Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (20)
- Beitrag zu einem Tagungsband (10)
- Forschungsdatensatz (5)
- Beitrag zu einem Sammelband (3)
- Vortrag (2)
- Sonstiges (2)
Sprache
- Englisch (42) (entfernen)
Schlagworte
- Additive manufacturing (5)
- Elastic modulus (4)
- Fatigue (4)
- Shear modulus (4)
- Ti-6Al-4V (4)
- Young's modulus (4)
- Cast iron (3)
- Thermal shock (3)
- AGIL (2)
- AISI 316L (2)
Organisationseinheit der BAM
- 5 Werkstofftechnik (12)
- 5.2 Metallische Hochtemperaturwerkstoffe (12)
- 9 Komponentensicherheit (6)
- 9.6 Additive Fertigung metallischer Komponenten (5)
- 5.5 Materialmodellierung (2)
- 8 Zerstörungsfreie Prüfung (2)
- 8.5 Röntgenbildgebung (2)
- 5.1 Mikrostruktur Design und Degradation (1)
- 5.6 Glas (1)
- 9.3 Schweißtechnische Fertigungsverfahren (1)
Eingeladener Vortrag
- nein (2)
The knowledge of the temperature-induced changes of the superconductor volume and of the thermomechanical behavior of the different coil and tooling materials is required for predicting the coil geometry and the stress distribution in the coil after the Nb3Sn reaction heat treatment. In this paper, we have measured the Young’s and shear moduli of the HL-LHC 11 T Nb3Sn dipole magnet coil and reaction tool constituents during in situ heat cycles with the dynamic resonance method. The thermal expansion behaviors of the coil components and of a free standing Nb3Sn wire were compared based on dilation experiments.
The elastic properties (Young's modulus, shear modulus) of titanium alloy Ti-6Al-4V were investigated between room temperature and 400 °C in an additively manufactured variant (laser-based directed energy deposition with powder as feedstock, DED-LB/M) and from a conventional process route (hot rolled bar). The moduli were determined using the dynamic resonance method. The data set includes information on processing parameters, heat treatments, microstructure, grain size, specimen dimensions and weight, Young’s and shear modulus as well as their measurement uncertainty.
The dataset was generated in an accredited testing lab using calibrated measuring equipment. The calibrations meet the requirements of the test procedure and are metrologically traceable. The dataset was audited as BAM reference data.
The increased use of fibre-reinforced plastic (FRP) composites for improved efficiency and reliability in energy related applications e.g. wind and marine turbine blades, nacelles, oil and gas flexible risers, also increases the demand for innovative non-destructive testing technologies. Thus, in order to achieve increased acceptance of suited and optimized non-destructive testing (NDT) methods in industry, the European Metrology Research Programme (EMRP) project ENG57 Validated Inspection Techniques for Composites in Energy Applications (VITCEA) deals with the development and validation of innovative NDT technologies. In this contribution, results concerning thermographic investigations at test specimens during tensile loading and active thermography testing after tensile loading are presented. Additionally, the determination of the optical properties (relative transmittance and directional spectral emissivity) of CFRP and GFRP test specimens is described.
The fatigue behaviour of cast iron is usually investigated on machined specimens. Components of cast iron, however, have a casting skin; therefore the investigation of the influence of the casting skin on the lifetime is of interest. To study this influence isothermal fatigue tests were carried out on heat-resisting spheroidal graphite cast iron EN GJS SiMo 4.05 in 4–point-bending set-up at 400 °C. Specimens with and without casting skin were investigated comparatively. The number of cycles to failure was significantly lower for specimens with casting skin. Metallographic investigations underline the reduction of lifetime caused by casting skin.
The increased use of fibre reinforced plastic (FRP) composites for improved efficiency and reliability in energy related applications, e.g. wind and marine turbine blades, nacelles, oil and gas flexible risers, also increases the demand for innovative non-destructive testing technologies. In this contribution, results concerning the characterisation of CFRP and GFRP during and after quasi-static tensile loading are presented. It includes the measurement of optical properties in the infrared spectral range, tensile loading tests with the observation of the temperature distribution at one or both sides of the specimens using an infrared camera for the preparation and monitoring of intended natural defects, and active thermography inspections after tensile loading. It is shown that the defect preparation was successful. Thermographic monitoring during and active thermography testing after tensile loading enable the detection of the lateral extend of the generated defects. Differences between CFRP and GFRP materials are discussed.
