Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (64)
- Beitrag zu einem Tagungsband (11)
- Sonstiges (1)
- Posterpräsentation (1)
Schlagworte
- Computed tomography (8)
- Electron tomography (8)
- Fuel cell (8)
- Neutron tomography (8)
- Radiography (8)
- Neutron imaging (7)
- Tomography (7)
- Water transport (7)
- Polymer electrolyte membrane fuel cell (PEMFC) (6)
- DIRECTT (5)
Organisationseinheit der BAM
Paper des Monats
- ja (1)
Water evolution in the gas diffusion layer of a polymer electrolyte membrane fuel cell was visualized in situ by means of synchrotron X-ray radiography. Cracks in the microporous layer were identified as start points of efficient liquid water transfer paths through the gas diffusion layer. Quantitative analysis of the water flow rate through those arbitrarily distributed cracks into the gas channel revealed that they have a strong influence on the overall liquid water transport. This could find entry into future material design and simulation.
X-ray compton tomography
(2014)
The potentials of incoherent X-ray Scattering (Compton) tomography are investigated. Imaging materials of very different density or atomic number at once is a perpetual challenge for X-ray tomography or radiography, in general. In a basic laboratory set-up for simultaneous perpendicular Compton Scattering and direct beam attenuation tomographic scans are conducted by single channel photon counting. This results in asymmetric distortions of the projection profiles of the scattering CT-data set. ln a first approach corrections of Compton scattering data by taking advantage of rotational symmetry yield tomograms without major geometric artefacts.
A cylindrical sample composed of PE, PA, PVC, glass and wood demonstrates similar Compton contrast for all the substances, while the conventional absorption tomogram only reveals the two high order materials.
Compärison to neutron tomography reveals astonishing similarities except for the glass component (without hydrogen). Therefore, Compton CT bears the potential to replace neutron tomography, which requires much more efforts.
We investigated the hydrogen distribution spatially and temporally in technical iron at room temperature. Samples were charged electrochemically and subsequently analysed by means of neutron radiography and tomography. The radiographic images allowed for a time-resolved analysis of hydrogen fluxes. The three-dimensional distribution of hydrogen measured by neutron tomography delivered valuable information for the damage analysis of hydrogen-induced cracks. For the first time hydrogen concentration gradients inside the material could be detect directly together with the cracks. The neutron radiography and tomography results were gained at the Research Reactor BER II of the HZB in Berlin.
We investigated hydrogen embrittlement and blistering in electrochemically hydrogen-charged technical iron samples at room temperature. Hydrogen-stimulated cracks and blisters and the corresponding hydrogen distributions were observed by neutron tomography. Cold neutrons were provided by the research reactor BER II to picture the sample with a spatial resolution in the reconstructed three-dimensional model of ~25 µm. We made the unique observation that cracks were filled with molecular hydrogen and that cracks were surrounded by a 50 µm wide zone with a high hydrogen concentration. The zone contains up to ten times more hydrogen than the bulk material. The hydrogen enriched zone can be ascribed to a region of increased local defect density. Hydrogen also accumulated at the sample surface having the highest concentration at blistered areas. The surfaces of the brittle fractured cracks showed micropores visualized by scanning electron microscopy. The micropores were located at grain boundaries and were surrounded by stress fields detected by electron backscattered diffraction. The cracks clearly originated from the micropores.
Magnetic domains have been the subject of much scientific investigation since their theoretical existence was first postulated by P.-E. Weiss over a century ago. Up to now, the three-dimensional (3D) domain structure of bulk magnets has never been observed owing to the lack of appropriate experimental methods. Domain analysis in bulk matter thus remains one of the most challenging tasks in research on magnetic materials. All current domain observation methods are limited to studying surface domains or thin magnetic films. As the properties of magnetic materials are strongly affected by their domain structure, the development of a technique capable of investigating the shape, size and distribution of individual domains in three dimensions is of great importance. Here, we show that the novel technique of Talbot-Lau neutron tomography with inverted geometry enables direct imaging of the 3D network of magnetic domains within the bulk of FeSi crystals.
