Filtern
Erscheinungsjahr
- 2021 (7) (entfernen)
Dokumenttyp
- Vortrag (4)
- Zeitschriftenartikel (2)
- Beitrag zu einem Tagungsband (1)
Schlagworte
- Welding (4)
- Creep-resistant steel (2)
- High Entropy Alloy (2)
- High-entropy alloy (2)
- Austenitic stainless steel (1)
- Compositionally complex alloy (1)
- Cracking (1)
- Diffusion (1)
- Electrochemical permeation (1)
- Friction stir welding (1)
Organisationseinheit der BAM
- 9.2 Versuchsanlagen und Prüftechnik (7) (entfernen)
Eingeladener Vortrag
- nein (4)
Multi-element systems with defined entropy (HEA - High Entropy Alloy or MEA - Medium Entropy Alloy) are rather new material concepts that are becoming increasingly important in materials research and development. Some HEA systems show significantly improved properties or combinations of properties, e.g., the overcome of the trade-off between high strength and ductility. Thus, the synthesis, the resulting microstructures, and properties of HEA have been primarily investigated so far. In addition, processing is crucial to achieve a transfer of potential HEA/MEA materials to real applications, e.g. highly stressed components. Since fusion welding is the most important joining process for metals, it is of vital importance to investigate the weldability of these materials. However, this has rarely been the subject of research up to date. For that reason, in this work the weldability depending on the surface preparation of a CoCrFeMnNi-HEA and a CoCrNi-MEA for TIG welding is investigated. The fusion welding of longer plates is described here for the first time for the CoCrNi alloy. The welds of both materials showed distinct formation of cracks in the heat affected zone (HAZ). Optical and scanning electron microscopy analysis clearly confirmed an intergranular fracture topography. But based on the results, the crack mechanism cannot be conclusively clarified as either a liquid metal embrittlement (LME) or hot cracking like liquid film separation occurred.
High entropy alloys (HEA) are a new class of materials. In contrast to conventional alloys, HEA are single-phase alloys with at least five alloying elements. HEAs have enormous application potential due to (postulated) excellent structural property combinations from low to high temperatures. For HEA-application as structural materials in real components, a key issue is the suitability for joining processing. Requirements for the reliable and safe joining of these materials are crucial regarding economical component manufacture for future applications. In this context, friction stir welding (FSW) is a promising joining process due to the welding process temperature below the material melting point avoiding major issues, e. g. formation of (hard and brittle) intermetallic phases, which may have detrimental influences on the weld joint properties.
This study presents elementary research about the FSW process influences on a CoCrFeMnNi-HEA with focus on the microstructure and mechanical properties. For that purpose, the FSW joint of the HEA is compared to that of an austenitic stainless steel AISI 304. The microstructures of the welds were investigated and characterized by means of light microscopy, SEM, EBSD and XRD. Hardness and tensile testing were applied to determine influences on the mechanical properties. Generally, a comparable weldability of HEA and AISI 304 in terms of metallurgical characteristics and resulting mechanical properties exhibited. For the weld joints of both materials typical characteristics regarding FSW were observed within the weld metal and thermo-mechanically influenced zone: fine-grained stirred zone with increased hardness and reduced fracture elongation compared with the respective base material.
This presentation summarizes the latest results on the BAM-Themenfeld project SURDIA on processing of high-entropy alloys (HEAs) at BAM. At first, the influence of machining by ultrasonic-assisted milling on the surface integrity is presented. Second, the weld processing by Tungsten Inert Gas (TIG) welding is presented and the results of the Friction Stir Welding (FSW), which is conducted at BAM for the first time.
For higher operational temperatures and pressures required in petrochemical plants, the modified 13CrMoV9-10 steel was developed providing high resistance against creep and compressed hydrogen. Extreme care during the welding procedure is necessary for this steel, attributed to low toughness, high strength in as-welded state, and increased susceptibility to stress relief cracking (SRC) during post-weld heat treatment (PWHT). Previous research of SRC in creep-resistant steels discussed mainly thermal and metallurgical factors. Few previous findings addressed the influences of welding procedure on crack formation during PWHT considering real-life manufacturing conditions. These investigations focus on effects of welding heat control on stresses during welding and subsequent PWHT operations close to realistic restraint and heat dissipation conditions using a special 3D testing facility, which was presented in parts I and II of this contribution. Part III addresses investigations on residual stress evolution affecting crack formation and discusses the transferability of results from large-scale testing to laboratory-scale. Experiments with test set-ups at different scales under diverse rigidity conditions and an assessment of the residual stresses of the weld-specimens using X-ray (surface near) and neutron diffraction analysis (bulk) were performed. This study aims to provide a way of investigating the SRC behaviour considering component-specific residual stresses via small-scale testing concepts instead of expensive weld mock-ups.
