Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (52)
- Vortrag (2)
- Sonstiges (1)
- Posterpräsentation (1)
Sprache
- Englisch (51)
- Deutsch (4)
- Mehrsprachig (1)
Schlagworte
- Mechanochemistry (5)
- Nanoparticles (5)
- XRD (5)
- Catalysis (3)
- Alkaline earth metal coordination polymers (2)
- Aluminium (2)
- Brown-rot fungi (2)
- Coordination polymers (2)
- Doped systems (2)
- Fluorides (2)
Organisationseinheit der BAM
- 6 Materialchemie (10)
- 6.3 Strukturanalytik (9)
- 4 Material und Umwelt (4)
- 4.1 Biologische Materialschädigung und Referenzorganismen (4)
- 8 Zerstörungsfreie Prüfung (2)
- 8.1 Sensorik, mess- und prüftechnische Verfahren (2)
- 1 Analytische Chemie; Referenzmaterialien (1)
- 1.9 Chemische und optische Sensorik (1)
- 4.3 Schadstofftransfer und Umwelttechnologien (1)
- 5 Werkstofftechnik (1)
Eingeladener Vortrag
- nein (2)
Lanthanides doped coordination polymers (CPs) with different binding motifs were synthesized to investigate the influence of the different fluorine positions in the structure on the decay time τ of the excited states. Fluorine can be integrated into the network mechanochemically via a fluorinated organic linker, here barium tetrafluoroterephthalate Ba(p-BDC-F4)2 or directly via a metal-fluorine bond (barium terephthalate fluoride BaF(p-BDC)0.5). The CP with a metal-fluorine bond shows the highest lifetime of the excited states of lanthanides (Eu3+, Tb3+ or Eu3+& Tb3+). The excitation of the lanthanides can be performed directly via the excitation wavelength typical for lanthanides and via the excitation wavelength of the linker. This enabled the simultaneous excitation of Eu3+ and Tb3+ in one CP. In the emission spectra (λem = 393 nm) of the mixed doped CPs (Eu3+ and Tb3+) the bands of both lanthanides can be observed. The integration into the crystal lattice and the homogeneous distribution of the lanthanides in the CPs is shown by X-ray diffraction, TEM, STEM-EDS measurements and the long decay times.
As the most electronegative element, fluorine has a strong influence on material properties such as absorption behaviour or chemical and thermal stability. Fluorine can be easily integrated into coordination polymers (CPs) via a fluorinated acetate, here trifluoroacetate in Ba(CF3COO)2, or directly via a metal fluorine bond (BaF(CH3COO)). In the present study both possibilities of fluorine integration were tested and their effect on structure and properties of barium coordination polymers was investigated in comparison with the non-fluorinated barium acetate (Ba(CH3COO)2). In addition to the study of their thermal behaviour and their decomposition temperature, the CPs structures were tested for their application as possible anode materials in lithium ion batteries and for their sorption of water and ammonia. The properties of the CPs can be traced back to the individual structural motifs and could thus trigger new design ideas for CPs in LIBs and/or catalysis.
Improved Durability of Wood Treated with Nano Metal Fluorides against Brown-Rot and White-Rot Fungi
(2022)
Low-water soluble metal fluorides such as magnesium fluoride (MgF2) and calcium Fluoride (CaF2) were evaluated for decay protection of wood. Initially, the biocidal efficacy of nano metal fluorides (NMFs) against wood destroying fungi was assessed with an in-vitro agar test. The results from the test showed that agar medium containing MgF2 and CaF2 was more efficient in preventing fungal decay than stand-alone MgF2 or CaF2. These metal fluorides, in their nanoscopic form synthesized using fluorolytic sol-gel synthesis, were introduced into the sapwood of Scots pine and beech wood and then subjected to accelerated ageing by leaching (EN 84). MAS 19F NMR and X-ray micro CT images showed that metal fluorides were present in treated wood, unleached and leached. Decay resistance of Scots pine and beech wood treated with NMFs was tested against Wood destroying fungi Rhodonia placenta and Trametes versicolor in accordance with EN 113. Results revealed that mass losses were reduced to below 3% in wood treated with the combination of MgF2 and CaF2.
It is concluded that NMFs provide full protection to wood even after it has been leached and can be used as wood preservatives in outdoor environments.
Rare-earth based luminescent materials are key functional components for the rational design of light-conversion smart devices. Stable Eu3+-doped strontium fluoride (SrF2) nanoparticles were prepared at room temperature in ethylene glycol. Their luminescence depends on the Eu content and changes after heat treatment. The crystallinity of heat-treated material increases in comparison with as-synthesized samples. Particles were investigated in solution using X-ray diffraction, small-angle X-ray scattering, and X-ray spectroscopy. After heat treatment, the size of the disordered nanoparticles increases together with a change of their local structure. Interstitial fluoride ions can be localized near Eu3+ ions. Therefore, non-radiative relaxation from other mechanisms is decreased. Knowledge about the cation distribution is key information for understanding the luminescence properties of any material.
