The tribological behaviour under dry sliding conditions of Magneli phase Ti4O7 and e-phase Ti2Cr2O7 with α-alumina as a sliding partner has been characterised at room temperature by oscillating sliding. The mechanical properties as well as Vickers hardness measurements do not reveal big differences between the materials, and 4-point bending strengths are around 200 MPa for both materials. Although the friction coefficients are in the medium range of 0.6 and do not differ much between the materials, the wear behaviour is very different. At room temperature, the wear coefficient of Ti2O7 is strongly dependent on relative humidity, and wear is highest under dry conditions when relative humidity is low as it is typically found for many ceramic materials. Ti2Cr2O7 shows remarkably different wear behaviour with the lowest wear in dry conditions. The measured coefficients of wear at low relative humidity of 4% are more than 2 orders of magnitude lower than those for Ti2O7.