The determination of chloride is still one of the main tasks for the evaluation of reinforced concrete structures.
The corrosion of the reinforcement induced by the penetrating chlorides is the dominant damage process affecting the lifetime of concrete structures. In the recent years different research groups demonstrated that LIBS can be a fast and reliable method to quantify chlorine in cement-bound materials. Because chlorine in concrete can only occur as solved ions in the pore solution or bound in salts or hydrated cement phases, the detected emission of chlorine can be correlated with the chloride concentration determined e.g. with potentiometric titration. This work inter alia describes the production of reference samples and possible side effects during the production process. Due to transport processes in the porous matrix of the cement a misinterpretation of the concentrations is possible. It is shown how to overcome these effects and higher precisions of the single measurements can be realised. Using the calibration method, blank sample method and noise method, three different ways of calculating the limit of detection (LOD) and limit of quantification (LOQ) are compared. Due to the preparation of the reference samples a precision of the whole calibration model of sx0 = 0.023 wt% is determined.
The validation of the model is based on different test sets, which are varying in their composition
(different Cl-salts, water-to-cement ratios and additives). The determined mean error of the validation is
0.595 ± 0.063 wt%, which is comparable to standardised methods like potentiometric titration, direct potentiometry
or photometry (0.40 ± 0.06 wt%) [1].
This paper will address the relevance of chloride measurements in practice for durability condition assessment and a description of the working principle of LIBS will be given. Examples of chloride profiles obtained by the common wet chemical analysis will be shown and compared with results from LIBS measurements as to demonstrate the accuracy of the LIBS-technique. The latter will be supported by clear graphs. In addition examples on the extra information resulting from measurements performed with LIBS for improvement of condition assessment and prediction will be shown.
Alle bislang angewendeten Verfahren zur Chloridbestimmung in Beton- und Stahlbetonbauwerken arbeiten über die Entnahme von Probenmaterial und dessen Analyse unter Laborbedingungen. Diese Methodik erfordert Zeit und generiert erhöhte Aufwendungen. Prüfverfahren, die direkt und zuverlässig solche Untersuchungen am Bauteil oder Bauwerk vornehmen können, standen bislang nicht zur Verfügung.
Eine bereits in früheren Kolloquien vorgestellte Methode der Laser-induzierten Breakdown Spektroskopie wurde innerhalb eines aktuellen Forschungsvorhabens so weiter entwickelt, dass mit Hilfe eines neuartigen mobilen und kompakten Analysegerätes die Chloridwerte nun direkt und unmittelbar auf den Betonflächen bestimmt werden können.
A big part of the infrastructure is made of concrete, which is a multiphase system made of cement, aggregates, water and pores. Concrete is often used in combination with steel as reinforced concrete. Environmental influences, especially the ingress of harmful ions in combination with the ingress of water, trigger different damage processes which reduce the designed lifetime of a structure. The ingress of chlorides from de-icing salt or sea water leads to corrosion of the reinforcement. In addition, the carbonation of the concrete may trigger the corrosion of the reinforcement. The ingress of alkalis from deicing salts may cause the expansion of the amorphous silica aggregates (alkali-silica reaction) through
formation of a swelling gel of calcium silicate hydrate if water is present. The ingress of sulphates may cause spalling of the concrete surface due to ettringite formation.
For the standard procedure in civil engineering cores are taken, cut in slices, grinded and the obtained homogenized powder is solved in acid and investigated by standard procedures.
BAM has developed the LIBS technique for the 2D evaluation of the chemical composition of concrete. The technique is established for automated laboratory use with high numbers of samples to investigate transport processes of harmful species (Cl-, CO2 , SO4 2-and alkalis) in concrete. Information about ingress depth and the quantitative values are important to estimate the remaining lifetime of the infrastructure. LIBS is a surface technique. To get information about the ingress depth, a drill core has to be taken and cut in the middle. The measurements are carried out at the cross section. The main advantages of LIBS are the direct measurement on the surface of the concrete, fast analysis (sample rate 100 Hz) with a spatial resolution of up to 100 µm, the consideration of the heterogeneity of the concrete and the possibility of automated measurements which save a lot of manpower and time. As an example the investigation of ingress profiles for standard diffusion and migration tests in civil engineering takes hours in comparison to just a few minutes using LIBS. At the same time a 2D-evaluation provides information about hot spots of elemental concentration which may not be found by standard methods.
The state of the art of LIBS technique for applications in civil engineering will be presented, including typical results of 2D investigation of concrete in laboratory. The performance is also demonstrated by examples for onsite applications using a mobile LIBS system. The road map to standardization is presented as well.
In den letzten Jahren sind im deutschen Bundesautobahnnetz vermehrt AKR-Schäden an Betonfahrbahndecken aufgetreten. Ursächlich hierfür ist die Verwendung alkaliempfindlicher Gesteinskörnung. Dies führt bei gleichzeitiger Anwesenheit von Wasser infolge der Exposition der Fahrbahndecke und des alkalischen Milieus durch den Einsatz alkalireicher Portlandzemente bei der Betonherstellung zu einer Alkali-Kieselsäure-Reaktion (AKR). Zusätzlich wird der AKR-Schädigungsprozess in Betonfahrbahndecken durch den externen Tausalzeintrag (primär NaCl) im Winter begünstigt. Vor diesem Hintergrund kommt der Ermittlung des Tausalzeintrags in den Fahrbahndeckenbeton eine große Bedeutung zu.
Die Analyse des Tausalzeintrags erfolgte bisher ausschließlich nasschemisch an gemahlenen Bohrkernsegmenten. Nachteilig sind hierbei der relativ hohe prüftechnische Aufwand und die eingeschränkte Ortsauflösung. Der alternative Einsatz von LIBS (Laser-induced breakdown spectroscopy) eröffnet in diesem Kontext neue Möglichkeiten. So wird in diesem Beitrag anhand von Bohrkernen aus einem repräsentativen AKR-geschädigten BAB-Abschnitt exemplarisch die Vorgehensweise bei der LIBS-Analyse zur Ermittlung der Na- und Cl-Verteilung an vertikalen Schnittflächen von Bohrkernen aufgezeigt. Da der Tausalzeintrag primär über den Zementstein erfolgt, wurde der verfälschende Na-Grundgehalt der Gesteinskörnung mittels eines Ausschlusskriteriums (Ca-Gehalt) eliminiert. Vergleichend durchgeführte Cl-Mappings mit Mikroröntgenfluoreszenzanalyse sowie nasschemische Analysen belegen die Güte der durchgeführten LIBS-Messungen. Allerdings bedarf es bei der quantitativen Ermittlung des Natriumgehaltes in der Betonfahrbahndecke noch weitergehender Untersuchungen.