CT (computed tomography) reconstructions of fuel cell components of a yet unrivaled spatial resolution and quality are presented. This is achieved by application of the novel DIRECTT (Direct Iterative Reconstruction of Computed Tomography Trajectories) algorithm. We focus on two different key issues which essentially rule the fuel cell's durability on different length scales and physical interactions. On the resolution scale of some 100 µm agglomerations of condensed water in flow-field channels are detected by means of quasi-in situ neutron CT (after operation). Five orders of magnitude below nanometer sized Ru catalyst particles on carbon black support are visualized by electron tomography. Both types of experiments are especially adapted to the type of material involved but they are accompanied by severe deviations from ideal CT measuring conditions, as well. In order to overcome the tremendous reconstruction artifacts of standard algorithms, we employ DIRECTT which is described in detail. Comparisons of DIRECTT reconstructions to the conventional filtered back projection, prove the significant improvements in both experimental methods.
Hydrogen interaction with metals is well known to have severe detrimental effects on their mechanical properties. The use of modern high-strength steels, which are attractive to improve fuel economy by reducing weight as well as candidates for H storage cylinders and other components, is currently being severely limited by the fact that the presence of H can cause embrittlement of the material. In addition to steel, several other metals and alloys used in the nuclear industry, like Ti and Zr, are susceptible to H degradation through hydride formation and subsequent cracking.
Microstructure-specific H mapping has been recognized as the most important challenge on the pathway towards a better understanding of the nature of H embrittlement in metallic alloys as well as the development of H storage solutions based on metal hydrides. Unfortunately, the characterization of H interactions with metals is an extremely challenging task and neutron-based techniques are of exceptional importance in this matter because – contrary to X-rays and electrons – thermal and cold neutrons interact strongly with the H nuclei, while the neutron beam is only weakly attenuated by the relevant metallic materials. Therefore, hydrogen distributions can be measured and quantified even in 3D by tomographic methods.
Here we present several neutron imaging investigations of embrittlement and cracking in Fe and Zr based metal alloys and optimization studies of hydrogen storage systems containing metal hydrides as an active substance. The advantages and the limitations of the experimental methods as well as the attempts for hydrogen quantification will be discussed in detail.
This work describes the effects of catalyst layers (CLs) consisting of hydrophobic PTFE on the performance and water management of PEM fuel cells. Catalyst inks with various PTFE contents were coated on Nafion membranes and characterized using contact angle measurements, SEX-EDX, and mercury porosimetry. Fuel cell tests and electrochemical impedance spectroscopy (EIS) were conducted under varying operating conditions for the prepared materials. At dry conditions, CLs with 5 wt.% PTFE were advantageous for cell performance due to improved membrane hydration, whereas under humid conditions and high air flow rates CLs with 10 wt.% PTFE improved the performance in high current density region. Higher PTFE contents (⩾20 wt.%) increased the mass transport resistance due to reduced porosity of the CLs structure. Operando neutron radiography was utilized to study the effects of hydrophobicity gradients within CLs and cathode microporous layer (MPLC) on liquid water distribution. More hydrophobic CLs increased the water content in adjacent layers and improved performance, especially at dry conditions. MPLC with higher PTFE contents increased the overall liquid water within the CLs and GDLs and escalated the water transfer to the anode side. Furthermore, the role of back-diffusion transport mechanism on water distribution was identified for the investigated cells.
While laser powder-bed fusion has overcome some of the design constraints of conventional manufacturing methods, it requires careful selection of process parameters and scan strategies to obtain favorable properties. Here we show that even simple scan strategies, complex ones being inevitable when printing intricate designs, can inadvertently produce local alterations of the microstructure and preferential grain orientation over small areas – which easily remain unnoticed across the macroscale. We describe how a combined usage of neutron imaging and electron backscatter diffraction can reveal these localized variations and explain their origin within cm-sized parts. We explain the observed contrast variations by linking the neutron images to simulated data, pole figures and EBSD, providing an invaluable reference for future studies and showing that presumably minor changes of the scan strategy can have detrimental effects on the mechanical properties. In-situ tensile tests reveal that fracture occurs in a region that was re-melted during the building process.
Die Computer-gestützte Laminografie (CL) wurde als komplementäre Methode zur Computertomografie für die dreidimensionale Bildgebung von lateral ausgedehnten Objekten entwickelt. Ursprünglich für medizinische Zwecke verwendet, wurde diese Methode kürzlich als zerstörungsfreie nicht-invasive Methode nicht nur in der Materialforschung, sondern auch mit steigendem Interesse für kunsthandwerkliche und historische Objekte eingesetzt. Hier wird die Computer-gestützten Laminografie mit polychromatischer Neutronenstrahlung an einer historischen Tsuba eingesetzt, einem Stichblatt eines japanischen Schwerts. Eine Analyse der Lötstellen gibt Rückschlüsse auf das Herstellungsverfahren. Zudem wurden unterschiedliche Materialsysteme gefunden, vermutlich um dem Tsuba lokal eine höhere Stabilität zu verleihen. Die Messungen wurden an der Imaging-Beamline CONRAD-2 an der Neutronenquelle BER 2 des Helmholtz-Zentrums Berlins (HZB) durchgeführt.
Neutron tomography was applied to study the 3D water distribution in full polymer electrolyte membrane fuel cell (PEMFC) stacks. The water distribution after switch-off of the fuel cell was analyzed over a period of 36 h. We found a slowly increasing water amount in the fuel cell, but only few changes within a time period of 5 h, which is about the time necessary for neutron tomography. In this way, the requirement for successful tomography was obtained. It is demonstrated how the quasi in-situ tomography technique enables us to study the water content in individual flow field channels of three-fold stacks. Flow field as well as stack design issues are addressed by this visualization method showing weak points due to a non-uniform water distribution that can be identified by means of neutron imaging.
While X-ray based darkfield imaging with grating interferometers is already widely used, darkfield imaging with neutrons has still a relatively small user community focused mostly on magnetic materials. Here, we demonstrate the application of neutron darkfield imaging byTalbot-Lau type grating interferometry to fiber reinforced plastics. Common carbon and glass fiber composites have been investigated including characteristic damage structures. The darkfield images show a strong signal response caused by fiber delamination, suitable fiber direction, particles, pores and cracks. The basic principles of neutron darkfield imaging applied to fiber composites are highlighted.