Solid-state phase transformations and the evolution of thermal and elastic strains in novel low temperature transformation (LTT) weld filler materials in the near surface region are monitored in real time by means of an innovative experimental set-up at the PDIFF (powder diffraction) beamline at the synchrotron light source ANKA (Angströmquelle Karlsruhe) at the KIT (Karlsruhe Institute for Technology). The key components of the diffraction set-up are two fast microstrip line detectors, which enables the strain evolution to be followed as a function of time and temperature for a 0.5?s counting time. During controlled heating and cooling cycles, as well as during near welding cycles, the martensite–austenite–martensite phase transitions are analysed. The transformation kinetics are monitored during resistance heating of small chips of the pure LTT alloys and during gas tungsten arc welding of simplified LTT welds using a specially designed welding rig for in-situ studies on the diffraction instruments. Under the mechanically unconstrained condition allowing free thermal expansion and shrinkage, the LTT alloys are found to exhibit decreasing transformation temperatures Ac and MS and increasing phase fraction of retained austenite for increasing Ni content. The strain evolution during welding reveals increased compressive stresses upon welding, which is attributed to the martensite formation upon cooling, which counteracts the thermal contraction strains. Comparison of the transformation temperatures reveals higher values than in the pure LTT alloys, but no variation between the different alloys. On the one hand, this is attributed to preferred grain orientation affecting the diffraction measurements and the determination of the transformation temperatures. On the other hand, it is possible that with the different chemical compositions of the LTT alloys and the mechanical constraints during welding, the evolution of the residual strain and stress may vary and result in counteracting affects with respect to lowered martensite start temperatures.
Various test methods are available for assessing the susceptibility of materials to solidification cracking during welding. In the widely used Varestraint test, the crack length is selected as a criterion as a function of the applied bending strain.
Unfortunately, the crack length does not characterize the material behavior alone but depends to varying degrees on the individual test parameters used, which makes the interpretation of the results difficult. In addition, the crack length is not comparable under different test conditions. To overcome these disadvantages, we have developed a novel evaluation methodology that decouples the machine influence from the material behavior. The measured crack length is related to the maximum possible value specified by welding speed and deformation time. This relative crack length is calculated numerically, considering the orientation of the cracks. Experiments on two high-alloy martensitic welding consumables show that, in contrast to the conventional evaluation, a comparison of different welding parameters becomes possible. Furthermore, the strain rate proved to be a suitable crack criterion in agreement with Prokhorov's hot cracking model.
Controlling the level of mostly detrimental residual stresses already during the welding process would be highly attractive as time and cost consuming post processing may be prevented. Innovative Low Transformation Temperature (LTT-) filler materials are specially designed for Controlling weld residual stresses by means of adjusted martensite formation already during welding. Numerous publications can be found on this issue, but they provide only little insight into the interaction between martensite formation and resulting welding residual stresses. Within this study a component weld test was performed in a special large-scale testing facility. In-situ load analysis revealed that the amount of stress reduction during deposition of the individual weld runs is dependent on the weld volume undergoing phase transformation related to the shrinking volume. The residual stresses found alter welding show that the desired residual stress control by using LTT alloys is sensitive to welding boundary conditions (i. e. weld geometry, plate thickness) and to be evaluated separately for varying weld scenarios.
For a newly developed 10% Cr and 10% Ni low transformation temperature (LTT) weld filler material, the local phase transformation kinetics and the strain evolution during gas tungsten arc welding (GTAW) under real welding conditions was studied. An experimental set-up and a measuring and evaluation strategy are presented to gain a real time insight into the welding process. The experiments were carried out at the beam line ID15@ESRF using a two detector EDXRD (energy dispersive X-ray diffraction) set-up and high energy synchrotron X-rays. The time-resolved diffraction analysis during welding was carried out locally throughout the weld in longitudinal as well as in transverse direction to the weld line to examine the interdependence of the strain state and the transformation kinetics. This comprehension is crucial for the optimization of the weld process, and thus for the tailoring of the resulting residual stress states, which is one of the main issues for the application of LTT alloys. Using the herein proposed approach EDXRD diffraction pattern can be monitored during real welding with a counting rate of 5 Hz. By means of the time resolved diffraction data the local transformation temperatures and times were determined and the local phasespecific strain evolutions are discussed with respect to the transformation rates and the time-delayed phase transformations.
Beside quenched and tempered (QT) high strength steels advanced technologies in steel manufacturing provide steels produced by the thermo-mechanical controlled process (TMCP) with yield strength of 960 MPa. These steels differ in the carbon and micro-alloying element content. With variation of heat control TIG-welded dummy seams on both steel types were performed. Analyses concerning microstructure and residual stress evolution due to welding showed typical stress distributions according to common concepts. Yet, the TMCP-steel shows higher residual stresses than the QT-steel.
Today high-strength structural steels (yield strength ≥ 960 MPa) are increasingly applied. Therefore, weldments have to achieve equal strength. Yet, high residual stresses in those welds diminish the components safety. Especially high restraint intensities can lead to crack-critical stress-levels. A special 2-MN-test facility allowed online-measurements of global reaction forces under defined restraint conditions during welding and cooling of multilayer-component MAG-welds. Local residual stresses were measured via X-ray diffraction before and after relief of the restraint. Local and global stresses were highly affected by heat control.
Modifying the level of mostly detrimental welding residual stresses already during the welding process would be highly attractive as time- and cost-consuming post processing may be prevented. The nature of stress buildup during welding-associated cooling is highly affected by phase transformations. Up to now, it is not clear in which way this is applicable to real component welding exhibiting high shrinkage restraint and complex heat input. In this study, two different low transformation temperature (LTT) alloys have been investigated concerning the stress development in restrained multi-run butt welding in order to evaluate the potential of stress reduction. Pulsed gas metal arc welding (P-GMAW) welding was executed on a testing facility designed to simulate real lifelike restraint conditions of component weldments. The effect of reducedMS-temperatures and the heat control on the globally acting stresses was monitored by in-situ measurement of the reaction forces during welding fabrication. Additional local residual stress measurements allowed analyzing global as well as local loading of the welded construction. Although phase transformation has a significant influence on unloading the joint during each weld pass, the reaction stress upon cooling to room temperature seems to be determined mainly by the heat input. On the surface, low longitudinal residual stresses were observed in case of LTT whereas transverse residual stresses are less affected.
Today’s efforts for lightweight design result in a growing application of high-strength structural steels from 960 MPa. In welded structures of these steels increased demands regarding component safety and a high elastic ratio should be considered. Hence, the prevention of an evolution of high weld-induced tensile residual stresses is required. Recent studies showed that component related restraint conditions of welds are able to elevate welding induced stresses to critical values, depending on material characteristics, the welding process and parameters. This work involves multi-axial welding loads as a consequence of the superposition of local residual stresses, global reaction stresses and moments, varying the welding parameters under different restraint conditions. The global welding loads are measured via GMA-weld tests in a special testing facility and via a DIC(Digital Image Correlation)-system in a slot weld. Local transverse residual stresses were analysed by means of X-ray diffraction. The application of a less amount of weld runs due to a modified welding parameters and welds seam configurations revealed as a beneficial approach to reduce welding loads in high-strength steels.