Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (143)
- Vortrag (51)
- Beitrag zu einem Tagungsband (30)
- Beitrag zu einem Sammelband (28)
- Posterpräsentation (13)
- Buchkapitel (10)
Schlagworte
- Femtosecond laser (28)
- Laser-induced periodic surface structures (LIPSS) (26)
- Femtosecond laser ablation (24)
- Laser ablation (23)
- Laser processing (14)
- Radiation protection (12)
- Silicon (11)
- Laser cleaning (10)
- Ablation (9)
- Materialbearbeitung (9)
Organisationseinheit der BAM
- 6 Materialchemie (56)
- 6.2 Material- und Oberflächentechnologien (56)
- 9 Komponentensicherheit (4)
- 9.5 Tribologie und Verschleißschutz (4)
- 6.7 Materialsynthese und Design (3)
- 4 Material und Umwelt (2)
- 4.1 Biologische Materialschädigung und Referenzorganismen (2)
- 6.1 Oberflächen- und Dünnschichtanalyse (2)
- 5 Werkstofftechnik (1)
- 5.1 Mikrostruktur Design und Degradation (1)
Paper des Monats
- ja (3)
The 125-fs laser ablation behaviour (800 nm) of aluminium and anodic oxide coatings on an AlMgSi1 alloy was investigated. The multi-pulse ablation threshold of aluminium at 1.2 J cm-2 was less than that of the oxides of 23 J cm-2. Aluminium exhibited a single pulse modification (melting) threshold of 0.3 J cm-2. These values derived from an evaluation of the crater geometry coincided with on-line acoustic measurements. The detected microphone voltage amplitude increased linearly with the laser fluence. The morphology of the ablation craters on aluminium indicated melt formation and displacement of a homogeneous melt phase due to the recoil action of the expanding metal vapour. The laser-processed ceramic oxide phases, on the other hand, showed a spongy resolidified melt layer, which denotes a collocated in-depth formation both of a melt and a gas phase. These phenomena are discussed in terms of the relative dominance of penetration depth of laser light and heat affected zones in the investigated materials with strongly varying optical and thermodynamical properties.
We investigated the initial modification and ablation of crystalline silicon with single and multiple Ti:sapphire laser pulses of 5 to 400 fs duration. In accordance with earlier established models, we found the phenomena amorphization, melting, re-crystallization, nucleated vaporization, and ablation to occur with increasing laser fluence down to the shortest pulse durations. We noticed new morphological features (bubbles) as well as familiar ones (ripples, columns). A nearly constant ablation threshold fluence on the order of 0.2 J/cm2 for all pulse durations and multiple-pulse irradiation was observed. For a duration of ,100 fs, significant incubation can be observed, whereas for 5 fs pulses, the ablation threshold does not depend on the pulse number within the experimental error. For micromachining of silicon, a pulse duration of less than 500 fs is not advantageous.
The ultrafast laser ablation of silicon has been investigated experimentally and theoretically. The theoretical description is based on molecular dynamics (MD) simulations combined with a microscopic electronic model. We determine the thresholds of melting and ablation for two different pulse durations =20 and 500 fs. Experiments have been performed using 100 Ti:Sap-phire laser pulses per spot in air environment. The ablation thresholds were determined for pulses with a duration of 25 and 400 fs, respectively. Good agreement is obtained between theory and experiment.
The multi-pulse ablation threshold of barium borosilicate glass was measured using 30-fs pulses of a high repetition rate (1 kHz) laser system. The threshold fluence was found to decrease with increasing beam radius ranging from 20 to 400 m. Two existing models are applied by considering thermal accumulation and point defects, respectively .
In this paper, safety-related experiments with ultra-short laser pulses (down to 30 fs) on various components
(goggles, curtains) for laser protection are presented. The damage and failure behaviour of
protective devices has been investigated dependent on practical conditions such as pulse duration, laser
.uence, pulse number, and repetition rate.