Hoch- und Mittelentropie-Legierungen (engl. High/Medium Entropy Alloys–HEA/MEA) sind relativ neue Werkstoffklassen. Im Gegensatz zu herkömmlichen Le-gierungen bestehen HEA aus fünf bzw. MEA aus drei oder vier Legierungselementen im äquiatomaren Gleichgewicht. Viele HEA weisen aufgrund hervorragender struktu-reller Eigenschaftskombinationen von sehr tiefen bis zu hohen Temperaturen enor-mes Anwendungspotential auf. Die Anwendung für reale Bauteile stellt jedoch die zentrale Frage der Eignung für die fügetechnische Verarbeitung. Dieser Aspekt findet in der weltweiten Materialforschung bisher kaum Beachtung. Anforderungen an die zuverlässige und sichere fügetechnische Verarbeitung dieser Werkstoffe sind von wesentlicher Bedeutung hinsichtlich wirtschaftlicher Bauteilfertigung für spätere po-tenzielle Anwendungsbereiche, bspw. in der Energietechnik. Das Rührreibschweißen (engl. Friction Stir Welding–FSW) stellt hierbei einen vielversprechenden Fügepro-zess dar, dessen Hauptvorteil in der Schweißprozesstemperatur unterhalb der Schmelztemperatur der zu fügenden Werkstoffe liegt. Dies bedingt die Vermeidung der Ausbildung von harten, versprödenden intermetallischen Phasen, wie sie z. B. beim konventionellen Schmelzschweißen von Eisen-Aluminium-Verbindungen auf-treten. Die vorliegende Arbeit stellt grundlegende Untersuchungen zur Schweißbar-keit einer CoCrFeMnNi-Legierung (HEA) und einer CoCrNi-Legierung (MEA) mit dem FSW-Prozess vor. Die Versuchsschweißungen werden mittels mikroskopischer Analysen hinsichtlich des Schweißnahtaufbaus sowie Schweißnahtfehlern charakte-risiert. FSW zeigt sich als grundlegend geeignet zur Verbindungsschweißung der HEA bzw. MEA. Anhand dieser Ergebnisse kann eine weitere Bewertung der Schweißbar-keit erfolgen.
Martensitic 9 %-Cr steels like P91 and P92 show susceptibility to delayed hydrogen assisted cracking depending on their microstructure. In that connection, effective hydrogen diffusion coefficients are used to assess the possible time-delay. The small number of available diffusion coefficients varies already at room temperature by several orders of magnitude (mostly regarded as result of present microstructure). Especially P91 weld metal diffusion coefficients are rare so far. For that reason, electrochemical permeation experiments had been conducted using P92 base metal and P91 weld metal (in as-welded and heat-treated condition) with different thicknesses. The diffusion coefficients are calculated by two methods (time-lag and inflection point method) were performed. The results show that, despite of microstructural effects, the sample thickness must be considered as it influences the calculated diffusion coefficients. Finally, the comparison of calculated and measured hydrogen concentrations (determined by carrier gas hot extraction) enables the identification of realistic diffusion coefficients.
High-entropy alloys (HEAs) and compositionally complex alloys (CCAs) represent new classes of materials containing five or more alloying elements (concentration of each element ranging from 5 to 35 at. %). In the present study, HEAs are defined as single-phase solid solutions; CCAs contain at least two phases. The alloy concept of HEAs/CCAs is fundamentally different from most conventional alloys and promises interesting properties for industrial applications (e.g., to overcome the strength-ductility trade-off). To date, little attention has been paid to the weldability of HEAs/CCAs encompassing effects on the welding metallurgy. It remains open whether welding of HEAs/CCAs may lead to the formation of brittle intermetallics and promote elemental segregation at crystalline defects. The effect on the weld joint properties (strength, corrosion resistance) must be investigated. The weld metal and heat-affected zone in conventional alloys are characterized by non-equilibrium microstructural evolutions that most probably occur in HEAs/CCAs. The corresponding weldability has not yet been studied in detail in the literature, and the existing information is not documented in a comprehensive way. Therefore, this study summarizes the most important results on the welding of HEAs/CCAs and their weld joint properties, classified by HEA/CCA type (focused on CoCrFeMnNi and AlxCoCrCuyFeNi system) and welding process.