Solid-state phase transformations and the evolution of thermal and elastic strains in novel low temperature transformation (LTT) weld filler materials in the near surface region are monitored in real time by means of an innovative experimental set-up at the PDIFF (powder diffraction) beamline at the synchrotron light source ANKA (Angströmquelle Karlsruhe) at the KIT (Karlsruhe Institute for Technology). The key components of the diffraction set-up are two fast microstrip line detectors, which enables the strain evolution to be followed as a function of time and temperature for a 0.5?s counting time. During controlled heating and cooling cycles, as well as during near welding cycles, the martensite–austenite–martensite phase transitions are analysed. The transformation kinetics are monitored during resistance heating of small chips of the pure LTT alloys and during gas tungsten arc welding of simplified LTT welds using a specially designed welding rig for in-situ studies on the diffraction instruments. Under the mechanically unconstrained condition allowing free thermal expansion and shrinkage, the LTT alloys are found to exhibit decreasing transformation temperatures Ac and MS and increasing phase fraction of retained austenite for increasing Ni content. The strain evolution during welding reveals increased compressive stresses upon welding, which is attributed to the martensite formation upon cooling, which counteracts the thermal contraction strains. Comparison of the transformation temperatures reveals higher values than in the pure LTT alloys, but no variation between the different alloys. On the one hand, this is attributed to preferred grain orientation affecting the diffraction measurements and the determination of the transformation temperatures. On the other hand, it is possible that with the different chemical compositions of the LTT alloys and the mechanical constraints during welding, the evolution of the residual strain and stress may vary and result in counteracting affects with respect to lowered martensite start temperatures.
As an approach towards more rough industrial laser welding applications, the Nd:YAG laser welding process has been coupled to the plasma powder welding process for the first time. Process stabilities have been achieved by such hybrid welding which are even better than those known from previous coupling of the laser process with gas metal arc welding (GMAW), for instance.
The present contribution focuses on the technology and potentials of the novel laser hybrid welding technique and addresses the realisation and the perspectives for practical applications. The experimental results demonstrate that the new process coupling enables welding of austenitic stainless steels in the thickness range between 3 mm and 8 mm at various weld geometries and joint configurations and at welding speeds exceeding 2 m/min. In addition it has been proven that the laser plasma powder arc welding (LPPAW) technique can also be applied to out-of-position conditions. Continuous advancement of the welding equipment ensures a high gap bridging ability and levelling of misalignment due to higher powder feeding rates. The recent development of a new plasma powder torch even provides a higher efficiency of powder feeding and guarantees smoth weld surfaces. Up to the present, the investigations demonstrated that the novel laser plasma powder hybrid welding technique offers all perspectives for application in pipe fabrication, ship building and offshore as well as transportation industry.
Modifying the level of mostly detrimental welding residual stresses already during the welding process would be highly attractive as time- and cost-consuming post processing may be prevented. The nature of stress buildup during welding-associated cooling is highly affected by phase transformations. Up to now, it is not clear in which way this is applicable to real component welding exhibiting high shrinkage restraint and complex heat input. In this study, two different low transformation temperature (LTT) alloys have been investigated concerning the stress development in restrained multi-run butt welding in order to evaluate the potential of stress reduction. Pulsed gas metal arc welding (P-GMAW) welding was executed on a testing facility designed to simulate real lifelike restraint conditions of component weldments. The effect of reducedMS-temperatures and the heat control on the globally acting stresses was monitored by in-situ measurement of the reaction forces during welding fabrication. Additional local residual stress measurements allowed analyzing global as well as local loading of the welded construction. Although phase transformation has a significant influence on unloading the joint during each weld pass, the reaction stress upon cooling to room temperature seems to be determined mainly by the heat input. On the surface, low longitudinal residual stresses were observed in case of LTT whereas transverse residual stresses are less affected.
