With our experiments we want to simulate a load situation which can result from a cask vertical drop test. The lid can lift a little for a very short moment and that can perhaps result in a little movement of the seal, a little rotation or a little lateral movement, so that the contact section can change. The aim of the project is to learn more about the sealing efficiency after the seal is compressed again. What we know from former component tests with non-aged seals is, that the leakage rate measured after one or more decompression /compression cycles with seal movement becomes significant higher. And this result is considered for specification of design leakage rates for release calculation in safety cases.
In the recent years we all have learned more about the significant influence of temperature and time on seal behavior and so the plan was to do similar experiments with aged seals, just to get an idea about seal behavior and achievable leakage rates.
What we did in detail is:
We compressed Helicoflex-seals of both design types, with Aluminum and Silver outer jackets, in testflanges and aged them in an oven at a temperature of 125°C for 3 months to produce seal properties comparable with properties after several years use at more typical operating temperatures between 90 and 100°C.
After this ageing procedure we opened the flanges completely, moved the seal a little to vary the contact area and compressed the flanges again. What we measured during all compression and decompression cycles was the load, the deformation and -as long as possible- the leakage rates.
In accordance with the IAEA transport regulations Special Form Radioactive Material (SFRM) is either an indispersible solid radioactive material or a sealed capsule containing radioactive material.
The design of special form radioactive material has to resist a severe transport accident without undue loss or dispersal of radioactive material. The safety assessment for design approval shall include besides the required test program (impact, percussion, bending and heat test) also the evaluation of the management system for design, manufacture, testing, documentation, use, maintenance and inspection. The specified quality assurance measures have to assure, that every specimen of the approved design is produced in the same verified quality and every specimen must be able to survive the severe mechanical and thermal tests at any time of its working life.
Due to the long-term use of SFRM the consideration of ageing is an important aspect in the approval procedure by BAM, the competent authority for SFRM approval in Germany. Different fields of application imply a wide range of environmental conditions, from clean room atmosphere to highly aggressive industrial conditions. So, besides of radioactive content, corrosion is a main factor for possible design degradation.
This paper will describe major influencing factors to be taken into account to assess the ageing behavior of a SFRM design and will emphasize that there is a need for a regulatory specification of a SFRM-working life as basis for the aging evaluations.
In accordance with the IAEA transport regulations, the design of special form radioactive material (SFRM) shall resist a severe transport accident without undue loss or dispersal of radioactive material. The safety assessment for design approval includes besides the program for physical tests (impact, percussion, bending and heat test) also the evaluation of the management system for design, manufacture, testing, documentation, use, maintenance, and inspection.
SFRM source design plus management system shall ensure, that every specimen of the approved design is able to survive the severe mechanical and thermal tests at any time of its SFRM-working life.
Due to the long-term use of SFRM designs in most cases, the assessment of the source ageing behavior is an important aspect in the approval procedure. Different fields of application imply a wide range of environmental conditions, from clean room atmosphere to highly aggressive industrial conditions. Besides of radioactive content, corrosion is a main factor for possible SFRM design degradation.
Although the IAEA Advisory Material SSG-26 already implies an indication of the need for considering ageing mechanisms, suitable amendments in the regulatory requirements of SSR-6 should be introduced to make the approval procedure more transparent and help to reduce rounds of questions by the authority. A supplementary requirement for considering of ageing mechanisms could be a helpful contribution to an international harmonization of the approval procedure.
This paper will describe major influencing factors to be considered to assess the ageing behavior of a SFRM design and will identify the need for a regulatory specification of a SFRM-working life as basis for the assessment of the SFRM design regarding time-dependent weakening. A proposal for an explicit requirement for consideration of ageing mechanisms in safety assessment of SFRM, which should be considered in the ongoing SSR-6 revision cycle, will be explained.
Acceptable limits for activity release from transport casks for high-level radioactive material specified in the IAEA regulations must be kept by the integrity of cask body and the cask sealing system. BAM as the German competent authority for mechanical, thermal and containment assessment of packages liable for approval verifies the activity release compliance with the regulatory limits. One of the fundamental aspects in assessment is the specification of conservative package design leakage rates.
To ensure the required package tightness for both, storage, and transport of the cask before and after storage usually metal seals of the Helicoflex® Type are used. Due to the long-term use the seal behavior is influenced by temperature and time. The mechanical and thermal loadings associated with the routine, normal and accident conditions of transport specified in the regulations can have a significant effect on the leak tightness of the sealing system. Whereas the safety for application of new, non- aged Helicoflex® seals is verified sufficiently, there are still technical data gaps concerning the efficiency of aged Helicoflex® seals.
BAM performed experiments to learn more about the sealing efficiency of aged Helicoflex® seals with Aluminum and Silver outer jackets. The seals were compressed in test-flanges and for artificial ageing the complete flange systems were stored in an oven for several month at a high temperature. During the compression and decompression tests after the aging, load-deformation characteristics of the seals, and leakage rates were measured. With these tests a load situation was simulated, which can occur in the regulatory drop test of the cask: Under high impact loads the bolted lid can lift a little for a short moment, allowing a little movement of the seal, so that the contact area can change before compressing again.
The poster presentation will show details about test conditions and first results.