In contrast to classical low temperature polymer electrolyte fuel cells (LT-PEFCs), the membrane conductivity in high temperature polymer electrolyte fuel cells (HT-PEFCs) (operating temperature ~ 160 °C) is based on proton transport within phosphorus-oxygen acids at different levels of hydration, orthophosphoric acid (H3PO4) being the simplest example. We present for the first time in-situ synchrotron X-ray radiography measurements applied to a HT-PEFC to gain insight into the local composition of the membrane electrode assembly (MEA) under dynamic operating conditions. Transmission changes during the radiographic measurements exhibit a clear influence of the formation of product water on the membrane composition.
CT (computed tomography) reconstructions of fuel cell components of a yet unrivaled spatial resolution and quality are presented. This is achieved by application of the novel DIRECTT (Direct Iterative Reconstruction of Computed Tomography Trajectories) algorithm. We focus on two different key issues which essentially rule the fuel cell's durability on different length scales and physical interactions. On the resolution scale of some 100 µm agglomerations of condensed water in flow-field channels are detected by means of quasi-in situ neutron CT (after operation). Five orders of magnitude below nanometer sized Ru catalyst particles on carbon black support are visualized by electron tomography. Both types of experiments are especially adapted to the type of material involved but they are accompanied by severe deviations from ideal CT measuring conditions, as well. In order to overcome the tremendous reconstruction artifacts of standard algorithms, we employ DIRECTT which is described in detail. Comparisons of DIRECTT reconstructions to the conventional filtered back projection, prove the significant improvements in both experimental methods.
The carbon dioxide evolution and bubble formation in an operating fuel has been studied by means of synchrotron X-ray radiography. Two different observation directions have been chosen: a through-plane insight has been employed to track the formation of bubbles starting at the corner of the lands of the flow field; a depth profile of the carbon dioxide evolution has been derived from cross sectional studies describing an affected area of up to 100 µm. The dynamics of the bubble formation and detachment of the bubbles from the position of formation is strongly correlated with the current density. Cracks and breaks in the catalyst layer which result from the preparation process are visible under operating conditions and a possible swelling of the catalyst layer does not reach a complete vanishing of the cracks.
Coarsening of grain-refined semi-solid Al-Ge32 alloy: X-ray microtomography and in situ radiography
(2007)
Als Alternative zur Neutronentomographie wird das Potenzial der Computertomographie (CT) mit inkohärenter Röntgen-Streustrahlung (Compton-Streuung) untersucht. Die gleichzeitige Abbildung von Materialien sehr unterschiedlicher Dichten (Ordnungszahlen) ist eine wiederkehrende Herausforderung für die Radiologie und die Computertomographie mit Röntgenstrahlung. Die Messungen ergeben asymmetrische Projektionsprofile für Sinogramme der Streuintensität. Am Beispiel verschiedener Polymere (Polyethylen, Polyamid, PVC), Glas und Holz wird in den Tomogrammen ein hochaufgelöster 'Comptonkontrast' vergleichbarer Dynamik erreicht, während der simultan gemessene 'Absorptionskontrast' ausschließlich die starken Absorber (Glas und PVC) zeigt. Der Vergleich mit ähnlich auflösender Neutronentomographie zeigt ähnliche Kontraste und eröffnet mithin die Möglichkeit, diese künftig durch Compton-Tomographie im Labormaßstab zu ersetzen.
We present an experimental approach to study the three-dimensional microstructure of gas diffusion layer (GDL) materials under realistic compression conditions. A dedicated compression device was designed that allows for synchrotron-tomographic investigation of circular samples under well-defined compression conditions. The tomographic data provide the experimental basis for stochastic modeling of nonwoven GDL materials. A plain compression tool is used to study the fiber courses in the material at different compression stages. Transport relevant geometrical parameters, such as porosity, pore size, and tortuosity distributions, are exemplarily evaluated for a GDL sample in the uncompressed state and for a compression of 30 vol.%. To mimic the geometry of the flow-field, we employed a compression punch with an integrated channel-rib-profile. It turned out that the GDL material is homogeneously compressed under the ribs, however, much less compressed underneath the channel. GDL fibers extend far into the channel volume where they might interfere with the convective gas transport and the removal of liquid water from the cell.