Powder x-ray diffraction (XRD) defined -Al2O3 has been investigated by x-ray photoelectron spectroscopy (XPS) and x-ray excited Auger electron spectroscopy (XAES). The Au 4f7/2 orbital is used for static charge referencing. This feature originates from well-defined and chemically inert 20 nm highly dispersed gold particles deposited on the sample surface. The particles, with a narrow particle size distribution, were obtained from a highly purified colloidal solution (sodium concentration below 1 mg/l). This procedure allows a determination of gold-referenced XPS and XAES data sets. ©2001 American Vacuum Society.
Solgel prepared ternary FeF3–MgF2 materials have become promising heterogeneous catalysts due to their porosity and surface Lewis/Brønsted acidity (bi-acidity). Despite the good catalytic performance, nanoscopic characterisations of this type of material are still missing and the key factors controlling the surface properties have not yet been identified, impeding both a better understanding and further development of ternary fluoride catalysts. In this study, we characterised the interaction between the bi-acidic component (FeF3) and the matrix (MgF2) on the nano-scale. For the first time, the formation pathway of FeF3–MgF2 was profiled and the template effect of MgF2 during the synthesis process was discovered. Based on these new insights two novel materials, FeF3–CaF2 and FeF3–SrF2, were established, revealing that with decreasing the atomic numbers (from Sr to Mg), the ternary fluorides exhibited increasing surface acidity and surface area but decreasing pore size. These systematic changes gave rise to a panel of catalysts with tuneable surface and bulk properties either by changing the matrix alkaline earth metal fluoride or by adjusting their ratios to Fe or both. The template effect of the alkaline earth metal fluoride matrix was identified as the most probable key factor determining the surface properties and further influencing the catalytic performance in ternary fluoride based catalysts, and paves the way to targeted design of next-generation catalysts with tunable properties.
Detection of suspended nanoparticles with near-ambient pressure x-ray photoelectron spectroscopy
(2017)
Two systems of suspended nanoparticles have been studied with near-ambient pressure x-ray photoelectron spectroscopy: silver nanoparticles in water and strontium fluoride—calcium fluoride core-shell nanoparticles in ethylene glycol. The corresponding dry samples were measured under ultra high vacuum for comparison. The results obtained under near-ambient pressure were overall comparable to those obtained under ultra high vacuum, although measuring silver nanoparticles in water requires a high pass energy and a long acquisition time. A shift towards higher binding energies was found for the silver nanoparticles in aqueous Suspension compared to the corresponding dry sample, which can be assigned to a change of surface potential at the water-nanoparticle interface. The shell-thickness of the core-shell nanoparticles was estimated based on simulated spectra from the National Institute of Standards and Technology database for simulation of electron spectra for surface analysis. With the instrumental set-up presented in this paper, nanoparticle suspensions in a suitable Container can be directly inserted into the analysis chamber and measured without prior sample preparation.
The dismutation of CHClF2 to CHF3 and CHCl3 was used to probe the effect of γ-Al2O3 fluorination on fluorine-against-chlorine (Cl/F) exchange reactions. X-ray photoelectron spectroscopy (XPS), X-ray excited Auger electron spectroscopy (XAES) and X-ray absorption near edge structure (XANES) spectroscopy were employed to probe the modifications at the surface of γ-Al2O3 accompanying the initial stages of fluorination. The results suggest that fluorine uptake by γ-Al2O3 starts initially at the surface of the oxide particles, with the formation of a fluorine species that is characterised by a single bond and a high effective charge q. Catalytic Cl/F-exchange is only observed after accumulation of higher fluorine concentrations, for which insertion of fluorine into the sub-surface region of the oxide crystallites has commenced. Quantitative XPS shows that the fluorination level must exceed approximately 10 atom% of the anions to achieve catalytic activity. The spectroscopic evidence suggests that the formation of aluminium oxofluorides is sufficient to provide catalytic activity. The presence of an AlF3 phase is not a condition for the observation of catalytic activity, even though defect-rich AlF3 is ultimately the endpoint of the fluorination process and is itself a Cl/F exchange catalyst.
Cr3+-doped MgF2 systems are synthesised by a novel non-aqueous soft chemistry route using different Cr precursors and varying Cr loading. These systems have been characterized by X-ray powder diffraction (XRD), BET surface area, TPD of ammonia, FT-IR pyridine adsorption analysis and X-ray photoelectron spectroscopy, and tested for their catalytic activity in dismutation of CCl2F2 and CF3CHClF. Catalysts synthesised starting from CrO3 or (CH3CO2)7Cr3(OH)2 showed better catalytic activity than those prepared with CrCl3. FT-IR pyridine adsorption studies reveal that the catalytic activity is highly correlated with the Lewis acid strength. In TPD of NH3 catalysts prepared from CrO3 and (CH3CO2)7Cr3(OH)2, precursors showed a similar behaviour, different from that of catalysts prepared from CrCl3.