and fully developed fire. Therefore an intermediate-scale approach (specimen size = 500 mm x 500 mm) is applied with compressive loads (up to 1 MN) and direct application of a burner to one side of the specimens, as established in aviation for severe burn-through tests. The influence of different core structures (polyvinylchloride foam, polyisocyanorate foam reinforced by stitched glass bridges, and balsa wood) was investigated for glass-fibre-reinforced sandwich specimens with and without flame retardants applied on the fabrics, in the matrix, and on surface for each specimen at the same time. Times to failure were increased up to a factor of 4. The intumescent coating prolongs the time to failure significantly.
What is more, using the intrinsic potential of the front skin together with the core to protect a load bearing back skin in sandwich panels, the design of the core – here using the wood core – is the most promising approach.