The room temperature tensile properties of iron with different purity levels (commercially pure, high-purity, and ultra-high-purity) were characterized at different strain rates in the framework of an international Round-Robin involving four laboratories (BAM, IMR-TU, NIST, and SCKCEN). The test results were collected and analyzed by NIST, and are presented in this Technical Note.
Data from all the participating laboratories were found in good agreement, thus allowing a clear assessment of the influence of strain rate and purity level on tensile properties (mechanical resistance and ductility). A clear increase of yield strength and, to a lesser extent, tensile strength was observed for all materials as strain rate increases and purity level decreases. The highest strain rate sensitivity was associated with the highest purity level (ultra-high-purity Fe). Ductility trends were less unequivocal, but typically an increase of elongation at fracture and reduction of area was detected as strain rate and purity level increase. Significant differences in tensile properties were observed between the two investigated types of high-purity Fe, which can be attributed to an influence of the production process in terms of melting environment (atmosphere and crucible), as well as differences in chemical compositions.
Computational methods for lifetime prediction of metallic components under high-temperature fatigue
(2019)
The issue of service life prediction of hot metallic components subjected to cyclic loadings is addressed. Two classes of lifetime models are considered, namely, the incremental lifetime rules and the parametric models governed by the fracture mechanics concept. Examples of application to an austenitic cast iron are presented. In addition, computational techniques to accelerate the time integration of the incremental models throughout the fatigue loading history are discussed. They efficiently solve problems where a stabilized response of a component is not observed, for example due to the plastic strain which is no longer completely reversed and accumulates throughout the fatigue history. The performance of such an accelerated Integration technique is demonstrated for a finite element simulation of a viscoplastic solid under repeating loading–unloading cycles.
Characterization of Ti-6Al-4V fabricated by multilayer laser powder-based directed energy deposition
(2022)
Laser powder-based directed energy deposition (DED-L) is increasingly being used in additive manufacturing (AM). As AM technology, DED-L must consider specific challenges. It must achieve uniform volume growth over hundreds of layers and avoid heat buildup of the deposited material. Herein, Ti–6Al–4V is fabricated using an approach that addresses these challenges and is relevant in terms of transferability to DED–L applications in AM. The assessment of the obtained properties and the discussion of their relationship to the process conditions and resulting microstructure are presented. The quality of the manufacturing process is proven in terms of the reproducibility of properties between individual blanks and with respect to the building height. The characterization demonstrates that excellent mechanical properties are achieved at room temperature and at 400 °C.
Creep and creep damage behavior of stainless steel 316L manufactured by laser powder bed fusion
(2022)
This study presents a thorough characterization of the creep properties of austenitic stainless steel 316L produced by laser powder bed fusion (LPBF 316L) contributing to the sparse available data to date. Experimental results (mechanical tests, microscopy, X-ray computed tomography) concerning the creep deformation and damage mechanisms are presented and discussed. The tested LPBF material exhibits a low defect population, which allows for the isolation and improved understanding of the effect of other typical aspects of an LPBF microstructure on the creep behavior. As a benchmark to assess the material properties of the LPBF 316L, a conventionally manufactured variant of 316L was also tested. To characterize the creep properties, hot tensile tests and constant force creep tests at 600 °C and 650 °C are performed. The creep stress exponents of the LPBF material are smaller than that of the conventional variant. The primary and secondary creep stages and the times to rupture of the LPBF material are shorter than the hot rolled 316L. Overall the creep damage is more extensive in the LPBF material. The creep damage of the LPBF material is overall mainly intergranular. It is presumably caused and accelerated by both the appearance of precipitates at the grain boundaries and the unfavorable orientation of the grain boundaries. Neither the melt pool boundaries nor entrapped gas pores show a significant influence on the creep damage mechanism.
The tribological behaviour under dry sliding conditions of Magneli phase Ti4O7 and e-phase Ti2Cr2O7 with α-alumina as a sliding partner has been characterised at room temperature by oscillating sliding. The mechanical properties as well as Vickers hardness measurements do not reveal big differences between the materials, and 4-point bending strengths are around 200 MPa for both materials. Although the friction coefficients are in the medium range of 0.6 and do not differ much between the materials, the wear behaviour is very different. At room temperature, the wear coefficient of Ti2O7 is strongly dependent on relative humidity, and wear is highest under dry conditions when relative humidity is low as it is typically found for many ceramic materials. Ti2Cr2O7 shows remarkably different wear behaviour with the lowest wear in dry conditions. The measured coefficients of wear at low relative humidity of 4% are more than 2 orders of magnitude lower than those for Ti2O7.