The steel–concrete interface (SCI) is known to influence corrosion of steel in concrete. However, due to the numerous factors affecting the SCI—including steel properties, concrete properties, execution, and exposure conditions—it remains unclear which factors have the most dominant impact on the susceptibility of reinforced concrete to corrosion. In this literature review, prepared by members of RILEM technical committee 262-SCI, an attempt is made to elucidate the effect of numerous SCI characteristics on chloride-induced corrosion initiation of steel in concrete. We use a method to quantify and normalize the effect of individual SCI characteristics based on different literature results, which allows comparing them in a comprehensive context. It is found that the different SCI characteristics have received highly unbalanced research attention. Parameters such as w/b ratio and cement type have been studied most extensively. Interestingly, however, literature consistently indicates that those parameters have merely a moderate effect on the corrosion susceptibility of steel in concrete. Considerably more pronounced effects were identified for (1) steel properties, including metallurgy, presence of mill scale or rust layers, and surface roughness, and (2) the moisture state. Unfortunately, however, these aspects have received comparatively little research attention. Due to their apparently strong influence, future corrosion studies as well as developments towards predicting corrosion initiation in concrete would benefit from considering those aspects. Particularly the working mechanisms related to the moisture conditions in microscopic and macroscopic voids at the SCI is complex and presents major opportunities for further research in corrosion of steel in concrete.
Alkalisch aktivierte Bindemittel (AAB) und Betone können herkömmliche Zemente beziehungsweise Betone potentiell in vielen Anwendungen ersetzen und dadurch den CO2-Fußabdruck der Bauindustrie wesentlich verkleinern. Zur Untersuchung der Stahlkorrosion in bewehrten („armierten“) Betonbauteilen werden elektrochemische Methoden wie Messungen des Freien Korrosionspotentials, des Polarisationswiderstands oder von Stromdichte-Potential-Kurven eingesetzt. Diese Methoden und die etablierten Grenzwerte zur Detektion von Korrosion sind für die Anwendung bei herkömmlichen Zementen beziehungsweise Betonen entwickelt und erprobt worden. Neue Forschungsergebnisse demonstrieren, dass Unterschiede zwischen den Porenlösungszusammensetzungen von herkömmlichen Zementen und bestimmten AAB sowie anderen schlackehaltigen Zementen erhebliche Unterschiede bei den Ergebnissen der elektrochemischen Messungen bewirken und damit zur fehlerhaften Detektion von Stahlkorrosion führen können. Ursache hierfür sind vor allem reduzierte Schwefelspezies in den Porenlösungen von AAB und anderen schlackehaltigen Zementen.
Application of electrochemical methods for studying steel corrosion in alkali-activated materials
(2023)
Alkali-activated materials (AAMs) are binders that can complement and partially substitute the current use of conventional cement. However, the present knowledge about how AAMs protect steel reinforcement in concrete elements is incomplete, and uncertainties exist regarding the application of electrochemical methods to investigate this issue. The present review by EFC WP11-Task Force ‘Corrosion of steel in alkali-activated materials’ demonstrates that important differences exist between AAMs and Portland cement, and between different classes of AAMs, which are mainly caused by differing pore solution compositions, and which affect the outcomes of electrochemical measurements. The high sulfide concentrations in blast furnace slag-based AAMs lead to distinct anodic polarisation curves, unusually low open circuit potentials, and low polarisation resistances, which might be incorrectly interpreted as indicating active corrosion of steel reinforcement. No systematic study of the influence of the steel–concrete interface on the susceptibility of steel to corrosion in AAMs is available. Less common electrochemical methods present an opportunity for future progress in the field.
Alkali-aktivierte Hüttensandbetone – CO2-reduzierte Bindemittel mit hohem Korrosionsschutzpotential
(2023)
Durch den Ersatz von Portlandzement können alkali-aktivierte Bindemittel einen bedeutenden Beitrag zur Verringerung der durch die Zementklinkerherstellung verursachten CO2-Emissionen leisten. Für die Verwendung von alkali-aktivierten Bindemitteln in Stahlbetonkonstruktionen, die Chloriden oder Carbonatisierung ausgesetzt sind, ist die Fähigkeit des Stahls, den passiven Zustand zu erreichen und aufrechtzuerhalten, von großer Bedeutung. Die Prozesse der Deckschichtbildung von Stahl in alkali-aktivierten Materialien unterscheiden sich jedoch zum Teil grundlegend von denen in Portlandzementen. Alkali-aktivierte Hüttensandbetone weisen gute technische Eigenschaften auf, bisher fehlen jedoch grundlegende Kenntnisse bzgl. ihrer schützenden Wirkung bei korrosiven Angriffen. Dies ist vor allem auf ihre sulfidhaltige Porenlösung zurückzuführen, welche die elektrochemischen Eigenschaften der Stahloberfläche beeinflusst und die Verwendung herkömmlicher Bewertungsmaßstäbe erschwert. Es werden erste Ergebnisse eines DFG-Forschungsprojektes vorgestellt, in dem das Passivierungsverhalten von Stahl in alkali-aktivierten Hüttensandmörteln unterschiedlicher Zusammensetzungen sowie in Mörteln auf Basis hüttensandhaltiger Normzemente untersucht wird. Über einen Zeitraum von mindestens 28 Tagen werden an Zylinderprüfkörpern im 3-Elektroden-Aufbau das Ruhepotential sowie die Polarisationswiderstände der Stahlelektroden ermittelt.