The e.ects of laser-irradiation on materials can be roughly divided into transient ones like laserinduced
transmission (LIT) or short-lived colour centres and permanent damages like the stable colour
centres and ablation. The former e.ects are particularly important for transparent devices like laser
goggles.
To obtain a complete overview on laser safety issues and the prevention of failure there are two
important .elds of investigation:
1. the e.ects of laser radiation on human eyes and skin, and
2. on the possible protection materials.
Both .elds have been addressed during the recently .nished German project SAFEST (safety aspects
in femtosecond technology). The amount of safety data available in the ultrashort pulse region has
been increased remarkably. This allows for a re-evaluation of known laser protection materials for this
region of pulse durations and for the evaluation of new designs that promise high protection levels
while being light-weight and convenient to use.
Curved substrates can be micro-structured by laser ablation, which is not possible with standard lithographic methods. The novel femtosecond-pulse laser technique allows the production of defined and reproducible micro-perforations of originally analyte-impermeable membranes. The trans-membrane analyte flux can be controlled both by the variation of the laser focus diameter resulting in different areas of single perforations, and the number of perforations in arrays on small membrane areas. This leads to a higher degree of variability as well as reproducibility of the diffusion qualities of sensor membranes, and marks the main innovation with this technique compared to the hand-made mechanical perforation by specially grinded needles used up to now. Touchless micro-perforation of small membrane areas with negligible heat damage of the structures adjacent to the perforation allows the application of analyte door membranes directly onto curved surfaces of miniaturized needle-sensors assigned for in vivo glucose monitoring, for the first time.
Laser cleaning of delicate biological composite materials such as ancient parchment manuscripts from the 15th and 16th century and printed paper from the 19th century is demonstrated with an ultraviolet excimer pulsed laser at 308 nm. Laser fluence levels must stay below the ablation and destruction threshold of the parchment or paper substrate, and have to surpass the threshold of the contaminant matter. Foreign layers to be removed must exhibit a higher optical density than the artifact substrates. Synthetic carbonaceous dirt modelled by water-soluble black crayons showed a characteristically weak featureless laser-induced plasma spectroscopy spectrum near the noise limit. It turned out that laser-induced plasma spectroscopy is of limited use in monitoring halting points (or etch-stops) because it relies on the destruction not only of the laterally inhomogenously distributed contaminant but also of pigment phases on a microscopically rough parchment substrate. Laser-induced fluorescence spectroscopy, however, promises to be a valuable non-destructive testing technique for etch-stop monitoring.
We report measurements of the optical breakdown threshold and ablation depth in dielectrics with different band gaps for laser pulse durations ranging from 5 ps to 5 fs at a carrier wavelength of 780 nm. For tau <100 fs, the dominant channel for free electron generation is found to be either impact or multiphoton ionization (MPI) depending on the size of the band gap. The observed MPI rates are substantially lower than those predicted by the Keldysh theory. We demonstrate that sub-10-fs laser pulses open up the way to reversible nonperturbative nonlinear optics (at intensities greater than 1014 W/cm2 slightly below damage threshold) and to nanometer-precision laser ablation (slightly above threshold) in dielectric materials.
Ablation experiments employing Ti:sapphire laser pulses with durations from 30 to 340 fs (centre wavelength 800 nm, repetition rate 1 kHz) were performed in air. Absorbing filters (Schott BG18 and BG36) served as targets. The direct focusing technique was used under single- and multi-pulse irradiation conditions. Ablation threshold fluences were determined from a semi-logarithmic plot of the ablation crater diameter versus laser fluence. The threshold fluence decreases for a shorter pulse duration and an increasing number of pulses. The multi-pulse ablation threshold fluences are similar to those of undoped glass material (~1 J cm-2). That means that the multi-pulse ablation threshold is independent on the doping level of the filters. For more than 100 pulses per spot and all pulse durations applied, the threshold fluence is practically constant. This leads to technically relevant ablation threshold values.