For a newly developed 10% Cr and 10% Ni low transformation temperature (LTT) weld filler material, the local phase transformation kinetics and the strain evolution during gas tungsten arc welding (GTAW) under real welding conditions was studied. An experimental set-up and a measuring and evaluation strategy are presented to gain a real time insight into the welding process. The experiments were carried out at the beam line ID15@ESRF using a two detector EDXRD (energy dispersive X-ray diffraction) set-up and high energy synchrotron X-rays. The time-resolved diffraction analysis during welding was carried out locally throughout the weld in longitudinal as well as in transverse direction to the weld line to examine the interdependence of the strain state and the transformation kinetics. This comprehension is crucial for the optimization of the weld process, and thus for the tailoring of the resulting residual stress states, which is one of the main issues for the application of LTT alloys. Using the herein proposed approach EDXRD diffraction pattern can be monitored during real welding with a counting rate of 5 Hz. By means of the time resolved diffraction data the local transformation temperatures and times were determined and the local phasespecific strain evolutions are discussed with respect to the transformation rates and the time-delayed phase transformations.
Low Transformation Temperature (LTT) alloys are high alloyed filler materials, which exhibit a martensitic phase transformation at comparatively low temperatures in order to prevent high tensile residual stresses. A number of publications have already shown that even compressive residual stresses can be observed when using LTT filler materials. Up to know it is not clear in which way this it applicable to multi-run welding exhibiting high shrinkage restraint and complex heat input. In this study the potential for stress reduction during welding of LTT alloys was studied by numerical simulation. This allows for evaluation of the stress development in every single weid run. Additionally, the impact of the structural stiffness was incorporated by modelling a special sample geometry exhibiting a high intensity of restraint. The results show that the stress formation in weid longitudinal direction is determined by the phase transformation as high compressive residual stresses were found here independent from the weid run. On the other hand the transformation induced stresses in weid transverse direction are superimposed by tensile stresses originated from shrinkage restraint. With increasing number of runs the tensile residual stress level is raised. The results were confirmed by residual stress measurements using diffraction methods.
When assessing the performance of welded components residual stresses are vital. The possibilities of transferring the real boundary conditions of welding, which influence the residual stress, into the laboratory are highlighted in this contribution. The potentials of a test system specially developed for this purpose are demonstrated. The component design induces global process-, geometry- and material-dependent stresses, which can be simulated and quantified in the system. In addition, the resulting local residual stress distribution can be exactly determined with high spatial resolution with the aid of X-ray diffraction. Examples are presented of how the conditions to be found during production are simulated in the laboratory.
Residual stresses are crucial when assessing the performance of welded components. The present work deals with the possibilities of transferring the real-life boundary conditions of welding, which influence the residual stress, into the laboratory. The possibilities of a test system with a load capacity of 2 MN specifically developed for online monitoring of stress formation and cracking are shown. Due to the structural design, global process, geometry and material-dependent stresses are induced, which can be quantified in-situ during welding and post weld heat treatment. Examples are presented how the conditions to be found during production are simulated in the laboratory. It is shown how welding residual stresses in high-strength steels are affected by the heat control. Elevated working temperatures significantly increase the tensile residual stresses in the heat affected zone (HAZ). The effect of mechanical stresses resulting from welding on stress relief cracking is demonstrated by the example of a creep resistant steel. Reheat cracks were monitored online during post weld heat treatment.
Residual stresses are crucial when assessing the performance of welded components. The present work deals with the possibilities of transferring the real-life boundary conditions of welding, which influence the residual stress, into the laboratory. The possibilities of a test system with a load capacity of 2 MN specifically developed for online monitoring of stress formation and cracking are shown. Due to the structural design, global process, geometry and material-dependent stresses are induced, which can be quantified in-situ during welding and post weld heat treatment. Examples are presented how the conditions to be found during production are simulated in the laboratory. It is shown how welding residual stresses in high-strength steels are affected by the heat control. Elevated working temperatures significantly increase the tensile residual stresses in the heat affected zone (HAZ). The effect of mechanical stresses resulting from welding on stress relief cracking is demonstrated by the example of a creep resistant steel. Reheat cracks were monitored online during post weld heat treatment.