Filtern
Erscheinungsjahr
Dokumenttyp
Sprache
- Englisch (420) (entfernen)
Schlagworte
- Laser beam welding (94)
- Welding simulation (26)
- Resistance spot welding (22)
- Solidification cracking (21)
- Laser metal deposition (20)
- Additive manufacturing (19)
- Microstructure (16)
- Numerical simulation (16)
- Mechanical properties (15)
- Laser welding (14)
Organisationseinheit der BAM
- 9 Komponentensicherheit (182)
- 9.3 Schweißtechnische Fertigungsverfahren (177)
- 9.6 Additive Fertigung metallischer Komponenten (3)
- 5 Werkstofftechnik (2)
- 5.2 Metallische Hochtemperaturwerkstoffe (2)
- 7 Bauwerkssicherheit (2)
- 7.7 Modellierung und Simulation (2)
- 9.0 Abteilungsleitung und andere (2)
- 5.5 Materialmodellierung (1)
Eingeladener Vortrag
- nein (25)
Laser-based Powder Bed Fusion of Metal (PBF-LB/M) is a broadly used metal additive manufacturing (AM) method for fabricating complex metallic parts, whose sizes are however limited by the build envelope of PBF-LB/M machines. Laser welding arises as a valid joining method for effectively integrating these AM parts into larger assemblies.
PBF-LB/M components must usually be stress-relieved before they can be separated from the build plate. An additional heat treatment can be beneficial for obtaining homogeneous mechanical properties across the seam or for the formation of desired precipitations in nickel-based-alloys.
Therefore, the tensile performance of laser welded hybrid (AM/wrought) and AM-AM tensile samples of Inconel 718 is examined after undergoing three different heat treatments and considering three relevant build directions. It can be shown that the build orientation is an influencing factor on weld properties even after two applied heat treatments.
Laser metal deposition (LMD) has been applied as coating technology for many years. Today, the technologies capacity to produce 3D depositions leads to a new field of application as additive manufacturing method. In this paper, 3D laser metal deposition of titanium alloy Ti-6Al-4V is studied with special regard to the demands of additive manufacturing. Therefore, only the powder nozzle is used to create the shielding gas atmosphere, which ensures high geometric flexibility. Furthermore, specimen with high aspect ratio and hundreds of layers are manufactured, which represent typical features in additive manufacturing.
Laser welding is an appropriate technique for joining Laser Powder Bed Fusion (L-PBF) parts together and to conventional wrought ones. The potential consists of profiting from synergies between additive and conventional manufacturing methods and overcoming the existing limitations of both. On the one hand, L-PBF is a widely spread metal-based additive manufacturing technique suitable for generating complex parts which can present intrinsic designed cavities, conformal cooling channels, and filigree structures contributing to sustainable manufacturing and efficiency-oriented designs. On the other hand, chamber sizes for producing L-PBF parts are limited, and the process is time-consuming. Thus, its employment is not for every geometry justified. Additionally, they are in most cases individual elements of a larger assembly and need to be joined together to conventionally fabricated parts.
The present research suggests laser welding parameters to adequately bond pairs of wrought and L-PBF processed plates and two L-PBF plates of Inconel 718 in butt position. L-PBF samples are printed in three different build-up orientations. Additionally, the influence of as-built L-PBF roughness qualities and usual pre-weld preparations such as edge milling are examined. The effect of normed pre-weld heat treatments is also contemplated. Identified cracks are analyzed by means of EDS in order to confirm the present phases on the areas of interest. EBSD is also employed to obtain a clear depiction of the crystallographic texture and distribution of the hot cracks.
The quality of the weldment was examined according to existing standards. Substantial differences in seam geometry and microstructure across different edge’s surface qualities and build directions of stress relieved L-PBF parts have not been detected. Nevertheless, even if no other irregularities are present in the seam, variability in liquation cracking susceptibility has been confirmed. This defect is prone to happen when parts made of this nickel-based superalloy are welded together when not enough precautions are taken. It has been determined that grain size and ductility of the material before welding play a crucial role and mitigating or intensifying these imperfections. Moreover, recommendations are presented to avoid this potential welding defect.
A transient simulation including the impact of the laser energy, the melting of the metal and the development of the weld pool was conducted to observe the evolution of the vapor capillary and the solidification of the melt in pulsed laser beam welding of AISI 304 steel. The phase field method was implemented to investigate the evolution and behavior of the liquid-gas interface during welding and to describe the condensed and vapor phases. The effects of phase transition, recoil pressure, thermo-capillary and natural convection, vaporization and temperature dependent material properties were taken into account. A Gaussian-like heat source under consideration of the Fresnel absorption model was used to model the energy input of the laser beam. The heat source model was extended by a newly developed empirical approach of describing multiple beam reflections in the keyhole. To validate this new model, the numerical results were compared to experimental data and good agreement regarding the size and shape of the weld pool was observed.