Neutron tomography has been applied to investigate the mechanism of hydrogen assisted cracking in technical iron and supermartensitic steel. Rectangular technical iron block samples showed blistering due to intense hydrogen charging and the tomographic method revealed in situ the spatial distribution of hydrogen and cracks. Hydrogen accumulated in a small region around cracks and the cracks are filled with hydrogen gas. Cracks close to the surface contained no hydrogen. Hydrogenous tensile test samples of supermartensitic steel were pulled until rupture and showed hydrogen accumulations at the notch base and in the plastically deformed region around the fracture surface.
This paper gives a brief overview on3D imaging of magnetic domains with shearing grating neutron tomography. We investigated the three-dimensional distribution of magnetic domain walls in the bulk of a wedge-shaped FeSi single crystal. The width of the magnetic domains wasanalyzed at different locations within the crystal. Magnetic domains close to the tip of the wedge are much smaller than in the bulk. Furthermore, the three-dimensional shape of individual domains wasinvestigated. We discuss prospects and limitations of the applied measurement technique.
Influence of artificial aging of gas diffusion layers on the water management of PEM fuel cells
(2014)
The influence of artificial aging of gas diffusion layers (GDL) on the water management within the GDL was investigated in-operando by synchrotron X-ray radiography. One GDL was subjected to an accelerated aging procedure in 30% H2O2 solution, while another GDL was pristine. Radiographic measurements were combined with temporally resolved electrical analyzes. Significant differences in cell voltage and water accumulation were observed during cell operation at steady-state conditions. The cell which contained the aged GDL featured a higher water amount especially at the anode side and a lower cell voltage.
Neutron Bragg-edge imaging was applied for the visualization of a γ-Austenite to α'-martensite phase transformation. In the present study, a super martensitic
stainless steel sample was heated until complete austenitization and was subsequently cooled down to room temperature. The martensitic phase Transformation started at Ms = 190 °C. Using a monochromatic neutron beam with λ = 0.390 nm, the transmitted intensity was significantly reduced during cooling below Ms, since the emerging martensitic phase has a higher attenuation coefficient than the austenitic phase at this wavelength. The phase Transformation process was visualized by filming the transmission images from a scintillator screen with a CCD camera with a temporal resolution of 30 s and a spatial
resolution of 100 µm.
In this investigation, synchrotron X-ray imaging was used to investigate the water distribution inside newly developed gas diffusion media in polymer electrolyte membrane fuel cells. In-situ radiography was used to reveal the relationship between the structure of the microporous layer (MPL) and the water flow in a newly developed MPL equipped with randomly arranged holes. A strong influence of these holes on the overall water transport was found. This contribution provides a brief overview to some of our recent activities on this research field.
An in-depth understanding of the degradation mechanisms is a prerequisite for developing the nextgeneration all solid-state lithium metal battery (ASSLMB) technology. Herein, synchrotron X-ray computed tomography (SXCT) together with other probing tools and simulation method were employed to rediscover the decaying mechanisms of LiNi0.8Co0.1Mn0.1O2 (NCM)|Li6PS5Cl (LPSCl)|Li ASSLMB. It reveals that the detachment and isolation of NCM particles cause the current focusing on the remaining active regions of cathode. The extent of Li stripping and the likelihood of Li+ plating into LPSCl facing the active NCM particles becomes higher. Besides, the homogeneity of Li stripping/plating is improved by homogenizing the electrochemical reactions at the cathode side by LiZr2(PO4)3 (LZP) coating. These results suggest a codependent failure mechanism between cathode and anode that is mediated by uneven Li ion flux. This work contributes to establish a holistic understanding of the degradation mechanisms in ASSLMBs and opens new opportunities for their further optimization and evelopment.