Surface Properties and Porosity of Silica Particles Studied by Wide-Angle Soft X-ray Scattering
(2020)
Wide-angle soft X-ray scattering on free silica particles of different porosity prepared in a beam is reported. The explored q region is mostly dominated by features due to surface roughness and bulk porosity. A comprehensive experimental and theoretical analysis of silica particles of different porosity is presented for various incident photon energies. A correlation analysis, based on the theory of Porod, is used to test the validity of exact Mie theory in different pore density limits. The ability of the discrete dipole scattering model (DDSCAT) to resolve local effects, caused by various pore distributions, is discussed. Characteristic differences between the soft X-ray scattering patterns of the particle samples of different surface properties and porosity are detected. For all mentioned cases, it was confirmed that the effective radius concept of the Guinier model can be successfully extended to Mie theory and DDSCAT in describing the additive contributions of the primary particles, including a thin inhomogeneous solvent-rich surface shell and empty bulk pores. Close agreement, within ±15%, between the calculated and observed pore sizes and porosity values is reached. The influence of pores is alternatively described either in terms of secondary Mie scattering, which is modulated by the local internal electrical field within the particles, or by an independent Mie scattering process induced by the incident field on isolated pores. It is found that for the typical pore/particle size ratios the latter approach presents the best choice.
Wood products are often treated by different techniques to improve their longevity when used as building materials. Most of the time, the goal is to increase their resistance to weathering effects, deformations in material dimensions or biotic decomposition. These wood treatment techniques have a significant impact on pyrolysis and burning behavior. The general effects of three different common wood treatments on flame retardancy were investigated by comparing treated woods with their untreated counterparts and with other kinds of wood. While the acetylation of beech leads to a slightly increased fire hazard, the thermal treatment of wood and crosslinking of cellulose microfibrils dimethyloldihydroxy-ethyleneurea show a limited flame retarding effect. Switching to woods with a higher lignin content, and thus higher char yield, however, results in a more pronounced improvement in flame retardancy performance. This article delivers a comprehensive and balanced assessment of the general impact of different wood modifications on the fire behavior. Further, it is a valuable benchmark for assessing the flame retardancy effect of other wood modifications.
Scientific publications addressing the durability of the flame retardance of cables during their long-term application are rare and our understanding lacks. Three commercial flame retardants, aluminum hydroxide, aluminum diethyl phosphinate (AlPi-Et), and intumescent flame retardant based on ammonium polyphosphate, applied in ethylene-vinyl acetate copolymer (EVA) model cables, are investigated. Different artificial aging scenarios were applied: accelerated weathering (UV-irradiation/temperature/rain phases), humidity exposure (elevated temperature/humidity), and salt spray exposure. The deterioration of cables’ surface and flame retardancy were monitored through imaging, color measurements, attenuated total reflectance Fourier transform infrared spectroscopy, and cone calorimeter investigations. Significant degradation of the materials’ surface occurred. The flame retardant EVA cables are most sensitive to humidity exposure; the cable with AlPi-Et is the most sensitive to the artificial aging scenarios. Nevertheless, substantial flame retardance persisted after being subjected for 2000 h, which indicates that the equivalent influence of natural exposure is limited for several years, but less so for long-term use.
The durability of flame retardancy is a challenge for cables over long lifetimes. The degradation of flame retardance is investigated in two kinds of exposures, artificial weathering and humidity. In this basic study, typical mineral flame retardants in two polymers frequently used in cable jackets are investigated to get the fundamental picture. Aluminum hydroxide (ATH) and magnesium hydroxide (MDH) are compared in ethylene‐vinyl acetate (EVA), and further in EVA and linear low‐density polyethylene (LLDPE) cables containing the same ATH. The changes in chemical structure at the surface are studied through attenuated total reflectance Fourier transform infrared spectroscopy (ATR‐FTIR), the formation of cracks, and changes in color are investigated. The cone calorimeter and a bench scale fire testing cable module are utilized to evaluate the fire behavior of the cables. Although the flame retardancy deteriorated slightly, it survived harsh exposure conditions for 2000 h. Compared to EVA/MDH and LLDPE/ATH, the fire behavior of EVA/ATH is the least sensitive. Taken together, all of the results converge to estimate that there will be no problem with flame retardancy performance, for materials subjected to natural exposure for several years; the durability of fire retardancy is questionable for longer periods, and thus requires further investigation.
Microplastic particles are currently detected in almost all environmental compartments. The results of detection vary widely, as a multitude of very different methods are used with very different requirements for analytical validity.
In this work four thermoanalytical methods are compared and their advantages and limitations are discussed. One of them is thermal extraction-desorption gas chromatography mass spectrometry (TED-GC/MS), an analysis method for microplastic detection that has become established in recent years. In addition, thermogravimetric analysis coupled with Fourier-transform infrared spectroscopy (TGA-FTIR) and mass spectrometry (TGA-MS) were applied, two methods that are less common in this field but are still used in other research areas. Finally, microscale combustion calorimeter (MCC) was applied, a method not yet used for microplastic detection.
The presented results are taken from a recently published interlaboratory comparison test by Becker et al. (2020). Here a reference material consisting of suspended matter and specified added polymer masses was examined, and only the results of the recoveries were presented. In the present paper, however, the results for the individual polymers are discussed in detail and individual perspectives for all instruments are shown.
It was found that TED-GC/MS is the most suitable method for samples with unknown matrix and unknown, variable kinds and contents of microplastic. TGA-FTIR is a robust method for samples with known matrix and with defined kinds of microplastic. TGA-MS may offer a solution for the detection of PVC particles in the future. MCC can be used as a very fast and simple screening method for the identification of a potential microplastic load of standard polymers in unknown samples.