Lanthanides doped coordination polymers (CPs) with different binding motifs were synthesized to investigate the influence of the different fluorine positions in the structure on the decay time τ of the excited states. Fluorine can be integrated into the network mechanochemically via a fluorinated organic linker, here barium tetrafluoroterephthalate Ba(p-BDC-F4)2 or directly via a metal-fluorine bond (barium terephthalate fluoride BaF(p-BDC)0.5). The CP with a metal-fluorine bond shows the highest lifetime of the excited states of lanthanides (Eu3+, Tb3+ or Eu3+& Tb3+). The excitation of the lanthanides can be performed directly via the excitation wavelength typical for lanthanides and via the excitation wavelength of the linker. This enabled the simultaneous excitation of Eu3+ and Tb3+ in one CP. In the emission spectra (λem = 393 nm) of the mixed doped CPs (Eu3+ and Tb3+) the bands of both lanthanides can be observed. The integration into the crystal lattice and the homogeneous distribution of the lanthanides in the CPs is shown by X-ray diffraction, TEM, STEM-EDS measurements and the long decay times.
The fluorolytic sol–gel synthesis is applied with the intention to obtain two different types of core–shell nanoparticles, namely, SrF2–CaF2 and CaF2–SrF2. In two separate fluorination steps for core and shell formation, the corresponding metal lactates are reacted with anhydrous HF in ethylene glycol. Scanning transmission electron microscopy (STEM) and dynamic light scattering (DLS) confirm the formation of particles with mean dimensions between 6.4 and 11.5 nm. The overall chemical composition of the particles during the different reaction steps is monitored by quantitative Al Kα excitation X-ray photoelectron spectroscopy (XPS). Here, the formation of stoichiometric metal fluorides (MF2) is confirmed, both for the core and the final core–shell particles. Furthermore, an in-depth analysis by synchrotron radiation XPS (SR-XPS) with tunable excitation energy is performed to confirm the core–Shell character of the nanoparticles. Additionally, Ca2p/Sr3d XPS intensity ratio in-Depth profiles are simulated using the software Simulation of Electron Spectra for Surface Analysis (SESSA). In principle, core–shell like particle morphologies are formed but without a sharp interface between calcium and strontium containing phases.
Surprisingly, the in-depth chemical distribution of the two types of nanoparticles is equal within the error of the experiment. Both comprise a SrF2-rich core domain and CaF2-rich shell domain with an intermixing zone between them. Consequently, the internal morphology of the final nanoparticles seems to be independent from the synthesis chronology.