Casks for the transport and storage of heat generating radioactive waste in Germany are normally provided with screwed lid systems, which are in most cases equipped with double jacket metal seals with an inner spring wire to provide long term resistance to the seal compression force. Preservation of the high sealing quality of those seals under operational and accidental stress conditions is essentially important to the safety of those casks. Relative displacements of the lid system surfaces caused by specific impact scenarios cannot be excluded and have to be evaluated with respect to a possible increase in the leakage rate.
To get representative data for such metal sealed lid systems, BAM has developed a special conceptualised flange system placed in an appropriate testing machine for relevant mechanical loading of the metal seals under static and cyclic conditions. Furthermore, the flange system enables continuous measurement of the standard helium leakage rate during each test.
The primary aim of the investigation is to identify the correlation between variation of installation conditions (axial displacements) caused by external loads and the standard helium leakage rate. An essential parameter in this case is the useable resilience ru of a metal seal under relevant stress conditions. The useable resilience ru is the vertical difference in the cross-section between the seal's assembling status and the point where the leakage rate, by means of external load relieving, exceeds the quality criterion of 10-8 Pa m3 s-1. Load relieving can instantly occur due to modification of the seal groove dimension caused by accident impacts and deformation of the lid system. Furthermore, component specific basis data for the development of finite element calculation models should be collected. In the tests, seals are subjected to static and cyclic loads. All tests are performed at ambient temperature.
This paper presents the test configuration, different test series and results of the current experiments. Typical load-displacement-leakage rate correlations are presented and discussed.
Dual purpose casks for the transportation and storage of spent nuclear fuel and other radioactive materials require very high leak-tightness of lid closure Systems under accident conditions as well as in the long-term to prevent activity release. For that purpose metal seals of specific types with an inner helical spring and outer metal liners are widely used and have shown their excellent performance if certain quality assurance requirements for fabrication and assembling are satisfied. Well defined surface roughness, clean and dry inert conditions are therefore essential. No seal failure in a loaded cask happened under these conditions until today.
Nevertheless, the considered and licensed Operation period is limited and all safety assessments have been performed and approved for this period of time which is 40 years in Germany so far. But in the meantime longer storage periods might be necessary for the future and therefore additional material data will be required. BAM is involved in the qualification and evaluation procedures of those seals from the early beginning. Because long-term tests are always time consuming BAM has early decided to perform additional tests with specific test seal configurations to gain a better understanding of the long-term behavior with regard to seal pressure force, leakage rate and useable resilience which is safety relevant mainly in case of accidental mechanical loads inside a storage facility or during a subsequent transport. Main test parameters are the material of the outer seal jacket (silver or aluminum) and the temperature. This paper presents the BAM test program including an innovative test mock-up and most recent test results. Based on these data extrapolation models to extended time periods are discussed, and also future plans to continue tests and to investigate seal behavior for additional test parameters are explained.
Langzeituntersuchungen an Metalldichtungen mit innen liegendem Federkern und doppelter Ummantelung
(2013)
In Deutschland werden in Transport- und Lagerbehältern (TLB) wärmeentwickelnde radioaktive Abfälle gegenwärtig über einen Zeitraum von bis zu 40 Jahren zwischengelagert. Aufgrund der Situation der noch nicht abgeschlossenen Endlagersuche werden hier möglicherweise Verlängerungen in Betracht zu ziehen sein. Im Deckeldichtsystem der TLB werden in der Regel Metalldichtungen vom Typ Helicoflex® eines französischen Herstellers verwendet, die aus einem innen liegenden Spiralfederkern und zwei Ummantelungen bestehen. Die Ermittlung der Fliess- und Relaxationseigenschaften der Dichtungskomponenten über den vorgesehenen langen Betriebseitraum sind vor dem Hintergrund des Erhalte eines geforderten hohen Dichtniveaus ein wichtiger Untersuchungsgegenstand.
Langzeitversuche über 10 Jahre an Federkern-Metalldichtungen mit Aluminium- bzw. Silberummantelungen
(2023)
Federunterstützte Metalldichtungen mit Aluminium(Al)- oder Silber(Ag)-Ummantelung werden u.a. in Behältern für Wärme entwickelnde radioaktive Abfälle eingesetzt, da diese Dichtungen eine sehr gute Dichtheit gewährleisten sowie Langlebigkeit und Beständigkeit gegenüber erhöhten Temperaturen und radioaktiver Strahlung aufweisen. Auch wenn die Sicherheit solcher Behälter und der verwendeten Dichtungen vielfach belegt wurde, sind sie Gegenstand andauernder Forschung, etwa im Hinblick auf eine absehbar benötigte verlängerte Zwischenlagerdauer. Aus diesem Grund werden an der Bundesanstalt für Materialforschung und -prüfung (BAM) im Fachbereich 3.4 „Sicherheit von Lagerbehältern“ seit über 20 Jahren Versuche an solchen Metalldichtungen durchgeführt. Dabei sollen zusätzliche Erkenntnisse hinsichtlich der Sicherheitsreserven der Dichtungen in unterstellten Störfallszenarien (axiale Bewegung des Deckelsystems bzw. Aufweitung der Nutgeometrie) und insbesondere detailliertere Erkenntnisse zum Langzeitverhalten gewonnen werden.
It is important to evaluate the effect of thermal ageing on the sealing performance of metal gaskets under high temperature for long-term usage. Therefore, in order to gain representative data for this kind of metal-sealed lid System, BAM is currently performing laboratory tests of different gasket types with aluminum and silver jackets at three different temperatures under static conditions up to four years so far, using test flanges for gaskets with full scale cross section diameter but much smaller outer diameter. On the other hand, in order to investigate the applicability of the numerical methodology to evaluate the long-term behavior of the metal gaskets, such as a correlation between seal pressure force and holding time, CRIEPI is developing a modeling method including material tests (tensile and creep tests) at high temperature. In this paper, the applicability of the finite element method (ABAQUS) to predict the recovery displacement and residual seal pressure force of the gasket complex was verified by comparing the calculated values with BAM’s laboratory test results under the joint research agreement between BAM and CRIEPI.