The paper describes an experimental investigation of high power laser beam welding with an electromagnetic weld pool support for up to 20 mm thick plates made of duplex steel (AISI 2205) and mild steel (S235JR). The results of the welding tests show a successful application of this technology at ferromagnetic metals. Irregular sagging was suppressed successfully. An ac-power of less than 2 kW at oscillation frequencies between 800 Hz and 1.7 kHz is necessary for a full compasation of the hydrostatic pressure. Thus, it was demonstrated that the electromagnetic weld pool support is not only limited to non-ferromagnetic metals like austenitic steels. For future studies with duplex steel, the use of filler material has to take into account with regard to the balance of the mixed austenitic and ferritic phases.
Micrometric surface topologies are required for a wide range of technical applications.
While lowered surface features have been used for many years to improve the tribological behavior of contacting surfaces, there are also other fields of application, where the potential of elevated surface features is known, e. g. for metal forming tools. However, the demand for a high wear resistance of these structures often inhibits an industrial application. A solution is offered by structuring techniques that use additional material. A promising approach is the localized dispersing of hard ceramic particles by pulsed laser radiation, the so-called laser implantation. This paper describes the potential to adjust the geometry as well as the mechanical properties of laser implanted surfaces by means of microstructural and topological investigations. Afterwards, results of a wear test are given and different applications for this structuring technique are discussed. It can be shown that dome-shaped or ring-shaped structures on a micrometric scale can be produced with high hardness and wear resistance.
Laser beam welding of aluminum die casting is challenging. A large quantity of gases (in particular, hydrogen) is absorbed by aluminum during the die-cast manufacturing process and is contained in the base material in solved or bound form. After remelting by the laser, the gases are released and are present in the melt as pores. Many of these metallurgic pores remain in the weld seam as a result of the high solidification velocities. The natural (Archimedean) buoyancy is not sufficient to remove the pores from the weld pool, leading to process instabilities
and poor mechanical properties of the weld. Therefore, an electromagnetic (EM) system is used to apply an additional buoyancy
component to the pores. The physical mechanism is based on the generation of Lorentz forces, whereby an electromagnetic pressure is introduced into the weld pool. The EM system exploits the difference in electrical conductivity between poorly conducting pores (inclusions) and the comparatively better conducting aluminum melt to increase the resulting buoyancy velocity of the pores. Within the present study, the electromagnetic supported degassing is investigated in dependence on the laser beam power, welding velocity, and electromagnetic flux density. By means of a design of experiments, a systematic variation of these parameters is carried out for partial penetration laser beam welding of 6mm thick sheets of wrought aluminum alloy AlMg3 and die-cast aluminum alloy AlSi12(Fe), where the wrought alloy serves as a reference. The proportion of pores in the weld seams is determined using x-ray images, computed tomography images, and cross-sectional images. The results prove a significant reduction of the porosity up to 70% for both materials as a function of the magnetic flux density.
Laser metal deposition (LMD) has been applied as a coating technology for many years. Today, the technologies capacity to produce 3D depositions leads to a new field of application as additive manufacturing method. In this paper, 3D laser metal deposition of titanium alloy Ti-6Al-4V is studied with special regard to the demands of additive manufacturing. Therefore, only the coaxial LMD powder nozzle is used to create the shielding gas atmosphere, which ensures high geometric flexibility. Furthermore, specimen with high aspect ratio and hundreds of layers are manufactured, which represent typical features in additive manufacturing. The presented study contains the following steps: First, cylindrical specimens are manufactured with a standard shell-core build-up strategy and mechanical properties as well as fracture mechanisms are determined. Based on the results, experiments are conducted to improve the build-up strategy and new tensile test specimens are built with the improved strategy. The improved strategy incorporates variable track overlap ratios to achieve a constant growth in the shell and core area. As blanks, lean cylinders comprising more than 240 layers and a height of more than 120mm are manufactured. The specimens are analyzed by X-ray inspection for material defects. Fractured surfaces are observed via scanning electron microscopy and the composition of the surfaces is determined using energy dispersive X-ray spectroscopy. The tensile test results prove mechanical properties close to ASTM F1108 specification for wrought material.
The present paper investigates the electromagnetic porosity reduction in partial penetration laser beam welding of 6 mm aluminum die casting AlSi9MnMg. Applying an electromagnetic field, a significant reduction of the porosity as well as smoothing of the surface of aluminum die casting can be observed. Starting from the reference case without an electromagnetic support, the porosity was reduced by 76 %. Especially big pores can be removed from the weld pool effectively due to their beneficial volume-to-area ratio whereas very small metallurgical pores tend to remain within the weld pool even when higher magnetic flux densities are applied.
With regard to efficient production, it is desirable to combine the respective advantages of additively and conventionally manufactured components. Particularly in the case of large-volume components that also include filigree or complex structures, it makes sense to divide the overall part into individual elements, which afterwards have to be joined by welding.
The following research represents a first step in fundamentally investigating and characterizing the joint welding of Laser Powder Bed Fusion (L-PBF) components made of Inconel 718. For this purpose, bead-on-plate welds were performed on plates manufactured using the L-PBF process and compared with the conventionally manufactured material. Conventional laser beam welding was used as welding process. The weld geometry was investigated as a function of the L-PBF build-up orientation. It was found that the welding depth and weld geometry differ depending on this orientation and in comparison to the conventional material.