We report polyethylene glycol (PEG)-grafting antifouling surfaces using a plasma copolymerized (PcP) technique to monitor protease activity in complex media. By varying the mixing ratio of the PEG and ethylenediamine (EDA) precursors, the PcP-PEG-EDA (PcP-PE) film was able to easily control surface amine density with good preservation of the internal PEG structure. We found that nonspecific protein adsorption was dramatically reduced in serum-containing media on the PcP-PE films, as opposed to that on plasma polymerized-EDA (PP-E) films without PEG. When SPR sensor chips coated with PcP-PE film were employed to detect protease activity, biotinylated luciferase probes (luciferase-peptide-biotin) on streptavidin-conjugated SPR chips enabled real-time and label-free measurement of matrix metalloproteinase activity in cell culture media. Owing to its excellent antifouling ability, this newly developed method boasts minimal nonspecific binding and can serve as a biochip platform to promote a wide range of applications in the biological field.
Due to the extremely high specific surface area of nanoparticles and corresponding potential for adsorption, the results of surface analysis can be highly dependent on the history of the particles, particularly regarding sample preparation and storage. The sample preparation method has, therefore, the potential to have a significant influence on the results. This report describes an interlaboratory comparison (ILC) with the aim of assessing which sample preparation methods for ToF-SIMS analysis of nanoparticles provided the most intra- and interlaboratory consistency and the least amount of sample contamination. The BAM reference material BAM-P110 (TiO2 nanoparticles with a mean Feret diameter of 19 nm) was used as a sample representing typical nanoparticles. A total of 11 participants returned ToF-SIMS data,in positive and (optionally) negative polarity, using sample preparation methods of “stick-and-go” as well as optionally “drop-dry” and “spin-coat.” The results showed that the largest sources of variation within the entire data set were caused by adventitious hydrocarbon contamination or insufficient sample coverage, with the spin-coating protocol applied in this ILC showing a tendency toward insufficient sample coverage; the sample preparation method or the participant had a lesser influence on results.