Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (119)
- Beitrag zu einem Tagungsband (6)
- Buchkapitel (1)
Referierte Publikation
- ja (126) (entfernen)
Schlagworte
- Femtosecond laser ablation (19)
- Laser-induced periodic surface structures (LIPSS) (18)
- Femtosecond laser (15)
- Laser ablation (15)
- Silicon (8)
- Radiation protection (7)
- Laser cleaning (6)
- Laser processing (6)
- Titanium (6)
- High-speed optical techniques (5)
Organisationseinheit der BAM
- 6 Materialchemie (26)
- 6.2 Material- und Oberflächentechnologien (26)
- 6.7 Materialsynthese und Design (3)
- 9 Komponentensicherheit (3)
- 9.5 Tribologie und Verschleißschutz (3)
- 4 Material und Umwelt (2)
- 4.1 Biologische Materialschädigung und Referenzorganismen (2)
- 5 Werkstofftechnik (1)
- 5.1 Mikrostruktur Design und Degradation (1)
- 6.1 Oberflächen- und Dünnschichtanalyse (1)
Paper des Monats
- ja (2)
We investigated the initial modification and ablation of crystalline silicon with single and multiple Ti:sapphire laser pulses of 5 to 400 fs duration. In accordance with earlier established models, we found the phenomena amorphization, melting, re-crystallization, nucleated vaporization, and ablation to occur with increasing laser fluence down to the shortest pulse durations. We noticed new morphological features (bubbles) as well as familiar ones (ripples, columns). A nearly constant ablation threshold fluence on the order of 0.2 J/cm2 for all pulse durations and multiple-pulse irradiation was observed. For a duration of ,100 fs, significant incubation can be observed, whereas for 5 fs pulses, the ablation threshold does not depend on the pulse number within the experimental error. For micromachining of silicon, a pulse duration of less than 500 fs is not advantageous.
Multiple pulse investigations of 130-fs Ti:sapphire laser-induced damage of a high reflecting mirror consisting of alternating ?/4-layers of Ta2O5 and SiO2 and a single 500-nm Ta2O5 film were performed. In both cases, fused silica served as the substrate. For a fixed number of 1000 laser pulses per spot, a decrease in the damage threshold fluence of the mirror by a factor of two was observed by changing the repetition rate from 10 Hz to 1 kHz. A single 500-nm Ta2O5 film shows higher damage resistance compared to the mirror. The mirror and the Ta2O5 film samples were partially coated with a 300-nm-thick aluminium layer. The aluminium coating does not influence the damage threshold of the dielectrics underneath.
The irradiation of single-crystalline indium phosphide (c-InP) by Ti:sapphire femtosecond laser pulses (130 fs, 800 nm) in air is studied by means of in-situ time resolved reflectivity measurements [fs-time-resolved microscopy (100 fs-10 ns) and point probing analysis (ns - µs)] and by complementary ex-situ surface analytical methods (Micro Raman Spectroscopy, Scanning Force, and Optical Microscopy). The dynamics of melting, ablation, and optical breakdown as well as structural changes resulting from rapid solidification are investigated in detail. Different laser-induced surface morphologies are characterized and discussed on the basis of recent ablation and optical breakdown models.
Ablation experiments with ultrashort laser pulses (pulse duration 150 fs, wavelength 800 nm) on polymers (PC, PMMA) relevant for biomedical technology have been performed in air. The lateral and vertical machining precision was evaluated by optical, atomic force and scanning electron microscopy. The ablation threshold reaches values in the range of 0.52.5 J/cm2 and depends significantly on the number of laser pulses applied to the same spot. The hole diameters are influenced by the laser fluence and the number of laser pulses. The relation between the ablation threshold and the number of laser pulses applied to the same spot is described in accordance with an incubation model.
Single-pulse femtosecond laser-induced forward transfer (LIFT, 30 fs, 790 nm) is used to deposit micron-sized dots of copper and/or indium onto a molybdenum layer on glass. Such systems can serve as precursors for the bottom-up manufacturing of micro-concentrator solar cells based on copper-indium-gallium-diselenide. The influence of the thickness of the copper, indium and combined copper-indium donor layers on the quality of the transferred dots was qualified by scanning electron microscopy, energy-dispersive X-ray analysis, and optical microscopy. The potential for manufacturing of a spatial arrangement adapted to the geometry of micro-lens arrays needed for micro-concentrator solar cells is demonstrated.
Ultrafast laser processing can be used to realize various morphological surface transformations, ranging from direct contour shaping to large-area-surface functionalization via the generation of “self-ordered” micro- and nanostructures as well as their hierarchical hybrids. Irradiation with high-intensity laser pulses excites materials into extreme conditions, which then return to equilibrium through these unique surface transformations. In combination with suitable top-down or bottom-up manufacturing strategies, such laser-tailored surface morphologies open up new avenues toward the control of optical, chemical, and mechanical surface properties, featuring various technical applications especially in the fields of photovoltaics, tribology, and medicine. This article reviews recent efforts in the fundamental understanding of the formation of laser-induced surface micro- and nanostructures and discusses some of their emerging capabilities.